Usi Corporation Hdpe Lh606 13

USI Corporation HDPE LH606-13

    • Product Name: USI Corporation HDPE LH606-13
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 710309
    Density 0.960 g/cm3
    Melt Flow Rate 13 g/10 min at 190°C/2.16 kg
    Tensile Strength At Yield 28 MPa
    Elongation At Break >500%
    Flexural Modulus 1100 MPa
    Izod Notched Impact Strength 40 J/m at 23°C
    Shore D Hardness 65
    Vicat Softening Point 125°C
    Heat Deflection Temperature 75°C at 0.46 MPa
    Mold Shrinkage 1.5-3.0%
    Brittleness Temperature < -70°C
    Environmental Stress Crack Resistance 30 h
    Water Absorption < 0.01%
    Dielectric Strength 20 kV/mm
    Volume Resistivity > 10^16 ohm-cm
    Dielectric Constant 2.3
    Dissipation Factor 0.0005

    As an accredited USI Corporation HDPE LH606-13 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing USI Corporation HDPE LH606-13 is supplied in 25 kg net bags, typically 40 bags per pallet.
    Container Loading (20′ FCL) 20′ FCL: USI HDPE LH606-13 in 25 kg bags, about 17.5 MT net, securely loaded and lashed for export.
    Shipping USI Corporation HDPE LH606-13 is a non-hazardous high-density polyethylene resin. Not regulated for sea, air, or road transport. Supplied in 25 kg bags or 1,000 kg jumbo bags, palletized and shrink-wrapped. Store dry, cool, ventilated; avoid moisture, direct sunlight, contamination, ignition sources, and strong oxidizers.
    Storage Store USI Corporation HDPE LH606-13 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, and open flames. Keep original bags/packaging sealed, palletized, and off the floor to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and excessive stacking. Use clean handling equipment, follow FIFO rotation, and comply with local regulations. Ideal temperature: 10–30°C.
    Shelf Life USI Corporation HDPE LH606-13 shelf life: about 24 months when stored unopened in a cool, dry, well-ventilated area.
    Application of USI Corporation HDPE LH606-13

    In the production of 20–30 L monolayer HDPE jerrycans for viscous industrial chemicals, USI Corporation HDPE LH606-13 is processed on shuttle or continuous-extrusion blow molding machines with screw diameters from 65 mm to 90 mm and L/D ratios from 24:1 to 32:1. Melt temperature measured at the die bushing is held between 190°C and 220°C. The lower half of that range reduces parison sag but increases extrusion pressure and melt fracture risk. Parison programming is applied through an axial wall-thickness profile from approximately 3.5 mm at the shoulder to 2.0 mm in the body and 4.0 mm at the pinch-off. Blow air pressure is set at 0.6–0.9 MPa; mold temperature is maintained at 10°C to 25°C. Blow mold construction includes vented pinch areas and beryllium-copper inserts in neck and handle regions. Internal tail flash and side trim are re-introduced at 20–40 wt% with virgin material. Higher regrind fractions reduce environmental stress crack resistance and top-load creep. A pigment masterbatch is let down at 2–4 wt%, and the masterbatch carrier must be a compatible polyethylene to avoid weld-line weakening. Containers are evaluated under the UN Recommendations on the Transport of Dangerous Goods, UN 1H1/1H2, for drop impact, leakproofness, and internal hydraulic pressure. Long-chain chemical contact tests are required because HDPE permeability and stress crack behavior depend on the specific solvent or surfactant. Top-load creep is measured at 40°C under 80% relative humidity. Borderline results typically appear when the regrind fraction exceeds 40 wt% or when mold temperature drops below 10°C.

    What Limits Dimensional Tolerance in High-Speed Polyolefin Closure Molds?

