| HS Code | 183003 |
| Density | 0.919 g/cm3 (typical) |
| Melt Flow Rate | 1.0 g/10 min (190°C/2.16 kg) |
| Melting Point | 120°C |
| Vicat Softening Point | 95°C |
| Tensile Strength At Break | 30 MPa |
| Elongation At Break | 700% |
| Dart Drop Impact | 120 g |
| Elmendorf Tear Strength Md | 250 g |
| Elmendorf Tear Strength Td | 350 g |
| Haze | 12% |
| Gloss | 80% |
| Processing Method | Blown Film |
| Additives | Antioxidant |
| Slip Agent | No |
| Antiblock Agent | No |
| Recommended Film Thickness | 25 µm |
As an accredited Versalis Clearflex® CHH 196 Film Grade LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Versalis Clearflex CHH 196 LLDPE supplied in 25 kg polyethylene bags, palletized and stretch-wrapped for secure transport. |
| Container Loading (20′ FCL) | Versalis Clearflex® CHH 196 Film Grade LLDPE, 25 kg bags, loaded and secured in a 20′ FCL for ocean transport. |
| Shipping | Versalis Clearflex® CHH 196 Film Grade LLDPE is shipped as solid, non-hazardous polyethylene pellets in 25 kg bags or bulk containers. Pallets are stretch-wrapped and labeled. Transport in clean, dry trucks or containers, protected from heat, sunlight, moisture, and contamination. Follow SDS and local regulations. |
| Storage | Store Versalis Clearflex® CHH 196 Film Grade LLDPE in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, and flames. Keep in original sealed packaging on pallets to prevent moisture, dust, and contamination. Avoid excessive stacking and prolonged UV exposure. Maintain good housekeeping and follow the supplier’s safety data sheet and local regulations. Store separately from incompatible substances. |
| Shelf Life | Shelf life is 24 months from production when stored in original packaging in a cool, dry, ventilated area, away from direct sunlight and heat. |
In three-layer high-clarity food packaging operations, Clearflex CHH 196 is run as the core or non-seal skin layer at melt discharge temperatures of 210–230°C, die gaps of 1.8–2.2 mm, and frost line heights of 350–550 mm above the die face. The nominal density of 0.918 g/cm³ tested to ISO 1183-1:2019 and the melt flow rate of 1.0 g/10 min tested to ISO 1133-1:2022 provide a balance between bubble strength and drawdown in thin-gauge film. The frost line is maintained with an external dual-lip air ring supplying air at 8–15°C, while the blow-up ratio is held between 2.3:1 and 3.0:1 to reduce gauge variation. If the frost line falls below 300 mm, the quench rate increases film yield stress and lowers dart impact at thin gauges; if the frost line rises above 600 mm, bubble instability creates gauge bands outside ±5%. Recycle levels should not exceed 25 wt% because repeated extrusion at these temperatures raises gel counts and visible defects in film from 30 µm to 80 µm. Food-contact status must be confirmed on the finished printed laminate because Regulation (EU) No 10/2011 sets an overall migration limit of 10 mg/dm², and 21 CFR 177.1520 covers olefin polymers used in contact with food. Haze and light transmission are measured to ASTM D1003-21; published values for this specific grade in commercial films vary with die land length, die temperature variation, and additive package, so converter-specific verification is necessary.
Dart impact retention in heavy-duty shipping sacks and bag-in-box liners depends primarily on film gauge uniformity, comonomer distribution, and the concentration of high-pressure LDPE used for bubble stability. A dry blend containing 70 wt% Clearflex CHH 196 and 30 wt% LDPE with a melt flow rate of 0.25 g/10 min is processed on a 90 mm grooved-feed single-screw extruder with 30:1 L/D and a dual-lip air ring. Melt discharge temperature is held at 215–240°C, die gap at 2.0–2.5 mm, and blow-up ratio at 2.0:1–2.8:1 for film gauges from 100 µm to 180 µm. The LDPE component stabilizes the bubble and raises melt strength, but also increases die pressure. A pressure transducer placed upstream of the screen changer typically records 350–480 bar; sustained readings above 520 bar indicate screen pack blinding and require changing the 60/80/100 mesh screen pack. Gauge variation across the bubble should be controlled to ±7% at 120 µm because dart impact under ASTM D1709-22 Method B is highly sensitive to local thickness reduction. Tear propagation is measured to ASTM D1922-23, puncture resistance to ASTM D5748-19, and filled bag drop testing to ASTM D5276-19 or ISO 7965-1. Converter-specific acceptance thresholds apply because drop resistance depends on seam geometry, fill material, and storage humidity. Published statistical data for this specific Clearflex CHH 196/LDPE blend is limited; lower control limits should be generated from production trials on the intended line.
