Versalis Clearflex Cl 106 Hexene Copolymer Linear Low Density Polyethylene

Versalis Clearflex® CL 106 Hexene Copolymer Linear Low Density Polyethylene

    • Product Name: Versalis Clearflex® CL 106 Hexene Copolymer Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 629599
    Polymertype Linear Low Density Polyethylene (LLDPE)
    Comonomer Hexene-1
    Density 0.919 g/cm³
    Meltflowrate 190c 2 16kg 0.7 g/10 min
    Meltingpoint 124 °C
    Vicatsofteningtemperature 100 °C
    Tensilestrengthatyield 10 MPa
    Tensilestrengthatbreak 25 MPa
    Elongationatbreak 700 %
    Flexuralmodulus 260 MPa
    Hardness Shored 50
    Brittlenesstemperature < -70 °C
    Waterabsorption < 0.01 %

    As an accredited Versalis Clearflex® CL 106 Hexene Copolymer Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Typically supplied as pellets in 25 kg polyethylene bags; also available in 1000 kg bulk bags or bulk quantities.
    Container Loading (20′ FCL) 20′ FCL: Versalis Clearflex® CL 106 LLDPE hexene copolymer in palletized 25-kg bags, moisture-protected, securely stowed, max payload ~22 MT.
    Shipping Versalis Clearflex® CL 106 is typically shipped as non-hazardous polyethylene pellets in sealed 25 kg bags or octabins, palletized and stretch-wrapped. Transport in clean, dry, covered trucks, railcars, or containers at ambient temperature. Protect from moisture, direct sunlight, heat, and ignition sources. No UN dangerous-goods classification applies.
    Storage Store Clearflex® CL 106 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, and open flames. Keep original packaging closed, palletized, and off the ground to prevent moisture and contamination. Separate from strong oxidizers and incompatible materials. Use first-in, first-out stock rotation. Follow the manufacturer’s SDS and local regulations for safe storage.
    Shelf Life Shelf life is typically two years when stored unopened in a cool, dry, ventilated area, away from direct sunlight and moisture.
    Application of Versalis Clearflex® CL 106 Hexene Copolymer Linear Low Density Polyethylene

    On three-layer blown film lines equipped with grooved feed extruders of L/D 32:1 and barrier screws, Versalis Clearflex® CL 106 is run in the core and inner layers of heavy-duty shipping sacks and FIBC liners. Supplier-published typical density is 0.918 g/cm³ per ISO 1183-1:2019, and melt mass-flow rate is 1.0 g/10 min at 190°C/2.16 kg per ISO 1133-1:2022. In converter practice the die gap is held at 2.0 mm to 2.5 mm and melt temperature is controlled within 190°C to 215°C. A typical formulation uses 70 wt% CL 106, 20 wt% butene-copolymer LLDPE, 5 wt% carbon black masterbatch, and 5 wt% processing aid masterbatch. The carbon black loading is determined by ultraviolet exposure during outdoor storage. Frost line height is set between 1.5 and 2.5 die diameters with a blow-up ratio of 2.2:1 to 2.8:1. This balance controls machine-direction tear and cross-direction dart impact. Dart impact is measured by ASTM D1709 Method A, Elmendorf tear by ASTM D1922, and puncture resistance by ASTM D5748. On production lines, melt temperatures above 220°C increase oxidation-induced gel counts and reduce tear resistance, while temperatures below 185°C raise melt pressure and produce gauge bands at the die lip. Die lip gaps below 2.0 mm have been observed to initiate herringbone melt fracture in the outer skin layer under high-shear die land conditions. Terminal articles include FIBC liners, granular fertilizer sacks, and heavy-duty refuse bags. Heat seal strength is tested according to ASTM F88 with seal bar temperature set between 115°C and 145°C depending on line speed and film thickness.

    What Limits Draw Resonance in Cast Film Lines Running CL 106-Rich Blends?

    Cast stretch film downgauging below 12 µm is limited by draw resonance and edge neck-in when CL 106 is used as the primary hexene-copolymer component. A machine-direction oriented stretch film core layer is compounded with 50 wt% CL 106, 30 wt% metallocene hexene LLDPE, 10 wt% LDPE, and 10 wt% additive masterbatch containing anti-block and slip agents. The LDPE fraction is maintained not as a toughness modifier but as a long-chain branching source that reduces neck-in and stabilizes the melt curtain. Extrusion is performed with a cast film die lip gap of 0.5 mm to 0.7 mm, a chill roll temperature of 18°C to 25°C, and an air gap of 15 mm to 25 mm. Draw resonance appears as periodic gauge variation in the machine direction when the draw ratio exceeds the melt strength of the blend. Published data for this specific CL 106-rich configuration is limited; line trials are required to establish the upper draw ratio because die lip geometry, melt temperature, and quenching rate dominate. Neck-in is quantified by measuring film width reduction at the die edges. Cling and stretch performance are evaluated with ASTM D5458 and puncture with ASTM D5748. Tensile properties after stretching are measured according to ISO 527-3. In high-speed cast lines running above 400 m/min, edge trim can exceed 10% of die width when the CL 106 fraction is over 50 wt%; reduction of the CL 106 fraction to 30 wt% and increase of LDPE to 20 wt% are typical process adjustments, but ultimate puncture resistance falls accordingly. Terminal articles include pallet stretch film and machine-direction oriented wrapping film where puncture resistance is measured by ASTM D5748 and cling by ASTM D5458.

