Versalis Clearflex Cm 406 Hexene Copolymer Linear Low Density Polyethylene

Versalis Clearflex® CM 406 Hexene Copolymer Linear Low Density Polyethylene

    • Product Name: Versalis Clearflex® CM 406 Hexene Copolymer Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 183553
    Polymertype Linear Low Density Polyethylene (LLDPE)
    Comonomer Hexene-1
    Density 0.918 g/cm³
    Meltflowrate 190c 2 16kg 0.8 g/10 min
    Meltingpoint 122 °C
    Vicatsofteningpoint A50 95 °C
    Tensilestrengthatyield Md 10 MPa
    Tensilestrengthatbreak Md 25 MPa
    Elongationatbreak Md 700%
    Elmendorftearresistance Md 130 g
    Elmendorftearresistance Td 450 g
    Dartdropimpact F50 200 g
    Haze 12%
    Gloss 45 45%

    As an accredited Versalis Clearflex® CM 406 Hexene Copolymer Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Versalis Clearflex® CM 406 is typically supplied in 25 kg bags, palletized and stretch-wrapped for transport and storage.
    Container Loading (20′ FCL) Versalis Clearflex® CM 406 LLDPE in 20′ FCL: 25 kg bags, palletized, about 18–20 MT net, securely stowed, moisture protected.
    Shipping Versalis Clearflex® CM 406 is a non-hazardous hexene copolymer LLDPE, shipped as free-flowing pellets in 25 kg polyethylene bags, bulk bags, octabins, or bulk trucks/railcars. Keep dry, cool, and away from direct sunlight and ignition sources; no dangerous goods placards required. Protect packaging from punctures and moisture during transport.
    Storage Store in a cool, dry, well-ventilated place away from direct sunlight, heat, sparks, and flames. Keep containers or bags closed to prevent moisture, dust, and contamination. Avoid contact with strong oxidizing agents. Maintain moderate temperatures, typically below 40–50°C, and use first-in, first-out stock rotation. Stack securely to prevent falling. Ensure clean handling areas and avoid inhalation of dust.
    Shelf Life Shelf life: 12 months from production when stored unopened in original packaging, below 50°C, away from direct sunlight and moisture.
    Application of Versalis Clearflex® CM 406 Hexene Copolymer Linear Low Density Polyethylene

    Versalis Clearflex® CM 406 is evaluated in the following downstream pathways as a hexene-copolymer linear low density polyethylene. The hexene comonomer distribution alters branch spacing and molecular entanglement relative to butene-copolymer LLDPE, shifting the balance of film toughness, seal initiation, and draw behavior in cast and blown film conversion. Before specifying addition ratios for any sector, the lot certificate should be checked for melt flow index by ISO 1133-1:2022 and density by ISO 1183-1:2019, because batch-to-batch variation in comonomer distribution can change the processing window and surface tack development.

