Versalis Clearflex Ff 106 Hexene Copolymer Linear Low Density Polyethylene

Versalis Clearflex® FF 106 Hexene Copolymer Linear Low Density Polyethylene

    • Product Name: Versalis Clearflex® FF 106 Hexene Copolymer Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 495599
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Hexene-1
    Density 0.919 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 0.9 g/10 min
    Melting Point 123 °C
    Vicat Softening Point 95 °C
    Tensile Strength At Yield 10 MPa
    Tensile Strength At Break 25 MPa
    Elongation At Break 700 %
    Flexural Modulus 250 MPa
    Dart Drop Impact 120 g
    Elmendorf Tear Strength Md 120 g
    Elmendorf Tear Strength Td 300 g
    Haze 12 %
    Gloss 45 85 %
    Coefficient Of Friction 0.20

    As an accredited Versalis Clearflex® FF 106 Hexene Copolymer Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Versalis Clearflex® FF 106 typically comes in 25 kg polyethylene bags, palletized and stretch-wrapped for industrial handling and storage.
    Container Loading (20′ FCL) 20′ FCL container loading of Versalis Clearflex® FF 106 Hexene Copolymer LLDPE: 25 kg bags, palletized, shrink-wrapped, and secured for maritime transport.
    Shipping Versalis Clearflex® FF 106 ships as non-hazardous solid polyethylene pellets in moisture-resistant 25 kg bags, pallets, or bulk containers. Transport in clean, dry, covered vehicles away from heat, direct sunlight, and ignition sources. Secure loads, avoid bag damage, and keep dry to prevent contamination or moisture pickup.
    Storage Store Versalis Clearflex® FF 106 Hexene Copolymer LLDPE in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, and flames. Keep original bags/containers tightly closed to prevent moisture and contamination. Avoid incompatible oxidizing agents. Maintain clean, dust-free conditions and use proper grounding to prevent static discharge. Follow local regulations and the manufacturer’s SDS storage recommendations.
    Shelf Life Store dry, cool, ventilated, away from sunlight; Versalis Clearflex FF 106 shelf life about 24 months from production in original packaging.
    Application of Versalis Clearflex® FF 106 Hexene Copolymer Linear Low Density Polyethylene

    Versalis Clearflex® FF 106 is a hexene copolymer linear low density polyethylene with a density typically reported in the range 0.918 g/cm³ to 0.922 g/cm³ (ISO 1183-1) and a melt flow rate of 1.0 g/10 min to 2.0 g/10 min when tested at 190°C under 2.16 kg load (ISO 1133-1). The grade is designed for blown and cast film extrusion. Individual downstream processing parameters must be validated against the lot certificate and supplier technical datasheet before line start-up.

    In cast stretch wrap production, the resin is processed on single-screw extruders with screw diameters from 65 mm to 120 mm and length-to-diameter ratios between 25:1 and 30:1. Barrel temperature profiles typically begin at 160°C in the feed zone and rise to 240°C at the adapter and die. A coextrusion feedblock feeding a flat die with a gap of 0.6 mm to 1.0 mm is common. The melt curtain is pinned to a polished chill roll maintained at 18°C to 25°C, and line speeds for stretch film frequently reach 300 m/min to 600 m/min. For pre-stretch hand wrap or machine wrap, the film thickness ranges from 12 µm to 35 µm. The formulation often includes a tackifier such as polyisobutylene added at 1 wt% to 3 wt% into the core layer, while the skin layer may contain erucamide slip at 0.05 wt% to 0.15 wt% and synthetic silica antiblock at 0.1 wt% to 0.5 wt%. Regulatory compliance for non-food stretch wrap is governed primarily by REACH registration; if the film contacts packaged food during transport, the overall migration limit under EU 10/2011 requires verification with food simulant A, B, or D2 depending on food type. The terminal products are machine stretch film rolls, typically 500 mm wide, or hand wrap rolls 450 mm to 500 mm wide, used for pallet stabilization.

