Versalis Clearflex Dfh 20 Film Grade Lldpe

Versalis Clearflex® DFH 20 Film Grade LLDPE

    • Product Name: Versalis Clearflex® DFH 20 Film Grade LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 907490
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Density approx. 0.920 g/cm³
    Melt Flow Rate 190 C 2 16 Kg approx. 0.8 g/10 min
    Melting Temperature approx. 122 °C
    Vicat Softening Temperature approx. 95 °C
    Tensile Strength At Yield approx. 10 MPa
    Tensile Strength At Break approx. 25 MPa
    Elongation At Break approx. 800%
    Dart Drop Impact approx. 120 g
    Elmendorf Tear Strength Md approx. 120 g
    Elmendorf Tear Strength Td approx. 200 g
    Haze approx. 12%
    Gloss 45 approx. 60%
    Additive Antioxidant
    Slip Additive No
    Antiblock Additive No

    As an accredited Versalis Clearflex® DFH 20 Film Grade LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Versalis Clearflex® DFH 20 Film Grade LLDPE is supplied in 25 kg polyethylene bags, palletized and stretch-wrapped.
    Container Loading (20′ FCL) Container Loading (20′ FCL): Versalis Clearflex® DFH 20 Film Grade LLDPE, 25 kg bags, palletized, shrink-wrapped, approx. 18–20 MT net.
    Shipping Versalis Clearflex® DFH 20 Film Grade LLDPE is supplied in 25 kg polyethylene bags or 1000 kg octabins, palletized and stretch-wrapped. It ships by truck, rail, or container as a non-hazardous polymer. Store dry, away from heat and direct sunlight, per local regulations.
    Storage Store Versalis Clearflex® DFH 20 Film Grade LLDPE in a cool, dry, well-ventilated area, away from direct sunlight, heat, flames, and oxidizing agents. Keep bags or containers sealed, palletized, and off the floor to prevent moisture and contamination. Avoid prolonged UV exposure and excessive stacking. Follow manufacturer/SDS recommendations for safe handling and shelf life.
    Shelf Life Typically 24 months from production when stored unopened in original packaging, dry, cool, and away from direct sunlight.
    Application of Versalis Clearflex® DFH 20 Film Grade LLDPE

    Applications

    Clearflex DFH 20 is converted by air-cooled blown film extrusion into heavy-duty industrial sacks for polymer resin, fertilizer, and construction aggregate packaging. The processor should confirm grade-specific melt flow rate, density, and comonomer type from the Versalis technical data sheet before setting extrusion profiles. If the melt flow rate is in the 0.8–1.2 g/10 min range by ASTM D1238 at 190 °C/2.16 kg and density is near 0.920 g/cm³ by ISO 1183-1, a single-screw extruder with 25:1–30:1 L/D, barrier screw, and spiral mandrel die is appropriate. Barrel set points from feed to adapter are generally 160–180 °C, 190–210 °C, 210–225 °C, and 210–220 °C. Screen pack configuration of 40/60/100 mesh protects the die from gels and unmelted particles. Die diameter is selected in the 200–400 mm range for production-scale output. Die gap is set between 1.2 mm and 2.0 mm. Blow-up ratio is maintained at 2.0:1–2.8:1. Frost-line height is held at 6–10 die diameters to balance machine-direction and transverse-direction orientation. Surface treatment to 38–42 mN/m is applied when the sack body carries printed identification or handling instructions.

    A 70–80 wt% loading of Clearflex DFH 20 blended with 20–30 wt% high-pressure LDPE with melt flow rate 0.25–0.5 g/10 min provides bubble stability at 80–120 µm gauge. The LDPE contributes melt strength and reduces bubble flutter under high-speed winding. The same LDPE addition lowers dart impact and machine-direction tear resistance because high-pressure LDPE has a different short-chain branching distribution than linear low-density polyethylene. Antiblock masterbatch is added at 500–1500 ppm and slip additive at 300–800 ppm to permit sack opening and stacking without blocking. For dangerous goods packaging, the converted sack must meet UN certification requirements under 49 CFR Part 178, subpart M, where applicable. Typical converter acceptance targets for 100 µm film are dart impact above 400 g by ASTM D1709 Method A, Elmendorf tear above 200 g in machine direction by ASTM D1922, and tensile strength above 20 MPa by ASTM D882. These targets are line-specific and are not a substitute for DFH 20 lot-specific data.