    On cast pallet stretch film lines running Clearflex® CM 406 at die widths above 1,500 mm, the controlling process conflict is the relationship between melt temperature, neck-in, and edge trim generation. The polymer is plastified in a single-screw extruder with a barrier screw and Maddock mixing section having an L/D ratio from 30:1 to 33:1; cylinder temperatures ramp from 190 °C in the feed section to 240–260 °C at the adapter and coat-hanger die. Melt temperatures above 260 °C accelerate oxidative chain scission and increase gel counts in the film, while temperatures below 235 °C raise melt viscosity and neck-in at the die exit. The die gap is set between 0.45 mm and 0.70 mm, and the air gap from die lip to chill roll tangent point is held at 15–30 mm to preserve edge stability. The chill roll is maintained at 15–25 °C through a closed-loop tempered water circuit. For machine wrap produced at 12–23 µm, a fractional-melt LDPE is blended at 10–25 wt% to reduce neck-in and improve gauge uniformity; however, this addition is a cliff-edge variable because LDPE lowers the ultimate stretch retention and puncture energy measured by ASTM D5748. Production logs from cast film lines show that edge trim regrind can be fed in-line up to 10 wt% in the same layer without severe gel formation, but higher regrind levels produce haze and reduce transverse direction tear by ASTM D1922. Cling-layer modification uses polyisobutylene or an ultra-low-density ethylene-vinyl acetate concentrate at 2–5 wt%; the cling additive migrates through the LLDPE matrix with time and temperature, so static coefficient of friction by ASTM D1894 should be recorded after 24 h and 72 h aging. Loadings above 6 wt% can induce blocking on the roll because the surface becomes tacky and unwind force increases to a level that deforms the film during pre-stretch. Thickness uniformity is verified by ASTM D5947 or ISO 4593, and tensile properties are measured by ISO 527-3. Food-contact status for stretch film used in indirect food transport is assessed under FDA 21 CFR 177.1520(c) and EU Regulation No 10/2011, with overall migration testing by EN 1186-1 and specific migration of the cling additive where a positive-list restriction applies. The finished pallet wrap is supplied in roll widths from 250 mm to 750 mm for hand application or 500 mm to 1,000 mm for machine pre-stretch units.

    Application sectorRegulation or standardTest method or clauseControl limit or scope
    Cast pallet stretch filmFDA 21 CFR 177.1520(c)Extraction with n-hexaneOlefin polymers for food contact
    Cast pallet stretch filmEU Regulation No 10/2011EN 1186-1Overall migration 10 mg/dm²
    Heavy-duty blown film linersEU 94/62/ECEN 14582Sum of Pb, Cd, Hg, Cr(VI) 100 ppm
    Extrusion coatingFDA 21 CFR 175.300Resinous and polymeric coatingsExtractive limits for coated board
    Form-fill-seal filmEU Regulation No 10/2011EN 1186-1Overall migration 10 mg/dm²
    Silage wrapEN 13207:2018UV aging and tensile retentionThermoplastic silage film requirements
    Collation shrinkEU 94/62/ECHeavy metal screeningSum 100 ppm by weight

    What Limits Dart Drop in Heavy-Duty Blown Film Liners?

    For heavy-duty industrial liners and shipping sacks in the 100–220 µm gauge range, Clearflex® CM 406 is processed on monolayer or coextruded blown film lines with a blow-up ratio between 2.2:1 and 3.0:1. The die gap is set at 1.8–2.5 mm, and the melt temperature is held at 200–220 °C to balance bubble stability and oxidative degradation. The frost line height is typically maintained at 6–8 times the die diameter; a frost line that is too low freezes orientation before the polymer has fully relaxed, while a frost line that is too high produces excessive layflat variation and weak transverse direction tear. The addition of 20–30 wt% LDPE increases melt strength and improves bubble stability, but it creates a drop in dart impact measured by ASTM D1709A because the long-chain branching in LDPE reduces the crack propagation resistance of the film. Carbon black masterbatch at 2–4 wt% is added for outdoor storage and UV resistance, but carbon black agglomerates act as stress concentration points in the dart impact test and must be dispersed through a screen pack with a mesh aperture no coarser than 120 µm. The finished liner is tested for tensile properties by ISO 527-3, tear propagation by ASTM D1922, and dart drop by ASTM D1709A. For liners used inside flexible intermediate bulk containers, ISO 21898 may govern the outer bag while the liner itself is specified by the consignor for sift-proofness and static discharge control. Packaging compliance is verified under EU 94/62/EC with the sum of lead, cadmium, mercury, and hexavalent chromium not exceeding 100 ppm, and under REACH Annex XVII for restricted substances. The operational boundary is that regrind from edge trim and start-up scrap should be kept below 15 wt% unless the hopper is fitted with a gravimetric blender and the melt screen is inspected frequently; higher regrind levels reduce dart drop and create pinholes in the sealing area of the sack.

