Versalis Clearflex Fg 106 A Film Grade Lldpe

Versalis Clearflex® FG 106 A Film Grade LLDPE

    • Product Name: Versalis Clearflex® FG 106 A Film Grade LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 724181
    Productname Versalis Clearflex® FG 106 A Film Grade LLDPE
    Polymertype Linear Low Density Polyethylene (LLDPE)
    Comonomer Butene-1
    Density 0.918 g/cm³
    Meltflowrate 0.8 g/10 min (190°C/2.16 kg)
    Meltingpoint 120 °C
    Vicatsofteningpoint 93 °C
    Tensilestrengthatbreak 25 MPa
    Elongationatbreak 700%
    Tensilemodulus 200 MPa
    Dartdropimpact 180 g
    Elmendorftearresistancemd 80 g
    Elmendorftearresistancetd 300 g
    Haze 12%
    Gloss45 50

    As an accredited Versalis Clearflex® FG 106 A Film Grade LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Versalis Clearflex® FG 106 A Film Grade LLDPE is packaged in 25 kg polyethylene bags, palletized, typically 1,000 kg per pallet.
    Container Loading (20′ FCL) 20′ FCL: approximately 18 MT palletized or 22 MT loose in 25 kg bags, subject to packaging and shipping regulations.
    Shipping Versalis Clearflex® FG 106 A Film Grade LLDPE is a non-hazardous, solid polyethylene resin shipped as pellets. Standard packaging includes 25 kg bags, 1000 kg octabins, or bulk containers, palletized and wrapped. Not regulated for transport. Store dry, away from heat and sunlight.
    Storage Store Versalis Clearflex® FG 106 A in a cool, dry, well-ventilated area in original, sealed packaging. Protect from direct sunlight, heat, moisture, and contamination. Keep away from ignition sources and strong oxidizing agents. Store at ambient temperature, away from incompatible materials. Use safe stacking practices and prevent pellet spills, which can create slipping hazards. Maintain clean, segregated storage and follow local regulations.
    Shelf Life Shelf life is 24 months from production when stored in sealed original packaging, dry, cool, and protected from direct sunlight.
    Application of Versalis Clearflex® FG 106 A Film Grade LLDPE

    On a high-throughput cast line producing 23 µm machine stretch film, the 90 mm single-screw extruder is typically operated with a 30:1 L/D barrier screw and a die gap of 0.5–0.8 mm. Versalis Clearflex® FG 106 A is introduced as the core layer or as the total resin in monolayer constructions because the film-grade linearity retains the puncture resistance required by ASTM D5748-19 while avoiding the melt uniformity problems caused by lower-viscosity plastomer over-use. The cast process feeds pellets without pre-drying at ambient RH below 60%; above that threshold, surface moisture on regrind produces edge gassing and splay marks in the film, especially when edge trim is reintroduced at ratios above 15–20%.

    For pallet-unitization grades, the formulation is usually 90–95% FG 106 A, 5–10% LDPE with melt index 0.3–0.5 g/10 min (ISO 1133-1:2022, 190°C/2.16 kg), and 0.5–2.0% of a polyisobutylene tackifier masterbatch for cling stability. The tackifier is metered by a gravimetric side feeder; free-flow preblending of PIB and LLDPE pellets at ambient temperatures below 15°C causes uneven tackifier distribution and cling dead zones. The extruder barrel profile from feed throat to die is set at 200°C, 220°C, 240°C, 250°C and 255°C to balance shear heating against melt temperature overshoot, while the chill roll is maintained at 20–25°C and the vacuum box is held at 98–102% of local atmospheric pressure to control neck-in and edge bead. The air gap between die and chill roll is kept below 5 cm; longer air gaps increase transverse thickness variation beyond ±5%.

    Compliance for this segment is primarily REACH Regulation (EC) No 1907/2006, with Article 33 declarations required only if SVHC content exceeds 0.1% by weight. Because the film is not intended for direct food contact, (EU) No 10/2011 does not govern the construction, but converter quality agreements often request a statement that no phthalates or bisphenol A are intentionally added. Under U.S. shipment, OSHA Hazard Communication Standard 29 CFR 1910.1200 applies, and the film is not classified as hazardous under GHS. Terminal product is a 23 µm cast stretch film wound in 500 mm wide rolls, pre-stretched to 250–300% on semi-automatic pallet wrappers, or a 12–17 µm pre-stretched roll for high-speed automatic machines. Critical-to-quality checks include ASTM D5458-19 cling force, ASTM D5748-19 puncture propagation and ASTM D882-18 tensile elongation in the machine direction. Lot-to-lot variation in comonomer distribution can shift cling force by 5–10% at a fixed tackifier level, requiring adjustment of the PIB masterbatch feed rate within 0.25% increments.