    Food Contact Sealant Webs Where Hexene LLDPE Governs Seal Strength

    In coextruded food packaging, CL 106 is placed in the sealant layer at 20 µm to 40 µm thickness against ethylene-vinyl alcohol or polyamide barrier layers. The hexene-copolymer architecture gives a lower seal initiation temperature than butene-copolymer LLDPE of equivalent density, but the exact value is line-dependent and should be confirmed by differential scanning calorimetry under ISO 11357-3:2018. Melt temperature in the sealant extruder is controlled between 195°C and 210°C; die gap is maintained at 1.8 mm to 2.2 mm with a blow-up ratio of 2.0:1 to 2.5:1. Hot tack is measured according to ASTM F1921, seal strength according to ASTM F88, and puncture resistance according to ASTM D5748. The sealant layer must not be exposed to retort conditions above 121°C because seal interface thinning and barrier delamination occur at higher thermal loads. A compliance matrix for this application is given below.

    RequirementStandard or regulationTest conditionLimit or specification
    EU overall migrationRegulation (EU) 10/2011, Annex IFood simulant D1, 40°C, 10 d10 mg/dm²
    US food contactFDA 21 CFR 177.1520(c)Olefin polymer, extraction testCompliance per section
    REACH SVHCEC 1907/2006Candidate List substances0.1 wt%
    Seal strengthASTM F88Seal bar 130°C, 0.5 s dwellMinimum seal strength as specified by converter

    High seal bar temperatures above 160°C cause the sealant layer to extrude from the seal area and create weak edge tear propagation. Substrate moisture above 60% relative humidity before extrusion requires pre-drying of hygroscopic barrier layers to prevent steam-induced bubble defects in the sealant web. Terminal articles include lidding films, frozen food pouches, and dry food inner liners.

    Where agricultural greenhouse films are specified for 24-month exposure in high-ultraviolet environments, CL 106 is used as the base resin in a three-layer structure at 60 wt% of the core layer. The outer layer is formulated with 20 wt% LDPE and 10 wt% UV stabilizer masterbatch; the inner layer contains 5 wt% hindered amine light stabilizer masterbatch and 5 wt% anti-fog masterbatch. Film thickness is maintained between 150 µm and 200 µm. Extrusion is performed on blown film lines with internal bubble cooling, die diameters of 350 mm to 500 mm, die gap 2.0 mm to 2.5 mm, and a blow-up ratio of 2.5:1 to 3.0:1. Artificial weathering is evaluated according to ISO 4892-2; tensile properties after ageing are measured by ISO 527-3. Products are certified against EN 13206 for greenhouse covering films where mechanical retention after weathering is a defined threshold. Sulfur-burning vapor used for fungal control in some growing environments can deplete the hindered amine stabilizer system; exposure to sulfur combustion products should be considered in stabilizer masterbatch loading. Direct contact with agrochemicals containing halogens leads to surface crazing if not rinsed from the film. Terminal articles include greenhouse covers, low tunnels, and mulch films where tear propagation resistance is measured by ASTM D1922.

    Extrusion Lamination of Liquid Packaging Structures with CL 106

    CL 106 is applied as a laminating web in liquid packaging structures where the polymer is extruded between paperboard and aluminium foil or between foil and heat-sealable film. Processing is carried out on a single-screw extruder with L/D 30:1 and a flat die gap of 0.6 mm to 0.8 mm. Melt temperature at the die lip is controlled between 280°C and 320°C. This temperature range is required to achieve adhesion to the aluminium foil but also promotes oxidative chain scission if residence time exceeds 5 min. The melt curtain is treated with ozone and the substrate is corona-treated immediately before lamination. Peel adhesion is measured according to ASTM F904. Neck-in on this grade is higher than on LDPE coating grades; die width must be oversized by at least 10% to 15% relative to the substrate width. Edge trim is recycled into the extruder only after regrind is dried below 0.05% moisture. Published data for CL 106 in high-temperature extrusion lamination is limited, so pilot line trials under the target line speed and adhesion specification are required before production scale-up. Terminal articles include aseptic drink cartons, liquid packaging pouches, and multi-layer paperboard laminates.

