Tpi Polene Hdpe G2855

TPI Polene HDPE G2855

    • Product Name: TPI Polene HDPE G2855
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 295986
    Grade G2855
    Polymertype High Density Polyethylene (HDPE)
    Meltflowrate 8.0 g/10 min (190°C/2.16 kg)
    Density 0.955 g/cm³
    Tensilestrengthatyield 28 MPa
    Elongationatbreak 1000%
    Flexuralmodulus 1200 MPa
    Notchedizodimpactstrength 4 kJ/m²
    Vicatsofteningtemperature 127 °C
    Heatdeflectiontemperature 75 °C
    Shoredhardness 65
    Processingmethod Injection Molding
    Melttemperature 190-230 °C
    Moldtemperature 20-60 °C
    Moisturecontent <0.05%

    As an accredited TPI Polene HDPE G2855 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing TPI Polene HDPE G2855 packaging: 25 kg woven bags, plus 500 kg and 1,000 kg jumbo bags for bulk shipment.
    Container Loading (20′ FCL) For TPI Polene HDPE G2855, 20′ FCL loading: 25 kg bags, approximately 18 metric tons net, palletized or floor-loaded.
    Shipping TPI Polene HDPE G2855 is typically shipped as a non-hazardous solid resin in 25 kg PP woven bags or 1,000 kg jumbo bags, palletized and stretch-wrapped. It is transported in clean, dry closed containers or trucks, protected from moisture, heat, direct sunlight, and contamination.
    Storage Store TPI Polene HDPE G2855 in a cool, dry, well-ventilated warehouse at ambient temperature, away from direct sunlight, heat, and ignition sources. Keep original bags or containers tightly closed to prevent moisture, dust, and contamination. Stack on stable pallets; avoid excessive stacking. Maintain clean handling areas and use first-in, first-out rotation. Protect from UV radiation and mechanical damage.
    Shelf Life Store in a cool, dry, ventilated area away from direct sunlight; shelf life approximately 12 months in unopened original packaging.
    Application of TPI Polene HDPE G2855

    TPI Polene HDPE G2855 is a high-molecular-weight blow-moulding HDPE with a nominal density of 0.955 g/cm³ measured per ISO 1183-1:2019 and a melt flow rate at 190 °C/5 kg in the grade-specific datasheet, commonly reported in the 0.5–0.6 g/10 min band under ISO 1133-1:2022. The resin is processed on accumulator-head and continuous shuttle blow-moulding lines, where melt strength, parison sag, and environmental stress crack resistance control the feasible part envelope. Separate downstream segments are defined here because wall-thickness programming, regrind limits, and regulatory test paths diverge sharply between large open-head transport packaging and thin-wall household bottles.

    What Limits Parison Wall Thickness Stability in 200 L Open-Head Drum Production from G2855

    On a 200 L open-head drum line using an accumulator-head machine with an 80 mm grooved-feed extruder at L/D 24:1, the parison is extruded through a diverging die gap of 0.8–1.4 mm and programmed with 100-point axial wall control. Melt temperature at the die lip is held between 180 °C and 205 °C; excursions above 210 °C produce visible oxidation gels and reduce pinched-bottom weld integrity. Blow pressure is set at 0.6–0.8 MPa, and mould temperature is maintained at 15–30 °C via closed-loop chilled water. The material is processed as 100% virgin G2855 for the first certification run; subsequent production may incorporate up to 30% clean post-industrial regrind if the melt flow rate under ISO 1133-1:2022 condition 190 °C/5 kg remains within the qualified range. Final drum certification follows UN 1H1/Y1.9/250 performance tests: leakproofness at 30 kPa, hydraulic proof pressure at 250 kPa for 30 min, and drop impact from 1.2 m at −18 °C without rupture. Top-load creep is measured as stack load at 40 °C for 28 days; lid closure seats are rejected if radial shrinkage exceeds 11 mm on the opening diameter. The process boundary is the parison sag rate: at 200 °C, the high-molecular-weight distribution allows a 25 kg parison to hang for 10–14 s before wall thinning becomes unrecoverable. Die swell stabilizes only after 20–30 min of continuous cycling; short shots and fold defects are more common when start-up purge contains polypropylene traces above 0.5 wt%.

