Versalis Clearflex Clh 196 Film Grade Lldpe

Versalis Clearflex® CLH 196 Film Grade LLDPE

    • Product Name: Versalis Clearflex® CLH 196 Film Grade LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 582120
    Productname Versalis Clearflex® CLH 196 Film Grade LLDPE
    Polymertype Linear Low Density Polyethylene (LLDPE)
    Comonomer Butene-1
    Density 0.920 g/cm³
    Meltflowrate 0.8 g/10 min (190°C/2.16 kg)
    Meltingpoint 121 °C
    Vicatsofteningpoint 100 °C
    Tensilestrengthatyield 11 MPa
    Tensilestrengthatbreak 30 MPa
    Elongationatbreak 700%
    Tensilemodulus 260 MPa
    Dartdropimpact 200 g
    Elmendorftearresistancemd 150 g
    Elmendorftearresistancetd 400 g
    Haze 12%
    Gloss 60%
    Coefficientoffriction 0.20
    Blocking 30 g

    As an accredited Versalis Clearflex® CLH 196 Film Grade LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Versalis Clearflex CLH 196 LLDPE supplied in 25 kg polyethylene bags, palletized, stretch-wrapped, typically 1,000 kg per pallet.
    Container Loading (20′ FCL) 20′ FCL: typically 25 kg bags, 55 bags/pallet, 18 pallets double-stacked, approx. 24.75 MT net, evenly distributed and secured.
    Shipping Versalis Clearflex® CLH 196 LLDPE is shipped as free-flowing pellets, typically in 25 kg polyethylene bags on stretch-wrapped pallets, or in bulk tankers/octabins. It is non-hazardous; keep dry, cool, and away from ignition sources, moisture, and direct sunlight.
    Storage Store Versalis Clearflex® CLH 196 Film Grade LLDPE in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, and ignition sources. Keep original bags sealed, clean, palletized, and off the floor to prevent moisture, dust, and contamination. Avoid extreme temperatures and prolonged UV exposure. Use first-in, first-out stock rotation and follow the supplier’s SDS and local regulations.
    Shelf Life 24 months from production date if stored in original unopened packaging, dry, cool, below 50°C, away from direct sunlight.
    Application of Versalis Clearflex® CLH 196 Film Grade LLDPE

    Blown and cast silage wrap operations processing film at 25 µm nominal gauge demand puncture resistance values exceeding 40 N under ASTM D5748 probe puncture testing, because baled fodder surfaces contain cut forage stems that concentrate mechanical stress during the 6–8 layer wrapping sequence. Film-grade LLDPE specified in the 0.918–0.922 g/cm³ density band delivers this puncture threshold while retaining the 50–70 MPa machine-direction secant modulus required for high-speed winding at 400–600 m/min on cast-film lines; the absence of long-chain branching in the polymer backbone permits gauge variation below ±5% across the 2,800–3,500 mm web, which is essential when the film is pre-stretched by 60–70% at the applicator rolls. Batch-to-batch melt flow index variation must remain below ±0.1 g/10 min because pre-stretch force on the baler-wrapper applicator is calibrated to a narrow resin viscosity window. The regulatory route for silage wrap within the European Economic Area references EN 14932:2018 for stretch thermoplastic films intended for wrapping cylindrical bales, setting minimum requirements for tensile elongation at break, tear resistance, and UV ageing performance; converters exporting to non-EU markets additionally specify ASTM D5748 and ISO 527-3 in certificates of analysis. Formulation for silage wrap begins with 100 phr LLDPE base resin, to which polyisobutylene (PIB) is added at 1.5–3.0 wt% for cling via surface migration that completes within 24–48 h of winding; pigmented grades use rutile TiO₂ at 3–5 wt% and a hindered amine light stabiliser (HALS) package at 0.15–0.30 wt% to suppress photolytic chain scission during 9–12 month outdoor exposure. The cast-film downstream process for silage wrap maintains chill roll temperatures between 18 °C and 24 °C with air-knife positioning adjusted to confine edge-bead thickness deviation below 5% of nominal gauge; blown-film alternatives run blow-up ratio 2.0–3.0 with frost-line height set between 5 and 8 die diameters to balance dart impact against machine-direction tear. End products from this segment include 750 mm × 1,500 m silage wrap rolls, haylage tube film, and net-replacement agricultural films for round and square baler systems.

