| HS Code | 249003 |
| Polymer Type | High Density Polyethylene (HDPE) |
| Density | 0.952 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 20 g/10 min |
| Tensile Strength At Yield | 26 MPa |
| Tensile Elongation At Break | >1000% |
| Flexural Modulus | 1100 MPa |
| Vicat Softening Point | 125 °C |
| Heat Deflection Temperature At 0 45 Mpa | 75 °C |
| Shore D Hardness | 65 |
| Melting Point | 130 °C |
| Mold Shrinkage | 1.5-2.0 % |
| Water Absorption | <0.01 % |
| Thermal Conductivity | 0.4 W/m·K |
| Volume Resistivity | >1E16 ohm·cm |
| Dielectric Strength | 20 kV/mm |
| Dielectric Constant | 2.3 |
| Dissipation Factor | 0.0002 |
| Processing Method | Injection Molding |
| Processing Temperature | 200-230 °C |
| Mold Temperature | 20-60 °C |
As an accredited Tricon HDPE HDI20952 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Tricon HDPE HDI20952 is supplied in 25 kg net-weight bags, stacked on pallets and wrapped for shipment. |
| Container Loading (20′ FCL) | Tricon HDPE HDI20952 is loaded as bagged polyethylene resin in a 20-foot FCL, palletized, shrink-wrapped, and secured for export. |
| Shipping | Tricon HDPE HDI20952 is a non-hazardous high-density polyethylene resin, shipped as solid pellets in 25 kg bags, octabins, or bulk trucks/railcars. Not classified as dangerous goods for DOT, IMDG, or IATA. Keep dry, away from heat; no special transport placards required. |
| Storage | Store Tricon HDPE HDI20952 in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep original containers or bags closed, clean, and palletized off the floor. Avoid moisture, contamination, and strong oxidizers. Do not expose to prolonged UV radiation. Use first-in, first-out rotation. Consult the supplier’s SDS for specific storage, segregation, and incompatibility requirements. |
| Shelf Life | Tricon HDPE HDI20952 typically has a shelf life of 24 months under recommended storage: unopened, cool, dry, away from sunlight. |
In thin-wall dairy container molding, Tricon HDPE HDI20952 is processed as a high-shear, fast-fill injection grade to prevent short shots, sink marks, and warpage in stack molds with cavity counts ranging from 8 to 32. The compound is run neat at a melt temperature of 200–240 °C at the nozzle, with barrel profiling commonly set from 190 °C at the feed section to 230 °C at the metering section using a reciprocating screw with an L/D ratio of 20:1 to 24:1 and a non-return ring assembly maintaining a shot-to-shot cushion of 2–6 mm. Injection velocity is set between 150 mm/s and 300 mm/s, holding pressure between 50 MPa and 80 MPa, and mold cooling water between 12 °C and 25 °C for wall sections from 0.35 mm to 0.80 mm. Cycle times on high-speed stack molds typically fall within 2.8–5.5 s when low dew-point plant air at −40 °C prevents condensation on fast-ejecting cavity surfaces. Test specimen molding and shrinkage evaluation are anchored to ISO 294-1:2017 and ISO 294-4:2018. Regulatory compliance for food-contact dairy tubs and lids is established under FDA 21 CFR 177.1520(c) item 3.2a for olefin polymers, Regulation (EU) No 10/2011 Annex I with an overall migration limit of 10 mg/dm², and good manufacturing practice under Regulation (EC) No 2023/2006. The addition ratio for a certified food-contact container is 100 wt% virgin HDI20952, or up to 20 wt% closed-loop post-industrial regrind from the same resin when the scrap stream is clean, uncrosslinked, and revalidated for organoleptic neutrality. Where color is specified, a 1.0–3.0 wt% loading of PE-carrier masterbatch is metered at the feed throat. Terminal product types include injection-molded yogurt cups, cream cheese tubs, dairy spread containers, and snap-on lids. Published data for this specific configuration is limited; however, the processing window is consistent with high-flow HDPE thin-wall injection grades classified under ISO 17855-1:2014 and ASTM D4976-12a.
