| HS Code | 628715 |
| Elongation At Break | >=500 |
| Brittleness Temperature C | <-70 |
| Volume Resistivity Ohm Cm | >1e16 |
| Water Absorption | <0.01 |
As an accredited USI Corporation HDPE LH523 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | USI Corporation HDPE LH523 is supplied in 25 kg polyethylene-lined bags, typically palletized at 1,000 kg per pallet. |
| Container Loading (20′ FCL) | A 20′ FCL typically loads 18 MT of USI HDPE LH523, packed in 25 kg bags, either floor-loaded or palletized. |
| Shipping | USI Corporation HDPE LH523 is a non-hazardous high-density polyethylene resin, not regulated for transport. It is typically shipped in 25 kg bags or jumbo bags, palletized and stretch-wrapped, in dry containers or trucks. No special hazard class, UN number, or placard required. Keep dry and away from heat, sunlight, and contamination. |
| Storage | Store USI Corporation HDPE LH523 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, flames, and strong oxidizers. Keep original bags/containers sealed, palletized, and off the floor to prevent moisture and contamination. Avoid prolonged UV exposure and static buildup. Maintain stable temperature, good ventilation, and safe stacking; follow SDS/local regulations. Do not store near food, feed, or incompatible materials. |
| Shelf Life | Shelf Life: No defined shelf life; stable indefinitely if stored cool, dry, sealed, and away from direct sunlight and contaminants. |
Extrusion blow moulding of 20–30 L open-top jerricans from LH523 is carried out on accumulator-head machines with screw diameters between 80 mm and 120 mm, L/D ratios of 24:1 to 30:1, and shot capacities of 3–8 kg. The resin is a high-molecular-weight HDPE blow moulding grade; manufacturer-published data list a density of 0.952 g/cm³ (ASTM D1505) and a melt index below 0.30 g/10 min at 190°C/2.16 kg (ASTM D1238). Barrel temperatures are set at 170–180°C in the feed zone, 190–205°C in compression, and 200–215°C in metering, with the die head held at 195–210°C. Melt pressure at the die entrance is maintained between 250 bar and 350 bar; operation above 400 bar causes shear heating that initiates melt fracture and disrupts parison surface finish. Parison programming uses 15–30 wall-thickness points to compensate for parison sag; handle pinch points are programmed 0.4–0.8 mm thicker than the label panel because the parting-line weld remains a drop-impact stress concentrator. Clean in-plant regrind from trimmed flash and rejected pre-consumer containers is added at ≤20 wt%; higher additions reduce notched environmental stress crack resistance and lower the ductile-to-brittle transition of the pinch-off weld. Post-consumer recyclate is not used in UN-certified dangerous goods packagings unless the design type is retested and approved by the competent authority. Outdoor silo storage in high-humidity sites can leave surface condensation on cold pellets; hopper pre-warming at 60°C for 30–60 min avoids splay at the die lip. On-line defects include handle pinch-off thinning, parison curl from die temperature imbalance, and flash thickness variation above 10% causing clamp bounce. Terminal articles include 20 L open-top jerricans for liquid agrochemicals, 25 L UN 3H1 jerricans for hydrocarbon solvents, and 30 L containers for water-based emulsions. Qualification is documented under UN Model Regulations Chapter 6.1 and US DOT 49 CFR 178.509; periodic design revalidation covers drop testing at −18°C, leakproofness, hydrostatic pressure, and stacking at 40°C for 28 days.