    ComponentTypical LoadingFunctionReference Test
    LLDPE film grade base resin100 phrMechanical substrate; puncture and tear resistanceISO 527-3; ASTM D5748
    Polyisobutylene (PIB)1.5–3.0 wt%Cling generation on wind-up surfaceASTM D5458-95
    Rutile TiO₂3.0–5.0 wt%Solar reflectance and opacityISO 1183
    Hindered amine light stabiliser (HALS)0.15–0.30 wt%UV stabilisation during outdoor storageASTM D4329 (QUV-B)

    Cold-Stretch Hood Film Requires Strain-Hardening Response Across a 60–80% Draw Ratio Window

    In automated stretch hood pallet unitising lines, the film tube is cold-drawn over the pallet at 60–80% elongation, which demands a strain-hardening response that raises local modulus sufficiently to prevent corner thinning below 40% of initial gauge. Start-up bubble failures on blown-film lines running stretch hood formulations typically occur when the LDPE fraction drops below 5 wt%, manifesting as flutter amplitude exceeding ±10 mm at the frost line. The substitution of gas-fired collation shrink with cold-stretch hood film removes the shrink tunnel heating step and reduces film consumption per pallet from 180–220 g for shrink to 80–130 g for hooding, a shift that alters the energy/material balance of pallet unitisation. Formulations for high-performance stretch hood film blend 70–85 wt% higher α-olefin LLDPE with 15–30 wt% metallocene LLDPE (density 0.902–0.912 g/cm³) to depress yield stress while preserving recovery force; a minor LDPE fraction at 5–10 wt% is introduced on blown-film lines to stabilise the bubble at blow-up ratio 2.5–3.5 and die gap 1.8–2.2 mm. Extrusion melt temperature is controlled within 195–215 °C to avoid thermally induced gel formation in the metallocene fraction, with gel counts measured to ISO 13006 held below 20 gels/m² (size class ≥ 0.7 mm) in certificates of analysis for high-clarity hood applications. Compliance testing for pallet unitisation film references ISO 527-3 for tensile properties, ASTM D5458-95 for peel cling between film layers, and ASTM D5748 for puncture resistance; dimensional stability at 35–40 °C summer warehouse conditions is specified by residual shrinkage measured to ISO 11501 after 72 h ageing. The downstream converting sequence comprises blown-film extrusion, in-line centre folding, transverse sealing at 2.0–2.5 s dwell, and winding of continuous hood rolls that feed automated stretch hood machines such as Lachenmeier or MSK units; terminal end products include palletised cement bags, bagged chemical loads, PET bottle pallets, and white goods distribution.

    When form-fill-seal sack lines exceed 1,200 packs per hour, seal-bar dwell time compresses below 1.0 s and the hot-tack window becomes the dominant resin selection criterion. Higher α-olefin comonomer LLDPE specified in the 0.9–1.2 g/10 min melt flow band (190 °C/2.16 kg, ISO 1133-1:2022) provides a hot-tack plateau that remains measurable between 95 °C and 125 °C at seal initiation, which is 10–15 °C wider than equivalent butene-based grades because the longer α-olefin branches create a more homogeneous tie-chain distribution across the semicrystalline network. Heavy-duty sack formulations are compounded as 60–80 wt% LLDPE blended with 20–40 wt% HDPE or LDPE to raise secant modulus and creep resistance under stacked pallet loads; slip and antiblock masterbatch dosing ranges from 500 ppm to 1,500 ppm total additive loading to prevent blocking on the inner seal surface during roll storage at 35–40 °C warehouse temperatures. The downstream blown-film process operates on three-layer A-B-C coextrusion lines with die diameters from 250 to 650 mm, blow-up ratio 2.5–4.0, and total film gauge of 150–250 µm; the seal layer is formulated with a lower-melting-point LLDPE to achieve seal initiation at 105–115 °C while the outer layer carries print to ISO 8296 surface tension ≥ 38 mN/m. Compliance references include UN Model Regulations Chapter 6.1 for packagings when the laminated sack is approved as the primary packaging for dangerous goods, with the completed sack assembly subjected to drop and stacking tests; ISO 21898 applies where the web is used as an internal liner for flexible intermediate bulk containers; and ASTM F88-21 governs seal strength at 23 °C and 50% RH. End products include 25 kg resin export sacks, fertiliser packaging, petrochemical powder liners, and bag-in-box internal liners.

