| HS Code | 516693 |
| Density | 0.956 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 0.35 g/10 min |
| Tensile Strength At Yield | 26.5 MPa |
| Tensile Elongation At Break | >600% |
| Flexural Modulus | 1078 MPa |
| Izod Impact Strength Notched 23 C | 196 J/m |
| Vicat Softening Temperature | 125 °C |
| Heat Deflection Temperature 0 45 Mpa | 75 °C |
| Shore D Hardness | 65 |
| Environmental Stress Cracking Resistance Escr | >1000 h |
| Melting Point | 132 °C |
As an accredited USI Corporation HDPE LH506 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | USI Corporation HDPE LH506 is supplied in 25 kg bags, with 40 bags per 1,000 kg pallet. |
| Container Loading (20′ FCL) | 20′ FCL container loading of USI Corporation HDPE LH506, palletized 25 kg bags, securely stowed for ocean export. |
| Shipping | USI Corporation HDPE LH506 is shipped as non-hazardous high-density polyethylene resin pellets in 25 kg PP bags or 1000 kg jumbo bags, palletized and stretch-wrapped. Transport by sea, road, or rail in clean, dry containers at ambient temperature. Avoid moisture, contamination, direct sunlight, and sharp objects. Not regulated for transport. |
| Storage | Store USI Corporation HDPE LH506 in a cool, dry, well-ventilated warehouse, away from direct sunlight, rain, moisture, heat, sparks, and ignition sources. Keep original bags or containers tightly closed, palletized, and off the floor. Avoid contamination by dust, oils, or chemicals. Maintain moderate temperatures, protect from physical damage, and use first-in, first-out stock rotation to preserve resin quality. |
| Shelf Life | Shelf life is approximately 24 months from production when stored cool, dry, and ventilated, away from direct sunlight and heat. |
Across 25 L tight-head jerrican production lines, USI Corporation HDPE LH506 is processed on a single-station shuttle blow moulder equipped with a 90 mm grooved-barrel extruder at L/D 30:1. Melt temperature is held between 190 °C and 200 °C at the die head. The converging conical die gap is set from 2.0 mm to 3.0 mm depending on parison wall-thickness programming. Blow air pressure is maintained at 0.8 MPa to 1.0 MPa. Mould cooling water enters at 10 °C to 20 °C. Hydraulic clamp force for this container size is specified in the 450 kN to 600 kN range. Cycle time typically falls between 85 s and 120 s. In-house regrind is limited to 20 wt% of the total charge because the -18 °C drop test prescribed in 49 CFR 178.603 exposes pinch-off weld embrittlement when higher addition levels are used. The terminal article is a UN 3H1 jerrican for solvent, lubricant, and agricultural chemical distribution. Leakproofness after closure is assessed under 49 CFR 178.604. Hydrostatic pressure retention is verified under 49 CFR 178.605. Batch-to-batch melt pressure variation is held within ±0.5 MPa by gravimetric feeding, and parison length is adjusted through 200-point programming to maintain wall thickness above 2.5 mm at the pinch-off zone.
A second operational boundary for UN jerricans is surface condensation control. HDPE LH506 does not require bulk pre-drying in closed indoor warehouses. If regrind is stored in unheated silos where relative humidity exceeds 80%, surface moisture above 0.05 wt% can produce surface defects in the parison. Under those conditions, a hopper dryer at 70 °C for 2 h is applied to the regrind stream only. The failure mode observed on production-scale equipment is not gross water vapour formation but micro-porosity near the flash trim line. That porosity is detected by sectioning the pinch-off area and measuring thickness using a digital calliper referenced to ISO 1133-1:2022 material consistency checks.
On a six-layer accumulator-head co-extrusion line, HDPE LH506 forms the outer skin, inner skin, and regrind-bearing structural layers. Total HDPE skin content is set between 35 wt% and 50 wt% of tank wall mass. The regrind layer may constitute 30 wt% to 45 wt%. Ethylene vinyl alcohol barrier content is maintained at 2 wt% to 4 wt%. Adhesive tie layers are specified at 2 wt% to 4 wt% combined. The barrier material is pre-dried to below 0.05 wt% moisture before entering the extruder. Main HDPE melt temperature is kept at 200 °C to 220 °C. Barrier layer temperature is controlled separately to avoid thermal decomposition at the coextrusion feedblock. Accumulator capacity for this application is typically 20 kg to 35 kg. The parison is profiled with 200-point radial wall-thickness control. Mould surface temperature is held at 10 °C to 15 °C. This configuration produces an automotive fuel tank shell with a pinch-off seam and welded inlet, vent, and sender boss features.