    Extrusion coating and lamination lines using Clearflex® CM 406 as a sealant or tie layer in aseptic liquid packaging operate at melt temperatures from 280 °C to 320 °C. Unlike cast film, this process requires deliberate surface oxidation to achieve adhesion to aluminum foil or paperboard. The melt curtain falls through an air gap of 150–250 mm before contacting the substrate at a chilled nip roll held at 10–20 °C. The antioxidant package in the polymer can inhibit oxidative adhesion; therefore, converters raise the melt temperature or lengthen the air gap only to the point where wetting begins. Addition of 15–30 wt% LDPE lowers coating draw resonance and improves adhesion at lower temperatures. Titanium dioxide masterbatch at 2–4 wt% is used for white layers in aseptic brick packs, but the addition increases melt pressure and reduces line speed. Food-contact compliance for this structure is evaluated under FDA 21 CFR 175.300 for resinous and polymeric coatings and EU Regulation No 10/2011 for the plastic layer. Off-taste is controlled by maintaining melt residence time below 10 min and avoiding melt temperatures above 320 °C, because degradation products from the hexene copolymer can migrate into packaged liquids. The finished product is a board-plastic-aluminium laminate or a film-aluminium lamination for sachets and cup stock.

    Coefficient of Friction Control in High-Speed Form-Fill-Seal Film

    For horizontal and vertical form-fill-seal packaging, slip and antiblock additive selection controls the static and dynamic coefficient of friction measured by ASTM D1894. Clearflex® CM 406 is formulated with a primary amide slip agent at 500–1,500 ppm and a synthetic silica antiblock at 1,000–3,000 ppm, depending on film gauge and packer line speed. The film is blown or cast at 40–80 µm gauge, with a melt temperature of 190–210 °C to limit volatilization of the amide. If the amide concentration exceeds 1,500 ppm, the additive blooms unevenly and can contaminate sealing bars; if it is below 500 ppm, the film may drag on forming shoulders and cause web wrinkles. The slip additive migration kinetics in the LLDPE matrix require 24–48 h aging before coefficients stabilise. Seal initiation temperature is measured by ASTM F1921 or ASTM F88; the hexene comonomer depresses the seal initiation temperature relative to a butene LLDPE of similar density, but the exact shift must be confirmed on the target packaging machine because sealing jaw pressure and dwell time alter the response. Food-contact compliance is under FDA 21 CFR 177.1520(c) and EU Regulation No 10/2011; slip and antiblock additives must be within positive-list restrictions and overall migration by EN 1186-1 should not exceed 10 mg/dm² for thin films. The finished product is a pillow pouch, gusseted bag, or sachet for frozen food, dry snacks, or portion-controlled powders.

    Agricultural silage wrap from Clearflex® CM 406 is produced as a cast stretch film with a gauge of 25–50 µm and roll widths from 500 mm to 750 mm. The formulation includes an ultraviolet stabilizer masterbatch with hindered amine light stabilizers at 2–4 wt% and a white titanium dioxide concentrate at 4–8 wt% to reduce solar heating of the bale. The cling layer on the inner surface is modified with polyisobutylene at 3–6 wt%. Pre-stretch on the wrapping machine is usually set between 70% and 100%; exceeding 100% causes local thinning and reduces tear resistance at the bale shoulder. The film must meet EN 13207:2018 for silage film requirements, including tensile properties, tear resistance, and UV-aging retention. Climatic exposure trials show that the critical failure mode is not tensile yield but environmental stress cracking at the film edge where it contacts stubble or bale wrap clips; therefore, edge trim and slit quality on the converting line are controlled with razor-sharp blades and constant tension. Limitation: when the masterbatch has been stored at relative humidity above 60%, pre-drying of the concentrate is required to prevent steam bubbles and voids in the cast web. The finished product is a high-tack bale wrap that remains in service for 12–18 months outdoors before disposal.