| Control point | Reference standard or regulation | Applied criterion |
|---|---|---|
| Olefin polymer food-contact compliance | FDA 21 CFR 177.1520(c) | Item 3.2a homopolymer HDPE |
| EU plastic food-contact migration | Regulation (EU) No 10/2011 | Article 12 OML ≤ 10 mg/dm² |
| Good manufacturing practice | Regulation (EC) No 2023/2006 | Traceability and contamination control |
| Test specimen molding and shrinkage | ISO 294-1:2017 / ISO 294-4:2018 | Defined cavity pressure and shrinkage baselines |
The injection-compression conversion of HDI20952 for 29/25 mm carbonated soft-drink closures requires a highly aligned cavity-pressure profile because the tethered-strap hinge and slit-tamper-evident band are formed simultaneously during the same stroke. In this application, the addition ratio is typically 100 wt% virgin HDI20952 with 1.5–3.0 wt% of a PE-based slip and antioxidant masterbatch, while internal closure regrind is limited to 10 wt% due to the risk of microgel formation in the hinge. Melt temperatures of 215–250 °C and mold temperatures of 8–15 °C are used in 32- to 96-cavity injection or injection-compression tools; the post-injection compression stroke is 0.3–0.8 mm, and cycle times range from 3.0 s to 8.5 s depending on liner distribution and wall thickness. Closure production must satisfy the tethered-cap design requirements of Directive (EU) 2019/904 for single-use plastic beverage containers, while food-contact compliance is maintained under FDA 21 CFR 177.1520(c) and Regulation (EU) No 10/2011. Torque retention after application is measured per ASTM D2063-12, and slit bridges are expected to fracture at 15–25 N ejection force after controlled scoring. Terminal product types include tamper-evident single-piece closures for carbonated soft drinks, bottled water, and isotonic beverages. The process limitation is operational: cavity filling must avoid excessive shear heating above 260 °C, which accelerates peroxide decomposition and produces acetaldehyde-type organoleptic defects.
Returnable logistics crates molded from HDI20952 are structural, thick-section parts in which sink, warpage, and impact toughness constrain cycle-time optimization more than wall thickness alone. The standard production addition ratio is 100 wt% virgin HDI20952, with 20–40 wt% closed-loop post-industrial regrind drawn from sprues, runners, and rejected crates; if the crate is destined for outdoor or UV-exposed return applications, a PE-carrier UV masterbatch is added at 0.3–0.8 wt%. The melt is processed at 200–230 °C with a back pressure of 0.5–1.0 MPa and a screw recovery time of 8–18 s on machines with clamp force of 600–1600 t and tie-bar spacing above 1200 mm. Multi-valve hot-runner gates or sequential valve gating are used to balance flow lengths across vented produce crate sidewalls; packing pressure is 60–100 MPa for 12–20 s, and mold water is held at 15–30 °C to deliver total cycle times of 22–45 s for wall sections of 2.5–5.0 mm. Mechanical conformity is anchored to ISO 178:2019 for flexural modulus, ISO 179-1:2020 for Charpy impact, and ASTM D638-14 for tensile yield. Environmental stress-cracking resistance is tested per ASTM D1693-15, Condition B, 10% Igepal, 50 °C, to separate acceptable crate grades from higher-density blow-molding grades that fail prematurely. Terminal product types include 24-bottle beverage crates, bread trays, vented agricultural crates, and folded dairy crates. A known operational boundary is post-mold shrinkage: unsupported sidewalls can continue to contract for 24–48 h after ejection and require post-cooling fixtures to maintain stackability dimensions.
