| HS Code | 865704 |
| Density | 0.954 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 0.35 g/10 min |
| Tensile Strength At Yield | 24 MPa |
| Tensile Elongation At Break | >500% |
| Flexural Modulus | 1000 MPa |
| Izod Notched Impact Strength 23 C | 80 J/m |
| Vicat Softening Point | 125°C |
| Heat Deflection Temperature 0 45 Mpa | 70°C |
| Hardness Shore D | 65 |
| Environmental Stress Crack Resistance F50 | >1000 h |
| Melting Point | 130°C |
| Brittleness Temperature | <-70°C |
As an accredited USI Corporation HDPE LH901 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | USI Corporation HDPE LH901 is packaged in 25 kg net bags, palletized and stretch-wrapped for industrial shipment. |
| Container Loading (20′ FCL) | USI Corporation HDPE LH901 is loaded in a 20-foot full container load, palletized in bags, securely stowed for ocean shipment. |
| Shipping | USI Corporation HDPE LH901 is non-hazardous high-density polyethylene pellets. It is typically shipped in 25 kg bags or 1000 kg jumbo bags, palletized and stretch-wrapped. Transport as general cargo; no UN number or hazard class. Store dry, away from direct sunlight and heat. |
| Storage | Store USI Corporation HDPE LH901 in a cool, dry, well-ventilated warehouse, away from direct sunlight, ignition sources, and strong oxidizers. Keep original bags or containers closed, palletized, and off the floor to prevent moisture, dust, and contamination. Avoid excessive heat, flames, and static discharge. Use first-in, first-out rotation and follow local regulations. Protect from UV radiation and moisture; maintain moderate temperatures. |
| Shelf Life | USI Corporation HDPE LH901 has no fixed shelf life; store cool, dry, sealed, away from sunlight. Stable under normal conditions. |
Collapsible crates for beverage, dairy, and agricultural distribution are injection-molded with sidewall thickness ranging from 2.5 mm to 4.5 mm and load-bearing floor ribs that carry repeated top-load and drop impact. The tensile yield stress of unfilled HDPE in this product class is approximately 26 MPa when tested per ISO 527-2:2012, and flexural modulus is approximately 1,100 MPa per ISO 178:2019. Rib height above 6 mm without adequate base radius increases the unsupported free edge and can initiate buckling during stacking; rib-to-wall transitions with radius below 1.5 mm act as stress risers under low-temperature impact. Molding shrinkage measured per ASTM D955-21 on a 3.2 mm plaque falls between 1.5 % and 2.5 %, but rib intersections and thick bosses may shrink at 2.5-3.5 %, generating sink marks that reduce flatness on the crate floor. On production-scale tools with hot-runner drops feeding multiple gates, cavity-to-cavity fill imbalance produces batch-to-batch variation in hinge boss diameter and sidewall bow. Molders use conformal cooling inserts in rib tips and sequential valve gates to delay fill behind the rib network, lowering differential shrinkage. Ejection temperature above 75 °C measured at the part surface can cause post-ejection warpage; forced cooling fixtures are used for large crates with flatness requirements tighter than ±1.0 mm over 600 mm span. Low-temperature drop impact is evaluated with ASTM D5276-19 methods on production crates, with fracture commonly initiating at stacked corner radii or gate weld lines.
In stack-mold production of thin-wall dairy and deli containers, USI Corporation HDPE LH901 is selected for short filling time and low injection pressure in wall sections between 0.45 mm and 0.80 mm. Flow-length-to-wall-thickness ratios in multi-cavity stack tools often exceed 180:1, which requires injection screw advance speeds of 160-240 mm/s and clamp force above 4,500 kN on dual-face platens. The material is processed with a reverse heat profile in the screw, where rear zones are set at 190-200 °C and front zones at 210-225 °C, reducing screw recovery torque while limiting residence-time degradation. Mold temperature is held at 8-15 °C to achieve cycle times of 4-6 s for lids and shallow tubs; this low mold temperature increases the frozen skin layer and can amplify warpage on containers with in-mold label panels. Cavity pressure at transfer from velocity to pack is typically 300-500 bar, and gate seal detection via cavity pressure flattening prevents sink and part-to-part weight drift. Since HDPE has high crystalline shrinkage, a 0.75 mm wall container may exhibit 1.4 % flow-direction shrinkage and 1.8 % transverse shrinkage, measured per ASTM D955-21 on plaque specimens. Stack-mold venting is critical at high injection velocity; vent land depth above 0.03 mm creates flash, while insufficient venting below 0.015 mm produces gas burn at the fill end. Regulatory compliance for dairy tubs, margarine containers, and delicatessen packaging follows FDA 21 CFR 177.1520 and EU No 10/2011, including specific migration testing under fatty food simulant D2 or vegetable oil.UN-rated high-density polyethylene pails for detergents, agricultural chemicals, and liquid food concentrates are molded with wall thickness between 1.6 mm and 2.5 mm. Failure in aggressive service is often environmental stress cracking rather than