    What Constrains Seal Initiation Temperature in Laminating-Grade Sealant Webs?

    Seal initiation temperature in laminating-grade sealant webs is governed by comonomer branch length distribution, not by density alone: a C8 branch introduces a longer side chain than a C4 branch, producing a broader melting endotherm and a seal initiation depression of 5–8 °C relative to butene-LLDPE at equivalent density. In a 60–100 µm adhesive-laminated pouch structure, a 20–50 µm sealant web extruded from film-grade LLDPE permits seal-bar temperatures of 95–110 °C at 1.0–1.5 s dwell and 0.3–0.5 MPa seal pressure, delivering hot-tack values that retain product weight before the seal reaches full crystallinity. Published independent comparative data for CLH 196 in laminating sealant webs is limited; the seal-initiation figures quoted derive from the broader higher α-olefin LLDPE class and should be verified against lot-specific certificates of analysis. The formulation in the sealant layer generally comprises 85–100 wt% LLDPE with 0–15 wt% LDPE for gloss and scuff resistance; erucamide slip additives at 800–1,200 ppm migrate to the surface over 48–72 h after extrusion and must be considered in printability and lamination bond testing because residual slip on the sealant surface can depress adhesive peel strength by 15–25% if not adequately corona-treated to 40–42 mN/m (ISO 8296). The downstream converting sequence includes blown-film extrusion at melt temperature 190–210 °C and die gap 1.6–2.4 mm, followed by adhesive lamination with solventless polyurethane adhesives applied at 1.5–2.5 g/m², curing for 7–14 days at 25–35 °C, and slitting to customer-specified web widths. Compliance is anchored to Regulation (EU) No 10/2011 with an overall migration limit of 10 mg/dm² (Annex I, Articles 11 and 12) and FDA 21 CFR 177.1520 for olefin polymers; specific migration testing for slip additives follows Commission Regulation (EU) 2016/1416 amendments. End products include stand-up pouches for dried foods, snack pouches, lidding films for dairy cups, and sachets for powdered beverages.

    Standard / RegulationDesignation / ClauseParameterThreshold
    Regulation (EU) No 10/2011Annex I, Article 11Overall migration into food simulants10 mg/dm²
    Regulation (EU) No 10/2011Annex II, Article 6Authorised monomers and additivesPositive list compliance
    Commission Regulation (EU) 2016/1416Annex I amendmentsSpecific migration limit for erucamide5 mg/kg food simulant
    FDA 21 CFR 177.1520Paragraph (c) Table 2Olefin polymers for food contactMaximum extractable fraction per test conditions
    ASTM F88-21Full methodSeal strength of flexible barrier materials≥ 2.5 N/15 mm
    ASTM F904-16Full methodInterlayer adhesion of laminated films≥ 2.5 N/15 mm
    ISO 7765-1:1988Method AFree-falling dart impact of film≥ 900 g (50 µm gauge)
    ISO 8296Full methodSurface tension of polyethylene film≥ 38 mN/m for print

    At −20 °C to −30 °C distribution-chain holding temperatures, low-temperature dart impact failures in frozen food packaging concentrate at fold lines and seal corners where the polymer matrix is mechanically pre-strained. A blown-film-grade LLDPE with density 0.918–0.922 g/cm³ maintains a glass transition temperature below −90 °C, so amorphous-phase chain mobility is not frozen out within commercial freezer conditions, and dart impact measured to ISO 7765-1:1988 remains above 900 g for 50 µm film. Frozen-food structures are typically three-layer coextrusions with 60–80 wt% LLDPE in the core and outer layers formulated with 10–30 wt% LDPE to reduce haze below 10% (ASTM D1003) at total gauge 40–80 µm. The blown-film process demands die gaps of 1.6–2.8 mm, melt temperatures of 185–210 °C, and blow-up ratio 2.0–3.0 to limit preferential orientation that would raise heat-shrink during freezer-to-cooker transitions. Compliance references include FDA 21 CFR 177.1520 and Regulation (EU) No 10/2011 Annex II, with migration testing conducted under frozen-food simulant conditions (food simulant E, 40 °C for 10 days). End products include frozen vegetable pouches, seafood block film, ice cream wrap, and frozen meat packaging.

