| HS Code | 104419 |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | Butene-1 |
| Density | 0.918 g/cm3 |
| Melt Flow Rate | 1.0 g/10 min (190°C/2.16 kg) |
| Melting Point | 120°C |
| Vicat Softening Temperature | 95°C |
| Tensile Strength At Break Md | 35 MPa |
| Tensile Strength At Break Td | 30 MPa |
| Elongation At Break Md | 550% |
| Elongation At Break Td | 700% |
| Elmendorf Tear Resistance Md | 50 g |
| Elmendorf Tear Resistance Td | 100 g |
| Dart Drop Impact | 90 g |
| Haze | 12% |
| Gloss 45 | 70% |
As an accredited Versalis Clearflex® FF 106 A Film Grade LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Versalis Clearflex® FF 106 A Film Grade LLDPE comes in 25 kg polyethylene bags, palletized at 1,000 kg and shrink-wrapped. |
| Container Loading (20′ FCL) | Versalis Clearflex® FF 106 A Film Grade LLDPE loaded in a 20′ FCL container, palletized and secured for ocean shipment. |
| Shipping | Versalis Clearflex® FF 106 A Film Grade LLDPE is shipped as non-hazardous solid pellets in 25 kg polyethylene bags, stacked on pallets, stretch-wrapped, and secured. Transport in clean, dry, covered trucks or containers at ambient temperature, protecting from moisture, direct sunlight, heat, and contamination. Follow local transport regulations and retain documentation. |
| Storage | Store Versalis Clearflex® FF 106 A in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, flames, and strong oxidizers. Keep original packaging sealed, palletized, and off the floor to prevent moisture, dust, and contamination. Avoid prolonged UV exposure. Maintain ambient temperature, observe good housekeeping, and follow the supplier’s SDS and local regulations. Use first-in, first-out stock rotation. |
| Shelf Life | Recommended shelf life is 12 months from production when stored unopened, dry, away from direct sunlight, and below 40°C. |
In blown film extrusion of heavy-duty industrial sacks made from Clearflex® FF 106 A, the exact melt flow rate and density from the current Versalis technical datasheet define the final set-points. The processing ranges below are class-wide for film-grade LLDPE with melt flow rate between 0.9 g/10 min and 1.1 g/10 min at 190 °C and 2.16 kg. For this narrow-molecular-weight linear resin, the die gap is normally set between 1.2 mm and 1.8 mm. The melt temperature at the die lip is held between 190 °C and 220 °C. Temperatures above 230 °C reduce melt strength and increase gel formation. Bubble stability is maintained with a blow-up ratio between 2.0:1 and 2.6:1. Blow-up ratios above 3.0:1 commonly produce bubble oscillation because linear-chain extensional viscosity cannot dampen internal air pressure fluctuations. Frost line height is set between 6 and 9 die diameters to balance quench rate and orientation. The film gauge for heavy-duty sacks ranges from 80 µm to 150 µm. Dart impact resistance is tested according to ASTM D1709 Method A. Tensile properties are measured by ASTM D882. Elmendorf tear resistance is measured by ASTM D1922. On a grooved-feed extruder with 25:1 L/D, barrel temperatures are profiled from 170 °C at the feed zone to 210 °C at the metering zone. Back-pressure is kept below 350 bar to limit shear heating. The processing window for stable bubble geometry is restrictive: a change of ±5 °C in die lip temperature or ±0.3 in blow-up ratio shifts frost line height and creates gauge variation greater than ±8%.