| Standard or regulation | Scope | Relevant application |
|---|---|---|
| ISO 1133-1:2022 | Melt flow rate, 190°C, 2.16 kg | Incoming lot verification for all film sectors |
| ISO 1183-1:2019 | Density, immersion method | Material identification |
| ASTM D1709-22 | Dart impact, Method A/B | Food packaging, heavy-duty sacks |
| ASTM D1922-23 | Elmendorf tear propagation | Sacks, freezer film |
| ASTM D1894-21 | Static/kinetic COF | Cast stretch wrap, lamination |
| ASTM F2029-16 | Seal initiation temperature | Lamination sealant webs |
| ASTM F1921-12 | Hot tack | Lamination, VFFS |
| ASTM F88-21 | Seal strength | Pouch and bag seals |
| Regulation (EU) No 10/2011 | Overall migration limit 10 mg/dm² | Food-contact packaging |
| 21 CFR 177.1520 | Olefin polymers for food contact | US food packaging |
| EN 13206 | Agricultural film durability | Greenhouse covers |
Because cast film quench rates govern cling additive migration, Clearflex CHH 196 is run on multi-layer cast lines with chilled roll temperatures held between 18°C and 25°C. The melt discharge temperature is set at 240–270°C, the die-to-chill-roll gap at 25–45 mm, and the line speed at 400–600 m/min for film thicknesses of 10–20 µm. Cling is generated by dosing polyisobutylene or sorbitan monooleate at 0.5–1.2 wt% into the surface layer through gravimetric feeders. If chill roll temperature exceeds 30°C, the slower post-extrusion crystallization traps the cling additive in the amorphous phase and reduces surface tack. Static and kinetic coefficient of friction are measured to ASTM D1894-21; machined steel sled surfaces are used because steel-to-film COF is most relevant for pallet wrap. Kinetic COF is typically maintained between 0.20 and 0.30, while static COF above 0.50 can generate blocking at high-speed unwinds. Stretch force and load retention are validated on a wrap rig according to ASTM D5458-08 or equivalent; tensile elongation at break to ISO 527-3 commonly exceeds 300% in machine direction at 15 µm. Multilayer structures may place a stiffer LLDPE or LDPE core adjacent to two cling skins to control modulus and pre-stretch. Published data for this specific configuration is limited because cling performance depends on chill roll surface finish, air knife position, and film winding tension.
Agricultural greenhouse films made with Clearflex CHH 196 require a stabilizer package that remains effective under high UV radiation and sulfur exposure. A typical formulation uses hindered amine light stabilizers at 0.8–1.5 wt%, a triazine or benzophenone UV absorber at 0.2–0.5 wt%, and an acid absorber at 0.05 wt%. Sulfur-based pesticides can migrate into polyolefin film and deactivate certain nickel quenchers; when sulfur exposure is expected, a sulfur-resistant HALS package is selected and metal stearate concentrations in the skin layer are held below 0.1 wt%. The film is coextruded on a three-layer blown line at melt temperatures of 210–240°C, die gap of 2.0–2.4 mm, and blow-up ratio of 2.5:1–3.2:1. Film thickness ranges from 150 µm to 200 µm for multi-season greenhouse covers. Silica antiblock is added to the skin layers at 0.1–0.3 wt% to prevent roll blocking during high-humidity storage. Internal bubble cooling is used with frost line heights of 600–900 mm to stabilize the tall bubble at high output. Light transmission in the photosynthetically active region is measured to EN 13206; accelerated weathering is conducted to ISO 4892-2:2013 with irradiance of 65 W/m² at 340 nm for a minimum of 2000 h as a screening test. Field service life claims require multi-season trials because condensation, mechanical wear at arch contacts, and agrochemical exposure differ by region.