Closed-loop regrind ratios up to 30 wt% in HDI20952 houseware molding are not governed by a single regulatory threshold but by the end-use migration risk and the part surface finish specification. For food-contact kitchen storage items, the addition ratio is 100 wt% virgin HDI20952 or a 90/10 virgin-to-regrind split, with 1.0–4.0 wt% color masterbatch and, where nested stacking is required, 0.5–2.0 wt% slip additive masterbatch. The process uses 200–800 t injection molding machines with melt temperatures of 190–240 °C, screw L/D of 20:1, mold water at 15–30 °C, and cycle times of 15–35 s for wall thicknesses from 1.5 mm to 4.0 mm. For storage totes and drawer organizers, gate placement follows a two-stage velocity profile: initial injection velocity of 60–100 mm/s through the first 60–70% of fill volume, then a reduction to 25–40 mm/s to prevent jetting and flow marks on textured A2-polished cavity surfaces. Compliance for food-contact utility totes is established under FDA 21 CFR 177.1520(c) and Regulation (EU) No 10/2011; non-food storage products are evaluated for mechanical durability under ISO 178:2019 and impact by ISO 179-1:2020. Terminal product types include modular under-bed storage containers, freezer-grade stackable totes, drawer dividers, and stackable utility bins. The specific shrinkage of HDI20952 in deep, free-standing sidewalls is not fully covered by generic injection datasheet values; published data for this specific configuration is limited, so mold trials with 12–16 h dimensionally stable post-ejection are required before finalizing cavity dimensions.
Industrial open-top pails produced from HDI20952 are subjected simultaneously to stacking compression loads, hydrostatic leak testing, and drop-impact certification that makes regrind management a primary process-control variable. The addition ratio for a UN-certified pail body is 100 wt% virgin HDI20952 or a maximum of 20–30 wt% verified closed-loop post-industrial regrind; the lid may use a separate gasket composition depending on the chemical compatibility classification of the intended filling. Melt temperatures of 200–230 °C and mold temperatures of 12–25 °C are used on 800–1200 t machines with injection pressure of 80–120 MPa and packing pressure of 60–80 MPa for 15–30 s. Gate design is normally a central sprue or valve-gated hot runner, with sidewall thickness from 1.4 mm to 2.8 mm and cycle times of 25–60 s. Certification is performed under the UN Model Regulations Chapter 6.1 performance test schedule, with packages marked as 1H2 for a specified specific gravity and hydrostatic test pressure; drop testing at −18 °C is a critical pass-fail condition for HDPE pail bodies. Food-grade pails additionally conform to FDA 21 CFR 177.1520(c) and Regulation (EU) No 10/2011. Terminal product types include 5–25 L open-top pails, tamper-evident lids, industrial chemical containers, and paint cans with wire-bail handles. A processing boundary is the deterioration of impact resistance if melt temperature exceeds 250 °C in hot-runner channels; oxidative chain scission in dead spots creates brittle zones that lower drop-test performance at −18 °C.
| UN packaging test | Method reference | Typical HDPE pail criterion |
|---|---|---|
| Drop test | UN Model Regulations 6.1.5.3 | No leakage after drop, conditioned at −18 °C |
| Stackability | UN Model Regulations 6.1.5.6 | No buckling or instability at 40 °C for 28 days |
| Hydrostatic pressure | UN Model Regulations 6.1.5.5 | No leak at specified kPa marking |
| Leakproofness | UN Model Regulations 6.1.5.4 | No perceptible leak at 20 °C |
For child-resistant dispensing overcaps, HDI20952 is processed in 24- to 48-cavity cold-runner or hot-runner tools where gate sequencing determines thread roundness, strap hinge thickness, and consistent child-resistant engagement. The addition ratio is 100 wt% virgin HDI20952 or 90/10 virgin-to-regrind with 1.0–3.0 wt% color masterbatch; no external slip additive is used when the closure must pass torque-removal and senior-use panel testing. Melt temperatures of 200–240 °C, mold water at 8–15 °C, and injection speeds of 80–150 mm/s are maintained to fill overcap wall sections between 0.8 mm and 2.0 mm. Cycle times range from 8 s to 15 s, with a maximum hot-runner nozzle temperature of 250 °C to reduce the risk of molecular-weight degradation at the gate tip. Child-resistant function is validated under ISO 8317:2015, with failure criteria based on the standardized child-resistance and senior-use panel protocols. If the overcap is intended for food-contact or oral-care packaging, compliance with FDA 21 CFR 177.1520(c) and Regulation (EU) No 10/2011 is verified separately. Terminal product types include child-resistant overcaps for disinfectant bottles, agrochemical trigger overcap assemblies, and personal-care pump shells. The operational boundary is the gate vestige: excessive gate depth above 0.10 mm above the undercap surface can create interference during closure application and reduce child-resistance consistency across multi-cavity production.
