    Specifications
    HS Code 699768
    Polymer Type High Density Polyethylene
    Density 0.960 g/cm3
    Melt Flow Index 17 g/10 min (190°C/2.16 kg)
    Tensile Strength At Yield 31 MPa
    Elongation At Break 1000%
    Flexural Modulus 1200 MPa
    Izod Notched Impact Strength 40 J/m
    Hardness 65 Shore D
    Vicat Softening Temperature 126°C
    Heat Deflection Temperature 75°C at 0.45 MPa
    Melting Point 133°C
    Water Absorption <0.01%
    Bulk Density 0.58 g/cm3
    Processing Method Injection Molding
    Color Natural
    Form Pellets

    As an accredited TPI Polene HDPE OGH-R1760 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing TPI Polene HDPE OGH-R1760 is packaged in 25 kg polyethylene-lined woven bags, or 1,000 kg jumbo bags for bulk shipment.
    Container Loading (20′ FCL) 20′ FCL container loading of TPI Polene HDPE OGH-R1760: 25kg bags, palletized, shrink-wrapped, evenly stacked, and secured for export transport.
    Shipping TPI Polene HDPE OGH-R1760 is shipped as non-hazardous HDPE resin pellets, generally packed in 25 kg bags, palletized and shrink-wrapped. Use clean, dry trucks or containers. Store away from moisture, heat, direct sunlight, and contamination. Handle carefully to prevent bag damage.
    Storage Store TPI Polene HDPE OGH-R1760 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, and open flames. Keep original bags closed, palletized, and off the floor. Prevent moisture, dust, oil, and chemical contamination. Observe stacking limits to avoid bag deformation. Use FIFO rotation. Avoid prolonged UV exposure. Store separately from incompatible materials. Ensure good ventilation.
    Shelf Life TPI Polene HDPE OGH-R1760 typically has a 24-month shelf life when stored unopened, cool, dry, and out of sunlight.
    Application of TPI Polene HDPE OGH-R1760

    Within chemical storage tank fabrication, the powdered feedstock is dry-blended with 0.10–0.20 wt% primary hindered phenolic antioxidant, 0.05–0.10 wt% secondary phosphite process stabilizer, and 0.05–0.10 wt% acid-neutralizing hydrotalcite, then pulverized to a nominal 35 mesh (500 µm) particle size with fines passing 200 mesh (75 µm) limited to ≤15% to prevent dry-flow segregation during mold charging. The production process on a carousel rotomolding line places the powder into cast aluminum molds with a biaxial rotation ratio of 4:1 for vertical cylindrical geometries; oven set temperature is held at 280–300°C until peak internal air temperature reaches 190–205°C. Cooling is staged to avoid warpage: ambient air to a mold shell temperature of 80–90°C, water spray at 10–20°C, and demolding at 45–55°C. Wall thickness for 1,000–15,000 L chemical tanks is maintained at 5–10 mm, with post-mold inspection for voids and pinholes at weld lines and insert bosses. Regulatory compliance for the finished tank body is assessed under ASTM D1998-21, and where European chemical containment applies, EN 13575:2012; long-term chemical compatibility is screened per ASTM D543-20 using the specific reagent at 23°C and 60°C for 28 days. Terminal product types include vertical chemical dosing tanks, double-wall secondary containment basins, acid/alkali storage vessels, and sodium hypochlorite day tanks. Published data for OGH-R1760 after continuous immersion in chlorinated solvents or 50% nitric acid is limited; such service requires fluorinated surface treatment or an internal liner.

    What Limits Drop Impact Performance in Rotomolded Agricultural Tanks?

