    Specifications
    HS Code 560532
    Density 0.960 g/cm3
    Melt Flow Rate 6.0 g/10 min
    Tensile Strength At Yield 28 MPa
    Tensile Elongation At Break 500 %
    Flexural Modulus 1100 MPa
    Izod Notched Impact Strength 40 J/m
    Shore D Hardness 65
    Vicat Softening Point 126 °C
    Heat Deflection Temperature At 0 46 Mpa 75 °C
    Melting Point 135 °C
    Brittleness Temperature -70 °C
    Environmental Stress Crack Resistance >1000 h
    Water Absorption <0.01 %
    Dielectric Constant 2.3
    Volume Resistivity >1.0E16 ohm-cm

    As an accredited USI Corporation HDPE LH606 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing USI Corporation HDPE LH606 is packaged in 25 kg bags, typically palletized and stretch-wrapped for shipment.
    Container Loading (20′ FCL) 20′ FCL container loading for USI Corporation HDPE LH606: approximately 18 MT in 25 kg bags, palletized, standard dry container.
    Shipping USI Corporation HDPE LH606 is shipped as non-hazardous polyethylene pellets, typically in 25 kg woven bags, 500–1000 kg jumbo bags, or bulk containers. Transport in clean, dry trucks, railcars, or shipping containers. Store away from heat, direct sunlight, moisture, and contamination. Standard international packaging applies.
    Storage Store USI Corporation HDPE LH606 in a cool, dry, well-ventilated area away from direct sunlight, rain, moisture, heat, and ignition sources. Keep original packaging closed, clean, and palletized; avoid crushing, over-stacking, and physical damage. Prevent contamination by oils, chemicals, or dust. Use first-in, first-out rotation and good housekeeping. Store at ambient temperature, away from incompatible materials.
    Shelf Life Shelf life is typically two years when stored cool, dry, ventilated, away from direct sunlight and heat.
    Application of USI Corporation HDPE LH606

    In thin-gauge T-shirt sack production, USI Corporation HDPE LH606 is processed on single-screw blown-film lines with a 24:1 to 30:1 L/D barrier screw and a spiral mandrel die. Each incoming lot is characterized by melt-flow index per ISO 1133-1 at 190 °C / 2.16 kg and density per ISO 1183-1. The melt temperature at the die is kept within 200–225 °C; excursions above 225 °C produce bubble flutter and surface roughness, while excursions below 200 °C raise melt pressure beyond 35 MPa on a 65 mm extruder. The die gap is set at 0.8–1.2 mm. A blow-up ratio of 3:1–5:1 and a stalk height of 6–10 die diameters are required to align the high-molecular chains. The long stalk is not decorative; it creates the machine-direction tear resistance necessary for 10–18 µm sack film. Film is converted on rotary sealing machines with seal temperatures between 150–170 °C. Tear and impact are measured according to ASTM D1922 and ASTM D1709 Method A because these methods respond to different failure modes. If 10–20 wt% linear low-density polyethylene is dry-blended, dart impact rises but film stiffness falls; beyond 20 wt% LLDPE, the film becomes too extensible for automated bag indexing. Regrind is accepted up to 20–30 wt% only when the melt filtration pack is at least 60/80/100 mesh. Higher regrind fractions create gel specks at 25 µm thickness. The terminal sack is non-food grocery carryout. No pre-drying is required because the polymer is non-polar and supplied with moisture below 0.05 wt% according to incoming plant data.

    What Limits Bubble Stability When LH606 Is Run on a Low-Neck Coextrusion Line?

    The core-layer viscosity mismatch is not a laboratory observation. In three-layer coextruded film for dry-food pouches and bag-in-box liners, LH606 is used as the stiffening core at 25–40 % of total film thickness. The total film thickness ranges from 35 µm to 60 µm, and the LH606 core is enclosed by LLDPE or LDPE skins. Core melt temperature is held at 210–225 °C, while skin melt temperatures are typically 170–200 °C to protect heat-sensitive additives. When the viscosity difference between core and skins exceeds the equipment design limit, wavy die-lines and interfacial instability appear at line speeds above 80 m/min. A melt pump after the core extruder reduces surge and maintains layer thickness within ± 1 µm. The die gap is set at 1.5–2.0 mm because the larger gap prevents molecular-weight buildup and reduces melt fracture in the HDPE layer. Blow-up ratio is limited to 2.5:1–3.5:1 with a low stalk height of 2–4 die diameters; this configuration minimizes bubble cooling demands but reduces MD transverse balance. Seal strength is checked to ASTM F88 because the final pouch must survive drop transport without seal delamination. For dry-food contact, final packaging is evaluated under EU Regulation (EU) No 10/2011 overall migration limit of 10 mg/dm²; EU simulant selection depends on final food type, not on resin alone. Published line data for LH606 in this exact three-layer structure is limited, so most converters qualify the structure by film thickness profile and seal strength rather than theoretical viscosity matching.