| Test | US DOT method | UN Model Regulation reference | Typical failure mode observed on line |
|---|---|---|---|
| Drop impact | 49 CFR 178.603 | 6.1 design type | Brittle pinch-off weld at −18°C |
| Leakproofness | 49 CFR 178.604 | 6.1 design type | Cap gasket compression set |
| Hydrostatic pressure | 49 CFR 178.605 | 6.1 design type | Wall thinning at handle pinch point |
| Stacking | 49 CFR 178.606 | 6.1 design type | Creep at 40°C |
Monolayer extrusion blow moulding of 500 mL to 1.5 L bleach and detergent bottles from LH523 is performed on continuous-extrusion shuttle machines with 2–4 cavities, clamp force from 8 t to 20 t, and blow-up ratios between 2.2:1 and 3.0:1. Mold temperature is held at 10–18°C; mold surfaces below 8°C promote condensation and pinhole defects. The cycle time for a 1 L bottle is 14–18 s, with blowing air pressure at 0.6–0.8 MPa and exhaust time of 2–3 s before mold opening. Wall thickness at the label panel is set at 0.35–0.55 mm, while the bottom pinch-off is retained at 0.6–1.2 mm because hypochlorite-induced environmental stress cracking tends to initiate at the weld line. Pigment masterbatch is added at 2–3 wt% with an LLDPE carrier; direct pigment powders above 1 wt% alter die swell by 10–15% and disturb parison programming. Clean in-house regrind from flash is limited to ≤15 wt%; above that level, stress crack resistance under hypochlorite contact declines below the internal threshold. Stress crack resistance is verified per ASTM D1693-15 Condition B in 100% Igepal CO-630 at 50°C, with an internal specification of F50 above 100 h. If melt temperature at the bottom parting line drops below 190°C, the weld fails before the sidewall ESCR limit is reached. Terminal articles include hypochlorite bleach bottles, liquid laundry detergent bottles, and hard-surface degreaser packs. Compliance for packaging waste is assessed under EU Directive 94/62/EC; resin and additive components are screened under REACH Article 33.
In six-layer co-extrusion blow moulding for 1–10 L agricultural chemical containers, LH523 is used as the virgin outer and inner structural layers, with an EVOH barrier layer and maleic anhydride grafted tie resins. The layer distribution is commonly 25% LH523 outer skin, 35% in-house regrind core, 5% tie, 3% EVOH, 5% tie, and 27% LH523 inner skin. Extruder temperature profiles are set at 185–210°C for HDPE and 190–210°C for EVOH, while the co-extrusion die head is held at 200–215°C. Melt viscosity mismatch at the EVOH/HDPE interface is managed by keeping the EVOH layer below 8% of total wall thickness and selecting tie resins with melt flow rates within 1.0–2.0 g/10 min of the LH523 layer. Interfacial instability appears as a zig-zag pattern at the EVOH layer when die gap variation exceeds 0.05 mm. Chemical compatibility is evaluated by filling molded containers with the actual formulation and storing at 40°C for 30 days; weight loss and weld-line permeation are then measured chromatographically. Terminal products include 1 L bottles for emulsifiable concentrates, 5 L containers for suspension concentrates, and 10 L containers for solvent-based adjuvants. UN 3H1 qualification applies to formulations containing xylene or cyclohexanone; drop impact after hot storage and stack creep at 40°C must be revalidated when active ingredient concentration changes. Published data for LH523 in extended immersion with high-polarity organophosphate formulations is limited; end users must validate each commercial formulation.
