Tpi Polene Hdpe 7000 F

TPI Polene HDPE 7000 F

    • Product Name: TPI Polene HDPE 7000 F
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 683124
    Polymer Type High Density Polyethylene
    Grade HDPE 7000 F
    Form Pellets
    Melt Flow Rate 190 C 2 16 Kg 0.05 g/10 min
    Density 0.954 g/cm³
    Melting Point 130 °C
    Vicat Softening Temperature 125 °C
    Tensile Strength At Yield 25 MPa
    Tensile Strength At Break 35 MPa
    Elongation At Break >600 %
    Flexural Modulus 1100 MPa
    Shore D Hardness 65
    Environmental Stress Crack Resistance F50 >1000 h
    Dart Impact Strength 150 g
    Haze 10 %
    Gloss 45 70

    As an accredited TPI Polene HDPE 7000 F factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing TPI Polene HDPE 7000 F resin is packed in 25 kg polyethylene-lined woven sacks, stacked on pallets for industrial shipment.
    Container Loading (20′ FCL) 20' FCL container loading of TPI Polene HDPE 7000 F in 25 kg bags, palletized, stretch-wrapped, and secured for ocean shipment.
    Shipping TPI Polene HDPE 7000 F is a non-hazardous high-density polyethylene resin supplied as pellets. It ships in 25 kg bags, jumbo bags, or bulk containers, typically palletized and stretch-wrapped. Keep dry, away from heat and direct sunlight. No special dangerous-goods handling required; standard polymer transport applies.
    Storage Store TPI Polene HDPE 7000 F in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, flames, and strong oxidizing agents. Keep original bags sealed and palletized off the floor to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and excessive stacking. Store separately from incompatible materials. Follow supplier SDS, local regulations, and first-in, first-out inventory.
    Shelf Life Stored cool, dry, ventilated, away from sunlight and heat, TPI Polene HDPE 7000 F has indefinite shelf life if uncontaminated.
    Application of TPI Polene HDPE 7000 F

    In high-stalk blown film conversion, TPI Polene HDPE 7000 F is processed on monoextrusion lines configured with 25:1 to 30:1 L/D grooved-feed extruders and barrier screws designed for high-viscosity film resins. Melt temperature measured at the adaptor is typically held between 205 °C and 225 °C, with the feed throat water-cooled to 60–80 °C to prevent premature pellet melting in the grooved section. Die gap is generally set at 1.2–1.5 mm for down-gauged retail carrier bags and refuse sacks in the 8–30 µm thickness range. Blow-up ratio is maintained between 3:1 and 5:1, while frost-line height is positioned at 8–12 die diameters above the air ring to stabilise the high-molecular-weight melt bubble. Under these conditions, transverse direction orientation is controlled primarily by internal bubble cooling flow rather than by increasing air-ring venturi velocities alone. A silica-based HDPE antiblock masterbatch in the range 2–4 wt% is added at the hopper only when roll-to-roll slip becomes a constraint on downstream bag machines. Finished monolayer film is evaluated for tensile modulus and elongation using ISO 527-3:2018 and for dart drop impact using ASTM D1709. Film thickness profile is verified on-line by beta or X-ray scanning and is referenced to ISO 4593:2020 mechanical sectioning when off-line verification is required.

    The same high-stalk process window also feeds inline bag converters, where the collapsed web is sealed into T-shirt bags or wicketed refuse sacks. Seal bars are maintained below 160 °C to reduce heat-seal distortion of the oriented high-density polyethylene film. Because the resin has a high extensional viscosity, the rewind and dancer controls are set with longer distance-to-torque response than conventional low-viscosity film grades. Bag machine feed instability is typically traced to gauge variation above ±5 % of target thickness, which shifts seal dwell time and causes mis-indexing.

    What Compliance Evidence Is Required for Frozen Food Contact Liners?

    A converter placing TPI Polene HDPE 7000 F into direct contact with frozen or dry foods must first obtain the resin manufacturer’s lot-specific food-contact statement covering the complete additive package. In the United States, olefin polymers used as food-contact articles are covered by 21 CFR 177.1520, provided the finished article meets applicable extractive limitations for the intended use condition and food type. In the European Union, Regulation EU 10/2011 requires an overall migration test on the finished contact layer, commonly under OM2 conditions for long-term storage at frozen or refrigerated temperatures. The converter cannot rely solely on the resin grade designation because printing inks, slip additives, and converter-added masterbatch change the migration profile of the final film. For multi-layer structures, the entire composite must be evaluated, not only the HDPE layer. Where the film is used for fatty frozen food contact, simulant D1 under EU 10/2011 is applied if the product falls under long-term storage classification.

