| HS Code | 797206 |
| Density | 0.900 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 0.8 g/10 min |
| Melting Point | 115 °C |
| Vicat Softening Point | 75 °C |
| Tensile Strength At Break | 24 MPa |
| Elongation At Break | 600 % |
| Tensile Modulus | 100 MPa |
| Shore D Hardness | 40 |
| Dart Drop Impact | 250 g |
| Elmendorf Tear Strength | 100 g |
| Haze | 8 % |
| Gloss 45 | 75 % |
| Brittleness Temperature | -70 °C |
| Coefficient Of Friction | 0.8 |
As an accredited Versalis Clearflex® FF D0 Very Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Versalis Clearflex® FF D0 Very Low Density Polyethylene is supplied in 25 kg polyethylene bags, palletized and stretch-wrapped. |
| Container Loading (20′ FCL) | 20′ FCL container loading: Versalis Clearflex® FF D0 Very Low Density Polyethylene in palletized bags, securely stowed for ocean transport. |
| Shipping | Versalis Clearflex® FF D0 Very Low Density Polyethylene is typically shipped as non-hazardous solid pellets in 25 kg bags, big bags, or bulk trucks/containers. Keep dry, cool, and away from direct sunlight, heat, and ignition sources. No special dangerous-goods labeling is normally required. |
| Storage | Store in a cool, dry, well-ventilated area away from direct sunlight, heat, flames, and strong oxidizing agents. Keep original containers closed, clean, and undamaged; palletize and stack safely to prevent bag rupture. Avoid excessive temperatures and moisture. Use first-in, first-out stock rotation. Protect bags from punctures and crushing. Observe good housekeeping and local regulations; consult the SDS for detailed storage requirements. |
| Shelf Life | Shelf life is typically 12 months when stored unopened in original packaging, cool, dry, and away from direct sunlight. |
In cast pallet stretch wrap production, Clearflex FF D0 is incorporated into the core layer or cling layer at 15 wt% to 35 wt%, depending on the required balance between puncture resistance and unwind force. Five-layer cast film lines fitted with 65 mm to 75 mm single-screw extruders, L/D 30:1 to 33:1, barrier screws with compression ratios from 2.4:1 to 3.0:1, are used. Melt temperatures are held at 235°C to 250°C, with adapter and die temperatures set 5°C to 10°C above the melt to offset shear heating across the feedblock. Die gap settings of 0.5 mm to 0.8 mm are typical, and the primary chill roll is maintained at 18°C to 25°C to stabilise film crystallinity before the secondary cooling drum and thickness scanner. The very low density reduces zero-shear viscosity relative to conventional butene LLDPE, which can require 5% to 10% lower screw speed to avoid melt fracture. Pre-stretch ratios on turret winders are set between 250% and 350%, with film elongation at break measured by ISO 527-3, puncture resistance by ASTM D5748, dart drop by ISO 7765-1, and cling force by ASTM D5458. Terminal products are machine pallet wrap from 12 µm to 23 µm and hand stretch wrap from 15 µm to 25 µm. Industrial pallet wrap is not covered by EU food-contact legislation, but REACH registration and RoHS Directive 2011/65/EU Annex II restrictions on restricted substances apply when export documentation requires a Safety Data Sheet.
Density of the grade is reported below 0.910 g/cm³ per ISO 1183-1, and the melt flow rate is in the range 0.5 g/10 min to 1.5 g/10 min per ISO 1133-1 at 190°C/2.16 kg; the converter must verify lot-specific values against the certificate of analysis because seal initiation and cling performance track crystallinity shifts. Pre-drying is not required for polyethylene unless cold storage has produced surface condensation; hopper loading in an unheated warehouse under high relative humidity can introduce melt pressure fluctuations and film thickness variability. Avoid excessive levels of migratory slip additives in the cling layer during long roll storage because migration can depress cling force below the ASTM D5458 minimum specified by the pallet wrap purchaser.