    Impulse sealing and hot-bar welding are used to close the sack at 140–170 °C jaw temperature. Seal quality is checked by ASTM F88 peel testing. The end product is a heavy-duty sack of 100–150 µm thickness with printed outer surface and welded bottom seam. Published data for this specific configuration is limited, so pilot-line trials are required before conversion of DFH 20 into safety-critical packaging.

    What Limits Dart Impact Retention in Agricultural Film Based on Clearflex DFH 20?

    The agricultural film converter should attribute dart impact loss during service life to thermal oxidative degradation during extrusion, UV absorber depletion, and frost-line cooling rather than to base resin alone. DFH 20 is used in three-layer blown film lines for silage cover and greenhouse film. The core layer contains 60–70 wt% DFH 20. The skin layers contain UV-stabilised LLDPE/LDPE blends at 20–30 wt%. Hindered amine light stabiliser masterbatch is added at 0.15–0.40 wt%. UV absorber masterbatch is added at 0.10–0.25 wt%. These loadings are based on total blend weight. The three-layer die gap is kept at 1.6–2.4 mm. Blow-up ratio is set at 2.5:1–3.0:1. Frost-line height is set at 8–12 die diameters. Melt temperature is controlled at 200–220 °C to limit gel formation without degrading the stabiliser package. A blow-up ratio above 2.5:1 improves dart impact through transverse orientation but reduces machine-direction tear. The film design must match the stress pattern of the end use.

    For silage film at 25–40 µm, machine-direction elongation above 400% by ISO 527-3 and dart impact by ISO 7765-1 Method A are common converter targets. For greenhouse cover at 150–200 µm, light transmission above 85% by ASTM D1003 and haze below 25% by ASTM D1003 are typical acceptance values. UV durability is evaluated by xenon-arc exposure under ISO 4892-2 or fluorescent UV exposure under ASTM G154. DFH 20-specific weathering data is not published. Converter-specific xenon-arc exposure of 1000–3000 h is required before commercial specification. Agricultural film is not regulated as direct food contact. REACH and national feed hygiene rules may apply when silage film contacts animal feed. The end product is either a black or white silage cover or a greenhouse cover with stabilised outer surfaces.

    The limiting factor for dart impact retention is usually additive dispersion. Poor dispersion of HALS or UV absorber creates domains that initiate brittle failure. A twin-screw melt-blended masterbatch with carrier resin compatible with DFH 20 reduces this risk. A freeze-thaw cycle test at −20 °C for 100 h is recommended before specification. Processors should avoid regrind above 15 wt% in agricultural film because gel contamination from degraded stabiliser residues lowers dart impact retention.

    In flexible packaging lamination, Clearflex DFH 20 is converted into a sealant web when low seal-initiation temperature and high hot-tack strength are required. The converter blends 70–85 wt% DFH 20 with 15–30 wt% high-pressure LDPE. Antiblock is added at 1000–3000 ppm. Slip is added at 500–1000 ppm. The blown film line uses a die gap of 2.0 mm, melt temperature of 210–230 °C, and blow-up ratio of 2.0:1–2.2:1. Surface treatment to 38–42 mN/m is applied for adhesive lamination to PET, BOPP, or aluminium foil. Seal-initiation temperature is normally 95–110 °C for LLDPE sealant webs. The exact value depends on comonomer type and should be confirmed by differential scanning calorimetry and hot-tack testing. Hot-tack strength is measured by ASTM F1921 at 0.2 s dwell and 0.5 N/mm² seal pressure. Seal strength is measured by ASTM F88 after 24 h ageing.

    Direct food contact compliance requires the olefin polymer to meet FDA 21 CFR 177.1520(c). The finished film must comply with EU Regulation 10/2011 overall migration limit of 10 mg/dm² by EN 1186-1. The table below summarises the main compliance matrix for a laminated food-contact sealant web.