In cast film production for pallet stretch wrap, the primary chill roll sets quench rate and crystalline morphology. Chill roll temperature is maintained between 18 °C and 28 °C. Surface temperatures above 35 °C slow nucleation and produce film with lower gloss retention and inconsistent elongation. The melt curtain is extruded through a flat die with a die gap between 0.4 mm and 0.8 mm. The film is pinned to the chill roll by air knife or electrostatic edge pinning. Line speeds for LLDPE cast stretch film normally range from 300 m/min to 600 m/min. Above 600 m/min, draw resonance appears as periodic thickness bands unless edge pinning and melt temperature are adjusted. Final film thickness is typically 12 µm to 30 µm. Pre-stretch ratio on pallet wrappers is set between 200% and 300%. The film must survive this elongation without localized necking. Tensile elongation at break is tested by ISO 527-3. Puncture resistance is measured by ASTM D5748. Cling force between layers is measured by ASTM D5458. When a cling additive is compounded, migration to the surface is time-dependent and temperature-dependent. Equilibrium cling is generally reached only after 24 h of aging at 23 °C. A low chill roll temperature improves clarity but increases internal stress. Subsequent pre-stretch above 250% may initiate transverse micro-tears at the film edges. Published data for this specific configuration is limited; the ranges cited are class-wide for LLDPE cast stretch film.
Sealant webs for flexible packaging laminates use Clearflex® FF 106 A in the seal layer because low seal initiation temperature and adequate hot-tack strength reduce jaw dwell time. A monolayer sealant web or a coextruded structure with a sealant skin of 10 µm to 30 µm is produced by blown or cast extrusion. Heat seal strength is measured by ASTM F88. Hot-tack strength is measured by ASTM F1921. Coefficient of friction is measured by ISO 8295. Seal initiation temperature for LLDPE film grades generally falls between 95 °C and 110 °C. At sealing jaw temperatures above 130 °C, seal strength reaches a plateau but the film becomes susceptible to thinning at the seal root. Slip and antiblock additives are dosed between 500 ppm and 1,500 ppm to control coefficient of friction below 0.25. Higher slip doses reduce friction but can increase migration of erucamide into food simulants. Additive migration in the polymer matrix is controlled by the solubility limit of erucamide in LLDPE; above 1,500 ppm, surface bloom occurs rapidly and reduces seal strength. Compliance is evaluated under FDA 21 CFR 177.1520(c) for olefin polymers and EU Regulation No 10/2011 Annex I. Overall migration limit is 10 mg/dm² under test condition OM2. The following table lists the control points.
| Regulatory reference | Test method | Test condition | Limit or criterion |
|---|---|---|---|
| FDA 21 CFR 177.1520(c) | Extraction specifications for olefin polymers | Food simulants per 21 CFR 177.1520(c) | Conforms to olefin polymer extractives |
| EU Regulation No 10/2011 Annex I | EN 1186-1 | OM2, 10 days at 40 °C | 10 mg/dm² |
| REACH 1907/2006 | Polymer exemption | Article 2(9) | No registration |
When this film grade is used in silage covers and agricultural barrier films, replacement of LDPE alters tear propagation behaviour and UV stabilizer demand. A silage cover of 150 µm to 250 µm thickness is produced by blown film extrusion. The film is often coextruded with a white outer layer and a black inner layer. Carbon black is added as a UV stabilizer at 1.0 wt% to 2.5 wt%. For non-black greenhouse films, hindered amine light stabilizers are used at 0.2 wt% to 0.6 wt%. Tensile strength and elongation after UV exposure are measured by ISO 527-3. Tear resistance is measured by ASTM D1922. Haze and light transmission are measured by ASTM D1003. The critical operational boundary is UV stabilization. Without adequate hindered amine light stabilizer, film embrittlement can occur within 6 months of high-UV outdoor exposure. LLDPE has lower oxygen barrier than EVOH or PA. Silage films function by restricting air infiltration and maintaining anaerobic conditions rather than by intrinsic oxygen transmission rate. Thickness integrity and puncture resistance therefore carry more weight than gas barrier. Additive compatibility is constrained: avoid brominated flame retardants and certain sulfur-containing stabilizers because they can interfere with hindered amine light stabilizer regeneration. Bubble gauge uniformity must remain below ±10% because thin spots become preferential failure points under wind load. Corona treatment is applied to raise wetting tension to at least 38 mN/m for adhesive tape sealing. Wetting tension is measured by ISO 8296. Published data for this specific outdoor exposure is limited; the listed stabilizer loadings are class-wide for agricultural LLDPE film.