    Unlike thin-gauge high-stalk production, heavy-duty liner conversion on conventional blown-film towers uses a low stalk height of 2–4 die diameters and a blow-up ratio of 2.5:1–3.5:1. LH606 is fed neat or with 10 wt% LLDPE. The die gap is set at 1.5–2.0 mm, and total film thickness is 80–200 µm. Melt temperature is maintained at 215–235 °C. Internal bubble cooling is added when the frost line climbs above 70% of the tower height; chilled air at 10–15 °C increases output by reducing the cooling-air residence time. Tear and tensile properties are measured to ASTM D882, while puncture resistance is characterized to ASTM D4833. For construction debris and asbestos abatement liners, project-specific minimums are often written around ASTM D4833 because it measures index puncture rather than film tensile elongation. If the liner is specified for outdoor storage, a UV masterbatch is added at 2–4 wt%; for exposures beyond 30 days, accelerated weathering per ASTM G154 is used to validate carbon black or HALS packages. The terminal product is a non-food liner for construction, demolition, and containment use. Regrind from edge trim is usually limited to 20 wt% to avoid reducing puncture resistance; converters who exceed this limit report more frequent star-seal failures at the bottom fold, especially when film thickness falls below 100 µm.

    When 20 wt% LLDPE Is Dry-Blended for Tear-Balance Modification in Refuse Sacks

    A dry blend of 80 wt% LH606 and 20 wt% LLDPE is hopper-fed into a single-screw extruder to shift the Elmendorf tear balance toward the transverse direction. The film is produced at 25–40 µm. The screw must include a Maddock mixing element; without it, low-viscosity LLDPE pools form and produce irregular gauge bands at the frost line. Melt temperature is held at 210–230 °C. The die gap is 1.2–1.5 mm, and the blow-up ratio is 3:1–4:1. The LLDPE fraction modifies tear anisotropy. If LLDPE exceeds 25 wt%, the film becomes excessively ductile for automatic bag insertion and MD tensile yield falls below internal specifications, so the ratio is not a convenience variable. Dart impact is checked to ASTM D1709 Method A; Elmendorf tear is checked to ASTM D1922; tensile yield is checked to ASTM D882. Published data for this specific dry blend under LH606 is limited, so converters set the final blend ratio through plant trials with the exact extruder screw and die configuration. Terminal products are star-sealed wave-cut refuse sacks and drawstring bags. No pre-drying is required for either component unless the LLDPE arrives with surface moisture from contaminated conveying air; condensation is drained from hopper loaders and the feed throat is kept above 30 °C in high-humidity plants.

    Reclaim Compounding with Post-Consumer HDPE Letdown for Non-Food Sacks

    For non-food refuse sacks containing post-consumer HDPE, LH606 is fed into a co-rotating twin-screw extruder with 40:1 L/D and vacuum venting at -0.08 MPa to -0.095 MPa. Post-consumer HDPE regrind is let down at 30–50 wt%; LH606 constitutes the balance at 50–70 wt%. The melt is filtered through 100–150 mesh screens before water-ring pelletizing. Melt temperature at the die plate is kept at 200–220 °C to limit degradation of unknown contaminants in the recycle stream. The objective is not tensile strength alone; LH606 restores stress-cracking resistance and dilutes gels that would otherwise tear in thin films. Pelletized blend is then converted on a blown-film line with a 60/80/100 mesh pack. Stress-cracking resistance is measured to ASTM D1693 Condition B; gel count has no universal standard, so converters use camera-based gel scanners calibrated at 25 µm. Each reclaim lot must be qualified separately because post-consumer HDPE varies in ash, density, and contamination. A film trial with 50 µm thickness is the final acceptance gate; dart impact to ASTM D1709 and tear to ASTM D1922 are recorded on every lot. The terminal product is a heavy-duty non-food refuse sack for municipal and commercial waste. If regrind content exceeds 50 wt%, bubble stability deteriorates and the frost line drops, requiring lower output and a wider die gap of 1.8 mm or more.