    Agrochemical jerrican production places G2855 under a different stress-crack regime than large open-head drums. The 25 L parison is programmed to place 2.5–2.8 mm at the handle pinch-off and bottom corners while pulling the centre wall to 1.5–1.8 mm. The extruder barrel is zoned 160–190 °C, the die head 185–195 °C, and the mould 12–25 °C; blow pressure is 0.7 MPa, and the blow cycle is 25–35 s. Shuttle clamp force for a dual-parison tool is set at 180–250 kN. The neck is finished with a 63 mm buttress or PCO thread, and the inner orifice must not ovalize more than 0.4 mm at demould. Qualification follows UN 3H1/Y25/S for liquids: drop from 1.2 m at −18 °C, leakproofness at 30 kPa, and stacking at 40 °C for 28 days with 125 kg top load. For concentrated ester-type emulsifiable concentrates above 30 wt%, the grade's resistance to environmental stress cracking under ASTM D1693-15 Condition B in 10% Igepal CO-630 at 50 °C must be verified against the specific solvent package. Published data for this specific configuration is limited; a barrier layer or fluorination is recommended for aggressive aromatic blends.

    When G2855 Is Screwed into a Six-Layer Fuel Tank Coextrusion Line

    Automotive fuel tank coextrusion uses G2855 as the outer capstock and the regrind-containing core only when the barrier layer is EVOH and the tie resins are anhydride-modified LLDPE. The line is a six-layer accumulator-head blow moulder with a 90 mm primary extruder and a 60 mm barrier extruder. Layer distribution is given in the table below.

    Layer orderFunctionMaterialTypical thickness shareProcess or test anchor
    1Outer impact shellTPI Polene G2855 plus UV stabilizer10–15%ISO 179-1/1eA at −40 °C
    2Regrind coreClean tank regrind plus G285540–50%ISO 1133-1:2022 melt-flow stability
    3Tie layerMaleated LLDPE2–3%ASTM D1876-08 T-peel
    4Barrier32 mol% ethylene EVOH2–3%Permeation per SAE J1737
    5Tie layerMaleated LLDPE2–3%ASTM D1876-08 T-peel
    6Fuel contact layerTPI Polene G285520–30%ISO 179-1/1eA at −40 °C

    The melt stream for G2855 should be maintained at 190–205 °C; localized die-lip temperatures above 220 °C cause gel contamination in the parison core. Preblow is delayed 0.3–0.6 s after mould close, and final blow pressure is 0.6 MPa. The pinch-off weld at the tank perimeter is pulled to 3–4 mm; weld integrity is tested by drop impact at −40 °C and by sectioning for EVOH layer fold-back. Fuel permeation is evaluated under SAE J1737. Monolayer use of G2855 in fuel tanks is not recommended because permeation and pinch-off low-temperature impact data are outside the published certification scope.

    On a high-cavity reciprocating-screw wheel machine producing 500 mL to 5 L household chemical bottles, G2855 is run at a melt temperature of 175–195 °C and the parison is extruded through 0.6–0.9 mm die gaps. The mould temperature is 8–15 °C for fast frost. Blow pressure is 0.5–0.7 MPa, with cycle times of 9–14 s per cavity. Wall thickness distribution is set at 0.6–0.8 mm for body sidewalls and 1.0–1.4 mm at the shoulder and base chime. Colour masterbatch is added at 2–4 wt%; only high-density polyethylene carrier masterbatch is used to avoid die-lip build-up. Bottles for detergent and sodium hypochlorite solutions are tested for environmental stress cracking after filled storage at 40 °C for 21 days; the failure mode is circumferential cracking at the handle root when the neck insert temperature falls below 8 °C. Leak testing is done at 3–5 kPa internal air pressure; top load for a 1 L bottle is specified at 250 N at 23 °C. Food-contact containers must meet FDA 21 CFR 177.1520 and EU Regulation 10/2011 with overall migration below 10 mg/dm². No pre-drying is required for virgin G2855, but regrind above 30% should be kept below 0.05% moisture to prevent surface splay.

    ApplicationStandard or regulationTest conditionAcceptance boundary
    200 L open-head drumUN 1H1Drop 1.2 m at −18 °C; hydraulic 250 kPa/30 minNo rupture, no leak
    25 L jerricanUN 3H1/Y25/SDrop 1.2 m at −18 °C; stack 28 days at 40 °CNo rupture, no leak
    Food-contact bottleFDA 21 CFR 177.1520, EU Regulation 10/2011Overall migrationBelow 10 mg/dm²
    Underbonnet reservoirISO 179-1/1eANotched Charpy at −30 °CAbove 4 kJ/m²