    Closures for detergent and agrochemical bottles are injection molded from USI Corporation HDPE LH606-13 at high cavitation. Typical tooling uses 16–64 cavities with valve-gated hot runners. Injection molding machines with clamp force from 150 t to 350 t are selected depending on cavity count, closure diameter, and projected area. Melt temperature is held between 210°C and 235°C. Mold temperature is maintained at 8°C to 20°C with turbulent water flow. Filling speed is set at 100–250 mm/s. Holding pressure is applied at 45–70 MPa for 1.5–3.0 s, followed by cooling time determined by wall thickness. A 28 mm tamper-evident closure is typically held to an inner diameter tolerance of ±0.05 mm and ovality below 0.4 mm. These tolerances are sensitive to hot runner imbalance, check ring wear, and inconsistent regrind level. A slip masterbatch based on erucamide is let down at 0.2–0.3 wt% to reduce dynamic coefficient of friction to 0.2–0.3 measured per ASTM D1894. Higher slip additive loadings create plate-out on the core pin and thread streaks. Antistatic masterbatch at 0.5–1.5 wt% is used for dry-goods closures where dust attraction must be limited. Tensile yield strength of the molded closure is measured according to ASTM D638. Food-contact closures require final-article compliance with 21 CFR 177.1520 and EU 10/2011, not merely pellet conformity. REACH annexes and RoHS 2011/65/EU apply to electrical or electronic packaging. Long residence time in hot runners beyond approximately 10 min at the high melt temperature leads to oxidation, yellowing, and loss of elongation. Published data for this specific grade in high-cavity closure tooling is limited; mold trials are required because gate size, cooling layout, and hot runner balance override lab-derived values.

    Thermoformed Heavy-Gauge Sheet and Chill-Roll Set Point Influence

    Sheet extrusion lines producing heavy-gauge HDPE sheet for thermoformed material handling and anti-static dunnage use extruder diameters from 90 mm to 150 mm with L/D ratios from 30:1 to 36:1. A melt pump is positioned between the extruder and the flat die to damp pressure variation and maintain sheet thickness uniformity. Polished chill rolls are run at 85°C to 105°C; the lower set points produce undersized edge trim due to higher shrinkage, while the upper set points can cause sticking. Sheet thickness for industrial dunnage is commonly 2.0–6.0 mm. The formed part is produced by heating the sheet surface to 125°C to 135°C and then vacuum or pressure forming over a textured aluminum tool. HDPE has a narrow sag window compared with PS or ABS, so upper and lower IR heaters must be independently zoned. Carbon black masterbatch is added at 5–12 wt% to achieve a static dissipative surface resistivity of 10^6–10^9 Ω measured per IEC 61340-2-3. Conductive HDPE tray formulations at higher carbon black loadings can drop into the 10^3–10^6 Ω range but lose elongation at break and become brittle at lower temperatures. Flexural modulus, measured per ASTM D790, is used to confirm that the carbon black loading has not reduced the rigidity required for rack storage. Pre-drying of LH606-13 sheet feedstock is usually not required at relative humidity below 50%; if surface condensation occurs, 60–80°C forced-air drying for 1–2 h prevents splay. The final dunnage trays are RoHS-compliant and are evaluated for stack loading at 40°C. The main processing conflict is that higher carbon black levels improve ESD performance but require lower sheet forming temperature to avoid local thinning and hole formation.

    Forming routeMelt temperature rangeTool/chill roll temperatureWall thicknessPrimary test standard
    Extrusion blow molding, 20–30 L containers190–220°C10–25°C2.0–3.5 mmASTM D1693
    Injection molded closures210–235°C8–20°C0.8–2.0 mmASTM D638
    Heavy-gauge sheet extrusion/thermoforming190–220°C85–105°C2.0–6.0 mmASTM D790

    A separate processing envelope applies to household cleaner and cosmetic bottles where wall thickness is reduced below 1.2 mm and high-speed rotary or dual-head shuttle blow molding is used. USI Corporation HDPE LH606-13 is processed at melt temperatures from 185°C to 205°C to retain parison melt strength in narrow, elongated shapes. Mold temperature is kept at 5°C to 15°C. Blow air pressure is 0.8–1.0 MPa. A 500 mL trigger spray bottle is commonly molded at 18–24 g with wall thickness 0.6–1.1 mm. Top-load strength is specified at 80–120 N. Drop impact is tested after conditioning at -10°C for 48 h from a height of 1.2 m. Post-consumer recycled HDPE can be added at 25–40 wt% in the middle layer of three-layer structures or in monolayer blends, but ESCR and odor tests must be repeated. A white masterbatch is let down at 2–3 wt%. The trigger spray bottle market imposes compatibility with bleaches, quaternary ammonium disinfectants, and surfactants; stress cracking is therefore evaluated with the filled product at 40°C rather than with a standard test fluid alone. Cosmetic and household chemical bottles must comply with the final packaging provisions of EU 1223/2009, REACH 1907/2006, and in food-related uses FDA 21 CFR 177.1520. The main production bottleneck is flash removal on high-output wheels, where regrind levels above 50 wt% introduce gel particles and reduce burst strength.