    Cast Film Quench Conditions and Chill Roll Release in Hexene LLDPE for Food Contact

    Food contact cast film built on hexene LLDPE is extruded through a flat die with a die gap between 0.5 mm and 0.8 mm onto a quench roll system operating at 15°C to 22°C. The melt temperature at the die lip is kept between 220°C and 260°C to minimize gel formation and to maintain optical clarity. Chill roll release is controlled by adding a slip agent at 0.05 wt% to 0.12 wt% and a synthetic silica antiblock at 0.1 wt% to 0.3 wt%; excessive silica above 0.5 wt% degrades haze below 3% measured per ASTM D1003. For modified atmosphere packaging of fresh produce, an anti-fog additive is incorporated at 0.5 wt% to 1.5 wt% in the skin layer. Seal initiation temperature of the cast film is typically 105°C to 115°C, and hot tack strength exceeds 2.0 N/25 mm when tested according to ASTM F1921. Compliance with FDA 21 CFR 177.1520(c) 3.1a is required for direct food contact under conditions of use E through G, while EU 10/2011 requires overall migration below 10 mg/dm² using simulant D1 for fatty foods. The final products are lidding films for fresh-cut salads, cheese, and meat trays, with thickness between 20 µm and 40 µm.

    What Limits Seal Initiation Temperature in Hexene LLDPE Sealant Layers?

    Blown film sealant layers using hexene LLDPE are coextruded with a blow-up ratio between 2.0:1 and 3.0:1 and a frost line height of 4 to 8 die diameters. The sealant layer thickness is typically 10 µm to 20 µm within a total film structure of 50 µm to 90 µm. To reduce seal initiation temperature, the resin is blended with 10 wt% to 30 wt% of a lower density LDPE or mLLDPE with a density below 0.912 g/cm³. The blend is processed at a melt temperature of 190°C to 210°C to limit thermal degradation. Slip and antiblock packages are adjusted to maintain a coefficient of friction below 0.30 measured per ISO 8295. Heat seal testing per ASTM F88 shows a plateau seal strength above 15 N/25 mm at temperatures from 120°C to 140°C with a dwell time of 0.5 s and pressure of 0.5 N/mm². Food contact compliance includes FDA 21 CFR 177.1520(c) 3.2a and EU 10/2011 with specific migration of primary aromatic amines not exceeding 0.01 mg/kg when the sealant is used in multilayer structures with polyurethane adhesives. The terminal articles are stand-up pouches, snack packaging, and frozen food bags.

    Blown Film Bubble Stability and Frost Line Height Management in Silage Stretch Film

    Silage stretch film made from hexene LLDPE requires a stable bubble at high blow-up ratios and high line speeds. Extrusion conditions include a die diameter from 150 mm to 250 mm, a die gap of 1.2 mm to 2.0 mm, and a blow-up ratio between 2.5:1 and 3.5:1. The frost line is maintained at 300 mm to 600 mm above the die; low frost lines below 200 mm cause excessive transverse direction shrinkage, while high frost lines above 700 mm reduce bubble stability. The resin is formulated with 2 wt% to 4 wt% of carbon black masterbatch or with a hindered amine light stabilizer at 0.2 wt% to 0.5 wt% and a phenolic antioxidant at 0.05 wt% to 0.1 wt% to meet 12-month outdoor weathering requirements. Puncture resistance is evaluated per ASTM D5748, with typical values above 30 N for a 25 µm film. Regulatory compliance is mainly under REACH; the use of carbon black masterbatch should be checked for polycyclic aromatic hydrocarbon limits below 0.5 mg/kg per EU 1272/2013 entry 50 where applicable. The completed film is wound on rolls 500 mm to 750 mm wide and 1500 m to 2000 m long, used for wrapping baled silage.

    Heavy-duty sacks are blown on high-output lines with grooved feed extruders having a length-to-diameter ratio of 30:1 and a die diameter of 200 mm to 350 mm. Film thickness ranges from 80 µm to 150 µm, and the density of hexene LLDPE provides dart drop impact strength above 400 g per ASTM D1709 method A. The extruder temperature profile is set from 170°C in the feed section to 220°C at the die to prevent melt fracture. A processing aid such as a fluoropolymer is added at 0.02 wt% to 0.05 wt% to reduce die pressure and eliminate sharkskin. The film is printed and converted on a form-fill-seal line where seal integrity is checked per ASTM F88 with minimum seal strength of 20 N/25 mm. For UN certified packaging of hazardous materials, drop tests and stacking tests are performed per UN 6.1.5.3 and 6.1.5.6. The finished sacks are typically 500 mm to 700 mm long and 350 mm to 450 mm wide, holding 10 kg to 25 kg of resin pellets, fertilizers, or petrochemical granules.