On form-fill-seal bagging lines for polymer pellets, fertilizers, and fine chemicals, seal through dust contamination is the primary reliability variable. Bags made from Clearflex® FF 106 A are filled at rates between 20 bags/min and 30 bags/min. The film must resist puncture from sharp particles and retain seal strength through product contamination. Seal strength is measured by ASTM F88. Puncture resistance is measured by ASTM D5748. Dart impact resistance is measured by ASTM D1709. Film thickness for heavy-duty form-fill-seal bags is generally 100 µm to 180 µm. The critical threshold is dust loading in the seal area. A dust loading above 0.5 mg/cm² can reduce seal strength by more than 40% unless seal bar temperature and dwell time are increased. Seal bar temperature is typically set between 120 °C and 150 °C. Dwell time is set between 0.5 s and 1.5 s. Seal pressure is set between 2 bar and 4 bar. Coefficient of friction must be maintained between 0.20 and 0.35. Below 0.20 the bag may slip during transfer. Above 0.35 the bag may jam in the fill spout. If slip additive exceeds 1,500 ppm, seal strength may drop below the minimum required for 50 kg bag drop resistance. Bag drop performance is tested by ISO 7965-1.
In secondary packaging, Clearflex® FF 106 A is used where pallet containment and load retention are governed by stiffness, puncture resistance, and stretch or shrink recovery. Stretch hood film thickness ranges from 80 µm to 120 µm. The film is stretched on automatic stretch hood equipment at a stretch ratio between 55% and 85%. Recovery force after stretching is evaluated by tensile stress retention or by ISO 14616 for shrink force. Puncture resistance is measured by ASTM D5748. Tear propagation resistance is measured by ASTM D1922. For collation shrink film, LLDPE is blended with LDPE to control shrink tension and seal temperature. Shrink temperature for LLDPE-containing collation film is generally between 120 °C and 150 °C. Above 160 °C, the film tends to melt-seal to itself and create machine waste. The main processing conflict is orientation memory: LLDPE has a narrow re-crystallization window, and unbalanced machine-direction/transverse-direction orientation leads to curl. Film curl above 5 mm per linear metre disrupts automatic sleeve application. Gauge uniformity should be held within ±8% to avoid non-uniform recovery force distribution. Mechanical properties are evaluated by ASTM D882 for tensile modulus and ASTM D1922 for tear resistance. Published data for this specific grade in stretch hood configuration is limited; the ranges are class-wide for LLDPE-based secondary packaging films.
Competitive Versalis Clearflex® FF 106 A Film Grade LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Versalis Clearflex® FF 106 A is a film-grade linear low-density polyethylene (LLDPE) produced by Versalis S.p.A. and supplied in pellet form for blown-film extrusion. The manufacturer’s technical data list a melt mass-flow rate of 1.0 g/10 min at 190 °C under 2.16 kg load according to ISO 1133-1:2022 and a base density of 0.918 g/cm³ according to ISO 1183-1:2019. The grade is positioned for general-purpose packaging film, agricultural film, carrier bags, collation-shrink overwrap, liners, and similar thin-gauge blown-film applications. The A designation identifies the stabiliser formulation rather than the polymer backbone.
The density of 0.918 g/cm³ corresponds to a volumetric crystallinity in the region of 45–50% when referenced against a polyethylene enthalpy of fusion of 293 J/g. That crystallinity level explains the intermediate modulus and seal onset found between high-density rigid grades and lower-density plastomers. The LLDPE is a copolymer of ethylene and an α-olefin; published data for the specific comonomer type in this grade are limited, but the density and melt-flow envelope place it among conventional film-grade C4–C6 copolymers. The grade is not formulated as a high-clarity metallocene product, although downstream haze depends strongly on quench rate, die gap, and blow-up ratio.