    Standard or RegulationTest ObligationComponent Controlled
    21 CFR 177.1520Olefin polymer compliance with end-use limitations and additive clearanceBase HDPE resin and antioxidant package
    EU 10/2011 Annex IOverall migration under OM2 or other condition specified by food typeFinished food-contact film or composite
    EC 1907/2006SVHC article notification if concentration exceeds 0.1 wt% in imported film rollsFinished film roll

    Sealing of frozen food liners is usually performed on automated vertical form-fill-seal equipment with seal bar temperatures between 120 °C and 150 °C. Lower sealing temperatures within this range reduce off-flavour carryover from low-density sealant skins. The HDPE layer itself provides stiffness for freezer display and resists puncturing from irregular frozen contents, but puncture resistance is not assigned a universal value without referencing ASTM D5748 or equivalent end-use testing performed on the filled bag.

    In coextruded flexible packaging laminates, TPI Polene HDPE 7000 F is employed as the high-stiffness core layer in three-layer or five-layer films for dry particulate foods, pet-food pouches, and cereal liners. The HDPE core is typically run at 50–70 % of total film thickness, with skin layers of linear low-density polyethylene or metallocene polyethylene providing seal integrity. Layer distribution is controlled through a spiral mandrel die with independent melt temperature zones, and die gap is held between 1.4 mm and 2.0 mm to stabilise the high-viscosity core at line speeds above 120 m/min. The high melt strength of TPI Polene HDPE 7000 F resists draw resonance when the coextruded structure is stretched through machine-direction orientation units after reheating. Water vapour transmission rate of the finished laminate is measured by ASTM F1249-20; published data for this specific grade in multi-layer structures is limited, so convertors obtain perforation and seal-strength data from their own pilot runs. Finished pouch performance is further checked for seal strength under ISO 527-3:2018 and for leak integrity by vacuum decay testing on the filled pouch line.

    When Heavy-Duty Liners Must Withstand Creep During Outdoor Storage

    TPI Polene HDPE 7000 F is converted into heavy-duty industrial liners for dry powder and granular chemicals at thicknesses from 100 µm to 250 µm. The formulation for outdoor storage commonly includes a UV-stabilised masterbatch at 2–5 wt%, with carbon black or hindered amine light stabiliser content adjusted to the expected ultraviolet exposure. Extrusion is performed through a wide die with a gap of 2.0–2.4 mm and a lower blow-up ratio of 2:1 to 3:1 to produce a flatter, stiffer web with improved machine-direction tear resistance. The finished liner is inserted into woven polypropylene sacks or paper multiwall sacks and must hold granular fertiliser, resin pellets, or mineral fillers without short-term creep splitting at the bottom gusset. Creep resistance is referenced to ISO 899-1:2018, while tensile strength and elongation of the liner are characterised by ISO 527-3:2018. For dangerous goods packaging, the outer sack must meet UN 6.1 performance requirements, but the internal HDPE liner alone does not constitute a certified dangerous goods package.

    In paper-like film conversion for envelope windows, drawer liners, and stiff bag stock, the high-viscosity melt of TPI Polene HDPE 7000 F is processed at a high blow-up ratio and a low frost-line position to generate a balanced orientation with elevated bending stiffness. The resulting film is perceived as paper-like in stiffness and is used in applications where a crisp flat web is required. The converter maintains the die gap at 1.2–1.6 mm and limits melt temperature to below 230 °C to preserve surface clarity. If the film is printed or lacquered, corona treatment is applied at 42–50 mN/m dyne level and verified by wetting fluids referenced to ISO 8296:2003. The final product is evaluated for blocking resistance because high-static surface charges on thin HDPE film can build up on collator equipment. Where blocking becomes a line constraint, a converter adds an HDPE-compatible antiblock masterbatch at the lowest level that maintains printable surface uniformity.

    Strain-Hardening Behaviour in High-Stalk Bag Stock at Elevated Frost-Line Heights

    When TPI Polene HDPE 7000 F is run on high-stalk bag stock lines with frost-line heights above 10 die diameters, the deformation history of the bubble changes from a predominantly machine-direction orientation profile to a more biaxial orientation profile. The high melt strength of this resin reduces bubble sag and stabilises the stalk, but only if the internal bubble cooling system is balanced against the high-viscosity melt exiting the die. If the frost line is raised without increasing internal bubble cooling flow, the bubble begins to oscillate at frequencies between 0.2 Hz and 1.0 Hz, producing periodic transverse direction gauge variation. On 90 mm high-stalk extruders, melt pressure before the screen changer for this grade commonly operates in the 300–380 bar range when die gaps are below 1.5 mm. If melt pressure exceeds 420 bar, the breaker plate or screen pack should be inspected for plate-out from degraded polymer fractions. To bring film thickness below 10 µm while maintaining bubble stability, many converters increase die gap to 1.6–1.8 mm and reduce the blow-up ratio to 3:1–3.5:1. This adjustment lowers die lip shear stress and shifts orientation balance toward machine direction bag propagation. Finished loop film is checked for thickness profile and blocking, and the converter records melt pressure trend data against roll length because pressure drift is an early indicator of gel accumulation or screen pack blinding.