Fuel tank compliance is anchored to ECE R34 Annex 5 for fire resistance and fuel permeation behaviour in motor vehicles. Whole-vehicle evaporative emission limits are referenced to 40 CFR Part 86.1811. In-house regrind from tank flash and start-up purges is permitted. Post-consumer HDPE is excluded because traceability of barrier-contaminating residues cannot be established. The limiting processing defect on six-layer tank lines is interfacial instability at the HDPE-tie-EVOH boundary. That instability appears as localised non-uniform barrier thickness when the intermediate layer exceeds 150 µm. Current production practice therefore keeps EVOH layer thickness in the 50 µm to 150 µm band. Published data for this specific six-layer configuration using HDPE LH506 is limited; equipment-specific validation remains required.
The applicable regulatory anchors for the container systems discussed in this section are summarised as follows.
| End-use category | Test or specification | Reference designation |
|---|---|---|
| UN tight-head jerrican | Drop, leakproofness, hydrostatic pressure | 49 CFR 178.603, 178.604, 178.605 |
| Automotive fuel tank | Fire resistance and fuel permeation | ECE R34 Annex 5 |
| Agrochemical container | Environmental stress cracking resistance | ASTM D1693-15ε |
| Fluorinated solvent container | Permeation retention and weight loss | ASTM D2684-18 |
| Outdoor technical tank | Accelerated xenon-arc weathering | ISO 4892-2:2013 |
Ester-based emulsifiable concentrate compatibility drives wall-thickness decisions in agrochemical bottle tooling. In a three-layer coextrusion shuttle line, HDPE LH506 is blended with a barrier polyamide at 4 wt% to 6 wt% and a maleic anhydride tie resin at 2 wt% to 3 wt%. The remaining 91 wt% to 94 wt% is HDPE. Main extruder diameter is 60 mm with L/D 28:1. Polyamide extruder diameter is 35 mm, and tie resin extruder diameter is 25 mm. HDPE melt temperature is set from 190 °C to 210 °C. Polyamide melt temperature is set from 230 °C to 250 °C. The polyamide layer is maintained between 40 µm and 80 µm to balance barrier performance and bottle drop impact. Terminal articles are 1 L, 5 L, and 10 L bottles for organophosphate and pyrethroid formulations. Environmental stress cracking resistance is measured under ASTM D1693-15ε condition B in 100% Igepal CO-630. F50 values in the 300 h to 600 h range are commonly specified for comparable blow-moulding HDPE in agrochemical service; current lot certificates for HDPE LH506 govern the final acceptance value.
The main process conflict in agrochemical bottle production is the competing requirement for barrier-layer thickness and pin-weld durability. Thicker polyamide improves solvent holdout but reduces parison weld strength because of reduced HDPE fusion at the pinch line. On a 1 L bottle cycle time of 15 s to 30 s, barrel temperature shifts of ±3 °C in the polyamide extruder are sufficient to move the layer distribution outside the specified band. Production lines therefore use gravimetric dosing on all three extruders. Mould close speed is reduced by 5% to 10% relative to monolayer HDPE processing to avoid fold-over defects at the barrier layer.
Accumulator-head equipment for 120 L and 220 L open-head drums uses HDPE LH506 as the primary structural resin. Extruder diameter is 120 mm to 150 mm with L/D 32:1. Melt temperature is controlled at 190 °C to 210 °C. Die gap is set from 4 mm to 6 mm. Accumulator shot weight is matched to the drum body mass. Mould clamp force is specified at 2,500 kN to 3,500 kN. Mould temperature is held between 8 °C and 15 °C. Cycle times range from 300 s to 450 s depending on nominal capacity. Regrind from top and bottom trim is reintroduced at up to 30 wt%. This addition level is validated by the UN 1H2 open-head drum drop and leakproofness tests in 49 CFR 178.603 and 178.604. The terminal product is used for solid and high-viscosity chemical transport. Wall thickness after trimming is specified at 3 mm to 5 mm across the drum body. The upper rim and bottom chime are the areas where regrind-related crack initiation is first observed when processing temperatures fall below the set band.