ductile burst; it initiates at injection gates, weld lines, or sharp transitions in the pail body. High-flow injection HDPE grades such as USI LH901 favor thin-wall fill and reduced cycle time, but homopolymer HDPE has lower stress-crack resistance than bimodal blow-molding copolymers, so design and processing must compensate. Internal corner radius below 3 mm and thickness transition exceeding 30 % over 5 mm length concentrate frozen-in stress and shorten time to cracking. Environmental stress-crack resistance is measured per ASTM D1693-21 condition B at 50 °C in 100 % Igepal CO-630; published data for LH901 in full pail geometry is limited, so molders should validate production-tool specimens because the plaque F50 value does not capture gate notch effects and flow-induced stress. Processing to minimize residual stress includes lower melt temperature from 190 °C to 210 °C, high mold temperature at 25-35 °C, and packing pressure set just below flash threshold. Excessive injection speed above 200 mm/s increases molecular orientation and ESCR anisotropy, while very low speed creates hesitation marks at flow-front convergence. UN performance compliance for dangerous goods pails follows 49 CFR 178.603 drop, 49 CFR 178.604 leakproofness, and 49 CFR 178.606 stack testing; drop height depends on packing group, with 1.8 m for Packing Group I, 1.2 m for Packing Group II, and 0.8 m for Packing Group III.
| Compliance Requirement | Standard/Regulation | Test Condition or Threshold |
|---|---|---|
| Olefin polymer food contact, US | FDA 21 CFR 177.1520 | Conditions of use A-H; extraction per subpart 177.1520(c) |
| Plastic food contact, EU | EU No 10/2011 | Overall migration limit 10 mg/dm²; simulant selection by food type |
| Pail drop integrity | 49 CFR 178.603 | Drop height 1.8 m, 1.2 m, or 0.8 m by Packing Group |
| Pail leakproofness | 49 CFR 178.604 | Internal air pressure per closure size and wall rigidity |
| Pail stacking | 49 CFR 178.606 | Load duration and temperature per transport requirement |
Household storage bins, drawer towers, and organizer systems use USI Corporation HDPE LH901 in panels with wall thickness from 1.8 mm to 3.0 mm. Dimensional stability in the lid-to-base interface is governed by directional shrinkage, because HDPE crystalline orientation parallel to flow differs from transverse orientation. Typical plaque shrinkage per ASTM D955-21 for this product class is 1.2-1.5 % in the flow direction and 1.6-2.0 % in the transverse direction; that differential causes long sidewalls to bow inward after ejection if mold temperature varies more than ±3 °C across the cavity face. Multigating and sequential valve-gate activation reposition weld lines away from latch bosses and improve impact at the living joints. Molders use cavity pressure switchover at 350-500 bar and hold time sufficient for gate seal, because early release creates dimensional drift in the engagement ribs that control stacking and drawer slide clearance. Parts are sometimes ejected onto flat cooling fixtures for 15-30 s to stabilize shrinkage before stacking; this is especially relevant for clear-overmolded corner bumpers or molded-in latch features where post-mold warpage above 1.0 mm prevents assembly. Injection screw recovery is set at low back pressure below 10 bar to avoid excessive shear heating and color shift in thin sections. The material is not predried under normal indoor humidity; only surface condensation from outdoor silo storage requires hopper drying at 70-80 °C for 1-2 h prior to processing.
Industrial HDPE pallets with nine-block or perimeter-foot designs use thick foot pockets of 5-8 mm and top deck sections of 4-6 mm. The melt is delivered through multiple hot-runner valve gates to manage clamp force and reduce flow length; each gate produces a weld line at the junction of flow fronts. Weld line strength in high-flow HDPE is lower than fully fused bulk material, and low-temperature impact at -20 °C tends to propagate cracks along these knitlines. Puncture impact testing per ISO 6603-2:2023 on injection-molded plaques is used for comparative evaluation, but published data for LH901 in full pallet geometry is limited, so production-tool trials with instrumented drop impact per ASTM D5276-19 are required to establish gate-position-specific performance. Processing changes that improve foot pocket fusion include raising mold temperature from 15 °C to 30 °C and increasing effective fill velocity above 200 mm/s; the upper velocity is bounded by jetting at the gate and gas burn at the vent end. Vent land depth is maintained between 0.015 mm and 0.025 mm, and vent width above 8 mm is used in deep ribs to evacuate air without flash. Differential shrinkage measured per ASTM D955-21 on thick HDPE sections produces top deck warpage; pallet flatness requirements tighter than 5 mm over 1,200 mm often require post-mold cooling in a press-side fixture rather than uncontrolled shrink on the cooling conveyor. The material should be processed at the lower end of the melt-temperature range to limit molecular weight reduction during long residence time in large accumulator heads and hot-runner manifolds.