    Application ContextRegulation or StandardTest or Requirement
    Food-contact polymer baseFDA 21 CFR 177.1520(c)Olefin polymer use subject to end-use limitations and migration testing
    Finished food-contact filmEU Regulation 10/2011Overall migration ≤ 10 mg/dm² per EN 1186-1
    Heavy metals in packagingEU Directive 94/62/ECSum of Pb, Cd, Hg, Cr(VI) ≤ 100 mg/kg
    Hot-tack performanceASTM F1921Hot-tack force at 0.2 s dwell and 0.5 N/mm²
    Seal strengthASTM F88Seal strength after 24 h ageing

    The lamination process applies a solvent-based or solvent-free adhesive at 2.5–4.0 g/m² dry coat weight. The sealant web must be free of migrating slip additives that reduce lamination bond strength. End products are pouches for snacks, condiments, and powdered beverages at 30–60 µm sealant layer thickness. The main operational boundary is that slip additive levels above 1500 ppm can reduce lamination bond strength and seal strength.

    When Low-Temperature Puncture Resistance Determines Form-Fill-Seal Runability

    A frozen-food packaging line running Clearflex DFH 20 at 50–80 µm gauge on a vertical form-fill-seal machine must maintain low-temperature dart impact and seal integrity through rapid jaw cycling. The blend is 80–90 wt% DFH 20 and 10–20 wt% metallocene LLDPE to improve dart impact without increasing melt temperature. High-pressure LDPE is generally excluded from this structure because its branched architecture lowers low-temperature puncture energy. Antiblock masterbatch is added at 1000–2000 ppm. Slip is added at 400–700 ppm. The blown film die gap is 1.8–2.4 mm. Melt temperature is 190–220 °C. Blow-up ratio is 2.0:1–2.5:1. Frost-line height is 6–8 die diameters. A low frost-line height reduces crystallite size and increases puncture energy absorption at −20 °C.

    The vertical form-fill-seal machine seals the frozen food pouch at jaw temperature 120–150 °C with dwell time 0.3–0.8 s. Cooling air at 10–15 °C is directed to the seal area to reduce blocking and film shrinkage. Compliance for direct food contact is based on FDA 21 CFR 177.1520(c) and EU Regulation 10/2011 with overall migration testing by EN 1186-1. Low-temperature dart impact is measured after 24 h conditioning at −20 °C by ASTM D1709 Method A or ISO 7765-1 Method A. Puncture resistance is measured by ASTM F1306. Seal strength is checked by ASTM F88. DFH 20-specific low-temperature dart impact values should be generated on the packaging line before release. Antiblock above 3000 ppm in frozen food films increases haze by ASTM D1003 and reduces seal strength by ASTM F88. The end product is a direct food contact pouch for frozen vegetables, meat, or seafood with a printed outer surface and a clean-peel sealed top.

    The main failure mode on vertical form-fill-seal lines is seal contamination by slip additive migrating to the film surface. This is controlled by limiting slip masterbatch addition to 400–700 ppm and using a high-purity erucamide or oleamide grade. The packaging line tension must be below 10 N per 100 mm web width to avoid permanent deformation of the thin frozen food film.

    Collation film produced from Clearflex DFH 20 requires a balance of low coefficient of friction, gloss, and controlled shrink force. The film is used in bottom-seal collation machines for bundling bottles and cans at 30–60 µm gauge. The blend is 75–85 wt% DFH 20 and 15–25 wt% high-pressure LDPE. Slip additive is erucamide at 300–800 ppm. Antiblock is added at 1000–2000 ppm. Over-slip above 800 ppm contaminates seal jaws and leads to varying seal strength. The converter must monitor extractable slip by solvent extraction. The blown film line is set with die gap 1.2–1.8 mm, blow-up ratio 2.0:1, and melt temperature 190–210 °C. A low blow-up ratio is preferred because it produces anisotropic orientation suitable for machine-direction shrink force in collation systems.

    The coefficient of friction is measured by ASTM D1894 and is usually specified at 0.1–0.3 dynamic. Gloss at 60° is measured by ASTM D2457 and is typically specified above 70 for transparent collation film. Elmendorf tear is measured by ASTM D1922. Surface treatment to 36–40 mN/m is applied if the film carries printed banding information. Collation film is not direct food contact. Heavy metal limits in packaging per EU Directive 94/62/EC require combined lead, cadmium, mercury, and hexavalent chromium below 100 mg/kg. The end product is either perforated or unperforated shrink bundling film for beverage cans, bottled water, and household goods.

    The main processing limitation is melt instability at low melt temperature when high LDPE content is used. Bubble instability appears as visible shark-skin and causes gauge variation above 5% deviation. This is prevented by raising metering zone temperature by 5–10 °C or reducing LDPE to 15 wt%.