Clearflex CHH 196 is placed as a sealant web in solventless adhesive laminates to BOPP, PET, and metallized substrates. Seal initiation temperature is measured to ASTM F2029-16 using a heat-seal tester at 0.5 N/mm² sealing pressure and 0.5 s dwell. Hexene-based LLDPE sealant films at 40 µm frequently exhibit seal initiation between 95°C and 110°C, but actual values shift with slip and antiblock loadings, film gauge, and seal jaw alignment. Hot-tack force is measured to ASTM F1921-12, and seal strength to ASTM F88-21. Corona treatment is applied before lamination to raise surface energy above 38 mN/m; a 2.5 kW generator treating a 400 mm web at 100 m/min commonly produces 42–46 mN/m when checked with test inks conforming to ISO 8296. If slip additives are included, wait 24–48 h after film production before measuring COF or heat-seal properties because erucamide migration changes both surface friction and seal initiation. Seal bar temperatures above 130°C can cause seal burnout in thin-gauge laminates because the outer substrate can shrink before the sealant flows. Lower-temperature sealing is an advantage in high-speed form-fill-seal lines where dwell time is below 0.5 s, but heat-seal strength after hot filling must be verified with the filled product.
Deep-freeze packaging lines running Clearflex CHH 196 at film thicknesses below 60 µm require dart impact testing after conditioning at −18°C for 24 h because failure mode can shift from ductile to brittle under rapid quench. The film is coextruded on a 55 mm extruder with oscillating haul-off at melt temperatures of 205–225°C, die gap of 1.8–2.2 mm, and blow-up ratio of 2.2:1–2.8:1. High-density skin layers may be added to control coefficient of friction and improve heat-seal integrity. Cold-temperature bag drop testing is conducted to ASTM D5276-19 after filled bags are conditioned at −18°C for 24 h. Seal integrity in vertical form-fill-seal machines requires hot-tack force above 2 N at 115°C when dwell time is below 0.3 s; leaker formation occurs if the sealant layer has not fully wet the sealing bar surface. Melt temperatures above 230°C during extrusion promote oxidative degradation that increases gel counts in frozen food film, while temperatures below 195°C produce surface melt fracture on polished dies. The end product is used for IQF vegetables, frozen meat portions, and frozen seafood packaging where puncture resistance to ASTM D5748-19 and tear resistance to ASTM D1922-23 are converter-specific release criteria.
Competitive Versalis Clearflex® CHH 196 Film Grade LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Versalis Clearflex® CHH 196 is a metallocene-catalysed ethylene-1-hexene linear low-density polyethylene supplied as a film-grade pellet. The product model CHH 196 designates a hexene-comonomer LLDPE in the Clearflex® range; it is specified by density 0.918 g/cm³ (ISO 1183-1) and melt mass-flow rate 1.0 g/10 min at 190 °C under 2.16 kg (ISO 1133-1:2022). Differential scanning calorimetry gives a melting peak of 121 °C (ISO 11357-3). The grade is used in monolayer and coextruded blown and cast film structures where dart impact, tear propagation resistance, optical haze, and extractable content relevant to food-contact compliance are required simultaneously. The C6 branch length separates this material from conventional butene-based C4-LLDPE in property balance; when films of 25 µm are tested under ASTM D1709/A and ASTM D1922, the C6 architecture typically delivers higher dart-drop and tear values at equivalent density and MFR. Published data for this specific configuration is limited in open databases; the manufacturer’s current technical datasheet remains the controlling lot-release document.
| Property | Test method | Typical value | Unit |
|---|---|---|---|
| Density | ISO 1183-1 | 0.918 | g/cm³ |
| Melt mass-flow rate | ISO 1133-1:2022 | 1.0 | g/10 min |
| Melting peak | ISO 11357-3 | 121 | °C |
Polyethylene grades of identical density and melt index can differ substantially in solid-state fracture behaviour because of short-chain branch length and the breadth of the comonomer distribution. CHH 196 is produced with a metallocene catalyst; the resulting molecular weight distribution is narrower than that of Ziegler-Natta LLDPE, with Mw/Mn values for this family below 3.0 compared with 3.5 to 5.0 for conventional C4 grades. The low-molecular-weight tail is reduced, which lowers the concentration of chains that plasticise the amorphous phase, migrate under seal-jaw heat, and contribute to hexane-soluble extractables. The comonomer branch length is C6, not C4; at equivalent density, longer branches are less effective at disrupting crystallinity, so the crystalline lamellae remain more interconnected by tie molecules. Under ISO 11357-3, crystallinity for a density of 0.918 g/cm³ is typically 45–50%; this leaves a substantial amorphous fraction available for load transfer if tie-chain concentration is preserved. The practical consequence in film conversion is that ASTM D1709/A dart-impact and ASTM D1922 Elmendorf tear values are less anisotropic than in butene-based LLDPE, especially below 25 µm. This structural distinction also alters the heat-seal response: metallocene C6 grades tend to initiate sealing about 5–10 °C lower than C4-LLDPE of comparable density and MFR. Exact quantitative comparisons for this specific configuration are limited in publicly available databases; supplier’s technical datasheet and customer line trials are required to establish target values.