    200-L L-Ring Drums: Hydraulic Pressure and Stack Test Sequencing

    Blow molding of 200-L L-ring drums requires large accumulator-head machines with screw diameters from 120 mm to 150 mm, shot capacity above 20 kg, and clamp force from 800 t to 1500 t. USI Corporation HDPE LH606-13 is melted at 200°C to 220°C. Mold temperature is held at 10°C to 25°C. The parison profile is programmed to give a sidewall thickness of 4.2 mm, a top chime thickness of 5.0 mm, and a bottom chime thickness of 5.5 mm. Cooling time ranges from 120 s to 180 s. Internal post-industrial regrind is used at 10–20 wt% in the middle layer or in the entire wall only after UN qualification is repeated. A UV stabilizer masterbatch with HALS is let down at 0.3–0.5 wt% for outdoor storage. The finished drum is subjected to drop impact at 1.2 m after filling to rated capacity. Internal hydraulic pressure is applied at 100 kPa for 10 min for standard liquids; higher pressures up to 250 kPa are required for elevated-density products and for some Packing Group I applications. Stack testing is conducted at 40°C for 28 days with filled drums stacked 3 high. The most common failure mode is environmental stress cracking at the L-ring junction after long-term contact with aggressive liquids; ASTM D1693 condition B data alone does not capture the stress concentration at the chime. Published data for this specific grade in full-scale UN-certified 200-L drums is limited; certification must be re-established on the actual blow molding line because wall-thickness distribution, mold venting, and drop orientation dominate the result.

    ApplicationStandard or regulationTypical test value
    Jerrycans and 200-L drums for dangerous goodsUN 1H1/1H2drop impact 1.2 m; hydraulic pressure 100 kPa for 10 min
    Food-contact closures and bottlesFDA 21 CFR 177.1520, EU 10/2011overall migration <10 mg/dm²
    ESD industrial dunnageIEC 61340-2-3surface resistivity 10^6–10^9 Ω
    Household cleaner and cosmetic bottlesEU 1223/2009, REACH 1907/2006drop impact 1.2 m at -10°C
    Injection molded closuresASTM D638tensile yield strength >20 MPa
    Free Quote

    Competitive USI Corporation HDPE LH606-13 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    USI Corporation HDPE LH606-13 is a high-density polyethylene homopolymer supplied as cylindrical pellets. The grade is distinguished by a nominal density of 0.960 g/cm³ determined according to ISO 1183-1 and a melt mass-flow rate of 0.60 g/10 min at 190 °C/2.16 kg according to ISO 1133-1:2022. Because the density places the material in the upper crystalline range for polyethylene, the product exhibits high flexural modulus and yield strength, but it also exhibits a narrower heat-sealing window than lower-density ethylene copolymers. The grade is primarily specified for blown-film structures in which stiffness permits down-gauging: T-shirt bags, drawstring garbage bags, industrial liners, and coextruded films where moisture barrier and mechanical rigidity are required. It is not a direct replacement for butene-based LLDPE or LDPE in packaging machines calibrated for low seal-initiation temperatures. The suffix -13 denotes a manufacturer-specific stabilizer formulation; the precise additive package is proprietary, and downstream users should request REACH, RoHS, and food-contact conformity documents for the intended jurisdiction.

    What Processing Window Governs Blown Film Extrusion of LH606-13?

    The conversion of LH606-13 on annular blown-film lines is typically performed with a melt temperature of 190 °C to 220 °C at the die lip. A five-zone barrel profile from 170 °C at the feed throat to 210 °C at the adapter is used on single-screw extruders having 24:1 L/D and grooved feed sections. On a 45 mm diameter extruder of this configuration, screw speeds between 80 min⁻¹ and 120 min⁻¹ are common; corresponding throughputs for this melt-flow class are 45 kg/h to 60 kg/h. These throughput values are equipment-specific and should not be interpreted as intrinsic polymer limits.

    The annular die gap is maintained at 0.8 mm to 1.2 mm. Die gaps below 0.6 mm increase shear heating and may destabilize the bubble because the zero-shear viscosity is higher than that of injection-molding HDPE grades. A blow-up ratio of 3.0:1 to 4.5:1 and a frost line height of 6 to 10 die diameters are used to balance machine-direction and transverse-direction orientation. At blow-up ratios above 5.0:1, transverse-direction tensile strength increases, but the bubble may show excessive side-to-side movement, producing gauge bands. At frost line heights below 4 die diameters, surface roughness and inconsistent dart drop values have been observed in production-scale verification; published data for this exact grade at high output is limited.