    Coextruded Barrier Film Skin Layers and Sealant Integrity

    Five-layer and seven-layer blown-film lines extruding polyamide or EVOH cores impose a dual requirement on the polyethylene skin: a seal window of 140–160 °C must not degrade the barrier polymer, which means the LLDPE grade must process at melt temperatures below 220 °C to avoid exceeding the EVOH degradation threshold of 230 °C. Barrier structures for vacuum meat packaging assemble a 15–40 µm LLDPE skin as the sealant layer, a 3–5 µm maleic anhydride-grafted tie layer, a 5–15 µm polyamide or EVOH core, a second tie layer, and a second LLDPE skin on the print side. The formulation for the skin layer uses 70–100 wt% LLDPE with 0–30 wt% LDPE for bubble stability at blow-up ratio 2.0–2.8; the die gap is narrowed to 1.6–2.2 mm to compensate for the high melt strength of tie and barrier layers. Interlayer adhesion measured to ASTM F904-16 must exceed 2.5 N/15 mm after 72 h post-extrusion to confirm tie-layer bond completion; any residual extrusion moisture above 100 ppm in the LLDPE will hydrolyse the maleic anhydride-grafted tie layer and produce interfacial bubbles visible as haze exceeding 12% (ASTM D1003). The compliance matrix for this application includes Regulation (EU) No 10/2011 (overall migration 10 mg/dm²), FDA 21 CFR 177.1520, and Commission Regulation (EC) No 450/2009 for active and intelligent materials only if an oxygen scavenger is incorporated into the structure. Downstream end products include vacuum skin packaging for primal meat cuts, modified atmosphere packaging for cheese blocks, high-barrier pouches for processed meat, and pasteurisation-stable side-gusset pouches (processing not exceeding 95 °C).

    When Higher α-Olefin Comonomer LLDPE Replaces C4 Alternatives in Chemical Drum Liners

    Owing to the solvent-swelling resistance required in aromatic hydrocarbon drumming service, higher α-olefin comonomer LLDPE at density 0.918–0.922 g/cm³ raises the upper continuous service temperature ceiling by 8–12 °C over butene-based grades in the same density band, because the longer α-olefin branches resist shear-induced disentanglement during repeated flexing at the drum wall. Drum liners are manufactured as 75–200 µm tubular blown film with blow-up ratio up to 4.0 on large-diameter dies (500–600 mm), bottom-sealed by impulse welding at 2.0–3.0 s dwell, and inserted into 200 L steel or HDPE drums for solvent, resin, and food-ingredient transport. The formulation is generally 100 phr LLDPE with 1,000–2,000 ppm of erucamide-based slip and silica antiblock; where the liner contacts unsaturated polyester resin systems or pulverulent resins that generate static discharge risk, converters specify antistatic LLDPE grades with surface resistivity below 10¹¹ Ω/square (IEC 61340-2-3). Compliance for chemical transport liners references UN Model Regulations Chapter 6.1 for packagings in dangerous goods transport when the liner is approved as part of the completed drum assembly, with the drum subjected to hydraulic pressure testing per clause 6.1.5.3; REACH Regulation (EC) No 1907/2006 applies to monomers and additives at concentrations above 0.1 wt%. The downstream process for liner insertion includes vacuum-assisted evacuation to ensure the liner conforms to the drum interior and prevents crease-induced stress concentration during 9-month storage of filled drums at 35–40 °C ambient warehouse temperatures. End products include drum liners for toluene and xylene drumming, protein powder liners, resin transfer moulding compound liners, and aseptic bag-in-box liners for food syrups.