Clearflex FF D0 is used as a sealant layer in coextruded blown film or cast laminates for flow-wrap packaging, lidding films, and pouches. The low crystalline content depresses the seal initiation temperature into a range that converters typically validate between 75°C and 95°C, depending on dwell time, jaw pressure, and film gauge. Seal strength is measured per ASTM F88/F88M, and hot-tack force is measured per ASTM F1921 using a 25.4 mm wide specimen, 0.5 s dwell, and 0.275 MPa jaw pressure. In a three-layer blown film structure, the sealant layer is commonly 10 µm to 20 µm thick and is coextruded with an HDPE or LLDPE core to maintain stiffness. Blow-up ratios of 2.2:1 to 3.0:1 and frost-line heights of 3 to 5 die diameters are used; melt temperatures are held at 190°C to 215°C to limit oxidation and gel counts. Addition of 10 wt% to 20 wt% linear low density polyethylene with a C8 comonomer may be required if the converter demands modulus above 150 MPa per ISO 527-3 in the sealant web.
The critical processing window is the seal initiation temperature relative to the outer layer softening point; a ±5°C drift in seal jaw temperature can cause either incomplete seal formation or heat distortion of the printed outer layer. For contamination-tolerant sealing through dry product dust, the sealant layer is often formulated with 10 wt% to 20 wt% of a higher-crystallinity plastomer to maintain seal through contamination measured by ASTM F1921. Thin VLDPE sealant layers may exhibit blocking on the roll; antiblock based on synthetic silica at 5,000 ppm to 15,000 ppm is commonly dispersed in the sealant layer, with coefficient of friction measured by ISO 8295.
Compliance for food contact in Europe is assessed under Commission Regulation (EU) No 10/2011 as amended, with overall migration limit of 10 mg/dm² for food simulants and specific migration limits for additives identified in the declaration of compliance. In the United States, the olefin polymer must meet FDA 21 CFR 177.1520(c) for polyethylene, and end-use limitations are specified in 21 CFR 176.170(c) when the multilayer structure is part of paper and paperboard. The converter must verify that the finished sealant layer is not placed in contact with fatty foods above 60°C unless specific migration testing demonstrates compliance.
| Reference | Requirement | Condition or test method |
|---|---|---|
| EU 10/2011 Annex I | Overall migration | 10 mg/dm² for food simulants |
| EU 10/2011 Annex II | Specific migration of additives | As in declaration of compliance |
| FDA 21 CFR 177.1520(c) | Olefin polymer for food contact | Density and melt index within specification |
| ASTM F1921 | Hot tack | 0.5 s dwell, 0.275 MPa jaw pressure, 25.4 mm specimen |
| ASTM F88/F88M | Seal strength | 15 mm width, 300 mm/min jaw speed |
For extrusion coating operations running paperboard and aluminium foil at line speeds above 150 m/min, Clearflex FF D0 is added at 10 wt% to 25 wt% to LDPE-based formulations to reduce neck-in and improve fibre tear adhesion to corona-treated substrates. Coating lines with 90 mm single-screw extruders, L/D 30:1, and 1,200 mm to 1,500 mm slot dies operate at melt temperatures from 285°C to 305°C. The air gap is maintained at 150 mm to 250 mm, and the chill roll is kept at 15°C to 20°C, with coat weight controlled at 12 g/m² to 25 g/m². The addition of FF D0 to LDPE reduces the onset of draw resonance at high line speeds but lowers melt strength; converters compensate by reducing the draw ratio to below 80:1 or by increasing the coating weight. Adhesion to paperboard is improved by melt oxidation in the air gap, and corona treatment of the substrate at 2.0 W/m²/min to 4.0 W/m²/min is used before the nip. Terminal products include liquid packaging board for milk and juice cartons, aseptic brick inner liners, and multiwall paper sacks for dry mixes. Food-contact compliance follows EU 10/2011 and FDA 21 CFR 176.170(c) for the paperboard component; when aluminium foil is included, migration testing with simulant D1 and E for aqueous and fatty foods is required. Exceeding 315°C melt temperature may initiate thermo-oxidative degradation, increasing gel count measured by ASTM D7310 and causing odour defects in finished cartons.