    Underbonnet Reservoirs and the 60°C Continuous-Service Boundary

    Windshield washer fluid reservoirs and coolant overflow bottles are blow moulded from G2855 on single-station machines with 70 mm extruders and 50 mm accumulator heads. The melt temperature is kept at 185–200 °C; the parison is programmed to hold 2.0 mm at the mounting tabs and 1.4 mm on the body. The mould is maintained at 15–25 °C. The limiting design parameter is not impact but low-strain creep under sustained underhood soak. At continuous internal fluid temperatures above 60 °C, the reservoir body can sag at the mounting bosses and the cap thread can ovalize on repeated thermal cycles from −20 °C to 60 °C. G2855 is therefore used for washer reservoirs and overflow bottles with a design maximum continuous service of 60 °C, with short-term excursions to 80 °C for 30 min during fill-system testing only. The pinch-off seam around the reserve spigot is inspected by cutting and bending at −30 °C; any crack longer than 2 mm rejects the cavity. Automotive specification testing follows ISO 179-1/1eA Charpy impact at −30 °C, with failure below 4 kJ/m² at the pinch seam disqualifying the part. Resistance to methanol-water washer fluid is screened by storage for 14 days at 60 °C; the part must not lose more than 5% of its original top-load stiffness.

    Peracetic Acid Attack in Dairy Sanitizer Bottles: ESCR Data and Limits

    Blow-moulded dairy sanitizer bottles from G2855 operate in a narrow stress crack resistance window because peracetic acid-based sanitizers generate oxidative stress on the inner wall. Bottles of 1 L to 5 L are produced with 0.7–0.9 mm wall thickness on a continuous shuttle line at melt temperature 180–195 °C. The neck finish is a 38 mm three-start thread with an induction-sealable LDPE foam liner. Stress crack initiation testing is conducted on filled bottles containing 0.2–0.5% peracetic acid at 23 °C; bottles are stored for 30 days at 40 °C and then subjected to a 1.0 m drop. Published data for this specific configuration is limited; qualification requires lot-to-lot screening under ASTM D1693-15 Condition A with an F50 value above 200 hr before industrial disinfectant filling. The compatibility limit is set at 0.5% peracetic acid for continuous ambient use; higher concentrations require a fluorinated inner surface or a barrier layer. Post-consumer recycled content is not permitted in dairy sanitizer applications unless migration and oxidative aging data are submitted to the food-safety authority.

    Free Quote

    Competitive TPI Polene HDPE G2855 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    TPI Polene HDPE G2855 is a high-molecular-weight high-density polyethylene extrusion blow-moulding grade supplied by TPI Polene Public Company Limited. The resin is delivered as natural or uncoloured pellets and is intended for rigid packaging and industrial containers in which melt strength, environmental stress crack resistance, and controlled parison swell are more important than thin-wall injection flow. The grade is nominally characterized by a melt mass-flow rate of 0.28–0.35 g/10 min at 190 °C and 2.16 kg load under ASTM D1238-20 or ISO 1133-1:2022, and a density of 0.955 g/cm³ at 23 °C under ASTM D1505-15 or ISO 1183-1:2019. Applications include containers for liquid detergents, motor oil, agricultural chemicals, and non-food liquids in which stress cracking under hoop stress and moulded-in residual stress must be controlled.

    As a commercial identifier, G2855 is not a standardized chemical code and does not itself confer food-contact, potable-water, or dangerous-goods packaging approval. Compliance must be demonstrated against the current supplier certificate of analysis and the applicable end-use standard. The product differs from low-density film grades by its higher crystalline modulus and narrower processing window; it differs from injection-moulding HDPE by its substantially lower melt index and higher melt tension.

    How Does the Melt Rheology Constrain Extrusion Blow Moulding?

    The melt mass-flow rate of 0.28–0.35 g/10 min places G2855 in the low-flow segment of HDPE. In extrusion blow moulding, this low flow is used to resist parison draw-down before mould closure. The same viscosity raises extruder head pressure and reduces screw output per unit energy. Single-screw extruders with L/D ratios of 20:1 to 30:1 and barrier or Maddock mixing screws are recommended. Grooved-feed extruders may generate excessive melt temperature at high screw speeds. Typical barrel temperature zones range from 170–190 °C in the feed section to 190–210 °C in the metering zone, with head and die temperatures held at 195–210 °C. The melt stream should be maintained between 190 °C and 210 °C. Temperatures below 180 °C can produce sharkskin on the parison surface and increase die swell variability, while sustained temperatures above 220 °C accelerate oxidative chain scission and may cause colour shift in unpigmented parts.