    When Collation Shrink Film Requires Balanced Machine- and Cross-Direction Shrinkage

    In collation shrink film for bottled beverages, CL 106 is blended at 20 wt% to 40 wt% into a LDPE-rich matrix to increase puncture and tear resistance without eliminating the high shrinkage required for bottle bundle conformity. The blown film bubble is run at a blow-up ratio of 2.5:1 to 3.0:1 and a frost line height of 3 to 5 die diameters to orient the film in both axes. Shrinkage is tested in oil at 120°C and 140°C according to ASTM D2732. Exceeding 40 wt% CL 106 reduces machine-direction shrinkage below converter targets because the hexene-copolymer chains retain greater melt memory and resist orientation. Melt temperature is kept between 190°C and 205°C; lower temperatures increase melt viscosity and create bubble instability, while higher temperatures reduce orientation and lower shrink tension. Additive masterbatch containing anti-block and slip agents is held at 2 wt% to 3 wt% to avoid blocking on rewind. Terminal articles include shrink bundles for PET bottles, multipack wraps, and can collations where tear propagation resistance is measured by ASTM D1922 and puncture by ASTM D5748.

    Free Quote

    Competitive Versalis Clearflex® CL 106 Hexene Copolymer Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Versalis Clearflex® CL 106 is a 1-hexene copolymer linear low density polyethylene intended principally for blown film conversion. The resin carries a nominal density of 0.918 g/cm³ determined according to ISO 1183-1:2019 and a melt flow rate of 1.0 g/10 min at 190 °C/2.16 kg according to ISO 1133-1:2022. The 1-hexene comonomer introduces butyl short-chain branches along the polyethylene backbone; this molecular architecture differentiates CL 106 from butene-based LLDPE grades that carry ethyl branches and from octene-based grades that carry hexyl branches. The comonomer length and non-uniform distribution affect lamellar thickness distribution, tie-molecule concentration, low-temperature seal behaviour, and the balance between machine-direction and transverse-direction tear propagation. The melting peak observed by differential scanning calorimetry under ISO 11357-3 at 10 K/min typically falls between 118 °C and 126 °C for a C6 LLDPE of this density. The grade is supplied as pelletized reactor product and is normally stabilized for film extrusion; specific slip and antiblock loadings are selected by the converter according to film gauge and downstream packaging line requirements.

    How Does the Hexene Comonomer Affect Tie-Molecule Population and Tear Balance?

    The incorporation of 1-hexene reduces the linearity of the polyethylene backbone without increasing short-chain branch frequency to the level that would excessively depress crystallinity. Compared with a butene-based LLDPE at equivalent density and melt flow rate, the longer butyl branches generated by hexene incorporation are more effective in forming load-bearing tie molecules between crystalline lamellae. As a result, films produced from CL 106 generally show higher dart impact strength and improved puncture resistance than C4 LLDPE films of the same thickness. The effect is measurable at 25 µm under ASTM D1709 or ISO 7765-1, but published comparative data show that the absolute improvement depends on die gap, blow-up ratio, frost line cooling rate, and additive package. Because the comonomer distribution in conventional Ziegler-Natta resins is non-uniform, the seal initiation temperature is also reduced relative to many butene-based grades, although metallocene-catalysed C6 or C8 LLDPE can provide a narrower composition distribution and further seal improvement. The operational consequence is that the lower crystalline content and longer branch architecture modify the bubble stability envelope. Converters experienced with C4 LLDPE must re-evaluate frost line height and internal bubble cooling settings before increasing output; otherwise gauge variation and bubble oscillation can become the limiting defects.

    On blown-film lines equipped with grooved-feed single-screw extruders of 24:1 to 30:1 L/D and barrier screws, melt temperature at the die entry is generally maintained between 190 °C and 230 °C. A die gap of 1.5 mm to 2.5 mm is typical for gauge control. Wider gaps increase melt residence time and may raise gel formation during prolonged runs; narrower gaps raise die pressure and require higher melt temperature. Blow-up ratios from 2.0:1 to 3.0:1 and frost line heights in the range of 6 to 10 die diameters are used for balanced film properties. At frost line heights below 5 die diameters, the film surface may show elevated blocking or reduced gloss. At frost line heights above 12 die diameters, bubble stability frequently deteriorates and gauge variation may exceed ±2 µm on 25 µm film. Internal bubble cooling and automatic air ring control are required for stable operation below 20 µm; without these devices, freeze-line oscillation and tension-induced MD thickness variation become primary yield losses. The polymer does not require predrying in closed silo storage; however, when ambient relative humidity exceeds 60%, surface moisture adsorbed onto cold pellets can produce bubble pinholes. In such cases, a hopper dryer set at 70 °C to 80 °C for 2 h to 3 h is used. Melt temperatures above 250 °C should be avoided to limit oxidative chain scission and gel formation.