    Drop impact performance in rotomolded agricultural tanks at -20°C is controlled primarily by slow crack growth resistance at the sidewall-to-floor transition and by powder densification at the inner wall. Blending 8–15 wt% metallocene-catalyzed linear low-density polyethylene into the HDPE matrix raises low-temperature impact energy but creates a process conflict: above 15 wt%, top-load deflection and sidewall bulge become measurable at 40°C and may violate dimensional acceptance under AS/NZS 4766:2006. The downstream production process uses shuttle rotomolding machines with offset arm rotation ratios of 3.5:1 to 4.5:1; oven set point is 285–310°C and the mold is removed when internal air temperature reaches 195–205°C. Powder bulk density is controlled at 0.37–0.40 g/cm³ per ASTM D1895-17, because ±3% batch-to-batch variation alters fill weight and produces a 0.5–1.0 mm wall-thickness drift that can reduce drop impact resistance by more than 20% in production-scale falling-dart testing. Agricultural water and fertilizer tanks are certified to AS/NZS 4766:2006 for rotational moulded polyolefin water tanks and, where applicable, ASTM D1998-21 Section 7.4 for impact resistance; published data for the specific OGH-R1760/mLLDPE blend under -20°C dart impact is limited, so validation per ASTM D5628-18 is performed for each tank geometry. Terminal products include horizontal sprayer tanks, saddle tanks for orchard and vineyard booms, and fertigation batch tanks of 500–10,000 L capacity.

    Because outdoor play equipment and urban furniture are subjected to multi-year UV irradiance, wet–dry cycling, and periodic sanitizer contact, the stabilizer system shifts toward light and colour stability rather than low-temperature impact modification. The dry blend incorporates 0.30–0.50 wt% high-molecular-weight hindered amine light stabilizer, 0.10–0.20 wt% benzotriazole or triazine UV absorber, and 1.0–2.0 wt% heavy-metal-free pigment masterbatch; total stabilizer loading is kept below 0.70 wt% to prevent excessive frictional heating in the pulverizer and to avoid extraction failures under EN 71-3:2019+A1:2021 migration limits. The molding process uses independent-arm or carousel machines with a lower peak internal air temperature of 185–195°C, which reduces oxidative yellowing at the outer skin but demands 2–4°C tighter oven control to avoid incomplete sintering at deep mold radii. Wall thickness is specified at 3–6 mm depending on impact exposure, and cooling uses forced ambient air to 70°C before water misting to minimize warpage in flat panels longer than 1.5 m. Material compliance is verified under EN 71-3:2019+A1:2021, ASTM F963-23 for heavy-element solubility in toy substrates, and REACH Annex XVII Entry 51 for phthalate restrictions in childcare articles; antimony trioxide and cadmium-bearing pigments are excluded from the raw-material specification. Terminal products include rotomolded climbing panels, slide hoods, sensory play walls, park benches, and municipal landscaping planter structures.

    When Potable Water Contact Requires Long-Term Hydrostatic Integrity

    Potable water storage tanks require that all formulation components—base resin, antioxidants, acid scavengers, and colour masterbatches—are either listed in Commission Regulation (EU) No 10/2011 Annex I or cleared under FDA 21 CFR 177.1520(c), with finished products tested to NSF/ANSI/CAN 61-2023 and AS/NZS 4020:2018 for drinking-water contact. The formulation restricts total additive loading to <0.15 wt%, composed of 0.05–0.08 wt% phenolic antioxidant, 0.03–0.05 wt% phosphite process stabilizer, and 0.03–0.08 wt% acid scavenger; tin mercaptide, antimony trioxide, and lead-based pigments are not permitted. On a carousel line, potable water tanks are molded at a peak internal air temperature of 190–200°C with a rotation ratio of 4:1 for diameters above 1.2 m; after oven removal, forced-air cooling continues until the outer mold shell reaches 70°C, then water spray cooling at 12–18°C is applied to accelerate crystallization without generating interlaminar voids. Wall thickness is maintained at 5–8 mm for tanks of 1,000–20,000 L, and post-mold hydrostatic testing follows ASTM D1998-21 with a 24 h water-fill test at 23°C. Terminal products include rainwater harvesting tanks, drinking water buffer tanks for remote work camps, and potable water storage vessels for water purification skids.