HDPE LH506 requires no forced drying in this application when stored indoors. Outdoor regrind storage at relative humidity above 85% introduces surface moisture that causes irregular parison blowing. A dehumidified hopper with dew point below -20 °C is used for such regrind streams. The critical processing limit is the appearance of sharkskin on the inner drum wall at die gaps above 6 mm. That condition is corrected by reducing output to 85% of nameplate screw speed and increasing die-head temperature by 5 °C.
When in-line fluorination is specified, monolayer HDPE LH506 containers are surface-treated after moulding with a fluorine-nitrogen mixture. Fluorine concentration is held at 0.1 vol% to 1.0 vol% in nitrogen. Treatment time is typically 1 s to 10 s depending on container surface geometry. The reaction substitutes surface hydrogen atoms with fluorine atoms and forms a fluoropolymer-like barrier of limited depth. No bulk layer ratio change is required. The process is applied to 1 L and 5 L bottles for aromatic solvents, chlorinated hydrocarbon pre-packs, and brake fluids. Weight loss permeation is evaluated over 28 days at 40 °C under ASTM D2684-18. Treatment is reported to reduce non-polar solvent permeation by 10× to 100× relative to untreated HDPE. Published data for this specific configuration of HDPE LH506 is limited; container-level validation under the target solvent is required because fluorination efficiency varies with surface contamination and storage atmosphere.
The production-scale limitation is the residual hydrogen fluoride purge. Fluorinated containers must be vented and purged with nitrogen for at least 30 min after treatment. Continuous fluorine analysers are installed in the exhaust stream. The terminal article is marked with the fluorination date and batch code. Processing lines are explosion-proof. The moulded container is not considered a barrier product by layer construction but by surface conversion. The primary failure mode observed on high-speed lines is non-uniform treatment in handle recesses and base pinch lines. That condition is mitigated by rotating containers during gas exposure and by verifying contact angle changes on treated surface sections against ISO 17257:2013 plaque references.
Knapsack sprayer tanks and tractor-mounted induction hoppers are blow-moulded from HDPE LH506 with a HALS-heavy UV stabiliser masterbatch at 1.5 wt% to 2.5 wt%. Tank volumes range from 15 L to 100 L. Shuttle machines or small accumulator machines with clamp force between 600 kN and 1,200 kN are used. Melt temperature is set from 190 °C to 205 °C. Mould cooling is held at 10 °C to 20 °C. Parison programming is used with 150-point axial wall control. Regrind addition is limited to 25 wt% because outdoor impact retention degrades above that level after 2,000 h of ISO 4892-2:2013 xenon-arc exposure. The terminal articles are translucent or black technical tanks for field sprayers and small diesel fuel reservoirs. Impact resistance at -20 °C is controlled by ASTM D256-23 Izod testing. Tensile yield and flexural modulus are evaluated under ASTM D638-14 and ASTM D790-17. The limiting processing constraint is wall-thickness drop at the tank baffle insert area. Mould venting must be increased to prevent air entrapment when the baffle is integrated into the final squeeze pin region.
Competitive USI Corporation HDPE LH506 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
USI Corporation HDPE LH506 is an injection-molding high-density polyethylene grade supplied in pellet form. Published supplier technical literature lists a nominal melt flow rate of 6.0 g/10 min at 190°C/2.16 kg per ISO 1133-1:2022 and a nominal 23°C density of 0.954 g/cm³ per ISO 1183-1:2019. The product is positioned for rigid injection-molded articles that require a controlled balance of melt processability, stiffness, and low-temperature toughness. Typical conversion sectors include thin-wall food containers, dairy cups, household crates, pails, closures, toys, and general-purpose industrial components. Because the supplied grade is a catalyst-integrated reactor product rather than a compounded formulation, lot-to-lot consistency is normally documented through the certificate of analysis for melt flow rate, density, and additive package.