In dynamic oscillatory shear under ISO 6721-10, the terminal storage modulus of the metallocene C6 grade is lower than that of high-pressure LDPE, reflecting the absence of long-chain branching. The loss modulus crossover occurs at a higher frequency; this means shear thinning is less pronounced and the power-law index in the processing shear-rate range is typically 0.55–0.65. The consequence for blown-film die design is that spiral mandrel or radial-spiral die flow channels should be sized for a more Newtonian melt than LDPE; otherwise, gauge variation may arise at high outputs. In addition, because the molecular weight distribution is narrow, the transition from stable flow to sharkskin can be abrupt, so die-lip shear rate should not be increased without process-aid evaluation.
At the extruder, the grade shows shear-thinning behaviour typical of linear metallocene LLDPE. Capillary rheometry under ISO 11443 at 190 °C typically gives apparent shear viscosity near 900–1100 Pa·s at 100 s-1 for this product family; the exact batch value depends on molecular weight distribution and should be verified from the certificate of analysis. Because the melt is more linear than high-pressure LDPE, melt fracture onset can occur at lower apparent shear rates. On a 60 mm single-screw blown-film extruder with 30:1 L/D barrier screw and Maddock mixer, barrel set temperatures are profiled from 180 °C at the feed throat to 210 °C at the adapter, with die zones held at 210 °C; melt temperature at the die lip should remain below 240 °C to limit oxidation gel formation. The barrier screw should have a feed section length of 5–7 L/D, a compression ratio 2.8:1 to 3.2:1, and a mixing section that provides low shear; severe high-shear mixers can raise melt temperature above 240 °C and produce oxidation gels. Screw speed on a 60 mm line is typically 80–120 min-1. A die gap between 1.2 mm and 2.0 mm with a dual-lip air ring and internal bubble cooling stabilises the bubble at blow-up ratios 2.0:1 to 3.0:1. Frost-line height is controlled from 2 to 6 die diameters; below 2 die diameters, rapid quenching reduces crystallite size and improves ASTM D1003 haze but increases blocking force. Above 6 die diameters, the bubble may oscillate because the metallocene LLDPE has lower melt tension than high-pressure LDPE, particularly on high-stalk lines. If surface sharkskin appears on the film web, addition of 200–500 ppm of a fluoropolymer process aid is common, but the aid may slightly delay attainment of target haze and must be evaluated under production conditions. Melt pressure at a 60 mm line running 150 kg/h is typically 300–350 bar; a sustained rise above 400 bar indicates screen-pack blinding, feed bridging, or insufficient melt temperature. The grade is normally processed without predrying, but if moisture exceeds 0.05 wt%, a desiccant hopper dryer at 60 °C for 2 h is typical.
Down-gauging to 12 µm on a cast film line moves the process into a region where melt-curtain stability, edge pinning, and draw resonance dominate property consistency. On a 90 mm extruder with 33:1 L/D and a 2200 mm slot die, the melt temperature at the die exit is held at 220 °C to 235 °C. Lower temperatures raise die pressure and may trigger melt fracture; higher temperatures reduce melt tension and increase neck-in. The air gap between die lip and chill roll is set from 15 mm to 25 mm; a gap above 25 mm destabilises the curtain and increases transverse gauge variation. The chill-roll surface temperature is maintained at 15 °C to 25 °C to quench the web and keep haze low under ASTM D1003. Vacuum box or electrostatic pinning is mandatory below 15 µm to prevent air entrainment and transverse gauge bands. Edge pinning is set to produce uniform bead width 5–10 mm; excessive bead width creates trim waste, while insufficient bead width causes edge curl and web break. Draw resonance appears as periodic gauge variation along the machine direction; it is mitigated by reducing the draw ratio, increasing melt temperature, or adding 5–10 wt% high-pressure LDPE to the blend. If the line is equipped with a secondary chill roll, the second roll is typically set 5–10 °C warmer than the primary roll to reduce web curl. Because cast film orientation is predominantly machine-direction, dart impact values under ASTM D1709/A can be lower than in blown film of the same gauge, while machine-direction tensile modulus under ASTM D882 increases. Published data for this specific configuration is limited; line trials are required to validate gauge uniformity below 10 µm.