    End-use segmentPrimary compliance standardFormulation loading windowCritical processing boundary
    Chemical storage tanksASTM D1998-21; EN 13575:20120.10–0.20 wt% antioxidant; 0.05–0.10 wt% acid scavengerPeak internal air temperature 190–205°C; demold at 45–55°C
    Agricultural tanksAS/NZS 4766:2006; ASTM D1998-218–15 wt% mLLDPE; 0.10–0.20 wt% antioxidantOven set 285–310°C; internal air 195–205°C
    Outdoor playground equipmentEN 71-3; ASTM F963-23; REACH Annex XVII0.30–0.50 wt% HALS; 0.10–0.20 wt% UV absorberInternal air 185–195°C; wall thickness 3–6 mm
    Potable water tanksNSF/ANSI/CAN 61-2023; AS/NZS 4020:2018Total additives <0.15 wt%Internal air 190–200°C; water spray at 12–18°C
    Food-contact material handling binsEU 10/2011; FDA 21 CFR 177.1520(c)0.05–0.10 wt% antioxidant; 0.8–1.5 wt% TiO₂Internal air 190–200°C; post-mold shrinkage 1.5–2.0%
    Diesel exhaust fluid componentsISO 22241-1:2019; ASTM D1998-211.5–2.0 wt% carbon black; 0.08–0.15 wt% antioxidantCooling rate 4–8°C/min through 120–80°C

    Food-Contact Material Handling Bins and Cold-Chain Tote Liners

    Rotomolded food-contact bins are produced with a formulation limited to substances listed in Commission Regulation (EU) No 10/2011 Annex I and compliant with FDA 21 CFR 177.1520(c); migration testing uses food simulants under repeated-contact conditions prescribed in the European regulation. The additive loading includes high-purity phenolic antioxidant at 0.05–0.10 wt%, acid scavenger at 0.03–0.08 wt%, and titanium dioxide at 0.8–1.5 wt% for opacity and surface cleanability; total additive loading is maintained below 0.20 wt% to minimize sensory taint and migration risk. The molding operation on drop-arm machines uses secondary cooling stations and mold surface textures of 0.2–0.5 mm depth to mask sink marks on flat sidewalls; peak internal air temperature is controlled to 190–200°C, and cooling starts with ambient air to 75°C before water spray to limit post-mold shrinkage to 1.5–2.0%. Terminal products include fish storage boxes, meat lug containers, bakery tray dollies, and cold-chain tote liners used in food processing and distribution.

    Slow Crack Growth Resistance in Diesel Exhaust Fluid Handling Components

    Diesel exhaust fluid handling components are subjected to 32.5 wt% urea-water solution contact at service temperatures from -11°C to 40°C; although the solution is non-aggressive to high-density polyethylene, long-term hot aging and cyclic mechanical load can induce slow crack growth at insert bosses and threaded closures. The formulation uses 1.5–2.0 wt% carbon black masterbatch for UV opacity and 0.08–0.15 wt% high-molecular-weight hindered phenolic antioxidant; ester-based lubricants and amide slip additives are excluded because they can increase surface tension and promote urea crystal adhesion. Double-wall tanks with leak-detection channels are rotationally molded on carousel machines with peak internal air temperature of 195–205°C; after oven removal, cooling rate is controlled at 4–8°C/min through the recrystallization window of 120–80°C to reduce residual stress at the inner wall and closure bosses. Compliance for the tank body references ASTM D1998-21, while fluid-quality compatibility references ISO 22241-1:2019; long-term chemical resistance is screened per ASTM D543-20 using heated DEF at 60°C for 1,000 h. Published data for OGH-R1760 specifically after 1,000 h of 60°C DEF exposure is limited; the screening protocol is required before production qualification. Terminal products include DEF day tanks, intermediate bulk containers for urea solution, and agricultural urea ammonium nitrate storage vessels of 500–5,000 L capacity.