    Extraction Profile Shifts When the Seal Layer Is Thinned to 12 µm

    When monolayer food-contact film is thinned from 30 µm to 12 µm, the surface-to-volume ratio changes, and the extraction profile under food simulants shifts. LH606 is processed in this configuration for bakery bags, cereal liners, and lightweight produce film. The film is run at 200–225 °C melt temperature; the die exit is kept below 230 °C to minimize oxidative degradation products that would raise total extractables. Slip and antiblock masterbatches are used at 0.5–1.5 wt% only when the additive system is covered by a supplier food-contact statement referencing FDA 21 CFR 177.1520(c) and EU Regulation (EU) No 10/2011. The die gap is 0.8–1.0 mm. No pre-drying is required at relative humidities up to 60% because the resin is non-hygroscopic, but condensation from cold pellets transferred directly from outdoor silos into the feed throat causes die-hole streaks. The final film is evaluated under the applicable food simulant conditions; dry-food applications may require only Simulant E testing at 40 °C for 10 days under EU Regulation (EU) No 10/2011, whereas fatty-food contact requires higher-temperature simulants. The terminal products are food-contact bags and liners. The table identifies the relevant compliance references used during import and conversion.

    United States21 CFR 177.1520(c)Olefin polymer restrictions and use conditionsSupplier food-contact statement covers LH606 base resin
    European UnionEU Regulation (EU) No 10/2011Overall migration limit 10 mg/dm²Final film, including masterbatch, evaluated under specified food simulant conditions
    REACHRegulation (EC) No 1907/2006SVHC candidate list and restriction annexesImporter must maintain safety data sheet and compliance declaration
    Free Quote

    Competitive USI Corporation HDPE LH606 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    USI Corporation HDPE LH606 is a high-density polyethylene resin supplied in pellet form for injection molding applications requiring a controlled balance of melt flow, rigidity, and environmental stress crack resistance. The model designation LH606 identifies a medium-flow HDPE grade in the USI Corporation HDPE portfolio. Melt mass-flow rate measured at 190 °C with a 2.16 kg load under ISO 1133-1:2022 or ASTM D1238-20 is 6.0 g/10 min. Density tested by ISO 1183-1:2019 or ASTM D1505-18 is 0.960 g/cm³. The resin is used in rigid packaging, closures, housewares, pails, and industrial components where injection-cycle economics require a lower melt viscosity than blow-molding HDPE grades and a higher bending modulus than linear-low-density polyethylene grades. The values presented are typical release data, not specification limits, and should be verified against the certificate of analysis for each production lot.

    Incoming resin is supplied in 25 kg bags or bulk rail containers depending on regional distribution. Pellets should be stored in closed containers at 15 °C to 40 °C. The grade is not hygroscopic, so long desiccant drying is not normally required. At relative humidity above 60%, surface moisture can be picked up in open hopper loaders, producing splay in molded parts. Pre-drying for 2 h at 80 °C in a dehumidifying hopper dryer with a dew point of -30 °C or lower removes surface condensation.

    Typical property values for USI Corporation HDPE LH606
    PropertyMethodTypical valueUnit
    Melt mass-flow rateISO 1133-1:2022, ASTM D1238-206.0g/10 min
    DensityISO 1183-1:2019, ASTM D1505-180.960g/cm³
    Tensile yield stressISO 527-2:2012, ASTM D638-1429.0MPa
    Tensile elongation at breakISO 527-2:2012, ASTM D638-14300%
    Flexural modulusISO 178:2019, ASTM D790-171,200MPa
    Notched Izod impact at 23 °CISO 180/A, ASTM D256-235.0kJ/m²
    Shore hardness DISO 868:2003, ASTM D2240-1566—
    Vicat softening temperature, 10 NISO 306, ASTM D1525-17124°C
    Heat deflection temperature, 0.455 MPaISO 75-2:2020, ASTM D648-1875°C

    What Processing Limits Apply to Reciprocating-Screw Injection Molding of LH606?