| Layer position | Material | Weight proportion | Function |
|---|---|---|---|
| Outer skin | LH523 | 25% | ESCR shell |
| Core | In-house HDPE regrind | 35% | Cost recovery |
| Tie | MAH-grafted PE | 5% | Adhesion to EVOH |
| Barrier | EVOH | 3% | Solvent permeation control |
| Tie | MAH-grafted PE | 5% | Adhesion to inner skin |
| Inner skin | LH523 | 27% | Chemical contact layer |
Accumulator-head machines processing LH523 into 200 L tight-head drums operate with 15–25 kg shot capacities, clamp force from 80 t to 150 t, and die diameters of 300–500 mm. Barrel temperatures are set between 180°C and 220°C, with the accumulator and die held at 195–210°C. Parison programming uses 50–100 wall-thickness points; thickness is tapered from 3.0 mm at the top flange to 4.5 mm in the bottom corner. Cycle time ranges from 180 s to 300 s. Melt pressure at the die entrance is maintained at 250–350 bar; pressures above 420 bar increase melt temperature above 225°C and reduce the hoop strength of the pinch-off weld. Mold cooling circuits use chilled water at 8–12°C; inlet-to-outlet coolant delta T is kept below 3°C to avoid differential shrinkage and top-load deformation. The bottom parting line is formed when the mold closes on the parison at a flash thickness of 0–10 mm. Under-clamping produces flash thicker than 12 mm; that excessive flash acts as a heat sink, cooling the weld below crystalline recrystallization temperature and producing a brittle joint that fails drop impact. Increasing mold closing speed to 300–500 mm/s and maintaining melt temperature above 195°C at the pinch-off improves weld strength. Clean internal regrind from flash and rejected drums is added at ≤25 wt%. Design qualification for hazardous liquids uses UN 1H1 drum standards; drop testing from 0.8 m at −18°C and stacking for 28 days at 40°C are re-run when regrind content changes. Finished products include 200 L tight-head drums for industrial lubricants and solvents, open-head versions for solid chemical slurries, and 120 L open-top drums for viscous resins.
Automotive windshield washer reservoirs of 2–5 L are blow-moulded from LH523 on suction blow moulding machines after continuous parison extrusion. Mold temperature is 10–16°C; clamp force is 30–50 t for a 3 L reservoir. After demolding, the part is held in a sizing fixture for 30–60 s to control neck insert shrinkage. Clean regrind from flash is limited to 10 wt% because weld strength and surface appearance are validation concerns. Sustained underhood exposure above 80°C causes creep and fitting loosening; LH523 reservoirs are therefore limited to fender- or cowl-mounted locations unless a 10–20 wt% talc-filled HDPE compound is used. Thermal cycling validation follows OEM procedures, commonly 10 cycles from −30°C to 80°C at 50% relative humidity, followed by pressure pulse testing at 0.3 bar. Blow pin neck geometry is maintained at 58–62 HRC; a hardness drop below 55 HRC and mold surface roughness above 0.8 µm increase thread ovality and cap leakage. Terminal products include 3 L washer reservoirs, 2 L headlamp wash bottles, and 5 L coolant overflow bottles for cold-climate programs. Published data for LH523 in underhood fluid reservoirs is limited; qualification against OEM thermal cycling and vibration standards is required before replacement of PP copolymer.
When high-gloss personal care bottles are moulded from LH523, neck calibration and blow pin geometry dominate dimensional stability. Long-stroke shuttle machines with 6–10 cavities are used. Polished stainless-steel molds with 0.05–0.10 µm surface roughness preserve gloss without flame treatment. Neck finishes are calibrated to PCO 28/410 or 24/410 dimensions; blow pin diameter is set 0.20–0.35 mm below the neck insert ID to limit ovality. Post-mold dimensional audit uses a plug gauge for PCO 28/410 thread ID; allowable ovality is 0.25 mm maximum across the parting line. Compressed air at 0.55–0.75 MPa is introduced for 3–6 s; exhaust time before mold opening is 2–4 s to prevent post-mold expansion. Pigment masterbatch is added at 1.5–2.5 wt%, and silicone-based mold release is limited to 0.1–0.3 wt% to avoid stress cracking at the bottle shoulder. Terminal articles include 200–750 mL shampoo bottles, body wash bottles with snap-fit hinge closures, and lotion bottles with shrink-sleeve label panels. Compliance for skin-contact packaging is assessed under EU Regulation (EC) No 1223/2009 for cosmetic products and REACH; US distribution typically relies on 21 CFR 177.1520 olefin polymer status for the base resin. Incompatibility arises with acetone-containing nail polish removers; those formulations require barrier packaging or a different substrate.