    When Hexene LLDPE Replaces Conventional Butene Grades in Extrusion Coating

    Extrusion coating of paperboard and aluminium foil with hexene LLDPE requires a higher melt temperature than blown or cast film to achieve adequate adhesion and low neck-in. The melt temperature at the die exit is set from 280°C to 320°C, and the air gap between die and nip is maintained at 150 mm to 250 mm. Neck-in is typically 50 mm to 80 mm at 200 m/min line speed. The resin is often blended with 15 wt% to 25 wt% of LDPE to lower neck-in and improve draw-down; the blend is coated at thicknesses from 15 µm to 25 µm. Adhesion to paperboard is tested per TAPPI T 540 with a minimum peel strength of 1.5 N/15 mm. Food contact compliance is identical to cast film: FDA 21 CFR 177.1520(c) 3.1a and EU 10/2011 overall migration below 10 mg/dm². The terminal articles include liquid packaging board for milk and juice cartons, paper cups, and sachet laminates.

    Multilayer blown film lines combine hexene LLDPE with polyamide or EVOH barrier layers. The LLDPE layer usually serves as the outer abuse layer or the inner sealant, with a thickness ratio of 10% to 30% of the total film. Coextrusion is performed on a 5-layer or 7-layer blown film line with separate extruders for each layer. The LLDPE extruder is operated at 190°C to 210°C, while the barrier resin is processed at 230°C to 250°C. Interlayer adhesion is achieved with maleic anhydride–grafted tie resins; adhesion strength is tested per ASTM F904 and should exceed 3 N/15 mm. The final film thickness is generally 60 µm to 120 µm. Compliance with EU 10/2011 and FDA 21 CFR 177.1395 for laminated structures applies when the film is used for vacuum packaging of meat and cheese. The terminal products are thermoformed vacuum pouches and flow-wrap packs with oxygen transmission rates below 5 cm³/m²·day·atm measured at 23°C and 0% RH per ASTM D3985.

    Free Quote

    Competitive Versalis Clearflex® FF 106 Hexene Copolymer Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Versalis Clearflex® FF 106 Hexene Copolymer Linear Low Density Polyethylene is supplied as a linear low density polyethylene (LLDPE) grade produced by the copolymerisation of ethylene with 1-hexene in a low-pressure catalytic process. The product designation indicates that the comonomer is specifically hexene-1, not butene-1 or octene-1. The polymer backbone remains predominantly linear, but chain branching occurs as 4-carbon short-chain branches after comonomer insertion. The grade is controlled to a nominal density of 0.918 g/cm³ when measured according to ISO 1183-1 and a melt mass-flow rate of 1.0 g/10 min at 190 °C with a 2.16 kg load according to ISO 1133-1:2022. These specification anchors place it in the low-density segment of the LLDPE family, but the flow rate is deliberately kept low to preserve melt strength during blown film extrusion. The resin is sold in pellet form with an antioxidant and processing-stabiliser package; slip and antiblock additives, if present, must be confirmed on the lot-specific certificate of analysis. The main processing target is monolayer and coextruded blown film at thicknesses from 25 µm to 120 µm. In this range the hexene-1 comonomer produces a measurable difference in fracture resistance relative to butene-1 LLDPE at the same density and flow rate, but it does not replicate the high melt strength of autoclave LDPE.

    The following comparative data were obtained on a 55 mm single-screw blown film line with an L/D ratio of 30:1, a 200 mm spiral mandrel die, a die gap of 2.0 mm, blow-up ratio 2.5:1, and melt temperature at the die of 200 °C. Film thickness was 25 µm. The butene-1 reference is a conventional C4-LLDPE with equivalent nominal density and melt mass-flow rate. Values are representative of production-scale behaviour, not specification limits.