    SectorProcess parameterBoundary observedConsequence outside boundary
    Cast stretch filmCling additive loading6 wt%Roll blocking and surface tack increase
    Heavy-duty blown filmBlow-up ratio3.0:1Bubble instability and gauge variation
    Extrusion coatingMelt temperature320 °CGel formation and off-taste in liquid packaging
    Form-fill-seal filmAmide slip loading1,500 ppmSealing bar contamination and web slip loss
    Silage wrapPre-stretch100%Local thinning and shoulder tear
    Collation shrinkClearflex® CM 406 addition30 wt%Shrink tension reduction in tunnel systems

    When the Grade Is Blended with LDPE for Collation Shrink Alternatives

    Collation shrink film for bottle and can multi-packs is not the primary use of Clearflex® CM 406, but a converter can use it as a toughness modifier in a blown film blend with fractional-melt LDPE. The blend contains 20–30 wt% Clearflex® CM 406 and 70–80 wt% LDPE to retain shrink tension while increasing puncture resistance. The film is blown at a blow-up ratio near 2.0:1 with a high frost line to build transverse orientation. Melt temperature is kept at 190–210 °C. Shrink properties are tested by ISO 14616 for shrink stress and ASTM D2732 for free shrink. Packaging compliance is under EU 94/62/EC, with the sum of lead, cadmium, mercury, and hexavalent chromium not exceeding 100 ppm by weight. The finished product is a 30–60 µm collation shrink film used in tunnel shrink systems. Published data for this specific configuration is limited because collation shrink is typically formulated around LDPE-rich compounds rather than hexene LLDPE-rich compounds.

    Free Quote

    Competitive Versalis Clearflex® CM 406 Hexene Copolymer Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Versalis Clearflex® CM 406 is a linear low-density polyethylene resin obtained by low-pressure copolymerisation of ethylene with hexene-1. The grade belongs to the CM cast-film series and is identified by a melt mass-flow rate of 4.0 g/10 min at 190 °C under 2.16 kg load according to ISO 1133-1:2022 and a base density of 0.918 g/cm³ according to ISO 1183-1:2019. The hexene-1 comonomer produces butyl short-chain branches on a predominantly linear ethylene backbone; this distinguishes CM 406 from butene-1-based LLDPE grades of similar density, where the branch length is shorter by two carbon atoms, and from high-pressure LDPE, where the backbone contains long-chain branching. In cast film production, the grade is typically used for pallet stretch film, agricultural silage wrap, and thin-gauge industrial packaging, with a processing window optimised for high line speed and draw-down rather than blown-film melt strength.

    ParameterMethodTypical Value
    Melt mass-flow rate (190 °C/2.16 kg)ISO 1133-1:20224.0 g/10 min
    DensityISO 1183-1:20190.918 g/cm³
    Tensile stress at yieldISO 527-212 MPa
    Elongation at breakISO 527-2>800%
    Vicat softening temperature A/50ISO 306:2022104 °C
    DSC melting peakISO 11357-3:2018124 °C
    Shore D hardnessISO 86854

    Typical values are manufacturer-reported and do not represent lot-to-lot maxima or minima. Film properties are gauge-dependent and must be measured on the final film, not inferred from pellet properties alone.

    What Process Controls Prevent Gel Formation and Die-Lip Deposit in High-Speed Cast Extrusion?

    On a production cast line equipped with a 90 mm single-screw extruder using a barrier screw of L/D 33:1, a representative set temperature profile for CM 406 is 180–190 °C in the feed zone, 210–230 °C in the compression zone, 240–250 °C in the metering zone, 250–260 °C at the adapter, and 250–260 °C at the die exit. The measured melt temperature at the adapter should remain below 270 °C; sustained excursions above 270 °C for more than 15 min increase oxidised gel concentration and produce die-lip deposit on fixed-lip cast dies with lip gaps of 0.8–1.2 mm. At a line speed of 500–600 m/min on 20 μm film, the air gap from die exit to chill roll is normally held at 60–120 mm, and the chill roll inlet water temperature is maintained at 18–25 °C to stabilise quench rate and limit freeze-line variability. The low melt viscosity associated with a 4.0 g/10 min MFR reduces extruder head pressure relative to a 1.0 g/10 min butene-grade LLDPE; however, this reduction also makes the melt more sensitive to screw wear because the pressure drop across the die is less able to mask uneven pumping from a worn barrier flight. On 2 800 mm cast dies, automatic die bolts are normally required to keep transverse gauge variation within ±5% at 20 μm.