Competitive Tricon HDPE HDI20952 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Tricon HDPE HDI20952 is an injection-grade high-density polyethylene copolymer with a nominal density of 0.952 g/cm³ measured according to ASTM D792 and ISO 1183-1, and a nominal melt flow rate of 20 g/10 min at 190 °C/2.16 kg under ASTM D1238-23 and ISO 1133-1:2022. The grade designation separates it from high-molecular-weight blow-moulding and film grades: HDI20952 is formulated for thin-wall injection moulding of closures, housewares, caps, and rigid packaging, where short cycle time and high cavity replication take precedence over melt strength.
In multi-cavity tooling, the 20 g/10 min melt flow rate reduces filling pressure and can permit fewer gates, but it also reduces melt elasticity and increases the likelihood of nozzle drool, gate blush, and visible weld lines. The combination of 0.952 g/cm³ density and 20 g/10 min MFR places HDI20952 among high-flow HDPE injection grades that should be processed with check-ring injection machines, balanced hot-runner flow paths, and closed-loop process control. Where lot-specific certificate values are not available, the class benchmarks below define the processing and application boundaries.
Nominal melt temperature for HDI20952 is 220 °C to 250 °C. Residence times above 5 min at 250 °C cause chain scission and oxidative branching, producing an upward shift in melt flow rate, yellow streaking, and reduced environmental stress crack resistance. On 20:1 L/D general-purpose polyolefin screws, rear barrel temperature should be held at 180 °C, centre zones at 200 °C to 220 °C, and front zone plus nozzle at 230 °C to 250 °C. Back pressure from 0.5 MPa to 1.0 MPa is sufficient for melt homogeneity. Back pressure above 1.5 MPa does not improve colour dispersion and extends recovery time. Shut-down procedure uses purging with the same resin and lowering the rear barrel zone to 170 °C. Purging compounds containing fluoropolymers are not recommended unless the screw is disassembled, because residual fluoropolymer may reduce low-temperature impact.
Virgin HDPE does not require desiccant drying unless surface moisture is present from humid bulk handling or regrind storage. If condensation is visible, pellets should be dried at 80 °C for 2 h with a drying air dew point below -20 °C. Overdrying is unnecessary and may generate static charge.
No. The 2.16 kg melt flow index is a low-shear single-point measurement and does not capture shear-thinning slope, pressure-volume-temperature cooling paths, or gate freeze-off. For a 2 mm spiral at 230 °C and 80 MPa injection pressure, high-flow HDPE grades in the 0.952 g/cm³, 20 g/10 min class typically produce spiral lengths between 30 cm and 50 cm. When wall thickness falls to 0.8 mm, spiral length is reduced by 40–60%, and fill is controlled more by gate diameter and cavity air venting than by MFR. Mould-filling trials with cavity pressure transducers and short-shot series are required to establish the actual injection pressure-compensation curve for HDI20952. Published data for this specific configuration is limited; therefore, the spiral values are class benchmarks rather than lot-specific certification.