    Free Quote

    Competitive TPI Polene HDPE OGH-R1760 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    TPI Polene HDPE OGH-R1760 is a high-molecular-weight high-density polyethylene grade specified for thin-gauge blown film applications in which stiffness, dart impact resistance, and environmental stress crack resistance must be balanced against stable bubble formation. The resin is supplied as pellets and is characterized by a nominal density of 0.956 g/cm³ when tested according to ASTM D1505 or ISO 1183-1, and a high-load melt index of 6.0 g/10 min at 190 °C under a 21.6 kg load when measured in accordance with ASTM D1238-20 Condition F or ISO 1133-1:2022. The grade is produced by TPI Polene using gas-phase polymerization technology and is positioned at the high-molecular-weight end of the film-grade HDPE portfolio. Typical downstream use includes high-strength shopping bags, T-shirt bag film, drum liners, and refuse sacks where downgauging from 20 µm to 12 µm is required without sacrificing load-bearing capacity or split resistance.

    What Separates OGH-R1760 from Medium-Molecular-Weight HDPE Film Resins?

    The primary technical distinction is the combination of high molecular weight and a controlled short-chain branching distribution. Conventional medium-molecular-weight HDPE film grades with melt index values near 0.5 g/10 min at 190 °C/2.16 kg display lower melt viscosity and easier processing, but they commonly show reduced dart impact and environmental stress crack resistance when the film is drawn below 15 µm. OGH-R1760 is not characterized by a standard 2.16 kg melt index for specification purposes; the relevant flow parameter is the high-load melt index of 6.0 g/10 min at 21.6 kg, which reflects the presence of high-molecular-weight chains while retaining processability through shear thinning. The density of 0.956 g/cm³ places the grade in the high-density range and contributes to flexural stiffness, but the comonomer placement and broad molecular weight distribution reduce crystallinity gradients that can initiate environmental stress cracking. Compared with LLDPE, OGH-R1760 exhibits higher stiffness and lower elongation at break. Compared with LDPE, the grade delivers higher melt strength and improved bubble stability, permitting higher blow-up ratios and thinner walls. Published data for systematic comparison of film properties under identical processing conditions is limited; selection should therefore be validated by film line trials using the intended die geometry, frost-line height, and masterbatch formulation.

    Environmental stress crack resistance reported by the manufacturer using ASTM D1693-15 Condition B in 10 % Igepal CO-630 is typically above 800 h, whereas many conventional monomodal HDPE film grades with similar density may exhibit 100 h to 400 h under the same test. This difference is significant in drum liners and chemical packaging where stress cracking at folded creases is the dominant failure mode. The improvement is partly attributable to the bimodal or broad molecular weight distribution characteristic of the high-molecular-weight film class, though the supplier’s published molecular weight distribution curves should be consulted for lot-specific confirmation.

    Extruder Configuration, Die Geometry, and Melt Temperature Set Points

    Processing experience on production-scale blown film lines indicates that OGH-R1760 requires sufficient extruder torque and residence time distribution to melt high-viscosity HMW-HDPE without excessive shear heating. Typical lines use a grooved-feed extruder with screw diameter between 45 mm and 90 mm, an L/D ratio from 24:1 to 33:1, and a barrier screw with a Maddock or spiral mixing section. Melt temperature measured at the adapter should be controlled between 190 °C and 220 °C. Barrel temperature profiles from the feed throat to the metering zone are commonly set from 160 °C to 210 °C, with die zones maintained at 200 °C to 220 °C. The die gap is typically set at 1.5 mm to 2.5 mm for HMW-HDPE, and the blow-up ratio is maintained between 3:1 and 5:1. Frost line height is usually adjusted to 6 to 10 times the die diameter to balance machine-direction orientation with dart impact retention. Die-lip build-up can occur if die temperatures fall below 200 °C because the high-molecular-weight fraction resists flow at the lip exit and can accumulate oxidized material over extended runs.

    Pre-drying is not routinely required because polyethylene is non-hygroscopic; moisture absorption is typically below 0.01 % at 23 °C and 50 % RH. However, pellets stored below the dew point should be conditioned or hopper-dried at 40 °C to eliminate surface condensation defects. The resin should not be subjected to melt temperatures above 240 °C or residence times exceeding 10 min, as oxidative chain scission and gel formation may occur. Incompatibility has been observed with high-acid-number post-consumer recyclate and with polyamide or EVOH barrier residues; blends containing these materials should be evaluated for gel formation and viscosity mismatch before production use. The grade is not intended for injection molding or sheet extrusion because its high melt viscosity at low shear rates reduces flow length and makes thick-section filling difficult. For injection molding applications, lower-viscosity HDPE grades with melt flow rates above 5 g/10 min at 2.16 kg are typically used.