    Parison sag is the primary process conflict in large-part extrusion blow moulding. On shuttle machines with unsupported parison lengths above 250 mm, die temperature and melt index must be controlled within a narrow band. Production-scale observations on accumulator-head machines indicate that a melt temperature increase of 10 °C can alter parison length by several millimetres before mould closure, creating non-uniform wall thickness. Die gap settings for G2855 are typically 1.0–3.0 mm, depending on container volume, target wall section, and accumulator shot size. Blow air pressure is commonly set at 0.6–0.8 MPa, and mould temperature is held at 10–20 °C to accelerate crystalline solidification while avoiding condensation on chilled mould surfaces.

    Short-term tensile response under ISO 527-1:2019 or ASTM D638-14 typically shows a yield stress in the range of 26–30 MPa and elongation at break greater than 600 %. Flexural modulus, measured under ISO 178:2019 or ASTM D790-17, is commonly reported between 1,000 MPa and 1,300 MPa, indicating stiffness typical of medium-crystallinity HDPE. Izod impact values at 23 °C are generally above 5 kJ/m² under ISO 180:2019, with notched values dependent on specimen preparation and cooling rate. The property balance is intended for containers that must survive filled-weight drop testing rather than for structural injection components with tight dimensional tolerances.

    Environmental Stress Crack Resistance and Chemical Contact Boundaries

    Environmental stress crack resistance is a primary specification for rigid packaging grades. Published trade data for TPI Polene HDPE G2855 cite ESCR values from approximately 30 h to more than 100 h when tested under ASTM D1693-15 condition B at 50 °C with 10 % Igepal CO-630. The range reflects test variation and lot-to-lot differences in comonomer distribution. Exact values for a given shipment should be confirmed against the supplier certificate of analysis. The same property distinguishes this grade from lower-molecular-weight blow-moulding HDPE grades that exhibit higher melt flow indices but fail earlier in stressed polar detergent environments.

    Suitable chemical service includes dilute inorganic acids, dilute sodium hydroxide, aqueous brines, aliphatic alcohols, and many water-based detergent formulations at ambient temperature. The grade is not intended for continuous exposure to strong oxidizing acids, aromatic hydrocarbons, chlorinated solvents, or concentrated surfactant systems at temperatures above 40 °C. Aliphatic hydrocarbons cause progressive swelling; permeability and loss of mechanical strength increase with solvent chain length and exposure time. The converter must perform product-specific stored-liquid tests because stress-cracking behaviour depends on the combined effect of hoop stress, moulded-in residual stress, and the specific wetting agent in the packaged liquid.

    Typical nominal property profile of TPI Polene HDPE G2855 reported in trade literature
    PropertyNominal value or rangeTest method
    Melt mass-flow rate, 190 °C, 2.16 kg0.28–0.35 g/10 minASTM D1238-20, ISO 1133-1:2022
    Density, 23 °C0.955 g/cm³ASTM D1505-15, ISO 1183-1:2019
    Tensile yield strength26–30 MPaISO 527-1:2019, ASTM D638-14
    Elongation at break>600 %ISO 527-1:2019, ASTM D638-14
    Flexural modulus1,000–1,300 MPaISO 178:2019, ASTM D790-17
    ESCR, condition B, 10 % Igepal, 50 °C30 to >100 hASTM D1693-15
    Vicat softening temperature, 10 N120–126 °CISO 306:2013, ASTM D1525-17
    Izod notched impact strength, 23 °C5–8 kJ/m²ISO 180:2019, ASTM D256-23

    On conventional extrusion blow-moulding lines, the grade’s processing response is better captured by accumulated parison length before mould closure than by melt flow index alone. In multi-cavity continuous-extrusion machines, output per die head is typically governed by extruder screw diameter and screw speed rather than by resin flow alone. A 60–75 mm single-screw extruder with L/D 24:1 is sufficient for containers from 0.5 L to 10 L, while larger industrial containers require accumulator heads with shot capacities matched to part mass. Blow moulds should have venting channels no deeper than 0.03 mm to avoid flash formation while permitting air escape. Shrinkage after demoulding is normally 1.5–3.0 %, with larger values on thick sections; post-mould dimensional audits should be performed after 24 h of conditioning at 23 °C and 50 % relative humidity.