    FIBC Liner Film: Purity, Antistatic Balance, and Seal Integrity

    Clearflex DFH 20 can be converted into 80–120 µm tubular liners for flexible intermediate bulk containers used in hygroscopic chemical and food ingredient packaging. The blend is 80–100 wt% DFH 20. For antistatic liners, 0.5–1.0 wt% antistatic masterbatch is added when surface resistivity below 1011 ohm per IEC 61340-2-3 is required. Conductive compounds at 5–10 wt% are necessary only when surface resistivity below 106 ohm is specified. Blown film processing uses die gap 1.8–2.4 mm, melt temperature 190–220 °C, blow-up ratio 1.8:1–2.2:1, and frost-line height 6–9 die diameters. In-line gusseting produces a form-fit liner. Heat sealing is performed at 130–160 °C with a 5–10 mm wide seal bar to prevent leakage under hydrostatic load.

    Food ingredient liners require FDA 21 CFR 177.1520 and EU Regulation 10/2011 compliance. Chemical liners require UN compatibility testing for the specific fill material because the liner must not degrade or permeate dangerously. REACH SVHC disclosure is required for both paths. Seal integrity is checked by ASTM F88 and by air-inflation leak testing under 10–20 kPa internal pressure. The end product is a gusseted tubular liner with a welded bottom seal, inserted into an FIBC body before filling. Specific antistatic liner performance for DFH 20 is not published. Surface resistivity and charge decay must be verified by IEC 61340-2-3 and IEC 61340-2-1 on production samples.

    The main incompatibility is with excessive antistat loading above 1.0 wt%. It can cause die lip build-up and a decrease in seal strength. Processors must clean the die lip every 8–12 h when running antistatic grades. Moisture-sensitive fill materials require the liner film moisture vapour transmission rate to be measured by ASTM F1249 at 38 °C and 90% RH before qualification.

    Free Quote

    Competitive Versalis Clearflex® DFH 20 Film Grade LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Versalis Clearflex® DFH 20 Film Grade LLDPE is a linear low-density polyethylene intended for blown-film extrusion in monolayer and coextruded structures. Under the ISO 1872-1 designation system for polyethylene moulding and extrusion materials, the grade falls within the LLDPE film-extrusion class; class-typical data for this designation indicate a density of approximately 0.920 g/cm³ when tested under ISO 1183-1 and a melt flow rate of approximately 1.0 g/10 min when measured at 190 °C under a 2.16 kg load in accordance with ISO 1133-1:2022. The pelletised product is directed to heavy-duty packaging films, industrial liners, collation shrink film, agricultural films, and lamination webs in which tear resistance, sealability, and adequate drawdown are required. Published raw-material data for the specific DFH 20 configuration beyond class-typical values is limited; exact values should be confirmed against the manufacturer’s batch certificate of analysis. The material should not be confused with high-pressure low-density polyethylene, which contains long-chain branching and differs in melt rheology, or with higher-MFR LLDPE grades that provide easier processing at the expense of toughness.

    In production-scale blown-film conversion, DFH 20 class resin is processed on single-screw extruders with screw L/D ratios of 24:1 to 30:1 and grooved feed sections. Barrel temperatures from 180 °C to 220 °C and die-head temperatures up to 230 °C are common; melt temperature should be kept below 240 °C to limit oxidative gel formation. A die gap of 1.8 mm to 2.5 mm and a blow-up ratio of 2.0 to 3.0 are typical for monolayer film. Frost-line height is typically maintained at 4 to 8 die diameters to balance bubble stability and optical quality. The grade can be run with internal bubble cooling and high-stalk bubble configurations. Because LLDPE of this class has lower melt strength than high-pressure LDPE, the addition of 10 wt% to 20 wt% high-pressure LDPE is a standard corrective action for bubble instability; the long-chain branching of LDPE raises elongational viscosity and stabilises the bubble.

    Drying is not normally required for polyethylene film extrusion. If pellets are stored under conditions that create free surface moisture, condensation should be removed with ambient air or gentle material warming; high-temperature drying above 60 °C is generally unnecessary because the polymer is hydrophobic and does not undergo hydrolytic degradation.