Competitive USI Corporation HDPE LH901 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
USI Corporation HDPE LH901 is a high-density polyethylene homopolymer supplied as an injection-moulding grade for thin-walled rigid packaging, closures, crates, housewares, and similar fast-cycle articles. Supplier lot-average data list a melt flow rate of 9.0 g/10 min at 190 °C under 2.16 kg load when tested to ASTM D1238 or ISO 1133-1, and a density of 0.953 g/cm³ determined by ASTM D1505 or ISO 1183-1. These values place the product in a high-flow HDPE class that differs from high-molecular-weight HDPE grades used for blown film, thick-walled blow moulding, and pressure pipe. The grade is organized for injection-moulding economy: at the high shear rates encountered in gates and thin walls, apparent viscosity falls sufficiently to reduce fill pressure and cycle time. The same molecular structure lowers melt strength, so continuous extrusion blow moulding and blown film processing are outside the intended manufacturing window.
The density above 0.940 g/cm³ indicates a linear polyethylene with low short-chain branching. The resulting crystallinity contributes rigidity, moisture-barrier behaviour, chemical resistance, and opacity. However, crystallinity also controls shrinkage and cooling demand. In moulded parts, differential cooling between thick and thin sections generates anisotropic contraction; published mould shrinkage for parallel flow direction is commonly 1.5–2.0 % when measured on a standard plaque according to ASTM D955 or ISO 294-4. Designers should treat that value as a starting point, not a tooling constant, because gate placement, packing pressure, orientation, and wall-stock variation alter final part dimensions more than the resin shrinkage value alone.
The first processing limit in LH901 is not barrel temperature alone; it is the interaction between screw recovery, check-valve flow, gate freeze-off, and cavity venting. On general-purpose injection machines with screw L/D ratios of 20:1 to 25:1 and compression ratios from 2.0:1 to 3.0:1, the melt is typically dosed at back pressures of 0.35–1.0 MPa (50–150 psi) and screw speeds that avoid adiabatic melt-temperature rise above 250 °C. A melt cushion of 2–5 mm with decompression of 3–8 mm is usual. Insufficient cushion prevents stable transfer of packing pressure through the check valve and produces shot-to-shot weight variation when the valve leaks during inject. Multi-cavity thin-wall tools with flow-length-to-wall-thickness ratios above 200:1 may require fill-time control in the 0.5–2.0 s range. Delayed filling permits the advancing melt front to freeze at the outer edges and generates short shots before the measured cavity pressure reaches the programmed packing value.
Clamp-force estimates for thin-wall HDPE are commonly 2.5–4.0 tons per square inch (35–55 MPa) of projected part area, but the actual requirement depends on gate location, wall stock, packing pressure, and mould construction. Operators should monitor hydraulic pressure at switchover as well as cavity pressure, because compressibility at packing pressures above 40 MPa can mask hot-runner imbalance. Gate freeze-off becomes the critical production boundary: for a 1.0 mm nominal wall, gate freeze time after fill is often on the order of 0.5–1.0 s. If the packing phase is not established within that interval, sink marks at rib-to-wall junctions and dimensional variation across the cavity are not correctable by extending hold time later in the cycle.
Degradation boundaries are set by melt temperature and residence time. Above 260 °C, oxidative chain scission and cross-linking compete, producing viscosity shifts, discoloration, and black specks in hot-runner channels. Below 180 °C, homogenization is incomplete and injection pressure rises sharply. During interruptions, barrel residence time should be kept below 10 min at 230 °C; idle machines should be purged with a general-purpose HDPE or eased to a lower barrel profile. Mould surface temperatures below 10 °C create oriented skin stresses and warpage, while temperatures above 60 °C extend cycle time and may cause ejection-imparted distortion when draft angles are insufficient. Peripheral vents at 0.02 mm depth prevent burn marks and diesel ignition in trapped air; deeper vents flash HDPE immediately.
Cooling demand is dominated by part thickness, not by the 9.0 g/10 min melt flow rate. For a 1.0 mm wall, the gate-freeze interval is short, but conductive heat removal through the mould steel remains the cycle-time constraint. Increasing nominal wall thickness from 1.0 mm to 1.5 mm can increase cooling time by roughly the square of the thickness ratio, approximately 2.25× in classic mould-cooling approximations. High-flow HDPE does not remove that thermal load; it only shortens fill time and permits lower packing pressure in thin sections.