| Property | Test method | Representative value |
|---|---|---|
| Melt flow rate, 190 °C/2.16 kg | ASTM D1238-23; ISO 1133-1:2022 | 20 g/10 min |
| Density, 23 °C | ASTM D792; ISO 1183-1 | 0.952 g/cm³ |
| Tensile stress at yield, 50 mm/min | ASTM D638-14 Type I; ISO 527-2 | 25–28 MPa |
| Elongation at break | ASTM D638-14 Type I; ISO 527-2 | >300% |
| Flexural modulus | ASTM D790-17; ISO 178:2019 | 1,050–1,200 MPa |
| Notched Izod impact, 23 °C | ASTM D256-23; ISO 180/A | 3.5–5.0 kJ/m² |
| Vicat softening point, A50 | ISO 306:2022 | 122–126 °C |
| Heat deflection temperature, 0.45 MPa | ASTM D648-18; ISO 75-2 | 65–75 °C |
The above values are representative of the high-flow HDPE class and are not a substitute for a lot-specific certificate of analysis. Mechanical data generated on 4 mm compression-moulded plaques differ from moulded-part properties because of orientation, weld lines, cooling rate, and colourant concentration. At wall thicknesses below 1 mm, flexural modulus measured on plaques overestimates part stiffness; actual short-term stiffness should be measured on the final moulded article under the relevant loading speed.
High-flow HDPE is selected over polypropylene when low-temperature impact and hinge behaviour dominate over heat deflection requirements. At -20 °C, unreinforced polypropylene homopolymer notched Izod impact commonly falls below 2.0 kJ/m², while HDPE in the 0.952 g/cm³ class can retain 3.0–5.0 kJ/m², depending on comonomer content, gate orientation, and additive package. The trade-off is thermal resistance. HDPE heat deflection temperature at 0.45 MPa is typically 65–75 °C, compared with 90–110 °C for polypropylene homopolymer. HDI20952 is therefore not recommended for load-bearing components exposed continuously above 60–65 °C. Stiffness is also lower than polypropylene: polypropylene flexural modulus commonly exceeds 1,400 MPa, while high-flow HDPE is near 1,100 MPa. Thin-wall parts designed for polypropylene require a wall-section increase of 10–20% or additional ribbing to maintain equivalent bending stiffness when converted to HDI20952. The benefit is lower density and better sub-zero impact, particularly in closures and thin-walled living hinges where HDPE provides better crack growth resistance under repeated flexing at -10 °C to 0 °C.
The environmental stress crack resistance of high-flow injection HDPE is typically lower than that of lower-MFR blow-moulding or film grades. Under ASTM D1693, a high-flow resin may show an F50 value of 3–20 h, while a lower-MFR, lower-density film grade may exceed 100 h. HDI20952 should be qualified by ESCR testing on the actual moulded part if the article contacts fatty or oily substances, aggressive detergents, or alcohols. Sharp gate vestige, weld lines, and high packing stresses concentrate stress and reduce crack initiation time. A radius of at least 0.2 mm at weld line exits and gate boundaries is recommended for crack-sensitive designs.
Because HDI20952 is an injection grade with a melt flow rate of 20 g/10 min, it has markedly lower melt strength than blow-moulding HDPE grades with MFR below 1.0 g/10 min. Blow-moulding HDPE withstands parison sag under gravity and yields melt tension above 10 cN to 30 cN in elongational rheometry, whereas high-flow injection grades exhibit lower elongational viscosity and insufficient parison stability for large bottles. Extrusion blow moulding of containers with HDI20952 is therefore not practical. The narrow molecular weight distribution also reduces die swell, which is beneficial for injection mould filling but reduces the self-supporting character required for film blowing and sheet thermoforming. Compared with pipe-grade PE100 materials having MFR near 0.3 g/10 min and slow crack growth resistance required by ISO 13479, HDI20952 lacks the high-molecular-weight fraction and tie-molecule concentration needed for pressurised piping. It should not be used in pressure pipe or fittings requiring PE100 classification.
Cold mould warpage and post-mould shrinkage are controlled by cooling rate and crystallinity. At 0.952 g/cm³ density, crystallinity is approximately 60–70%. In moulds with wall sections from 0.4 mm to 1.2 mm, mould temperature should be controlled between 15 °C and 40 °C to promote rapid solidification. Lower mould temperatures reduce cycle time but increase orientation and warpage in closure skirts. Higher mould temperatures above 50 °C increase gloss and reduce moulded-in stress, but extend cycle time and risk sink mark formation in thicker sections. Typical linear mould shrinkage for HDPE is 1.5–3.0%; for thin-wall sections the lower part of this range may apply, but 24 h post-mould shrinkage must be measured. On multi-cavity closure tools, cavity-to-cavity variation can exceed 0.1% if cooling circuits are unbalanced; this is a common cause of ovality and thread-fit failures.