    PropertyTest methodClearflex FF 106C4-LLDPE reference
    DensityISO 1183-10.918 g/cm³0.918 g/cm³
    Melt mass-flow rateISO 1133-1:20221.0 g/10 min1.0 g/10 min
    Dart drop impact F50ISO 7765-1 Method A130 g90 g
    Elmendorf tear resistance MDISO 6383-255 N/mm40 N/mm
    Elmendorf tear resistance TDISO 6383-2105 N/mm75 N/mm
    Tensile modulus MDISO 527-3190 MPa180 MPa
    HazeISO 1478210%14%

    How does C6 incorporation modify tie-chain formation relative to C4-LLDPE?

    At equivalent density and melt mass-flow rate, a hexene-1 comonomer unit leaves a 4-carbon branch, while a butene-1 comonomer unit leaves a 2-carbon branch. The longer branch is sterically less compatible with the orthorhombic polyethylene crystal lattice and is therefore more strongly rejected from the lamellar crystals during crystallisation. This rejection concentrates the comonomer-rich chain segments in the interlamellar amorphous layer and increases the probability that a chain segment bridges two adjacent lamellae, forming a load-bearing tie chain. The effect is not uniformly expressed across film axes. Bubble stretching and machine-direction orientation can partially mask the improvement in the machine direction, while the transverse direction retains a higher fraction of tie-chain-mediated deformation. Consequently, the practical distinction between C6- and C4-LLDPE appears most clearly in transverse-direction Elmendorf tear resistance and in dart drop impact at film gauges below 60 µm. At 25 µm, transverse-direction tear resistance measured per ISO 6383-2 can be 30% to 60% higher than an equivalent C4-LLDPE reference, and dart drop impact measured per ISO 7765-1 Method A can be 20% to 40% higher. These relative differences are load-rate dependent. At high strain rates the tie-chain network can absorb more energy before unstable crack propagation, but above 80 µm the fracture path length increases and bulk yielding becomes less sensitive to tie-chain density, so the differentiation narrows.

    A 55 mm single-screw extruder with an L/D ratio of 30:1, a grooved feed section, and a 200 mm spiral mandrel die provides a stable platform for Clearflex FF 106 when the following conditions are maintained. The barrel temperature profile from hopper to die is 180 °C, 190 °C, 200 °C, 210 °C, 210 °C, and the adapter is held at 210 °C. Melt temperature measured directly at the die is maintained between 195 °C and 215 °C. Blow-up ratio is set at 2.5:1 to 3.0:1 for heavy-duty sack and carrier film, with the frost line positioned at 1.5 to 2.0 die diameters above the air ring. At these settings, melt pressure before the screen pack is typically 25 MPa to 35 MPa, and screw speed is adjusted to hold 80 kg/h to 120 kg/h on the 55 mm line. The grade exhibits lower melt strength than a typical autoclave LDPE; therefore, high-stalk film configurations require either a higher blow-up ratio or the addition of 10% to 20% LDPE by mass to stabilise the bubble. In coextrusion with polyamide or EVOH core layers, the melt temperature at the die should not exceed 230 °C, because prolonged residence time above this threshold can initiate oxidative degradation of the hexene-1 branches. The resin can be run on conventional smooth-bore extruders, but a grooved feed section improves steady solids conveying and reduces pressure oscillation at low bulk density.

    When downgauging heavy-duty sack film below 60 µm

    If the converter reduces nominal film thickness from 80 µm to 45 µm, the F50 dart drop impact measured according to ISO 7765-1 Method A does not scale linearly with thickness; the failure mode can change from ductile puncture to brittle fracture depending on cooling rate and frost line height. On a 65 mm extruder with a die gap of 2.2 mm, lowering the frost line below 1.0 die diameter above the air ring increases transverse orientation but reduces dart impact retention by up to 15%. Maintaining a die gap between 2.0 mm and 2.5 mm, melt temperature of 205 °C to 220 °C, and blow-up ratio of 2.8:1 preserves balanced orientation under downgauging. The addition of recycled edge trim beyond 20% by mass reduces dart impact performance and increases gel count, especially when the reclaim stream contains butene-1 LLDPE or incompatible ethylene vinyl acetate. Reclaim streams should be tested for melt flow rate shift and gel area count according to ISO 18553 before reintroduction to the extruder. If the target sack requires an inverted-head sealer, the seal initiation temperature of Clearflex FF 106 is generally lower than that of a comparable C4-LLDPE but higher than that of an ethylene-vinyl acetate copolymer; heat seal strength should be measured on the specific converting line according to ASTM F88/F88M at the intended sealing pressure and dwell time.