Competitive USI Corporation HDPE LH523 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
USI Corporation HDPE LH523 is a high-density polyethylene blow molding grade supplied in pellet form. Manufacturer-published typical values list a melt flow rate of 0.30 g/10 min at 190 °C under 2.16 kg load in accordance with ISO 1133-1 and a density of 0.953 g/cm³ measured under ASTM D1505. Tensile yield strength is given as 28 MPa at 50 mm/min under ASTM D638, with elongation at break of 600 %. Flexural modulus is 1,100 MPa under ASTM D790, and notched Izod impact is 8.0 kJ/m² under ISO 180/A. Environmental stress cracking resistance is reported as 60 h F50 under ASTM D1693, condition B, 100 % Igepal CO-630. Vicat softening temperature is typically 125 °C under ISO 306/A50, and brittleness temperature is below -70 °C under ASTM D746. The grade is specified for monolayer blow molded containers from approximately 0.5 L to 30 L, including liquid detergent bottles, bleach containers, cosmetic bottles, edible-oil bottles, and industrial chemical jerrycans. It is not intended for rotomolding, blown film, or thin-wall injection molding because the melt flow rate is too low for thin-wall filling and the molecular weight is too high for stable film die lip behavior at commercial line speeds.
Relative to USI HDPE LH554, a high-molecular-weight blow molding grade for large or aggressive chemical containers, LH523 has a higher melt flow rate and therefore lower extruder head pressure for the same screw speed. LH554 offers ESCR values above 100 h F50 under ASTM D1693, condition B, and is selected for agricultural chemical containers; LH523 is normally selected where 60 h F50 is sufficient and shorter cycle time or higher surface gloss has operational value. Relative to USI HDPE LH614, a high-flow injection-molding grade with a melt flow rate near 20 g/10 min, LH523 retains the parison melt strength required for blow molding; LH614 exhibits severe parison sag in continuous extrusion and cannot be substituted without changing the processing route. Compared with blown film grades such as LH606, LH523 has a higher density and higher flexural modulus, producing stiffer container sidewalls but lower tear resistance in film geometries.
On continuous shuttle extrusion blow molding lines equipped with 65 mm diameter barrier screws and 24:1 L/D ratios, LH523 is typically processed at barrel temperatures of 160–190 °C and die head temperatures of 170–190 °C. Accumulator-head machines with shot capacities of 1–2 kg are frequently operated with die temperatures reduced to 160–180 °C to limit parison sag during slow extrusion. Mold clamping force for containers up to 30 L is calculated at 0.06–0.08 kN/cm² of parting line projected area, using blow air pressure of 0.6–0.8 MPa. Melt pressure at the die head generally remains below 35 MPa; sustained pressures above 40 MPa indicate restrictive tooling or insufficient barrel temperature. The melt exhibits moderate die swell and a relatively narrow molecular weight distribution; parison programming with 30–40 point servo-hydraulic control is used to maintain wall thickness above 0.5 mm at the container shoulder and chime. Production records on shuttle lines indicate that sustained barrel temperatures above 200 °C increase neck flash and fold-over defects, while temperatures below 150 °C raise melt pressure and limit output. Screw speed is normally constrained by the need to avoid excessive shear heating; specific output values depend on screw design and head tooling.
Tooling design for LH523 generally uses a diverging die gap of 0.5–1.5 mm to compensate for differential swell along the parison circumference. Mold temperatures between 10 °C and 25 °C allow clean pinch-off weld flash and cycle times appropriate for shuttle operations. At mold temperatures above 30 °C, flash thickness increases and cooling time may extend, reducing output on multi-cavity wheel machines. The pinch-off insert should be maintained with a sharp land; rounded pinch-off geometry has been associated with weak weld lines and lower drop-impact resistance measured under ASTM D2463. For handled containers, the handle pinch-off zone is a known thin point; parison programming locally increases the die gap by 0.2–0.5 mm to redistribute the wall. Blow air should be filtered to 5 µm and dried to a pressure dew point below -40 °C to avoid water spots in translucent containers.