    Comparative Film Property Benchmarks at 25 µm Blown Film

    Published data for this specific configuration is limited; however, typical film property ranges for C6 Ziegler-Natta LLDPE with density 0.918 g/cm³ and MFR 1.0 g/10 min can be used as a preliminary engineering estimate. Tensile elongation at break measured on 25 µm film according to ISO 527-3 is generally above 600% in the machine direction. Dart drop impact strength under ASTM D1709 Method A is commonly reported between 80 g and 150 g for such resins, with the exact value controlled by frost line height, die gap, and additive package. Elmendorf tear strength according to ISO 6383-2 is strongly anisotropic: machine-direction tear values are commonly lower than transverse-direction values by a factor of 2 to 4, and blow-up ratio reduction below 2.0:1 further depresses MD tear. Haze measured by ISO 14782 on 25 µm film is typically below 10% for well-stabilized C6 LLDPE; the grade should not be considered a clarity-grade metallocene replacement where haze below 5% is required. Hot-tack and seal strength are governed by ASTM F1921 and ASTM F88, respectively. Seal initiation temperatures near 95 °C to 105 °C are reported for hexene LLDPE films depending on seal bar geometry, dwell time, and contact pressure.

    If High Puncture Resistance and Downgauging Are Simultaneous Constraints

    Where downgauged stretch film is the target structure, puncture resistance and elastic recovery are evaluated on blown film lines at blow-up ratios near 2.5:1 to 3.0:1 to shift the tear balance toward the transverse direction. CL 106 is normally blended with LDPE at 10% to 30% by weight to increase melt strength and bubble stability. Higher LDPE addition reduces dart impact and raises haze, so the blend ratio is a process-dependent compromise between gauge stability and puncture performance. In agricultural films, the grade is formulated with hindered amine light stabilizers and carbon black or UV absorbers; screw design and residence time must be controlled to avoid additive degradation. The film property scatter at gauge below 15 µm is strongly influenced by cooling air temperature and internal bubble cooling efficiency, not by resin melt flow rate alone. Published data for this specific configuration is limited, and converter trials are required to confirm final gauge, cling, and puncture performance.

    Regulatory Compliance and End-Use Boundary Conditions

    Food-contact applications require confirmation against the current revision of FDA 21 CFR 177.1520(c) and Commission Regulation (EU) No 10/2011. The overall migration limit of 10 mg/dm² specified in EU food-contact legislation applies to the finished film after conversion; the actual migration depends on film thickness, food simulant, contact time, and temperature. For fatty food simulants, migration testing is performed with simulant D2 or D1 under the conditions prescribed in Annex III and Annex V of Regulation (EU) No 10/2011. The resin is subject to REACH Regulation (EC) No 1907/2006 registration duties; converters must verify that any formulated masterbatch, ink, or adhesive used with the resin does not introduce substances above the threshold specified for the intended food-contact application.

    Regulation/StandardScopeRelevant Condition
    FDA 21 CFR 177.1520(c)Olefin polymers in food-contact articlesCompliance depends on food type and temperature
    EU Regulation No 10/2011Plastic materials and articles intended to contact foodOverall migration ≤ 10 mg/dm²
    REACH (EC) No 1907/2006Registration, evaluation, authorisation of chemicalsConfirm substance status with current Candidate List

    The resin should not be dry-blended with high levels of organic peroxide concentrates because peroxide-induced macroradical formation can promote premature crosslinking and gel formation at standard blown film temperatures. It is not intended for use in medical implants or high-temperature sterilization above 121 °C unless the converter has validated the finished packaging structure for those specific conditions. Compared with butene-based LLDPE grades, the hexene comonomer in CL 106 provides a different processing latitude at low thickness because the longer branch population increases tie-chain density without the high gel levels associated with peroxide-modified materials. The main operational difference on existing equipment is that temperature and frost line settings optimized for C4 LLDPE do not transfer directly; the bubble may show greater oscillation sensitivity until internal bubble cooling is adjusted. Compared with octene-based LLDPE, CL 106 may exhibit lower ultimate dart impact at the same density and melt flow rate but remains suitable for agricultural and heavy-duty shipping sacks where seal bar temperatures above 105 °C can be maintained. The melt flow rate of 1.0 g/10 min places the grade outside high-flow injection molding use; the product is specifically intended for film extrusion and should not be substituted into injection molding applications requiring MFR values above 5 g/10 min.

    Top