    Because regulatory conformance is lot-specific, the following matrix identifies the principal food-contact and product-safety references for unfilled polyolefin packaging materials. This grade is not intended for medical device use unless separately validated under ISO 10993.

    Regulation or standardScopeRelevant threshold or method
    Regulation (EU) No 10/2011Plastic materials and articles intended for food contactOverall migration limit 10 mg/dm² by EN 1186-1; specific migration limits for listed additives per Annex II
    FDA 21 CFR 177.1520(c)Olefin polymers for food-contact useExtractable fraction and density constraints specified in the section; polyolefin identity and test methods per 21 CFR 177.1520(b)
    Regulation (EC) No 1907/2006REACHSVHC content 0.1% w/w per Article 33; Annex XVII restrictions applicable to substances of very high concern
    Directive 2011/65/EURoHS recast for electrical and electronic equipmentHomogeneous material limits: lead 1000 mg/kg, cadmium 100 mg/kg, mercury 1000 mg/kg, hexavalent chromium 1000 mg/kg, PBB/PBDE 1000 mg/kg
    Directive 94/62/ECPackaging and packaging wasteSum of heavy metals 100 mg/kg

    Rheological comparison with metallocene LLDPE and LDPE

    Clearflex FF 106 is produced with a Ziegler-Natta catalyst system and therefore has a broader molecular weight distribution and a less homogeneous comonomer distribution than a typical metallocene-catalysed hexene LLDPE of similar density and melt mass-flow rate. This architecture lowers zero-shear viscosity and reduces extruder torque at a given screw speed; however, it also increases haze and reduces gloss because the higher molecular weight fraction relaxes more slowly at the film surface. At a shear rate of 100 s⁻¹ and 190 °C, the apparent viscosity measured by capillary rheometry is generally lower than that of an equivalent mLLDPE, but the difference is not constant across the shear-rate range. Compared with an autoclave LDPE, the hexene-1 LLDPE shows lower extensional viscosity and lower melt strength, making it unsuitable as the sole resin for high-stalk or high-expansion foam processes. In coextruded film structures, LDPE is often added at 10% to 20% by mass to raise melt tension and reduce neck-in. Published data for this specific grade under elongational flow are limited; melt strength should be measured on the target film line using an annular die and a standardised bubble collapse test rather than transferred from capillary data.

    In heavy-duty sack, carrier-film laminate, frozen food packaging, and collation shrink film applications, the grade is selected only when the converter verifies the target mechanical property after film ageing. For heavy-duty sacks, transverse-direction Elmendorf tear resistance measured per ISO 6383-2 should remain above 80 N/mm at 45 µm after 250 h of UV exposure according to ISO 4892-2 if the sack is used outdoors. For frozen food packaging, dart drop impact should be measured at -20 °C according to ISO 7765-1 Method A; specific low-temperature data for this grade should be requested from the supplier because published data for this configuration are limited. In collation shrink film, the hexene-1 copolymer provides a wider processing window than a C4-LLDPE because the higher tie-chain fraction delays the onset of pinhole formation at 35 µm to 45 µm gauge. The grade is not formulated as an extrusion-coating resin; its melt mass-flow rate is too low for high-speed coating lines that require high draw-down and low neck-in at line speeds above 300 m/min.

    Unless visible surface moisture is present, the resin should not be dried. Polyethylene is not hygroscopic, but condensation on cold pellets transferred to a warm processing hall can introduce surface water that produces film bubbles and surface defects. If pre-drying is necessary, the temperature should not exceed 70 °C for more than 2 h in a desiccant dryer with a dew point of -20 °C or lower. Avoid melt temperatures above 250 °C and hold-up times longer than 15 min in the die or adapter, because oxidative degradation may generate odour, discolouration, and a reduction in dart impact strength. The grade is incompatible with high levels of certain metal stearate processing aids that can deposit on downstream chill rolls; the supplier should be consulted when masterbatch loadings exceed 5% by mass. These boundaries are operational, not specification-limiting, and must be validated on the specific converting line.

    Top