    Melt temperature measured at the nozzle should be maintained between 190 °C and 220 °C. Above 230 °C, residence time in the barrel becomes a critical limitation; thermo-oxidative chain scission can shift the melt flow rate upward and reduce notched Izod impact measured by ISO 180/A. The exact rate of property loss is machine-specific because it depends on oxygen ingress at the feed throat, screw speed, and barrel residence time; published data for this specific configuration is limited. Below 180 °C, melt viscosity rises sufficiently to create pressure-limited short shots when the flow length-to-wall-thickness ratio exceeds 200:1 in cold-runner tools.

    General-purpose reciprocating screws with L/D ratio 20:1 to 25:1 and compression ratio 2.5:1 to 3.0:1 are suitable. Low-shear metering sections are preferred over high-shear barrier or dispersive mixing sections because dispersive mixing can add melt temperature above the set barrel temperature. Back pressure between 0.3 MPa and 0.7 MPa and screw surface speed between 0.2 m/s and 0.4 m/s are common starting values on machines with clamp force between 800 kN and 12,000 kN. If a high-shear screw is retained, barrel temperatures should be reduced by 5 °C to 10 °C in the metering zone to compensate for shear heating. Screw cushion should be maintained at 4 mm to 8 mm to allow consistent switchover from velocity to pressure control.

    Injection velocity profiling is employed because thin sections freeze off rapidly at high mold-cooling rates. For caps and closures, a filling time between 0.3 s and 0.6 s reduces premature freeze-off in tamper bands. In thick-walled pails, filling time between 1.5 s and 2.5 s prevents jetting and flow marks. The transition from velocity control to pressure control should occur at 95% to 98% of the injected volume to avoid pressure spikes. Short-shot studies on the target tool are required because published data for this specific configuration is limited.

    Mold temperature affects surface finish and shrinkage. For wall sections below 1.0 mm, a mold temperature of 10 °C to 30 °C permits rapid tack-off and short cooling time. For wall sections above 3.0 mm, mold temperature between 40 °C and 60 °C reduces sink marks and improves dimensional stability after 24 h conditioning at 23 °C and 50% relative humidity. Holding pressure should be applied until gate freeze-off; premature gate freeze-off in thin-wall caps produces voids near the gate and increases rejects. A holding-pressure stage of 40 MPa to 70 MPa hydraulic is typical for medium-flow HDPE on machines with 40:1 intensification ratio.

    On production lines with hot-runner systems, a common failure mode is uneven gate freeze-off caused by hot-runner setpoint drift. Because LH606 solidifies within a narrow semi-crystalline freezing range, a 5 °C nozzle variation can translate to visible gate-stringing or short shots. Hot-runner controllers should maintain nozzle temperatures within ±2 °C of setpoint. In molds with tunnel gates, gate diameter below 0.8 mm can increase shear heating and require higher melt temperature, which then increases degradation risk. Rear zone 160 °C to 180 °C, center zone 180 °C to 200 °C, front zone 190 °C to 210 °C, and nozzle 190 °C to 220 °C are common barrel profiles on single-screw injection machines.

    Rheological Distinction from Blow-Molding and High-Flow Polyethylene Grades

    Against a typical blow-molding HDPE with nominal melt mass-flow rate of 0.3 g/10 min and density 0.955 g/cm³, LH606 has lower viscosity and shorter injection fill time in multi-cavity tools. The higher melt flow of LH606 reduces hydraulic pressure requirement and permits lower melt temperature, but the lower molecular weight proportionally reduces chain entanglement and can reduce environmental stress crack resistance measured by bent-strip testing under ASTM D1693. In thick-walled industrial pails exposed to aggressive detergent solutions, a lower-melt-index grade may outperform LH606, whereas in thin-walled closures and housewares the reduction in cycle time may justify the substitution.

    Compared with high-flow HDPE grades at 20 g/10 min, LH606 retains higher tensile yield stress and flexural modulus because the higher-molecular-weight fraction increases chain packing and resistance to plastic deformation. The same molecular-weight difference gives LH606 better low-temperature notched impact performance, but higher injection pressure is required at equivalent melt temperature. In high-cavitation cap tools with flow length-to-wall-thickness ratios above 300:1, high-flow grades may be preferred unless gas-assisted molding or higher melt temperature is available.