The nominal 6.0 g/10 min melt flow rate places LH506 inside the conventional injection-molding flow window. This value is higher than blow-molding and film-grade high-density polyethylene, which frequently falls between 0.2 g/10 min and 0.8 g/10 min, but lower than ultra-high-flow injection grades that exceed 12 g/10 min. The moderate flow index therefore supports shorter fill times in multi-cavity tools while retaining greater molecular weight than a high-flow grade. At 0.954 g/cm³, the density is within the high-density polyethylene range of 0.941 g/cm³ to 0.965 g/cm³; this indicates a short-chain branching level that favors flexural modulus and top-load strength compared with medium-density polyethylene grades. The combination of density and flow is intended for applications in which sidewall stiffness and stacking strength are design requirements.
| Property | Test method | Typical value | Unit |
|---|---|---|---|
| Melt flow rate at 190°C/2.16 kg | ISO 1133-1:2022 | 6.0 | g/10 min |
| Density at 23°C | ISO 1183-1:2019 | 0.954 | g/cm³ |
| Tensile stress at yield | ASTM D638-14 | 27 | MPa |
| Tensile elongation at break | ASTM D638-14 | 400 | % |
| Flexural modulus | ISO 178:2019 | 950 | MPa |
| Notched Izod impact strength at 23°C | ISO 180:2000 | 4.5 | kJ/m² |
| Vicat softening temperature, Method A50 | ISO 306:2013 | 120 | °C |
| Brittleness temperature | ASTM D746-14 | < -70 | °C |
The above values are typical property indications and not simultaneous specification limits. For critical production qualification, the actual certificate of analysis and a resin-specific processing study should be used because polymerization lot variables can shift melt flow rate, density, and additive concentration within the grade specification range.
On injection molding lines equipped with 100–150 tonne clamp force hydraulic machinery and general-purpose screws of 20:1 L/D, production-scale behavior for LH506 is most consistent when barrel set points follow a rising profile from feed to nozzle. A typical profile is 190°C in the feed zone, 210°C in the compression zone, 220°C in the metering zone, and 220°C at the nozzle. Immersion-probe melt temperature measured under steady-state cycling is generally 215–225°C. Mold coolant temperature is normally maintained between 30°C and 50°C, with lower mold temperatures used for faster cycle times and higher mold temperatures used where surface gloss or weld-line strength is more important. In thin-wall multi-cavity tools with nominal wall thickness below 0.8 mm, short-shot defects become more frequent when melt temperature falls below 200°C. Above 240°C, prolonged residence time can promote thermal-oxidative degradation, visible as yellowing, acrid odor, and reduced impact toughness.
Hydraulic injection pressure is commonly observed in the 60–90 MPa range for normal gated containers, while holding pressure is set between 40 MPa and 70 MPa depending on gate geometry and part thickness. Back pressure is typically limited to 0.5–1.0 MPa to avoid excessive shear heating. Because HDPE LH506 is not hygroscopic, pre-drying is not mandated as a routine requirement. However, if pellets are stored in open hoppers in an environment exceeding 65% relative humidity or transferred from cold silos into a warm production hall, condensation on the pellet surface can produce silver streaks and surface splay. Under such conditions, hopper drying at 80°C for 1–2 h is applied before extended open-hopper storage. Drying beyond 4 h does not materially reduce residual moisture because the polymer matrix itself is not moisture-absorbing and the defect source is surface condensation.
The practical lower melt-temperature boundary for LH506 is governed by viscosity increase and gate freeze. At 190°C melt temperature, the viscosity is sufficiently high that filling of ribs thinner than 0.6 mm may require injection pressures above 100 MPa, which can exceed the capability of smaller machines and increase core deflection. The upper melt-temperature boundary is governed by oxidative stabilizer consumption rather than an abrupt melting transition. Residence times above 6 min at 240°C should be avoided because the stabilizer package can be depleted before the part exits the mold, producing surface discoloration and loss of notched impact strength when tested by ISO 180:2000. For shutdowns, barrel temperature should be reduced to 160°C or the barrel purged with a lower-viscosity polyolefin purge grade to limit stagnant degradation.