    Rheological Response and Melt-Fracture Boundaries in DFH 20 Film Operations

    The predominantly linear molecular architecture of DFH 20 class LLDPE generates shear-thinning behaviour that differs from high-pressure LDPE. In narrow die gaps, the resin can exhibit sharkskin melt fracture when the die-lip shear stress reaches a critical value; the threshold is equipment-dependent and is influenced by die gap, melt temperature, and output rate. On conventional blown-film dies, widening the die gap from 1.2 mm to 2.0 mm or increasing the die-head temperature by 5 °C to 10 °C frequently suppresses the defect. A fluoropolymer-based polymer processing additive at 200 ppm to 1000 ppm can also delay melt fracture by coating the die-lip surface and reducing apparent die-lip shear stress. The addition of high-pressure LDPE at 10 wt% to 20 wt% modifies extensional behaviour and improves bubble stability, but excessive LDPE raises haze and reduces dart impact measured under ISO 7765-1. Since LLDPE has a relatively high molecular weight for a given melt flow rate, shear heating at high screw speed may produce temperature overshoot; melt-temperature monitoring at the die head is therefore a necessary control.

    For process control, melt-flow rate alone is insufficient. The melt-flow ratio, typically measured as the ratio of high-load MFR at 21.6 kg to standard MFR at 2.16 kg under ISO 1133-1, provides an indirect indication of molecular-weight distribution and shear-thinning. Film-grade LLDPE of this class usually exhibits a melt-flow ratio higher than that of high-pressure LDPE at comparable melt index; the value should be analysed against lot-to-lot variation because it influences die pressure and melt fracture. No single rheometer curve can replace actual extruder trials.

    At melt temperatures above 240 °C, oxidative gel formation may become visible as undispersed particles in the film. The risk is higher on long runs with high shear and no melt filtration. A screen pack with a fine-mesh breaker plate can reduce large gels, but high back-pressure may increase melt temperature and offset the benefit. Optical film inspection cameras are commonly used for surface gel detection; numerical gel limits should be agreed between converter and film customer because a universal ISO method for gel count is not available for this film class.

    What Distinguishes DFH 20 from Butene-Based LLDPE and High-Pressure LDPE in Film?

    The principal structural difference between DFH 20 class LLDPE and butene-based LLDPE is the length of the α-olefin comonomer. At comparable density and melt flow rate, a longer α-olefin comonomer increases the population of tie chains between lamellae and typically produces higher dart impact and Elmendorf tear resistance. In 25 µm to 50 µm films, a class-typical 0.920 g/cm³ LLDPE shows a higher dart drop impact value under ISO 7765-1 than a butene-based LLDPE of the same nominal density. Tensile properties measured under ISO 527-3 can be similar, but puncture and torn-crack resistance frequently improve. Against high-pressure LDPE, DFH 20 class LLDPE provides higher tensile strength, elongation, and puncture resistance because the linear backbone has less long-chain branching and the molecular weight is higher at a given MFR. However, its melt strength is lower, and optical properties can be poorer if the frost-line height is not managed. The lower melting range supports lower seal initiation temperatures in packaging; seal initiation should be confirmed with ASTM F88/F88M or ISO 20290 and recorded as a seal curve for the target film gauge.

    In coextruded films, DFH 20 class resin is often used in a core or sealant layer while an LDPE-rich skin supplies melt stability and optics. A typical structure may place the LLDPE in the inner layer to contribute hot-tack and seal strength while the outer LDPE-rich layer improves bubble stability and surface gloss. The layer ratio must be adjusted to maintain dart impact and tear resistance; excessive LDPE in the skin can reduce overall toughness measured under ISO 7765-1 and ISO 6383-2.

    Compared with metallocene-catalysed LLDPE of similar density, DFH 20 class resin may exhibit lower optical clarity and higher extractable levels if the catalyst system is conventional Ziegler-Natta; however, it may provide a wider processing window. Published data for this specific grade’s catalyst type is limited. Users requiring very high gloss and low organoleptics should test the grade directly against metallocene alternatives using ISO 14782, ISO 2813, and organoleptic evaluation methods.

    DFH 20 differs from other film grades in its balance of density and melt flow rate. If a converter compares DFH 20 with a grade having MFR 2.0 g/10 min, DFH 20 will generally have higher melt strength and better bubble stability at the expense of motor load and output on a given extruder. Conversely, a grade with MFR 0.5 g/10 min may show higher dart impact but require more melt pressure. The selection is therefore machine-specific; it should be supported by extruder pressure, melt temperature, motor load, and film property data.