Typical lot-average values are provided as engineering reference data. They are not lot-specific specification limits and should be confirmed against the manufacturer’s certificate of analysis. Unless the individual test method requires otherwise, specimens are conditioned at 23 ± 2 °C and 50 ± 10 % relative humidity for 40 h following ISO 291 or ASTM D618.
| Property | Test standard | Unit | Typical value |
|---|---|---|---|
| Melt mass-flow rate at 190 °C, 2.16 kg | ASTM D1238 / ISO 1133-1 | g/10 min | 9.0 |
| Density at 23 °C | ASTM D1505 / ISO 1183-1 | g/cm³ | 0.953 |
| Tensile yield strength, 50 mm/min | ASTM D638 Type IV / ISO 527-2 Type 1B | MPa | 26 |
| Tensile elongation at break, 50 mm/min | ASTM D638 / ISO 527-2 | % | 200 |
| Flexural modulus, 2 mm/min | ASTM D790 / ISO 178 | MPa | 1,100 |
| Notched Izod impact at 23 °C | ASTM D256 Method A | J/m | 50 |
| Vicat softening point, A/120 | ASTM D1525 / ISO 306 | °C | 124 |
| Mould shrinkage, parallel | ASTM D955 / ISO 294-4 | % | 1.5–2.0 |
Food-contact, potable-water, toy, and electrical applications require lot-specific conformity rather than reliance on typical values. HDPE homopolymer of this density can be evaluated under FDA 21 CFR 177.1520 for direct food contact, EU Regulation (EU) No 10/2011 for plastic materials intended for food contact, and REACH Article 33 declarations for candidate-list substances. The final additive package, catalyst residues, processing aids, and masterbatch additions determine actual compliance status. Published migration data for USI Corporation HDPE LH901 in specific food simulants is limited; therefore, a conformity statement must be requested from the supplier for the exact lot and application.
Drying is not normally required. If surface condensation occurs when pellets are moved from cold silos or containers into a hot, humid moulding hall above 60 % relative humidity, a hopper air dryer at 60–70 °C for 0.5–1 h removes surface moisture before gate splay appears. The resin itself is not hygroscopic in the manner of polyamide or PET, so extended desiccant drying is unnecessary and can increase energy use without improving melt quality.
The grade is not a pressure-pipe material. Unlike bimodal PE100 HDPE designed for long-term hydrostatic strength and slow crack growth resistance under ISO 9080, LH901 is intended for short-cycle injection moulding. It should not be used for gas, water, or chemical pressure piping, nor for continuous exposure to hot hydrocarbon fluids, strong oxidizing acids, or aromatic fuels above 23 °C. In such environments, excessive swelling, loss of tensile strength, or environmental stress cracking may occur. For outdoor articles, unpigmented HDPE is not an ultraviolet-stabilized material; a UV-stabilized masterbatch or suitable coating is required to retain impact resistance in weathering service.
In material substitution studies, the decisive variables are usually melt strength, flexural modulus, heat resistance, and environmental stress crack resistance. Compared with a low-MFR HDPE of 0.30 g/10 min used in extrusion blow moulding, LH901 sacrifices melt strength and slow crack growth resistance for mouldability. It is unsuitable for parison formation because gravitational sag and neck-in during continuous blow moulding increase at 9.0 g/10 min; a high-molecular-weight grade should be retained for containers produced by extrusion blow moulding or accumulator-head machines.
Compared with a random copolymer polypropylene of similar melt flow, LH901 has lower flexural modulus, lower heat deflection temperature, and a narrower processing-to-oxidation temperature window. Polypropylene remains the preferred choice where flexural modulus above 1,200 MPa or continuous service above 90 °C is required. LH901 HDPE is closer to a flexural modulus of 1,100 MPa and a Vicat softening point around 124 °C. Conversely, HDPE can provide better retained hinge behaviour and lower water-vapour permeability than polypropylene in many rigid packaging applications. When detergent, oil, or surface-active chemical resistance is required, environmental stress crack resistance must be screened using ASTM D1693 condition B on the actual moulded part; lot-specific F50 values are needed because regrind content and processing history shift the practical resistance of the article.
Compared with a bimodal HDPE pressure-pipe resin, LH901 is not engineered for slow crack growth. The difference is molecular architecture rather than density alone: PE100 grades use a controlled high-molecular-weight fraction to resist crack propagation under sustained stress. LH901’s injection-moulding molecular design shortens relaxation time and improves shear thinning at high flow, but it does not provide the same long-term hydrostatic design strength. Applications involving continuous hydrostatic pressure, hot hydrocarbon contact, or repeated impact below -30 °C are outside the expected design envelope for this injection-moulding grade unless validated on the actual moulded article under the governing application standard.