Agricultural bale wrap and silage cover film are produced on coextrusion blown film lines with die diameters from 350 mm to 500 mm and achievable outputs of 300 kg/h to 500 kg/h. Clearflex FF D0 is added to the outer or intermediate layer at 20 wt% to 40 wt%, replacing a portion of the LDPE or LLDPE to reduce low-temperature modulus increase. This is critical when the film must retain puncture resistance after conditioning at -20°C for 24 h per ASTM D5748. Blow-up ratios of 2.0:1 to 2.5:1 and frost-line heights of 5 to 7 die diameters are used, with a melt temperature of 185°C to 210°C and die gap of 1.4 mm to 2.0 mm to achieve final film thickness from 150 µm to 250 µm. Tear propagation resistance is monitored by ISO 6383-2, and elongation at break by ISO 527-3. The terminal products are silage bale stretch film and silage cover sheets. The film is subject to EN 14932 for thermoplastic stretch films for wrapping bales when specified in procurement contracts; UV stabilisation with HALS packages must be verified by ISO 4892-2 accelerated weathering. Outdoor exposure beyond the declared UV stabilisation level is an operational boundary and can cause embrittlement.
The substitution of LDPE by Clearflex FF D0 in silage film lowers the glass transition response of the amorphous phase, which maintains film ductility in freezing storage conditions. However, the reduction in crystallinity also lowers tensile modulus at room temperature, so the outer layer is usually coextruded with HDPE or a higher-density LLDPE to maintain roll handling stiffness. The converter must monitor frost-line height and bubble stability because the very low melt strength of the VLDPE-rich layer can lead to bubble sag if the frost line is set beyond 7 die diameters. When the film is intended for bale wrapping under high pre-stretch, the pre-stretch ratio is limited to 120% to 180% on some field wrappers, and retained stretch force is measured per EN 14932. Since silage film is not food-contact, EU 10/2011 is not applicable; EU REACH applies.
Post-consumer HDPE recyclate with a melt flow index of 0.3 g/10 min to 0.6 g/10 min per ISO 1133-1 and a notched Izod impact below 6 kJ/m² per ISO 180/A is dry-blended with 10 wt% to 25 wt% Clearflex FF D0 before extrusion. Compounding is performed on a corotating twin-screw extruder with a screw diameter of 40 mm to 75 mm and L/D 40:1 to 44:1, using distributive mixing elements and a temperature profile from 160°C at the feed throat to 200°C at the die. Degassing at 100 mbar to 200 mbar removes volatiles from the recyclate. The VLDPE domains are compatible with the HDPE matrix because both are polyethylene; at addition levels above 30 wt%, flexural modulus measured by ISO 178 declines below the level commonly required for rigid opaque packaging, and the grade becomes unsuitable for load-bearing crates. Published lot-specific data for this exact recycle stream is limited; therefore the converter must validate mechanical performance for each feedstock batch.
The pelletized compound is injection moulded on machines with clamp force of 1,500 kN to 5,000 kN, barrel temperatures of 180°C to 220°C, and mould temperatures of 10°C to 40°C. Terminal products include drainage pipe fittings, industrial pallets, and crates. REACH and RoHS Directive 2011/65/EU apply; if the recyclate contains legacy additives, the compounder must document compliance with the EU Waste Framework Directive. The addition of Clearflex FF D0 may increase melt flow index and affect wall thickness distribution in large mouldings; the injection moulder should re-qualify process parameters using pressure-volume-temperature data measured by ISO 22007-2 or equivalent in-mould instrumentation.
Medical device packaging uses Clearflex FF D0 in a coextruded sealant layer of 15 µm to 30 µm, coextruded with a polyester or polypropylene core, and sealed against uncoated Tyvek or rigid PETG trays. The seal initiation temperature is maintained below 100°C to avoid distortion of PETG trays at sealing stations. Seal dwell times of 0.5 s to 1.0 s and jaw pressure of 0.3 MPa to 0.5 MPa are used. Seal strength is measured per ASTM F88/F88M, and seal continuity after ethylene oxide or gamma sterilisation is verified per ISO 11607-1. The VLDPE sealant layer is not intended for high-abrasion surfaces; when package abrasion resistance is specified, a thicker outer layer of HDPE or PET is required. Compliance includes EU MDR 2017/745 for medical devices and FDA 21 CFR 177.1520(c) for olefin polymers. If gamma sterilised above 25 kGy, oxidation induction time measured by ISO 11357-6 should be monitored to avoid premature seal strength loss during shelf life.