    Regulatory compliance should be confirmed by lot-specific supplier certification. For food-contact packaging, converters should request a statement of compliance under FDA 21 CFR §177.1520, which covers olefin polymers of this density range. Because the grade is not formulated with heavy-metal pigments or phthalate plasticizers, it is generally aligned with EU Directive 2011/65/EU RoHS recast and Regulation (EC) No 1907/2006 REACH, but formal documentation for the specific production lot is required before use in regulated packaging.

    The representative values in the following table are extracted from the supplier’s published technical data and are not specification limits. Film values were obtained on a 25 µm blown film sample produced under manufacturer-recommended conditions.

    Property Test method Unit Typical value
    Density ASTM D1505 / ISO 1183-1 g/cm³ 0.956
    High-load melt index at 190 °C, 21.6 kg ASTM D1238-20 Condition F / ISO 1133-1:2022 g/10 min 6.0
    Tensile strength at yield ASTM D638-14 / ISO 527-2 MPa 26
    Elongation at break ASTM D638-14 / ISO 527-2 % 600
    Flexural modulus ASTM D790-17 / ISO 178 MPa 1,100
    Environmental stress crack resistance F50 ASTM D1693-15 Condition B h >800
    Vicat softening temperature ASTM D1525 / ISO 306 °C 125
    Dart impact F50 on 25 µm film ASTM D1709-16 Method A g 180
    Elmendorf tear MD/TD on 25 µm film ASTM D1922-15 / ISO 6383-2 g 20 / 80

    When Downgauging to 12 µm Requires a Broader Molecular Weight Distribution

    Thin-gauge T-shirt bags are the most demanding application for this resin class. At film thickness below 15 µm, conventional HDPE film resins often fail by dart impact puncture at the bag bottom seal or by tear propagation from handle perforations. OGH-R1760 is specified for these applications because the high-molecular-weight fraction raises melt strength and extensional viscosity, allowing stable bubble formation at blow-up ratios up to 5:1 while maintaining gauge uniformity across the web. The low melt index at standard load indicates long molecular relaxation times; during film blowing, this promotes higher machine-direction orientation and improves tensile strength at break, but it also increases the probability of oxidation-induced die-lip build-up if the die temperature is not maintained above 200 °C. Production lines typically operate with die pressure between 300 bar and 450 bar for a 90 mm die with a 1.8 mm die gap, but published data for this specific configuration is limited. Die pressure should be validated with the particular melt pump, screen pack combination, and adaptor geometry in use.

    Refuse sacks and drum liners produced from OGH-R1760 benefit from environmental stress crack resistance above 800 h and from the stiffness contributed by the 0.956 g/cm³ density. The stiffness provides crush resistance in stacked bags, while the comonomer distribution reduces stress-cracking sensitivity at folded edges and gusset corners. Compared with TPI Polene HDPE pipe grades, OGH-R1760 is not formulated for long-term hydrostatic pressure resistance and should not be used for pressure piping under ISO 4427; its melt flow characteristics and stabilization package are designed for thin-film oxidative stability during blown film extrusion rather than potable water service life. The grade is also distinct from rotational molding powders in the supplier’s R-series portfolio. Despite the R prefix in the designation, OGH-R1760 is a pelletized film resin and is not intended for pulverization or rotational molding.

    For thin-film applications requiring slip, antiblock, or ultraviolet stabilization, converters add masterbatch concentrates at the extruder throat. The base resin is not a universal compound and does not contain processing aids for all film line configurations. Trials on high-output lines should therefore record melt pressure, melt temperature, gland leakage, and film dart impact across at least three consecutive rolls to establish whether the grade remains within the converter’s quality window under sustained throughput.

    Top