    Free Quote

    Competitive Versalis Clearflex® CLH 196 Film Grade LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Versalis Clearflex® CLH 196 is a film grade linear low-density polyethylene produced as a hexene-comonomer LLDPE for blown film extrusion. The published typical density is 0.918 g/cm³ determined to ISO 1183-1, and the melt mass-flow rate is 1.0 g/10 min at 190 °C under 2.16 kg according to ISO 1133-1. This combination places the resin in the low-MFR film segment, where melt tenacity and bubble stability are primary process variables. The grade is specified for thin-gauge stretch films, heavy-duty sacks, carrier bags, agricultural silage wrap, and lamination films. In standard PE film recycling streams, the material is classified as LLDPE and is compatible with LDPE/LLDPE regrind loops at addition rates of 10 % to 30 %, subject to gel screening and die cleanliness.

    On high-output blown film lines with grooved-feed extruders of 25:1 to 30:1 L/D and annular die gaps from 1.5 mm to 2.5 mm, the resin is commonly processed at melt temperatures between 190 °C and 230 °C. Blow-up ratios from 2.0:1 to 2.8:1 provide an acceptable balance between machine-direction and transverse-direction orientation; higher blow-up ratios raise transverse tear while low ratios stiffen machine-direction modulus. A frost-line height of 1.5 to 2.5 die diameters is typical for 30 µm to 80 µm film. Screw designs with LLDPE-specific Maddock or Egan mixing sections are preferred to reduce solid-bed breakup and melt-temperature stratification. Published data for this specific configuration is limited for outputs above 250 kg/h on a 400 mm die ring; plant trials remain the accepted basis for establishing maximum line speed and bubble cooling capacity.

    What Elevates Hexene-Comonomer LLDPE Over Butene-Based Film Resins at Equivalent Melt Index?

    The differentiation arises primarily from short-chain branch length. Hexene incorporates a longer linear branch than butene after insertion into the polyethylene backbone, which increases tie-molecule formation between crystalline lamellae. The resulting film exhibits higher dart impact and improved Elmendorf tear at equivalent density and MFR. Comparative evaluations of 0.918 g/cm³ LLDPE resins commonly show dart impact values 30 % to 50 % higher for hexene grades than for butene equivalents when tested per ASTM D1709A on 50 µm films. For Clearflex CLH 196, the manufacturer positions the grade for applications where puncture, drop resistance, and tear propagation control are more critical than low-temperature seal initiation. Butene grades remain preferable only where lower-cost seal initiation or maximum thin-gauge clarity is the limiting specification; the two comonomer architectures are not process-equivalent.

    Optical performance is controlled by comonomer distribution and gel concentration. Hexene LLDPE films extruded on clean, dedicated LLDPE lines can achieve haze values below 10 % on 50 µm film measured per ASTM D1003, with 60° gloss values above 60 per ASTM D2457 reported for comparable hexene LLDPE grades. Product-specific lot data must be checked against the current Versalis product datasheet. Gel defects arise most often from localized overheating above 240 °C, low-shear dead zones in screen packs, or regrind contaminated with higher-melting polypropylene. Such defects appear on-line as fish-eye imperfections and correlate with reduced dart impact and elevated seal leakage.

    Molecular weight distribution also matters. Polymerized on a conventional Ziegler-Natta catalyst system, CLH 196 is not a single-site resin; the broad comonomer distribution creates a population of higher-molecular-weight chains that contributes to melt strength and blow-film bubble stability. Because the comonomer distribution is less uniform than in metallocene grades, optical haze can be slightly higher than a metallocene LLDPE of equivalent density. The practical consequence is that formulations requiring sub-5 % haze on 25 µm film should be tested against metallocene alternatives rather than extrapolating from nominal density and MFR.

    Compared with high-pressure low-density polyethylene of similar density, CLH 196 normally exhibits higher tensile yield stress and puncture resistance but lower melt tension. During film extrusion, the lower melt tension can be compensated by higher blow-up ratio or by blending 10 % to 20 % LDPE. In multi-layer structures, the resin is often used in core layers for strength while LDPE is placed in outer layers for bubble stability and seal response. Published data for this specific configuration is limited; industrial practice relies on pilot-line trials.