    Regrind from edge trim, start-up scrap, and roll tailings is returned to the same high-stalk lines at addition levels commonly held below 25–30 wt% of total feed to prevent excessive melt-pressure rise and gel count increase. The reuse stream is passed through a continuous backflush or candle filter with screen pack grades of 80/120/80 mesh. If the regrind contains printed film, paper labels, or EVA sealant skins from coextruded lots, screen changer cycle time shortens and head pressure rises over a single production shift. For closed-loop T-shirt bag production, the converter often blends clean fluff with virgin pellets in a gravimetric batch hopper and records regrind fraction against final bag thickness variation. The film properties for bags containing regrind are checked by ISO 527-3:2018 tensile testing and compared with the virgin reference because regrind history can shift elongation at break even when melt flow index remains within specification.

    Free Quote

    Competitive TPI Polene HDPE 7000 F prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    TPI Polene HDPE 7000 F is a high-molecular-weight high-density polyethylene supplied by TPI Polene Public Company Limited for blown film extrusion. The grade is assigned to the supplier’s film resins where melt strength, thin-gauge drawdown, and bubble stability are primary acceptance criteria. A melt mass-flow rate measured at 190°C/2.16 kg under ISO 1133-1:2022 typically falls below 0.10 g/10 min; routine quality control therefore uses the high-load condition of 190°C/21.6 kg. Resin density determined by ASTM D1505 is commonly 0.951–0.955 g/cm³. The high molecular weight and intermediate density produce a balance of dart impact resistance, stiffness, and moisture barrier that is different from LDPE and LLDPE film resins in the same converter portfolio.

    Extrusion of this grade is not interchangeable with general-purpose LDPE processing. The feed section should be a grooved or intensively cooled design to prevent pellet-skid and screw-slip pressure oscillations. A barrier screw with an L/D of 24:1 to 30:1 and a compression ratio of 2.8:1 to 3.5:1 is used; barrel profile from 180°C in the feed zone to 230°C in the metering zone is common. Adapter and die temperatures are held at 220–240°C. Melt temperatures above 260°C are avoided because they accelerate thermo-oxidative gel formation and off-flavour development.

    What Processing Window Preserves Bubble Stability in 7000 F?

    Die gap, blow-up ratio, and frost-line position are critical variables. Die gap is set at 1.0–1.4 mm for HMW-HDPE film; narrow gaps increase shear heating and can lower melt fracture resistance, while wide gaps reduce orientation and may create gauge streaks. Blow-up ratio is maintained at 3.5:1 to 5.5:1 to distribute machine-direction and transverse-direction mechanical properties. Frost-line height is adjusted to 6–10 die diameters. A low frost line produces fast quench and lower haze but may amplify MD/TD tensile imbalance; a high frost line improves transverse-direction stress relaxation but reduces bubble stability under cross-drafts.

    Production-scale observations on conventional HDPE blown film lines indicate die-entry pressures of 250–400 bar at normal throughputs. Internal bubble cooling and dual-lip high-velocity air rings are used when line speed exceeds 50 m/min or when film gauge is below 15 µm. The extruder drive should have a specific energy capability of 0.20–0.28 kW/(kg/h) for HMW-HDPE; inadequate torque results in screw-stall or pressure variation rather than controlling melt temperature.

    Rheological characterisation by oscillatory shear shows that HMW-HDPE film grade retains a high zero-shear viscosity; at 0.1 rad/s and 190°C the complex viscosity of similar materials is typically above 10,000 Pa·s, while at 100 rad/s it may fall to 1,000–2,000 Pa·s. This shear-thinning response supports high bubble stability at low shear and sufficient flow at high shear in narrow die lips.

    Melt pumps and gravimetric feeding reduce gauge variation. When a melt pump is installed, inlet pressure is maintained at 150–250 bar to prevent cavitation; automatic air rings can reduce web thickness variation to ±3%. Screen packs with 80/120/80 mesh layers are used to trap degraded gel particles and build back-pressure. A rise in melt pressure above 10% of baseline at constant output indicates screen pack fouling or die-lip degradation.

    Film Mechanical Property Benchmarks and QC Test Methods

    Published third-party data for this specific TPI Polene HDPE 7000 F grade is limited; the ranges in Table 1 are representative of HMW-HDPE blown film resins in the 0.951–0.955 g/cm³ density class and must not replace the manufacturer’s certificate of analysis. Mechanical values are gauge-dependent and change with blow-up ratio, frost-line height, and drawdown ratio.