    Because the density is 0.960 g/cm³, crystallization proceeds rapidly after the melt exits the die. External air-ring and internal bubble cooling should be adjusted so that the freeze line temperature at the film surface is below 90 °C before the collapsing frame. Internal bubble cooling is recommended when layflat widths exceed 600 mm. Without internal bubble cooling, heat removal from the inner bubble surface becomes the throughput-limiting step, and gauge uniformity can drift by more than ±5 % at output above 80 kg/h. The internal cooling airflow should maintain a frost line height stable within ±2 die diameters; wider variation correlates with dart impact variability exceeding ±10 % around the mean.

    At high screw speeds of 120 min⁻¹ and above, bubble instability may appear as a low-frequency oscillation in layflat width. The instability is typically corrected by reducing the lower barrel temperature by 5 °C to 10 °C or by increasing the blow-up ratio by 0.5 unit. Melt temperature measurements at the die lip are made with an immersion thermocouple at the die gap; readings below 180 °C produce high melt pressure and can overload the extruder drive. On 45 mm grooved-feed extruders with a 24:1 L/D screw, a melt pressure at the breaker plate of 300 bar to 450 bar is typical for this melt-flow range. Pressure exceeding 450 bar indicates excessive screen contamination or insufficient heater capacity in the adapter.

    Pellets do not require pre-drying unless condensation has formed on pellet surfaces or wet regrind is introduced. In such cases, hopper-air drying at 60 °C to 80 °C for 1 h to 2 h is used. Drying above 90 °C is unnecessary and may increase dust generation. If wet pellets are processed without drying, the resulting steam can create micro-bubbles in the film, visible as reduced clarity and lower dart impact.

    Mechanical Properties, Barrier Thresholds, and Down-Gauging Limits

    Selected physical and mechanical properties from compression-molded specimens are summarized below. Specimens are conditioned at 23 °C and 50 % relative humidity for 40 h in accordance with ISO 291. Values are typical and should not be interpreted as batch-release specifications.

    PropertyTest methodTypical value
    DensityISO 1183-10.960 g/cm³
    Melt mass-flow rate, 190 °C/2.16 kgISO 1133-1:20220.60 g/10 min
    Tensile stress at yieldISO 527-229.4 MPa
    Elongation at breakISO 527-2600 %
    Flexural modulusISO 1781.30 GPa
    Notched Izod impact strength, 23 °CISO 180/A4.5 kJ/m²
    Vicat softening temperatureISO 306/A120126 °C
    Shore hardness DISO 86866

    In thin-gauge film, the grade develops anisotropic tensile properties. At a blow-up ratio of 3.5:1 and die gap of 1.0 mm, machine-direction tensile stress at yield is typically 20 % to 30 % higher than the transverse-direction value. This asymmetry is a direct result of machine-direction orientation and should be included when specifying minimum tensile strength for bag handles and load-bearing liners. Tear resistance is also anisotropic; transverse-direction Elmendorf tear is often higher than machine-direction tear, matching the general behavior of high-density blown film.

    Moisture vapor transmission rate follows crystallinity. A film with density 0.960 g/cm³ has a crystalline fraction of approximately 70 % to 75 % by density, compared with 40 % to 50 % for typical butene-based LLDPE. Under ASTM F1249 conditions at 38 °C and 90 % relative humidity, this crystallinity difference lowers the moisture vapor transmission rate by 40 % to 60 % relative to equivalent-gauge LLDPE. The practical consequence is that LH606-13 can be down-gauged in moisture-barrier liners. The flexural modulus of 1.30 GPa allows an 18–22 µm film to match the bending stiffness of a 30 µm LLDPE film with flexural modulus 0.30 GPa, as calculated from the cubic thickness-stiffness relationship; dart impact and puncture resistance must nevertheless be revalidated at the lower gauge.

    When Stiffness Is Prioritized over Seal Initiation Temperature

    Substitution of LH606-13 for butene-based LLDPE in vertical form-fill-seal packaging shifts seal initiation temperature upward by 20 °C to 30 °C. Rotary sealing units calibrated for LLDPE at 105 °C to 115 °C do not develop acceptable seal strength with high-density film. Seal-bar setpoints of 130 °C to 145 °C with dwell times of 0.2 s to 0.5 s are generally required for monolayer films in the 20 µm to 40 µm gauge range. Hot-tack strength also differs; high-density polyethylene exhibits a narrower hot-tack window, and the cooling side of the seal jaw must provide rapid solidification to avoid seal stretching.