Gate freeze time controls packing. For HDPE with density 0.952 g/cm³, gate freeze time for a 1.0 mm diameter cold tunnel gate at 230 °C melt and 30 °C mould is approximately 0.5–1.5 s. Packing time must exceed gate freeze time to avoid sink marks and voids. Edge gates smaller than 0.8 mm in diameter may freeze before pressure compensation is complete. Hot-tip gates require thermal separation between nozzle tip and mould steel to prevent premature freeze or stringing; tip temperatures are usually 220 °C to 240 °C.
The usable injection pressure window is bounded by flash formation at the upper end and short shot formation at the lower end. For thin-wall closure cavities with 0.8 mm wall, filling pressures of 70–100 MPa are typical for high-flow HDPE. The lower limit for acceptable fill is usually 50 MPa; the upper limit is governed by flash in vents above 0.02 mm and by core shift in long cylindrical closures. A process window of ±10 MPa is generally workable, but rapid drops in nozzle melt temperature above 10 °C can move the process outside this window. This observation is a moulding engineering benchmark from high-flow HDPE thin-wall processing, not a class-specific certification.
| Requirement | Standard or regulatory reference | Boundary condition |
|---|---|---|
| Food-contact base resin | FDA 21 CFR 177.1520(c); EU 10/2011 | Application-dependent migration testing required on final article |
| RoHS environmental restriction | Directive 2011/65/EU | Base polyolefin normally compliant; pigment concentrates may alter final article |
| Melt flow rate | ASTM D1238-23; ISO 1133-1:2022 | 20 g/10 min nominal |
| Density | ASTM D792; ISO 1183-1 | 0.952 g/cm³ nominal |
| Environmental stress crack resistance | ASTM D1693 | 3–20 h class benchmark; part geometry and additives strongly influence result |
| Heat deflection temperature | ASTM D648-18; ISO 75-2 | 65–75 °C at 0.45 MPa |
For food-contact articles, the base HDPE may be formulated to meet FDA 21 CFR 177.1520(c) and EU 10/2011 migration limits. Compliance is application-dependent and must be confirmed with lot-specific documentation; specific migration data are generated under the final article's contact ratio, temperature, and food simulant, not on the pellet alone. RoHS restrictions on lead, mercury, cadmium, and hexavalent chromium are normally satisfied by the base polyolefin, but colour concentrates, fillers, and process aids can alter the final article. Medical or pharmaceutical applications require separate USP Class VI or ISO 10993 qualification; HDI20952 should not be assumed suitable for such uses without supplier certification.
On 1,200 kN toggle-clamp injection machines with 16-cavity closure tooling, common failure modes associated with high-flow 0.952 g/cm³ HDPE are nozzle drool during plastication, flash in vents exceeding 0.02 mm, and sink marks opposite ribs when gate freeze is not reached before packing release. Maintaining a cushion of 3–5 mm and packing time of 1.5–3 s per 0.8 mm wall section reduces sink mark depth below 0.01 mm. Hot runner manifold temperature should not exceed 250 °C; dead spots and stagnation zones generate oxidative degradation products and acetaldehyde. When regrind is used, the ratio should be controlled to maintain nominal MFR within ±2 g/10 min of virgin material, because multiple heat histories shift MFR upward and increase yellowing.
Letdown ratios for masterbatch in high-flow HDPE should be verified by notched Izod and MFR testing. Fatty acid amides and erucamide slip agents can reduce surface friction and improve part ejection; over-concentration above 1500 ppm may cause plate-out, reduced print adhesion, and environmental stress cracking. Antistatic additives that rely on surface migration are less effective at low mould temperatures; their discharge time after moulding can be 24–72 h.