The melt-flow value conditions screw-speed, die-pressure, and motor-load response on conventional single-screw blown-film lines. On a 60 mm diameter, 30:1 L/D grooved-feed extruder fitted with a 200 mm spiral-mandrel die and 1.8 mm die gap, processing typically begins with barrel zone temperatures of 180–210 °C, adapter and die temperatures of 200–220 °C, and a melt temperature between 210 °C and 240 °C. Bubble stability is highly sensitive to frost-line height. A frost-line distance below 300 mm can produce undercooled film with increased blocking, while a frost-line height above 600 mm may reduce quench rate sufficiently to alter secondary crystallisation and lower dart impact. Blow-up ratios are maintained between 2.5:1 and 3.5:1; outside this window, the machine-direction and transverse-direction tear balance shifts non-linearly.
The recommended die gap of 1.8–2.3 mm is wider than that commonly used for high-pressure LDPE. The lower strain hardening of linear LLDPE requires the larger opening to minimise melt fracture, bubble chatter, and die-lip build-up. Melt temperatures above 250 °C for extended residence time increase the probability of oxidative gel formation, while melt temperatures below 205 °C can reduce film clarity and raise motor load. The screw geometry should provide moderate shear mixing without excessive temperature rise. A barrier screw with a Maddock mixing head and compression ratio between 2.5:1 and 3.0:1 is adequate; high-shear screws designed for HDPE are not recommended because they may exceed the 240 °C processing threshold and consume the stabiliser package prematurely.
| Processing parameter | Recommended range or limit |
|---|---|
| Barrel zone 1 | 180–200 °C |
| Barrel zone 2 | 190–210 °C |
| Barrel zone 3 | 200–220 °C |
| Adapter and die | 210–230 °C |
| Melt temperature | 210–240 °C |
| Die gap | 1.8–2.3 mm |
| Blow-up ratio | 2.5:1–3.5:1 |
| Frost-line height | 300–600 mm |
| Maximum melt temperature | 250 °C |
Die inlet pressure should be monitored as a process-health indicator; on the equipment described above, normal pressure generally remains below 350 bar, but the actual value depends on die design, screen-pack condition, and output. No pre-drying is normally required for unopened pellets stored at ambient humidity. Sacks exposed for prolonged periods to relative humidity above 60% should be reconditioned with dry air to avoid surface moisture feeding and bubble defects. Internal bubble cooling, when fitted, raises output by increasing heat removal; the external air ring must then be adjusted carefully to avoid asymmetric quenching at the frost line.
Seal initiation in Clearflex® FF 106 A is governed primarily by short-chain branching distribution and crystallite melting rather than by the 1.0 g/10 min melt flow rate alone. On laboratory heat-seal equipment operating at 0.5 N/mm² jaw pressure and 0.5 s dwell, seal initiation is typically recorded in the 100–115 °C band on 50 µm blown film, with hot-tack strength increasing rapidly above 120 °C. These values shift with film thickness, corona treatment, and additive masterbatch. Operators converting the grade on vertical form-fill-seal machines should profile jaw temperature from 105 °C upward in 5 °C increments, because the sealing window narrows at web speeds above 25 m/min; published data for this specific configuration is limited. The grade is not formulated for high-temperature retort exposure and should not be specified for applications requiring sustained service above 80 °C.
Optical properties depend on quench rate and frost-line control. Films extruded at 50 µm with a 2.8:1 blow-up ratio typically show haze in the range of 8–14% when measured according to ASTM D1003 and gloss at 60° from 60 to 75 GU under ISO 2813. These values are indicative and will shift with slip and antiblock masterbatch addition. Water vapour transmission rate measured on 50 µm film at 38 °C and 90% RH by ISO 15106-3 is typically in the 5–10 g/(m²·day) band for LLDPE of this density, but the grade is not a barrier resin. If oxygen or moisture barrier is required, coextrusion with EVOH, nylon, or a metallised substrate should be considered.