    USI Corporation HDPE LH606 also differs from linear-low-density polyethylene of density 0.918 g/cm³ in bending stiffness, slow-crack growth resistance, and organoleptic performance. The higher density of LH606 provides higher flexural modulus but lower dart impact and lower elongation at break. It is therefore selected for rigid articles rather than unsupported films or deep-draw packaging. Comparative tensile values are shown in the property table above.

    When LH606 Is Substituted in Thin-Wall Caps, Pails, and Industrial Components

    In cap and closure tools with 32 or 48 cavities, the melt flow rate of 6.0 g/10 min permits filling of thin tamper-evident bands and hinge regions without excessive gate pressure. Hot-runner balance should be checked with injection-pressure monitoring; a cavity-to-cavity fill imbalance above 5% by part weight can indicate gate wear or melt-temperature drift. Parts ejected at 70 °C to 80 °C surface temperature show acceptable dimensional recovery after 24 h ambient conditioning when tested by ISO 291:2008 standard atmosphere.

    Industrial pails and rigid containers molded on machines with 2,000 kN to 10,000 kN clamp force are within the processing range of LH606 when wall thickness is at least 1.5 mm. For wall thickness below 0.8 mm, published data for this specific configuration is limited; flow-length validation should be performed with a capillary rheometer and short-shot studies before tool commissioning.

    When replacing a lower-melt-index HDPE in an existing mold, the injection velocity profile and holding-pressure time should be revalidated. LH606 will reach gate freeze-off differently because its higher melt flow under ISO 1133-1:2022 produces a lower pressure drop across the runner. A qualified process for a 0.3 g/10 min resin cannot be transferred without modification; switchover position and holding pressure should be established from short-shot studies.

    Regulatory Compliance Ends at the Pellet Unless Final Articles Are Revalidated

    Base resin compliance is commonly evaluated under FDA 21 CFR 177.1520 for olefin polymers and Regulation (EU) No 10/2011 for plastic food-contact materials. However, conversion additives, regenerated material, masterbatch carriers, and processing aids may alter overall migration or specific migration values. A molded article cannot be assumed to comply with FDA 21 CFR 177.1520 or Regulation (EU) No 10/2011 solely from pellet compliance; the finished article must be tested by the appropriate migration method.

    In food-contact articles, overall migration is not solely a function of base resin. The diffusion coefficient of additives in the semicrystalline HDPE matrix depends on crystallinity and temperature; migration testing must therefore be conducted on the finished article under Regulation (EU) No 10/2011 Annex V or EN 1186 methods. If the article contains post-consumer recyclate, EU recycled-material requirements may apply and require additional barrier or purity verification.

    Regulatory and standards checklist applicable to base-pellet evaluations of USI Corporation HDPE LH606
    AreaReference method or regulationApplication
    Melt mass-flow rateISO 1133-1:2022, ASTM D1238-20Incoming resin control
    DensityISO 1183-1:2019, ASTM D1505-18Incoming resin control
    Tensile propertiesISO 527-2:2012, ASTM D638-14Mechanical verification
    Notched Izod impactISO 180/A, ASTM D256-23Mechanical verification
    Heat deflection temperatureISO 75-2:2020 method B at 0.455 MPa, ASTM D648-18Thermal verification
    Vicat softening temperatureISO 306, ASTM D1525-17Thermal verification
    Food-contact olefin polymersFDA 21 CFR 177.1520Base resin for food-contact articles
    EU food-contact materialsRegulation (EU) No 10/2011Finished article migration testing
    EU chemical registrationRegulation (EC) No 1907/2006REACH substance registration
    Hazardous substancesDirective 2011/65/EU Annex IIRoHS restricted substance evaluation

    When reusing sprues, runners, or rejected parts, the addition level should not exceed 20 wt% to 30 wt% without testing the melt mass-flow rate of the blend because multiple heat histories can shift the value by several tenths of a gram per 10 min. Lot-specific verification of density, melt flow rate, and part dimensions remains necessary before production release when switching from another HDPE grade.