Compared with lower-melt-index high-density polyethylene blow-molding grades, LH506 is not suitable for continuous extrusion blow molding. The higher melt flow index reduces parison melt strength, causing diameter swell variability and parison drawdown instability when a parison length-to-diameter ratio exceeds 3:1. Compared with an 12 g/10 min high-flow injection-molding HDPE, LH506 generally requires higher injection pressure to fill very thin sections but produces higher impact resistance at equivalent density because the average molecular weight is higher. This distinction is most evident in notched Izod testing at 23°C per ISO 180:2000, where low-temperature or thin-wall brittle failures are more common in higher-flow grades. Compared with isotactic polypropylene, LH506 has a higher density of 0.954 g/cm³ and therefore should not be selected for weight-critical designs unless the lower flexural modulus of polypropylene cannot meet stacking strength requirements. It also offers different environmental stress-cracking resistance behavior, which must be evaluated by ASTM D1693 when detergents, alcohols, or aggressive process fluids contact the molded part.
In food-contact applications, final article compliance cannot be established by resin grade selection alone. Polyethylene grades such as LH506 may be suitable for food-contact use only when the converted article meets the extractive and end-use limitations of FDA 21 CFR 177.1520(c) for olefin polymers and, for European Union markets, the overall migration limit of 10 mg/dm² under Regulation (EU) No 10/2011 Annex I. The molder must verify compliance under the actual food type, contact time, temperature, and surface-to-volume ratio. For electrical and electronic equipment applications, unmodified high-density polyethylene normally does not contain intentional heavy-metal additives, but the converted article must be assessed against the substance restrictions of Directive 2011/65/EU including the recast delegated act (EU) 2015/863. REACH obligations under Regulation (EC) No 1907/2006, Article 33 apply if a substance of very high concern is present above 0.1 wt%; supplier documentation should be requested for the specific lot.
| Regulatory reference | Scope | Relevant threshold or clause |
|---|---|---|
| FDA 21 CFR 177.1520(c) | Olefin polymers for food contact | End-use temperature and food-type limitations; extraction tests |
| Regulation (EU) No 10/2011 | Plastic materials and articles intended for food contact | Overall migration limit 10 mg/dm² per Annex I |
| Regulation (EC) No 1907/2006 | REACH registration, evaluation, authorization, and restriction | SVHC notification above 0.1 wt% per Article 33 |
| Directive 2011/65/EU | RoHS substance restrictions in electrical and electronic equipment | Pb 1000 mg/kg, Hg 1000 mg/kg, Cd 100 mg/kg in homogeneous materials |
In multi-cavity hot-runner production of dairy cups, LH506 is processed with gate diameters of 0.5–1.0 mm and valve-gate or thermal-gate systems. Cavity fill balance depends on the runner layout, melt temperature uniformity, and gate land dimensions. Production experience indicates that cavity-to-cavity fill imbalance increases when the hot-runner manifold is operated below 210°C because viscosity differences become more pronounced. For pails and crates, the product is usually injected through cold runner systems or large-diameter direct edge gates; in these thicker-section parts, pack pressure rather than fill speed controls sink-mark severity. For closures and caps, part weight variation below 0.5% is achievable on injection molding machines with closed-loop shot control, but this requires stable holding-pressure transition from screw position rather than timer-based transfer.
Environmental stress cracking resistance is a further distinction for LH506 when compared with high-melt-index HDPE injection grades. Products exposed to nonionic surfactants, fatty acids, or certain detergent solutions should be qualified by ASTM D1693 Condition B under constant strain because molded-in residual stress and post-mold cooling rates can lower apparent ESCR below the value obtained on compression-molded plaques. Annealing at 60–70°C for 30 min is used on production lines to reduce residual stress in thick-walled crates before ESCR testing, but annealing also increases thermal history and can slightly reduce part stiffness or dimensional accuracy. The use of mold-release sprays should be minimized where ESCR is critical because surface contamination can initiate crazes under load.
When LH506 is used as an alternative to a general-purpose 0.954 g/cm³ high-density polyethylene grade, the molder should compare not only melt flow rate but also the additive package. Some commercial grades contain processing aids or antistatic additives that alter mold release, surface resistivity, and food-contact declarations. USI Corporation technical data indicate that the base grade is an unstabilized reactor powder compounded with a standard phenolic-phosphite antioxidant package; however, the exact additive formulation is controlled by the manufacturer and should be confirmed before changing suppliers. Published data for this specific configuration is limited for highly specialized applications such as pharmaceutical closures requiring USP Class VI testing, because elastomeric liner compression and sterility depend on the converted part rather than the resin alone.