When downgauging from LDPE to LLDPE, tensile, tear, and puncture response must be evaluated by standardised methods, not inferred from density alone. On 50 µm films produced at a 2.8:1 blow-up ratio, the grade exhibits machine-direction tear resistance lower than transverse-direction tear resistance, a characteristic inherited from LLDPE molecular orientation. This anisotropy is reduced by raising the blow-up ratio toward 3.5:1 or by increasing die gap. Tensile properties measured according to ISO 527-3 on 25 µm film typically show yield stress in the machine direction near 10 MPa and elongation at break exceeding 500%, although the values depend on draw ratio, frost-line height, and film gauge uniformity.
Dart impact is evaluated according to ISO 7765-1 or ASTM D1709A. The grade is specified for applications requiring higher puncture resistance in thin-gauge liners relative to conventional C4-LLDPE of similar melt flow. Elmendorf tear resistance should be tested in both machine and transverse directions using ISO 6383-2, because the ratio of MD to TD tear is a better predictor of sack toughness than single-point values. The density of 0.918 g/cm³ produces a lower secant modulus than high-density grades, which is advantageous for conformability in agricultural films but requires continuous thickness monitoring to avoid local thinning and split failure.
A line previously running a conventional Ziegler-Natta C4-LLDPE of comparable melt index can usually accept Clearflex® FF 106 A without major screw changes, but three operating parameters must be re-profiled. First, the melt-temperature setpoint may require a 5–10 °C reduction because the stabiliser package is designed for a specific processing window; temperatures above 240 °C can consume antioxidants prematurely and produce gel-like defects. Second, frost-line height should be re-established after the first reel because the molecular structure of the Clearflex grade changes the quench-rate response. Operators often observe a more transparent bubble and a sharper frost-line boundary. Third, the external air ring and internal bubble cooling flows must be rebalanced to avoid low-frequency bubble breathing at high take-off speeds.
Differences from metallocene LLDPE are also relevant. The grade does not provide the same ultra-low haze as high-clarity metallocene plastomer grades, but it retains a practical sealing window for general packaging. Compared with high-pressure LDPE, it offers higher dart impact at equal thickness and permits downgauging. However, the absence of long-chain branching reduces bubble stability under high stalk draw; therefore the die gap should not be reduced below 1.8 mm unless the line is equipped with a bubble stabilisation cage or advanced multi-lip air-ring control.
Compliance statements for the grade are governed by the specific pellet formulation and by the additives introduced at conversion. The matrix below reports only the polymer producer’s declared framework; converted film must be tested in its final article form under the intended conditions of use.
| Regulatory framework | Applicable condition or test basis |
|---|---|
| EU food-contact plastics | Regulation (EU) 10/2011 as amended; final article migration testing required |
| US food-contact olefin polymers | FDA 21 CFR 177.1520(c) 3.1a/3.2a; end-use limitations apply |
| REACH | Regulation (EC) No 1907/2006; supplier registration must be confirmed for the specific material lot |
| RoHS II | Directive 2011/65/EU; no intentional addition of restricted heavy metals or phthalates |
| Good manufacturing practice for food-contact materials | Regulation (EC) No 2023/2006 |
The A-grade stabilisation system includes a phenolic antioxidant and a phosphite process stabiliser at concentrations typical for blown-film LLDPE. The polymer is not intended for prolonged outdoor UV exposure without additional carbon black or HALS-based UV stabiliser masterbatch; unprotected film degrades within months under direct solar radiation. Contact with strong oxidising agents, chlorinated solvents, or long-term exposure to aromatic hydrocarbons can cause swelling or environmental stress cracking. For food-contact applications, the converter must verify migration limits for the specific additive package under the conditions of use; the base polymer is not the sole determinant of compliance.