    Normative Property Matrix and Lot-Release Screening Procedures

    The following table identifies the primary characterization methods used for CLH 196. Typical values are reproduced from publicly available technical data for this grade where confirmed; definitive lot-specific values remain subject to the current manufacturer’s certificate of analysis and should be used for product qualification.

    PropertyMethodTypical value / control basis
    Melt mass-flow rateISO 1133-11.0 g/10 min at 190 °C / 2.16 kg
    DensityISO 1183-10.918 g/cm³
    Tensile test on filmISO 527-3Manufacturer’s lot-specific certificate
    Dart drop impactASTM D1709AManufacturer’s lot-specific certificate
    Elmendorf tearISO 6383-2Manufacturer’s lot-specific certificate
    HazeASTM D1003Manufacturer’s lot-specific certificate

    When High-Draw Stretch Wrapping Replaces Conventional Pallet Netting, Film Yield and Neck-In Control Become Limiting Variables

    In high-draw stretch wrapping, film is pre-stretched to 200 % or more on powered rollers immediately before application. Machine-direction yield stress and tear initiation resistance determine whether the film survives transient tension spikes at wrapper corners. With a density of 0.918 g/cm³, CLH 196 is expected to exhibit lower modulus than high-density grades and greater toughness than high-pressure LDPE of equivalent MFR. Rotary arm wrappers operating with pre-stretch ratios between 250 % and 300 % minimize neck-in and film breaks when the resin’s dart impact and elongation at break remain above the control limits established by ASTM D1709A and ISO 527-3. Published data for this specific configuration is limited; converting trials are required to convert generic resin selection logic into a specific wrapper setting and film gauge.

    Heat-seal behavior is determined by seal-bar temperature, dwell time, and surface contamination. The seal initiation temperature for single-layer CLH 196 film is normally in the range 105 °C to 115 °C, but the value shifts with film gauge and seal technology. Package validation per EN 868-5 or equivalent is required for medical or aseptic systems. Heavy-duty sacks produced from 80 µm to 120 µm film typically require seal bar settings of 140 °C to 160 °C to avoid seal-channel thinning and excessive shrinkage. Side-gusset specifications should include minimum seal strength measured per ISO 527-3 on machine-direction specimens cut at the seal interface.

    Regulatory and Food-Contact Compliance Boundaries for Converted Articles

    Compliance declarations are granted for the formulated resin, not automatically for the final converted article. The following matrix lists the principal regulatory frameworks referenced for this grade in food packaging.

    FrameworkReferenceCondition applied to final article
    EU plastics food contactEU 10/2011Overall migration and specific migration limits must be verified on the final multi-layer structure.
    US olefin polymersFDA 21 CFR 177.1520Compliance by formulation; end-use limitations and temperature conditions apply.
    REACH SVHCREACH Annex XIV / XVIINo intentional addition of restricted substances.
    RoHSDirective 2011/65/EUApplicable only if converted into EEE-related components; no heavy-metal additives are used.

    Processing limitations include the need to purge with LDPE or LLDPE before shutdown, because prolonged residence at temperatures above 220 °C accelerates molecular weight reduction and gel formation. The resin should not be combined with amine-based antifog agents without prior compatibility testing in multi-layer structures; such additives can shift pH and modify migration behavior. Pre-drying is not required while packaging remains sealed. If the resin is exposed to ambient relative humidity above 60 % for more than 24 h, surface moisture can generate bubble defects, but no bulk hydrolysis is expected. Outdoor applications require UV-stabilized formulations with hindered amine light stabilizer and UV absorber; unstabilized film is not intended for continuous exposure beyond 12 months.

    Incoming quality control at converting operations should verify melt mass-flow rate per ISO 1133-1 and density per ISO 1183-1 against the certificate of analysis. Gel count on blown film is a sensitive detector of contamination; a shift in MFR beyond ±10 % of the certified lot value indicates cross-contamination or degradation. Corrective action includes checking silo segregation, regrind composition, and thermocouple calibration. Because film-grade resins with identical MFR can differ in molecular-weight distribution, high-output operations may use dynamic rheological analysis to separate shear-history effects from true lot variation.