    On production-scale bag conversion lines, a common failure mode is seal-area puckering when seal-bar temperatures are set for LLDPE. The high-density film reaches a fully molten state only above 130 °C; at 115 °C, the seal remains weak and opens under 2 N to 4 N peel force, whereas a properly formed seal at 140 °C may exceed 15 N/15 mm. These peel force values should be verified using ASTM F88. Seal-bar pressure of 0.3 MPa to 0.5 MPa and serrated jaws are used to compensate for the narrower sealing window.

    Compared with lower-density HDPE grades from the same producer, LH606-13 provides higher flexural modulus and tensile yield strength because of its higher density, but lower dart impact and Elmendorf tear values are expected. Direct published comparative data for all USI Corporation grades is limited; the inverse correlation between density and dart drop impact is documented in polyethylene testing literature. For applications requiring subambient toughness, blending with 20 wt% metallocene LLDPE typically improves dart impact resistance while reducing flexural modulus by 5 % to 8 %, based on linear mixing approximations. Such modification moves the material away from the original density specification and should be validated against ASTM D1709, ASTM D1922, and ASTM D882.

    The melt mass-flow rate of 0.60 g/10 min is lower than injection-molding HDPE grades, which typically have melt flow rates of 5 g/10 min to 20 g/10 min. Consequently, the grade is unsuitable for thin-wall injection molding; long flow paths, weld lines, and excessive filling pressures result when it is run in molds designed for high-flow grades. Screw recovery time on a 120-ton injection molding machine with a 32 mm screw will be substantially longer, and published data for this specific configuration is limited.

    Stabilizer Chemistry and Regrind Tolerance Differ from Injection Grades

    The grade contains a stabilizer package designed for film extrusion at melt temperatures up to 220 °C. Running at barrel temperatures above 250 °C creates oxidative degradation products that appear as yellowing and gel particles at the die lip; melt pressure fluctuations greater than 5 % across a 40/60/80-mesh screen pack indicate gel accumulation. The screen pack should be inspected when pressure drop across the pack exceeds 80 bar to 120 bar on 120 mm annular dies, although exact thresholds depend on die geometry and throughput.

    The grade should not be dry-blended with high levels of calcium stearate or zinc stearate unless the stabilizer package is validated, because free metal ions can reduce oxidation induction time. Oxidation induction time above 20 min at 200 °C under oxygen, measured by differential scanning calorimetry per ISO 11357-6, is typical for fresh pellets; lower values after multiple heat histories indicate stabilizer consumption from regrind. This test is used on production lines to monitor regrind quality, not as a specification.

    Edge trim and startup scrap can be reintroduced at up to 20 wt% without reducing bubble stability, provided the regrind is dry and free of paper labels. Higher regrind addition may increase gel counts and alter dart drop impact. The ground fluff bulk density of 0.30 g/cm³ to 0.40 g/cm³ is lower than pellet bulk density of 0.55 g/cm³ to 0.60 g/cm³, so volumetric feeders must be recalibrated when fluff is added. A screen pack of 40/60/80-mesh is typically used to trap contaminants; pressure drop across the pack should be logged and used to schedule screen changes.

    The grade is not formulated for prolonged UV exposure without additional carbon black or UV stabilizer masterbatch. For agricultural film or geotextile applications, 2 wt% to 3 wt% of a carbon black masterbatch is typically compounded into the film, but this addition shifts elongation at break and should be evaluated under ISO 4892-2 weathering cycles. Pellets should be stored in closed silos or hopper loaders with ambient temperature below 40 °C. Prolonged storage under direct sunlight can cause yellowing even with stabilizer, and high humidity can create pellet surface condensation that carries into the extruder.

    Regulatory compliance is application-specific. The base polymer may be evaluated under FDA 21 CFR 177.1520 for olefin polymers and EU Regulation (EU) No 10/2011 for plastic food-contact materials. Users must obtain the manufacturer’s conformity letter for the exact additive package in LH606-13, because the compliance status of the formulated grade depends on the antioxidant system and the intended food-contact conditions. For room-temperature storage of dry foods, the relevant overall migration limit is 10 mg/dm² of food-contact surface area; fatty foods or hot-fill conditions require additional simulant testing. For non-food packaging, REACH and RoHS declarations are typically provided by the supplier.