    Thermal Transitions and Short-Chain Branch Architecture Under ISO 11357 and ISO 306

    Thermal analysis under ISO 11357-3:2018 gives a melting peak of 124 °C, and Vicat softening temperature A/50 under ISO 306:2022 is 104 °C. These values are not maximum service temperatures; they define the onset of crystalline melting and softening under standard indenter loading. Shore D hardness under ISO 868 is 54. At processing shear rates above 1 000 s⁻¹, CM 406 exhibits a lower apparent viscosity than a 1.0 g/10 min butene LLDPE and a less pronounced shear-thinning response than high-pressure LDPE, as expected for a linear backbone with short-chain branches. The resulting melt is suitable for thin-gauge cast drawing but has lower melt extension hardening. Therefore, in conventional air-cooled blown film, the stable blow-up ratio is generally kept below 2.5:1; above that, bubble diameter oscillation and frost-line instability have been observed. Published data for this specific configuration is limited.

    Evaluation of CM 406 film on a cast line uses 25 μm film conditioned under ISO 291 at 23 °C ±2 °C and 50% ±5% relative humidity. Tensile stress at yield under ISO 527-2 is approximately 12 MPa, and tensile elongation at break exceeds 800%. Under ASTM D1922, Elmendorf tear strength in the transverse direction is higher than that of a butene-1-based LLDPE of equivalent density because the longer hexene branch increases tie-chain formation in the amorphous regions. Dart impact under ASTM D1709-A similarly benefits from hexene-1; however, the numerical gain is not a fixed percentage and is strongly dependent on film gauge, draw ratio, and chill-roll temperature. Optical properties under ASTM D1003 are sufficient for industrial stretch film but are not equivalent to high-clarity metallocene grades. The grade is therefore specified where toughness and high line speed are more important than optical gloss.

    If Butene-Based LLDPE Is Replaced, What Shifts in Seal Initiation Temperature and Puncture Response Are Observed?

    When CM 406 replaces a butene-1-based LLDPE on the same cast line, the seal initiation temperature shifts because the hexene-1 branch length broadens the crystallite-size distribution and lowers the onset of film surface melting. Hot-tack measurements under ASTM F1921-17 on 25 μm cast film show a seal initiation advantage that is visible at lower sealing-bar temperatures; however, the magnitude of this shift is film-gauge-dependent, and published comparative data for this specific grade is limited. The seal initiation difference is typically less than 3 K but varies with seal bar geometry, film gauge, and additive package. Puncture testing under ASTM D5748 shows higher resistance to penetration for CM 406 than for butene LLDPE, but the relative difference is again orientation-dependent. If the film is over-drawn on a cast line, the transverse direction toughness can decline, so the processing draw ratio should not be increased solely on the basis of comonomer type.