Applications for CHH 196 are differentiated by gauge and end-use performance balance. In agricultural silage and bale-wrap film at 25 µm, the C6 architecture contributes to tear-propagation resistance after stalk puncture; cling is achieved by formulation with tackifying additives rather than by the base resin. In heavy-duty sacks at 80–120 µm, the reduced low-molecular-weight tail supports a low gel count and consistent dart impact under ASTM D1709/A. In lamination and form-fill-seal films at 20–30 µm, the lower seal-initiation temperature supports faster sealing on packaging machines, but the final seal window must be confirmed with the specific sealing layer and additive package. In stretch film, pre-stretch ratio on pallet wrapping is typically 250%; film must retain load after elongation. The C6 structure supports tear resistance during pre-stretch, but the exact pre-stretch retention is a function of the tackifier formulation and machine control. For each application, the final additive package and coextrusion structure determine the observed property profile; published data for this specific formulation is limited.
Metallocene C6-LLDPE generally seals at lower temperature than C4-LLDPE of equivalent density. For 40 µm film tested under ASTM F88, seal initiation is often observed between 95 °C and 105 °C, but the exact value depends on film construction, additive package, and sealing dwell. Hot-tack strength measured under ASTM F1921 at 0.5 s cooling time should be confirmed on vertical form-fill-seal machines running 60 to 80 pouches/min; the reduced low-molecular-weight fraction of the metallocene architecture helps limit seal-jaw contamination. Seal-bar pressure is typically 0.2–0.4 N/mm² at the seal area. If pressure is below 0.2 N/mm², incomplete wetting produces low hot-tack; above 0.4 N/mm², film thinning at the seal reduces strength. For food-contact applications, compliance is verified against FDA 21 CFR 177.1520 for olefin polymers and Commission Regulation (EU) 10/2011 Annex I for plastic materials. The EU overall migration limit is 10 mg/dm² for film articles and 60 mg/kg for food simulants; specific migration of 1-hexene and additives must be confirmed from the supplier’s declaration of compliance. Corona treatment for lamination should achieve surface energy of 38–40 mN/m under ASTM D2578; higher treatment can oxidize the surface and reduce seal strength. The grade should not be blended with high levels of acidic or unsaturated regrind streams without organoleptic evaluation under DIN 10955.
| Regulation or standard | Reference or clause | Verification basis |
|---|---|---|
| FDA 21 CFR 177.1520 | Olefin polymers | Supplier declaration; end-use food type and extraction limits apply |
| EU 10/2011 | Plastic food-contact materials | Overall migration 10 mg/dm² or 60 mg/kg simulant |
| REACH | SVHC candidate list | Declaration required; no SVHC above 0.1 wt% |
| RoHS 2011/65/EU | Annex II restricted substances | Lead 1000 ppm; cadmium 100 ppm; PBDE/PBB 1000 ppm |
In multilayer structures, CHH 196 can serve as the core or sealing layer; when coextruded with high-pressure LDPE skins, bubble stability improves because the LDPE contributes melt strength, but the seal-initiation temperature shifts upward in proportion to the LDPE content. The grade is compatible with EVA and polyolefin plastomers, but tear and hot-tack balance follows the blend ratio and must be measured under the final film construction. Predrying is generally unnecessary; however, surface condensation on cold pellets can cause feed-throat surging when material is introduced from outdoor silos below 10 °C into a warm production hall. In that case, a hopper dryer at 60 °C for 1–2 h is used. At high regrind levels above 30 wt%, gel accumulation can increase because of repeated shear history; inline melt filtration with a screen pack of 60/80/100 mesh is used to trap contaminants. If film is intended for high-speed automatic packaging, incorporation of slip and antiblock additives is necessary to control coefficient of friction under ASTM D1894; untreated film may block under roll pressure and humidity above 60% RH. Avoid uncontrolled blending with amine-based antistatic additives or antifog concentrates; some amine chemistries can interfere with organoleptic performance and increase water-contact migration. Incoming inspection should verify MFR under ISO 1133-1:2022, density under ISO 1183-1, and visual pellet contamination; lot-specific certificates of analysis remain the basis for release.