    PropertyTest methodRepresentative range
    Resin densityASTM D15050.951–0.955 g/cm³
    High-load melt index at 190°C/21.6 kgISO 1133-1:20227–10 g/10 min
    Tensile yield strength MD/TDASTM D88224–30 MPa / 22–28 MPa
    Tensile break strength MD/TDASTM D88235–48 MPa / 30–42 MPa
    Elongation at break MD/TDASTM D882500–800% / 550–850%
    Dart drop impact F50 at 25 µmASTM D1709 method A120–200 g
    Water vapour transmission rate at 38°C/90% RH, 25 µmASTM E96/E96M4–7 g/(m²·day)

    ESCR testing under ASTM D1693 condition B with 100% Igepal CO-630 usually exceeds 100 hours for HMW-HDPE film grades in this density class. Specific ESCR values depend on comonomer type, molecular weight distribution, and stabilizer package. Converters introducing post-consumer recycle should revalidate ESCR because stress-cracking resistance can fall with contaminated reclaim.

    When Coextrusion Uses HDPE 7000 F as the Core Layer in Barrier Film

    In coextruded structures, 7000 F is used as a high-stiffness core between LLDPE or metallocene-catalysed LLDPE skins. This arrangement preserves low seal initiation temperature and hot-tack performance in the skins while using the HDPE core to increase modulus and reduce water vapour transmission. Compared with a pure LLDPE monolayer of the same gauge, an HDPE core can reduce moisture permeation by 30–50% when tested at 38°C/90% RH using ASTM F1249 or ISO 15106-2. Heat-seal strength remains a function of the outer layer resin and seal bar conditions; the HDPE core does not provide sealant functionality.

    Skin-to-core ratios of 15:70:15 to 25:50:25 are common for high-speed packaging films. If the core exceeds 70% of the total structure, dart impact and tear resistance can decrease because the high-density core propagates fracture less ductilely than LLDPE at room temperature. Layer distribution around the die circumference should be controlled within ±10% to prevent gauge bands and heat-seal variability.

    In mono-layer applications, 7000 F is selected for T-shirt bags, shopping bags, fresh produce bags, cold-water food-contact packaging, and industrial liners. T-shirt bags are drawn down to 8–12 µm; the high melt strength permits this gauge without bubble chatter. In industrial liners, the grade is selected over LDPE when the service requires a higher yield stress and lower elongation under manual lifting. HDPE film typically shows tensile yield stress above 20 MPa, while many LDPE film grades are below 10 MPa; the trade-off is lower Elmendorf tear compared with LLDPE at equivalent gauge, so blends with 20–30 wt% LLDPE are commonly used to restore tear strength.

    Within the TPI Polene HDPE portfolio, 7000 F differs from blow-moulding and pipe grades because it is formulated for bubble stability and thin-gauge film extrusion rather than parison swell or long-term hydrostatic strength. Injection-moulding HDPE grades typically show melt mass-flow rates at 190°C/2.16 kg of 4–20 g/10 min, whereas HMW-HDPE film grade remains below 0.10 g/10 min. This difference prevents direct interchangeability of screws, barrels, and dies without rebalancing shear history and residence time.

    Processing variableStarting rangeLocation/condition
    Barrel feed zone temperature180–200°Cextruder zone 1
    Barrel metering zone temperature210–240°Cextruder final zone
    Adapter/die temperature220–240°Cdie body
    Melt temperature210–245°Cmelt thermocouple
    Die gap1.0–1.4 mmdie lip
    Blow-up ratio3.5:1–5.5:1bubble diameter
    Frost-line height6–10 die diametersbubble
    Melt pressure at die250–400 barpressure transducer

    Moisture absorption in HDPE is low, but surface condensation from cold storage and high-humidity warehouses can introduce film defects. If pellets are stored below 10°C and moved into a warm converting hall, condensation should be avoided or a pre-drying step at 65°C for 2–4 hours should be used. The grade should be purged with LDPE or LLDPE during shutdown to prevent long residence time at processing temperatures. Melt temperatures above 260°C accelerate thermo-oxidative degradation and raise gel counts and black specks.

    For food-contact evaluations, the base resin is typically represented as complying with FDA 21 CFR 177.1520 and EU 10/2011 under the converter’s specific conditions of use. Overall migration limits and organoleptic performance depend on final film structure, inks, and processing aids. The grade is not intended for medical implant, parenteral, or high-temperature sterilisation applications exceeding its softening range.

    Ultraviolet stabilisation is required for outdoor use beyond short service periods. Unstabilised HDPE film under continuous outdoor weathering can lose more than 50% of initial elongation at break within 12 months depending on geographic location and light intensity. Outdoor films should be formulated with UV-stabilised masterbatch at 2–5 wt% and validated under ASTM G154 or ISO 4892-2 before commercial release.

    Top