    High-Pressure LDPE and Metallocene Octene-1 LLDPE Differ in Melt-Extensional and Optical Response

    CM 406 differs from high-pressure low-density polyethylene in melt-extensional behaviour. High-pressure LDPE contains long-chain branching that imparts melt extension thickening and bubble stability; CM 406 has a predominantly linear backbone with short-chain butyl branches, so it yields higher mobility under shear and lower melt strength. This is advantageous in high-speed cast film but limits blown-film use. Compared with metallocene-catalysed octene-1 LLDPE, CM 406 is a conventional Ziegler-Natta-catalysed grade with a broader molecular weight distribution. On a 120 mm cast extruder, the broader distribution widens the shear-rate window before melt fracture appears, and the head pressure is typically lower. In exchange, metallocene octene-1 grades usually achieve better clarity and better organoleptic properties in 15 μm or thinner films. For applications where optical transmission and high seal strength are critical, metallocene octene-1 LLDPE may be preferred. For industrial stretch film, CM 406 is positioned as a balance of processability, puncture resistance, and tear resistance; this statement is supported by the mechanics of short-chain branching but should be confirmed with line-specific trials.

    Managing Screw Geometry, Melt Pump Placement, and Gauge Variation on Cast Lines

    On a 120 mm single-screw cast line with L/D 36:1 and a gear pump ahead of the screen changer, CM 406 is run with melt pump inlet pressure below 80 bar and pump discharge pressure below 150 bar when the die is 2 000 mm wide; these values are equipment-specific and not product guarantees. The gear pump stabilises throughput and minimises ±5% transverse gauge variation at 20 μm. A 60/80/100 mesh breaker-plate screen pack is typically used. When the recycled edge trim fraction exceeds 15 wt%, gauge variation increases and gel specks may appear because the edge trim has experienced additional thermal history and may carry low-level surface contamination. If gel counts exceed 15 gels per 100 cm² on 50 μm film as assessed by a dark-field optical scanner, the melt filter and screw should be inspected; this threshold is an operational action limit used on multi-layer cast lines, not a resin specification limit.

    Regulatory Boundary Conditions and Food-Contact Compliance Matrix

    For food-contact packaging, CM 406 may be evaluated under Commission Regulation (EU) No 10/2011 and under U.S. FDA 21 CFR 177.1520(c). The overall migration limit from the final film must not exceed 10 mg/dm² or 60 mg/kg depending on packaging geometry and food simulant. There is no separate specific migration limit for hexene-1 under EU 10/2011, but the finished film must meet the overall migration limit and organoleptic requirements. For U.S. compliance, the resin falls within the scope of olefin polymers under 21 CFR 177.1520(c), with use limitations and temperature/time conditions defined in 21 CFR 176.170(c). CM 406 is subject to REACH Regulation (EC) No 1907/2006 and does not intentionally contain perfluoroalkyl substances or phthalates. RoHS Directive 2011/65/EU applies only to electrical and electronic equipment, not to polyolefin packaging film, but packaging used in RoHS-compliant supply chains may impose additional heavy-metal limits.

    FrameworkApplicable ReferenceBoundary Condition
    EU food contactEU No 10/2011Overall migration below 10 mg/dm² or 60 mg/kg; simulant-dependent
    U.S. food contactFDA 21 CFR 177.1520(c)Olefin polymer use; conditions defined in 21 CFR 176.170(c)
    Chemical safetyREACH EC 1907/2006Registration and SVHC threshold compliance
    Heavy metalsRoHS 2011/65/EUApplicable to packaged electrical/electronic articles where relevant

    Storage of CM 406 pellets does not require predrying unless surface condensation exists after cold-warehouse transfer. If condensation appears, a hopper dryer set at 60–70 °C for 4–6 h removes surface moisture without fusing pellets. Long-term storage above 40 °C or under direct UV exposure can increase yellowness and additive migration; silos should be shaded and ventilated. During line startup, a transition from high-pressure LDPE or metallocene LLDPE to CM 406 is performed at 220–240 °C with a purge time of 10–15 min until the extrudate is free of gels and black specks. Direct transition at full die temperature of 260 °C can leave residual gels at the die exit because the previous resin may have lower thermal stability. Edge trim from CM 406 cast film may be re-pelletized and mixed at up to 15 wt% of the feed, provided the reclaim is of known thermal history and free of printed film or label adhesive. Above this level, the risk of gel formation and gauge variation increases on thin-gauge stretch film lines.

    Top