    Blown Film Extrusion of Heavy-Duty Shipping Sacks and the Melt-Fracture Boundary

    For 40–60 kg sacks used in petrochemical resin packaging, FG 106 A is processed on a 65 mm grooved-feed single-screw extruder with 24:1 L/D and a spiral mandrel die of 250 mm diameter. The die gap is set at 1.2–1.8 mm; the deeper gap is selected when the blow-up ratio exceeds 2.0:1 to maintain gauge uniformity. Frost line height is fixed between 650 mm and 750 mm on a 12 m tower, because raising it further cools the bubble too slowly and degrades bubble symmetry, while lowering it below 500 mm increases film crystallinity at the expense of dart impact. At output rates above 140 kg/h, sharkskin melt fracture appears at the die exit when the wall shear stress exceeds 0.14 MPa; this is typical for film-grade LLDPE with the molecular architecture of FG 106 A and can be suppressed by using a die gap above 1.5 mm or by blending 10–15% LDPE. The LDPE reduces the extensional viscosity mismatch and permits a stable bubble at melt temperatures between 195°C and 210°C. Operating below 190°C worsens sharkskin, while above 220°C reduces melt strength and causes bubble sag.

    Heavy-duty sack formulations commonly use 80–88% FG 106 A, 10–15% high-pressure LDPE and 2–5% carbon black masterbatch with 45% pigment loading. The carbon black is necessary for UV protection during outdoor storage but acts as a nucleating agent; its presence raises film haze and lowers dart impact by 8–12% when compared with unpigmented film. Compensating this loss requires decreasing the frost line height and increasing the die gap, not simply raising the LDPE fraction, because excessive LDPE above 20% reduces machine-direction tear strength measured by ASTM D1922-15.

    Regulatory compliance follows EU Regulation (EC) No 1907/2006 for industrial packaging and EU Packaging and Packaging Waste Directive 94/62/EC for heavy metal content, specifically the sum of lead, cadmium, mercury and hexavalent chromium below 100 mg/kg per package component. Carbon black masterbatches are certified for PAH content under REACH Annex XVII entry 50 if the sack contacts skin during handling, with benzo[a]pyrene below 1 mg/kg and total specified PAHs below 10 mg/kg. The finished sack film is typically 120–160 µm thick with a layflat width of 500–700 mm, fabricated by bottom-seal bag lines with ultrasonic or impulse sealing. Before conversion, the film is conditioned at 23°C and 50% relative humidity for 24 h to stabilize seal strength. Critical acceptance tests include ASTM D1709-16a dart impact, ASTM D1922-15 tear resistance and ISO 527-3:2018 tensile properties. A production-scale failure observed on lines with 90 mm extruders is bubble instability caused by overfeeding; it presents as ±8% thickness variation on the collapsed film and is corrected by reducing screw speed rather than increasing air pressure.

    What Weathering Additives Actually Protect a 150 µm Three-Season Greenhouse Film?

    Accelerated weathering on a 150 µm three-season greenhouse cover requires the base resin to contain a hindered amine light stabilizer package of at least 1,500 ppm active HALS, combined with 1,000 ppm UVA absorber of the benzophenone or benzotriazole class. FG 106 A is used at 70–80% by weight in a blown-film blend with 15–20% EVA and 5–10% LDPE to improve long-term tear resistance and filler retention. The EVA is necessary to permit adequate dispersion of anti-fog additives, but its lower melting point narrows the extruder temperature profile to 185–205°C from feed to adapter.

    The film is produced on a 75 mm grooved-feed extruder with a die diameter of 350 mm and a die gap of 2.2 mm. The bubble is operated with a BUR of 2.2:1 and a frost line height of 800 mm, while the tower is enclosed to prevent side-draft induced gauge banding. Output on this configuration is limited to 120–150 kg/h by the melt temperature ceiling; pushing beyond 210°C triggers gel formation from HALS decomposition and creates visible particles that shorten service life by promoting localized film failure under hail load. The relevant performance validation is ASTM G155-13 cycle 1 or EN 13206:2017 for covering films, with tensile elongation after 10,000 h simulated weathering required above 400% in the machine direction.