Competitive Versalis Clearflex® FF D0 Very Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Within the Versalis Clearflex portfolio, Versalis Clearflex® FF D0 Very Low Density Polyethylene is a very low density ethylene copolymer intended for flexible film structures requiring low seal initiation and high optical uniformity. The grade is classified as a VLDPE because its density is below 0.910 g/cm³ when determined by ISO 1183-1; the nominal density is commonly cited as 0.900 g/cm³ on annealed specimens at 23°C. Melt mass-flow rate, measured at 190°C under 2.16 kg load according to ISO 1133-1, is typically reported in the range 0.8–1.2 g/10 min. The lower crystallinity associated with this density class reduces flexural modulus and melting onset relative to conventional butene-grade LLDPE.
| Property | Test method | Clearflex® FF D0 | Conventional butene-LLDPE film reference |
|---|---|---|---|
| Density | ISO 1183-1 | 0.900 g/cm³ nominal | 0.918–0.920 g/cm³ typical |
| Melt mass-flow rate | ISO 1133-1, 190°C/2.16 kg | 0.8–1.2 g/10 min lot-dependent | 0.5–1.0 g/10 min typical |
| Density class | ISO 1872-1 | VLDPE, below 0.910 g/cm³ | LLDPE, 0.910–0.925 g/cm³ |
| Seal initiation region | ASTM F88, flat-jaw configuration | lower than butene LLDPE; structure-dependent | higher seal initiation temperature |
In monolayer and coextruded film applications, the grade is used in collation shrink film, frozen food packaging, heavy-duty sacks, and sealant webs laminated to biaxially oriented polypropylene or polyester. The principal differentiation from conventional LLDPE is the combination of lower sealing temperature and higher dart impact retention at low temperature. However, the same low-crystallinity network lowers melt strength and narrows the upper sealing window. Compared with metallocene-catalysed polyolefin plastomers of similar density, FF D0 may exhibit higher modulus and lower extensional viscosity, but published comparative data for this specific grade is limited. Compared with EVA containing 18 wt% vinyl acetate, FF D0 eliminates acetic acid generation and downstream die-lip corrosion, but does not reproduce the extreme low-temperature hot-tack of high-VA sealants. Substitution must be validated using ASTM F1921 hot-tack and ASTM F88 seal-strength curves, not by density or melt index matching alone.
The comonomer insertion responsible for the 0.900 g/cm³ density reduces lamellar thickness and increases the concentration of tie chains in the semicrystalline network. This shifts seal initiation downward because less thermal energy is required to mobilize chain segments and develop interfacial adhesion. Laboratory seal curves generated at 0.3–0.5 N/mm² jaw pressure and 0.5–1.0 s dwell in a flat-jaw heat sealer show that FF D0 initiates seal strength below typical butene LLDPE. The hot-tack plateau broadens when measured by ASTM F1921, but the upper sealing temperature narrows because film distortion and seal thinning occur at lower temperatures than with conventional LLDPE.
In coextruded sealant layers below 10 µm, published data for this specific configuration is limited. The heat sink of a polyester or polyamide substate can shift the apparent seal initiation temperature upward and compress the usable sealing window. Pilot-line seal maps are therefore required for each final laminate gauge and jaw profile. A production-scale converter cannot transfer a monolayer seal curve directly to a coextruded web without overestimation of the lower seal limit.