ASTM D1693 condition B is a constant-strain notched specimen test in 100 % Igepal CO-630 at 50 °C. The F50 value of 60 h reported for LH523 is a ranking criterion, not a direct container lifetime. Field ESCR failure occurs when surface-active agents penetrate amorphous tie-molecule regions under molded-in stress, producing craze growth followed by brittle crack propagation. Molded-in stresses at pinch-off welds, sharp corners, and handle attachment points can reduce the effective ESCR of a container below the value measured on compression-molded plaques. For detergent containers, stress concentrations above the fill line are typically minimized by increasing wall thickness above 0.7 mm and avoiding sharp transitions at the shoulder. If a container passes 60 h F50 material testing but fails in field service, the failure is often traced to excessive pinch-off weld orientation or to a higher service temperature than the test environment.
Regrind of LH523 flash and reject bottles can be reintroduced at ratios up to 30 % by weight without loss of extruder stability, provided the regrind is ground to particles below 8 mm and blended with virgin pellets before the hopper. Above 30 %, the additional thermal history increases gel formation and reduces ESCR; each additional pass through the extruder raises the gel count and can lower ASTM D1693 F50 below 30 h. Regrind containing detergent residues or bleach degradation products accelerates stress cracking and must be washed or rejected. Closed-loop systems should mix regrind and virgin material through an in-line gravimetric blender with accuracy of ±0.5 % on each component.
LH523 tolerates short-term melt temperatures up to 200 °C, but residence time at melt temperature should be kept below 15 min to avoid oxidative chain branching and gel formation. In accumulator-head machines with large shot capacity, the combination of high temperature and long residence time can produce yellowing, fish-eye defects, and burned material at the die lip. Purging with a low-molecular-weight HDPE or a dedicated purging compound is required after stalled production of more than 30 min. Nitrogen blanketing of the hopper is not normally required for natural grades, but colored or additive-containing compounds may require antioxidant protection validated by ISO 11358-1 thermogravimetric analysis.
Supplier documentation for LH523 indicates compliance with FDA 21 CFR 177.1520 for olefin polymers used in contact with food, subject to end-use limitations. For European Union applications, compliance with EU Regulation No 10/2011 requires converter validation of overall migration below 10 mg/dm² in the intended food simulant. The grade is generally not recommended for direct contact with fatty foods above 60 °C unless migration testing under OM2 conditions has been completed.
| Regulatory reference | Condition or limit | Status |
|---|---|---|
| FDA 21 CFR 177.1520 | Olefin polymers, food contact | Supplier declaration |
| EU Regulation No 10/2011 | Overall migration < 10 mg/dm² | Converter validation required |
| REACH SVHC | Concentration < 0.1 % w/w | Supplier declaration |
| RoHS | Pb, Hg, Cr(VI) < 1000 mg/kg; Cd < 100 mg/kg | Screened |
Although HDPE is not hygroscopic, pellet surface moisture can condense when material is transferred from cold storage to a warm production hall at relative humidity above 60 %. Surface moisture reduces visual clarity of the parison and can produce bubble defects in the container wall. In such conditions, a desiccant hopper with air inlet dew point below -20 °C and setpoint of 80 °C for 2 h is recommended. If regrind is used, moisture on stored bottle scrap should be removed before grinding; wet regrind can impede feeding and create blow holes at the pinch-off.
Chemical compatibility boundaries are critical for this grade because ESCR performance declines as stress, temperature, and oxidizing activity increase. LH523 is suitable for dilute sodium hypochlorite up to approximately 5 % active chlorine and for many household detergents at ambient temperature, but it is not recommended for strong oxidizing acids, aromatic hydrocarbons, or ketones above 40 °C. For agricultural emulsifiable concentrates, solvent-based car care products, or fuel-containing fluids, published data for this specific configuration is limited; high-molecular-weight grade LH554 or fluorination surface treatment should be evaluated. Continuous exposure to ultraviolet radiation requires a stabilizer package, and tests under ISO 4892-2 or ASTM G154 are necessary for outdoor storage containers.