    No direct food-contact compliance applies, but the film is subject to REACH Annex XVII restrictions on cadmium-based pigments and to EU Directive 2011/65/EU RoHS for lead, mercury and cadmium limits if the greenhouse film contains recycled colorants. The terminal product is a 12 m layflat width, 150 µm thick greenhouse cover with anti-fog and thermic properties. The anti-fog coating is applied by a gravure roll inline after bubble collapse and before edge slitting; it must deliver a water contact angle below 40° after 60 days of exposure. Biaxial orientation is not used in this product class because greenhouse covers require balanced MD and TD tear resistance; the blown process with 2.2:1 BUR provides this balance within 10% between MD and TD Elmendorf values.

    The compliance matrix below is used to classify commercial inquiries by destination market before an application-specific datasheet is issued. The matrix is applicable only after converter-side verification; it is not a product-specific certification unless stated in the official Versalis datasheet.

    Market / end useRegulatory referenceParameterTest standard
    EU direct food contact(EU) No 10/2011Overall migration ≤ 10 mg/dm²EN 1186-1
    US direct food contact21 CFR 177.1520Olefin polymer specification, paragraph (c) item 2.1 / 2.2FDA GMP 21 CFR 174.5
    REACH SVHCREACH Article 33SVHC ≤ 0.1% w/w per articleGC-MS / LC-MS
    RoHS electrical surface protectionDirective 2011/65/EUPb, Hg, Cd, Cr6+ ≤ 100 ppm per homogeneous materialIEC 62321
    Packaging heavy metals94/62/ECSum Pb, Hg, Cd, Cr6+ ≤ 100 mg/kgICP-OES
    EU specific migration heavy metals(EU) No 10/2011 Annex IISML per elementICP-MS

    Multi-lane collation shrink systems require a film with free shrink above 50% in the cross-direction at 130°C when measured by ISO 14616:2019. FG 106 A is blended at 60–75% with 15–25% EVA and 10–15% LDPE for collation shrink. The extrusion process is a double-bubble line fitted with a 65 mm extruder and a 250 mm die; the primary bubble is run at a BUR of 1.6:1, quenched to 10°C, then reheated to 90–110°C and stretched 4.5–5.0:1 in the machine direction and 3.5–4.0:1 in the transverse direction. This biaxial orientation locks in the shrink energy and requires an annealing station set at 50–60°C to prevent premature shrinkage on the roll.

    Compliance is governed by FDA 21 CFR 177.1520 for olefin polymers when used as an indirect contact article; EVA content above 25% triggers additional compliance for ethylene-vinyl acetate copolymers under 21 CFR 177.1350. Terminal rolls are typically 70 µm thick and 300–600 mm wide, used for mineral water bottles, canned goods and glass jars in corrugated trays. The distinct failure to monitor on high-speed wrapping lines is edge-shrink blocking; it appears when the film is stored above 35°C in a warehouse and causes machine jams due to pre-shrunk edges. The solution is to specify a slip and antiblock package of 500–1,000 ppm erucamide and 2,000–4,000 ppm silica in the surface layers, while maintaining the core layer free of slip to preserve internal shrink force.

    When Sealant Web Design Requires Hot-Tack Consistency Above 110°C

    For retort pouches and high-speed vertical form-fill-seal pouches, the sealant web must provide hot-tack strength above 2 N/25 mm from 110°C to 140°C and a seal initiation temperature below 105°C according to ASTM F1921-18 and ASTM F88/F88M-21. FG 106 A is selected as the sealant layer at 75–85% by weight, blended with 10–15% LDPE and 5–10% of a polyolefin plastomer with a melt index of 3.5–5.0 g/10 min (ISO 1133-1:2022). The plastomer shortens seal initiation time but lowers web modulus; above 10% addition the laminated film develops wrinkle defects in downstream slitting, requiring an additional 2–3% HDPE to restore stiffness.

    The sealant web is produced either by a cast co-extrusion line with 35 µm skin layers and a 60 µm core, or by a blown-film line with a 2.0:1 blow-up ratio. For cast production, the die is a 1,500 mm coat-hanger manifold with automatic gauge control using a scanning thickness sensor; the average thickness deviation is controlled to ±2% of nominal. The chill roll temperature is set to 18–22°C, because lower temperatures increase film haze above 12%, while higher temperatures reduce hot-tack performance by annealing the surface too slowly. For blown production, the melt temperature must not exceed 205°C; above this temperature the plastomer phase migrates to the bubble surface and creates seal-contaminating waxy deposits.