On cast film lines equipped with 30:1 L/D single-screw extruders and chill roll stacks, the lower melt strength of FF D0 manifests as edge neck-in and draw resonance at high draw-off ratios. A fixed die lip gap of 0.5–0.8 mm and an air gap of 15–30 mm are class-typical starting conditions. Barrel temperatures are profiled from 170°C in the feed zone to 240–260°C at the die, with the die maintained 10–20°C above the rear zones to reduce melt fracture. Melt temperature should not exceed 280°C during extended campaigns because gel formation and odour increase in the absence of adequate purging. Downgauging below 12 µm requires edge pinning and possibly 5–15 wt% of a higher-melt-strength LDPE or LLDPE to suppress draw resonance. The addition of LDPE increases density and raises seal initiation temperature, so the blend ratio must be recorded as a controlled process variable.
The same low melt strength constrains high-stalk blown film processing. On a 150 mm die with a 0.8 mm die gap, a blow-up ratio of 2.0:1–3.0:1 and internal bubble cooling are class-typical starting conditions. Frost line height must be held within ±5 cm to limit variation in dart impact and MD tear resistance measured under ISO 7765-1 and ASTM D1922. Published data for this specific grade on this equipment configuration is limited; converted-film property retention varies with cooling air humidity, melt temperature history, and back-pressure stability.
Coextrusion with biaxially oriented polyamide or polyester requires FF D0 to be processed at the lower end of its thermal window to avoid substrate softening. The melt viscosity of the VLDPE at the relevant shear rate should be matched to the structural layer to suppress interfacial instability. Capillary rheometry according to ISO 11443 is used to compare viscosity curves rather than single-point melt index. When the structural layer requires die temperatures above 260°C, the FF D0 layer may experience local overheating; immersion-probe melt-temperature measurement is preferable to barrel set-point readings because the low-viscosity melt can show a larger spread between barrel and melt temperature under high shear.
Substitution of EVA with 18 wt% vinyl acetate must be confirmed by seal-strength and odour panels, since FF D0 has a narrower low-temperature sealing window than a high-VA EVA sealant. It does, however, remove acetic acid generation and enables continuous extrusion without the acid-catalysed degradation that can corrode die lips and create carbonaceous deposit. The trade-off is process-specific: in frozen food packaging requiring rapid sealing at low jaw temperature, high-VA EVA may retain an advantage, while in high-speed collation shrink film the cleaner extrusion and controlled coefficients of friction of FF D0 may reduce downtime.
Under European food-contact legislation, the finished film must comply with Regulation (EU) No 10/2011, including overall migration limits of 10 mg/dm² in standardized food simulants under the applicable time and temperature conditions. In the United States, the base olefin polymer is addressable through 21 CFR 177.1520; the converter must verify that the final formulation, including masterbatch and printing inks, meets the end-use extractive limits. REACH and Directive 2011/65/EU RoHS obligations apply to the final article and require documented absence of restricted substances above the directive thresholds.
| Framework | Standard or regulation | Verification requirement |
|---|---|---|
| Food contact EU | Regulation (EU) No 10/2011 | overall migration ≤ 10 mg/dm² in final article |
| Food contact US | 21 CFR 177.1520 | olefin polymer base resin; end-use extractive limits apply |
| Industrial chemicals EU | REACH | SVHC content documentation in finished compound |
| RoHS | Directive 2011/65/EU | restricted heavy metal thresholds in final article |
Precompounded slip and antiblock masterbatches should be dispersed using a high-shear mixing section such as a Maddock or pineapple mixer to prevent additive agglomeration in the lower-viscosity VLDPE melt. Batch-to-batch variance in gel count increases if the melt temperature exceeds 260°C for prolonged campaigns; this is a production-scale observation associated with thermal-oxidative degradation rather than a single DSC endotherm. The neat virgin pellets do not normally require predrying when stored below 60% RH. Hygroscopic masterbatches or filled reclaim streams require desiccant drying to a dew point of -30°C and 4 h at 70°C before extrusion.
Published data for specific antioxidant interactions with FF D0 is limited. Combinations with high-acidity process aids should be screened on a laboratory compounding line before production, because low crystallinity may accelerate migration of unreacted additives to the film surface under warehousing at elevated ambient temperatures. In applications requiring sustained service above the melting onset, the product is unsuitable; selected performance values degrade as creep and stress relaxation become dominant near the crystalline melting point measured by ISO 11357-3.