    Die swell of a high-molecular-weight HDPE such as G2855 is usually higher than that of medium-molecular-weight injection grades; parison diameter and thickness must be compensated by die gap adjustment during start-up. In continuous-extrusion blow moulding, weight distribution across multiple parisons is affected by melt elasticity and land geometry. Die land length-to-gap ratio is typically maintained between 10:1 and 20:1 to minimize elastic memory effects. Operators commonly adjust parison programming to correct for wall thinning at the container shoulder and base; the axial thickness profile is set on the accumulator head using a servo-controlled die pin. The desired wall-thickness distribution for a 1 L detergent bottle is frequently specified as 0.6–1.2 mm, with the pin shifted to increase thickness at the pinch-off and shoulder regions.

    Lot-to-lot consistency in the low melt-index region is a significant production concern. A melt index tolerance of ±0.03 g/10 min around a nominal value may be sufficient for open-loop machines, but closed-loop parison programming can compensate for minor viscosity drift by adjusting extruder speed and die gap. Batch-to-batch variance in molecular weight distribution affects die swell and pinch-off weld strength more than melt index alone. Therefore, incoming resin should be checked by melt flow rate, density, and, where possible, melt viscosity at a shear rate representative of extrusion. Capillary rheometry at 190 °C and shear rates from 10 s⁻¹ to 1,000 s⁻¹ provides data for pressure-drop estimation in the die head.

    Melt Temperature Excursions and Parison Instability

    In continuous-extrusion and accumulator-head blow moulding, a melt temperature below 180 °C increases the elastic memory of the resin and produces pronounced sharkskin on the parison surface. This defect is more common in high-molecular-weight grades because the longer relaxation times preserve die-entry stress. The practical correction is not simply raising barrel temperature; the die land ratio and die temperature must also be adjusted to shift the surface roughness to a lower shear rate. At the opposite boundary, sustained melt temperatures above 220 °C degrade the parison’s melt strength and reduce the maximum unsupported parison length. The result is a thinner sidewall at the lower container sections and excessive pinch-off flash. In severe cases, the flash removal generates fines that contaminate regrind and lower the average bulk density of the recycled stream.

    When G2855 Is Benchmarked Against Injection-Moulding and Film HDPE Grades

    Compared with injection-moulding HDPE grades having melt-flow indices of 6–20 g/10 min, G2855 has a melt viscosity approximately 20–70 times higher. This makes it unsuitable for multi-cavity injection moulds with long flow paths and wall sections below 1.0 mm; short shots and weld-line weakness are likely. The benefit is higher melt tension and greater resistance to parison sag, which is irrelevant to injection moulding and therefore represents a genuine property trade-off. Injection-moulding HDPE also tends to have narrower molecular weight distribution to reduce warpage; blow-moulding grades such as G2855 are formulated for high shear sensitivity and controlled die swell.

    Relative to high-density film grades, G2855 generally has a similar density range but a different molecular weight distribution and additive package. Film grades are processed through blown-film dies with annular gaps below 2.0 mm and draw-down ratios exceeding 5:1, whereas G2855 is optimized for parison extrusion with low draw-down and high swell. HDPE pipe grades such as PE100 are distinguished by a different additive package, higher melt strength, and long-term hydrostatic strength grading under ISO 9080:2022; G2855 is not classified as a pressure-pipe material and must not be used where the pipe grade’s hydrostatic design basis is required.

    Food-contact and potable-water suitability are not automatic properties of the base resin. In the United States, the olefin polymer may qualify under FDA 21 CFR 177.1520 if the finished resin and any colourants or processing aids meet the extractables limits in that section. In the European Union, compliance is evaluated under Regulation (EU) No 10/2011, including overall migration and specific migration limits. The grade itself does not confer food-contact status; the final container must be tested under the intended food type, contact time, and temperature. TPI Polene’s technical data sheet and certificate of analysis should be reviewed for specific additive disclosure, including antioxidants and catalyst neutralizers.

    Recycled material can be incorporated into non-critical layers at typical regrind levels of 10–30 wt%, but higher percentages may reduce ESCR, widen molecular weight distribution, and increase odour. Moisture sensitivity of HDPE is low, but pellets stored in high-humidity conditions above 80 % RH may develop surface moisture that produces splay or bubbles in the parison. A hopper dryer at 70–80 °C for 1–2 h is recommended only when surface moisture exceeds 0.10 wt%. Incompatibility with polypropylene contamination should be controlled because small amounts of PP can reduce weld strength and create visible delamination at pinch-off seams. Chlorinated polymer contamination must be excluded to avoid corrosive degradation products.

    Top