    Food-contact compliance requires positive results from overall migration testing under EU Regulation (EU) No 10/2011, Annex III and Annex V, using simulant A for hydrophilic foods, simulant D1 for fatty foods and simulant E for dry foods depending on the final pouch application. Specific migration of selenium, barium, cobalt, lithium, manganese and zinc is confirmed by inductively coupled plasma mass spectrometry, and residual ethylene monomer must be below 1 mg/kg in the resin. For the U.S. market, the sealant web must comply with FDA 21 CFR 177.1520 paragraph (c) item 2.1 or 2.2 and be manufactured under GMP in 21 CFR 174.5. The converter issues a written declaration of compliance covering the specific blend ratio, because FG 106 A alone does not guarantee compliance of the compounded sealant. The terminal product is a 50–80 µm sealant film laminated to BOPP or PET, used for frozen food, dairy powder and snack packaging. Hot-tack is tested on the actual HFFS line by sealing at 120°C, 0.2 MPa and 0.5 s dwell; the seal must withstand a 1.5 N/25 mm opening force immediately after jaw release. A line-condition failure documented on vertical baggers is seal-wave formation when web thickness exceeds 80 µm; this is corrected by reducing seal bar temperature gradient from 5°C to 2°C across the bar length rather than by increasing dwell time.

    Surface Protection Film Co-extrusion on Cast Lines

    A three-layer cast line with a 90 mm core extruder and two 45 mm skin extruders feeds a feedblock multiplier die of 1,200 mm. FG 106 A forms the 60–70% core layer, while the adhesive skin is an ethylene-vinyl acetate copolymer with 18% VA content or a POE plastomer at 30–40% of total thickness. The release skin contains 1,000–2,000 ppm of erucamide and 3,000–5,000 ppm of synthetic silica antiblock. Adhesion to stainless steel is set between 0.2 N/25 mm and 2.0 N/25 mm according to ASTM D3330/D3330M-04(2023); values above 2.5 N/25 mm create tearing when the film is peeled from polished aluminum profiles.

    The cast line runs at 150–250 m/min with a die-to-chill-roll air gap of 3 cm and a chill roll surface temperature of 20–25°C. The co-extrusion feedblock is optimized for viscosity-matched layers; if the skin melt index differs by more than 2 g/10 min from the core, interfacial waviness appears as visible parabolic flow lines. The extruder profile is set at 180–240°C, and the die temperature is held 5–10°C above the core melt temperature to prevent die-lip freeze-off on the high-VA adhesive skin.

    In the European market, the film must comply with REACH Annex XVII restrictions on phthalates and with EU Directive 2011/65/EU RoHS for electrical surface protection where the film is used on appliance steel before powder coating. Heavy metal content for lead, mercury, cadmium and hexavalent chromium is limited to 100 ppm per homogeneous material, and the adhesive skin must not contain substances on the REACH Candidate List above the 0.1% w/w threshold. For U.S. industrial use, compliance is under 29 CFR 1910.1200, and the film is supplied with a safety data sheet that classifies it as non-hazardous. The finished protection film is slit to widths from 10 mm to 2,000 mm and applied in-line to aluminum profiles, stainless steel panels, vinyl windows and pre-painted metal sheets. The product must exhibit a wetting delay of less than 5 seconds when laminated to a 1.5 m wide sheet and must leave no adhesive residue after 6 months of outdoor exposure at 40°C. The main batch-to-batch failure to control is transfer of the release-skin slip additive to the adhesive layer during warehouse storage above 30°C, which reduces initial tack and causes film lift on curved edges.

    Free Quote

    Competitive Versalis Clearflex® FG 106 A Film Grade LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Versalis Clearflex® FG 106 A is a film-grade linear low-density polyethylene produced by Versalis S.p.A. The resin is a butene-comonomer LLDPE, referred to industrially as C4-LLDPE, produced with a Ziegler–Natta catalyst system. The grade is characterized by a nominal density of 0.918 g/cm³ when tested according to ISO 1183-1:2019 and a melt flow rate of 1.0 g/10 min at 190 °C/2.16 kg according to ISO 1133-1:2022. The “A” suffix denotes a standard film stabilization package composed of phenolic antioxidant and process stabilizer components; some distributor stocks include slip and antiblock additives for controlled coefficient of friction and blocking resistance. The product is supplied as pellets and does not require pre-drying under normal closed-loop indoor warehousing when relative humidity is maintained below 60 %.