    If High-Internal-Bubble-Cooling Is Used, Frost-Line Height Becomes a Process-Sensitive Variable

    Under internal bubble cooling, the frost-line height is controlled by the balance of internal and external air flow, air temperature, and bubble dwell time. Rapid cooling of the LLDPE melt lowers the frost line and reduces crystal size, which can improve haze and gloss measured under ISO 14782 and ISO 2813. However, an excessively low frost line can quench orientation and reduce dart impact because the chains do not have sufficient time to relax after being drawn; the result is a loss of toughness that may appear in ISO 7765-1 testing. A practical frost-line window of 3 to 7 die diameters is often used with internal bubble cooling. Excessive internal air volume can generate bubble oscillation and thickness variation at high output; the bubble cage and collapsing frame must be set to maintain symmetry. When the film is gusseted, the longitudinal crease may increase the local coefficient of friction and require slip additive adjustment, because gusseted areas are subject to blocking at high rewind tension.

    Slip and antiblock additives are commonly present in film-grade LLDPE. The additive loading may be adjusted to give a coefficient of friction in the range 0.1 to 0.3 measured by ISO 8295; these values are film-age-dependent because migration to the surface proceeds over time. If the film is used for food contact, the surface additives must comply with the positive lists in EU 10/2011 and FDA 21 CFR 177.1520. For printing, the presence of slip additive can reduce ink adhesion; corona treatment to 38 mN/m is not sufficient if the surface is contaminated with migrated additive. A dyne solution check should be repeated after aging to confirm that the wetting tension is retained.

    In high-speed form-fill-seal packaging, seal initiation and hot-tack are not interchangeable. DFH 20 class LLDPE tends to yield a broader hot-tack plateau than high-pressure LDPE because the lower melting point and linear structure allow sealing at lower temperatures, but the user must establish that the sealant layer reaches the required interface temperature. A seal initiation curve generated under ASTM F88/F88M using a 25 mm wide seal and a 0.5 s dwell time is a mandatory quality record for laminate structures. The actual seal temperature at the jaw face is often 10 °C to 20 °C lower than the setpoint due to heat transfer losses; thermocouple verification on the sealing bar is advised. Hot-tack should be measured under ASTM F1921 or the equivalent ISO method for the packaging line speed to avoid false-positive laboratory seal data.

    Quality control for DFH 20 film production is usually organised around the following methods.

    PropertyTest methodNotes
    Melt mass-flow rateISO 1133-1:2022190 °C, 2.16 kg
    DensityISO 1183-123 °C
    Tensile strength at breakISO 527-3500 mm/min, 40 µm film
    Elmendorf tear resistanceISO 6383-240 µm film
    Dart drop impactISO 7765-1F50, 40 µm film
    HazeISO 1478240 µm film
    GlossISO 281360° geometry
    Coefficient of frictionISO 8295 / ASTM D189423 °C, 50 % RH
    Seal strengthASTM F88/F88M25 mm sealed strip
    Wetting tensionISO 8296Target 38–42 mN/m

    Regulatory status for the grade should be confirmed for the intended food-contact or industrial application.

    RequirementReferenceRelevance
    EU food-contact plasticsEU Regulation 10/2011Overall migration limit 10 mg/dm²
    US food-contact olefin polymersFDA 21 CFR 177.1520Compliance subject to end-use conditions
    REACHEC 1907/2006SVHC content declaration
    RoHSEU 2011/65/EUNot intended for electronics; lead/cadmium restrictions do not exempt packaging
    Polyethylene designationISO 1872-1LLDPE film-extrusion class

    For heavy-duty sack and liner applications, downgauging from a 50 µm monolayer high-pressure LDPE film to a 35 µm DFH 20 class LLDPE film is justified only after comparative dart impact under ISO 7765-1, tear resistance under ISO 6383-2, and seal strength under ASTM F88/F88M confirm that the lower-gauge structure retains the required mechanical and seal performance. In high-speed form-fill-seal operations, hot-tack must also be characterised under ASTM F1921 at the intended line speed and jaw configuration, because laboratory seal tests at low dwell time do not fully reproduce production conditions.

    Top