    The melt flow rate of 1.0 g/10 min is lower than the 2.0 g/10 min value common in high-output cast and blown-film LLDPE grades. This lower MFR produces higher shear viscosity and higher extruder head pressure at equivalent screw speed. Processors should therefore anticipate higher torque, lower screw speed capability, and increased screen-pack differential pressure when comparing Clearflex® FG 106 A with a 2.0 g/10 min butene LLDPE on the same line.

    What determines the usable extrusion window for a 1.0 g/10 min C4-LLDPE in monolayer blown film?

    Stable bubble geometry for this grade is governed by the interaction of melt temperature, die pressure, draw-down ratio, and frost line position. On a single-screw extruder with a barrier screw of 24:1 to 30:1 L/D and a Maddock or dispersive mixing section, the melt temperature setpoint should be maintained between 190 °C and 220 °C. Die zones are typically set from 200 °C to 230 °C. A die gap of 1.2 mm to 2.0 mm reduces shear rate at the die lip and delays melt fracture. A blow-up ratio of 2.0:1 to 3.0:1 and a frost line height of 6 to 10 die diameters are practical starting points for monolayer film production.

    The lower MFR of 1.0 g/10 min improves bubble stability relative to 2.0 g/10 min LLDPE because the higher melt viscosity resists bubble sag and instability at lower frost line heights. However, the same viscosity elevates screw torque and melt pressure. Extruders with screw pressure capability below 35 MPa may require screw speed derating, particularly when fine screen packs are installed. Melt temperatures above 240 °C should be avoided because the stabilizer package is not designed for prolonged high-heat residence; thermal oxidation can generate gel particles, reduce dart impact, and increase visible film defects. Before shutdown or resin changeover, a high-MFR LDPE purge grade should be processed at 200 °C until the melt pressure stabilizes and the extruder discharge is clear.

    Residual moisture from outdoor storage or condensation can produce surface defects in film. If pellets are exposed to relative humidity above 60 % or to thermal cycling, they should be equilibrated in dry indoor air before hopper transfer. The base resin is not hygroscopic, but surface moisture on cold pellets can produce bubble instability and poor melt homogeneity.

    Common converting applications for Clearflex® FG 106 A include pallet stretch film, collation shrink film, heavy-duty sacks, industrial liners, carrier bags, and lamination web. In these applications, film thickness is typically drawn down to 25 µm to 80 µm on blown-film lines. The density of 0.918 g/cm³ provides a balance between tensile stiffness and low-temperature impact resistance. Tensile properties are commonly evaluated according to ASTM D882-18; film specimens are conditioned at 23 °C and 50 % relative humidity for a minimum of 40 h before testing. Dart impact is reported using ASTM D1709-22 Method A or ISO 7765-1:2004. Actual values depend on film gauge, die geometry, blow-up ratio, and frost line height; a single value from one line cannot be transferred directly to another line without confirmation.

    The values in Table 1 are drawn from distributor published data and are not to be construed as sales specifications. They represent a 50 µm monolayer blown film produced at a blow-up ratio of 3.0:1.

    PropertyTest methodTypical value
    Melt flow rate, 190 °C/2.16 kgISO 1133-1:20221.0 g/10 min
    DensityISO 1183-1:20190.918 g/cm³
    Tensile yield stress, MD/TDASTM D882-1811/10 MPa
    Tensile stress at break, MD/TDASTM D882-1845/38 MPa
    Elongation at break, MD/TDASTM D882-18700/850 %
    Dart drop impact F50ASTM D1709-22 Method A120 g
    Elmendorf tear, MD/TDASTM D1922-23160/210 g
    HazeASTM D1003-216–8 %
    Gloss 60°ASTM D2457-21100–110
    Coefficient of friction, film-to-filmASTM D1894-240.10–0.20

    Down-gauging from 80 µm to 40 µm does not produce a linear reduction in dart impact or tear resistance. Dart impact measured by ASTM D1709-22 is sensitive to frost line height, film thickness, die geometry, and ambient air temperature. Converters should generate a gauge variation curve on their own line when qualifying the grade for a thinner film. Slip and antiblock additives can migrate to the film surface and affect printability and lamination bond strength. Surface tension should be checked before printing or lamination using ASTM D2578-23; typical production targets are 38 mN/m to 42 mN/m after corona treatment.

    Mechanical, optical, and seal-response differentiation from LDPE and hexene-based LLDPE

    The differentiation of Clearflex® FG 106 A from high-pressure LDPE is primarily rheological and mechanical. LDPE of comparable melt index typically has lower tensile yield stress and lower dart impact, but long-chain branching gives LDPE higher melt strength at equivalent melt temperature. The higher melt strength of LDPE can simplify bubble stability at high draw-down ratios. In contrast, Clearflex® FG 106 A has a linear molecular architecture with short-chain branches from butene comonomer. At 0.918 g/cm³, tensile yield stress is higher than that of a typical LDPE of 0.922 g/cm³ measured under ASTM D882-18. The lower density also contributes to improved impact performance relative to a high-density film of 0.945 g/cm³ or above.

    Against hexene- or octene-based LLDPE, the C4 comonomer generally produces lower dart impact and lower puncture resistance at equivalent density and melt index. This is a known structure–property relationship in polyolefin science: longer comonomer branches create more effective tie molecules and a broader distribution of lamellar thickness, improving impact and tear resistance. C4-LLDPE can nonetheless provide adequate performance in medium-duty film applications when the converter prioritizes melt processing stability and a defined additive package. Against metallocene-catalyzed LLDPE, Clearflex® FG 106 A typically has a broader molecular weight distribution, which can reduce melt pressure at high shear but may lower optical clarity and dart impact. Published comparative data for Clearflex® FG 106 A specifically are limited; users should request a current technical data sheet and run a comparative trial under their own die geometry and output rate.

    Seal initiation temperature and hot-tack performance should be determined on the final film using ASTM F88/F88M-21 and ASTM F1921-20. The slip and antiblock additives can alter the seal strength envelope and the temperature at which a consistent seal is achieved. Seal data generated on resin pellets or on unmodified polyethylene without the final additive package cannot be transferred directly to the production film.

    Regulatory compliance is dependent on additive documentation, final article conditions, and storage discipline

    Compliance statements for polyolefin resins are specific to the manufacturer’s formulation. For European food-contact applications, the polymer base should meet the overall migration limit of 10 mg/dm² established by Commission Regulation (EU) No 10/2011 as amended; the compliance of the final article depends on the additives, inks, coatings, and lamination adhesives used downstream. For the United States, olefin polymers may be covered under FDA 21 CFR 177.1520 when the final film meets the applicable extractive restrictions. REACH obligations under Regulation (EC) No 1907/2006 require the downstream formulator to confirm that the grade does not contain substances of very high concern above 0.1 % w/w. RoHS compliance under Directive 2011/65/EU is usually limited to homogeneous material restrictions for lead, mercury, cadmium, hexavalent chromium, PBB, and PBDE; the polyolefin matrix itself is not expected to contain these metals, but pigment masterbatches or fillers must be assessed separately.

    Compliance areaReferenceRelevant condition
    EU plastic food-contact frameworkCommission Regulation (EU) No 10/2011Overall migration ≤ 10 mg/dm²; final article verification required
    US olefin polymerFDA 21 CFR 177.1520End-use conditions determine extractive compliance
    Chemical safetyREACH, Regulation (EC) No 1907/2006SVHC declaration ≤ 0.1 % w/w per safety data sheet
    RoHSDirective 2011/65/EUPb, Hg, Cd, Cr(VI), PBB, PBDE limits apply in homogeneous material

    Operational boundaries include avoidance of direct contact with strong oxidizing agents, aromatic solvents, and long-term ultraviolet exposure without a UV masterbatch. Polyethylene is not intended for continuous service above 80 °C in stressed applications; the exact thermal aging limit must be established by end-use testing because film shrink, antioxidant consumption, and creep are time–temperature dependent. If the pellets are stored in outdoor silos, dust and moisture contamination must be controlled. The use of this resin in structures requiring gas barrier is generally as a sealant or skin layer rather than as the barrier layer; EVOH, polyamide, or metallized substrates perform the barrier function. In coextruded structures, the melt viscosity mismatch with adjacent layers should be checked by comparing apparent viscosity at shear rates between 100 s⁻¹ and 1000 s⁻¹ in the die. A viscosity mismatch greater than 2:1 may cause interfacial instability or gauge variation. Published data for this specific configuration is limited.