TPI Polene HDPE 5604F
-
Product Name:
TPI Polene HDPE 5604F
-
Factroy Site:
Yinchuan, Ningxia, China
-
Price Inquiry:
sales8@ascent-chem.com
-
Manufacturer:
Ascent Petrochem Holdings Co., Limited
-
CONTACT NOW
-
TPI Polene HDPE 5604F is typically used in formulations when melt flow rate, density, and molecular weight distribution and extrusion temperature, die pressure, and blow-up ratio must be controlled within specific ranges.
Specifications
|
HS Code
|
557972
|
| Density |
0.956 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg |
0.04 g/10 min |
| Melt Flow Rate 190 C 21 6 Kg |
5.0 g/10 min |
| Tensile Strength At Yield |
28 MPa |
| Tensile Strength At Break |
30 MPa |
| Elongation At Break |
>600% |
| Flexural Modulus |
1200 MPa |
| Vicat Softening Point |
125°C |
| Melting Point |
130°C |
| Environmental Stress Cracking Resistance |
>1000 h |
| Hardness Shore D |
65 |
| Crystallinity |
70% |
As an accredited TPI Polene HDPE 5604F factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
Packing & Storage
| Packing |
TPI Polene HDPE 5604F is packaged in 25 kg polyethylene-lined woven bags, with 1,000 kg jumbo bags available. |
| Container Loading (20′ FCL) |
Container loading (20′ FCL): TPI Polene HDPE 5604F, 25 kg bags, palletized, shrink-wrapped, approx. 18–20 MT net, securely stowed. |
| Shipping |
TPI Polene HDPE 5604F is typically shipped as non-hazardous polyethylene resin pellets in 25 kg PP bags, palletized and stretch-wrapped. Transport in clean, dry containers or trucks, protected from moisture, direct sunlight, and heat. No special dangerous-goods documentation is required. |
| Storage |
Store TPI Polene HDPE 5604F in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, and flames. Keep original bags closed, palletized, and off the floor to prevent moisture and contamination. Avoid strong oxidizers, acids, and bases. Maintain moderate temperatures, avoid prolonged UV exposure, ensure adequate ventilation, prevent physical damage, and follow local regulations and the SDS. |
| Shelf Life |
TPI Polene HDPE 5604F: 24-month shelf life if stored unopened, cool, dry, and protected from direct sunlight and moisture. |
Application of TPI Polene HDPE 5604F
The 5604F grade processes on single-station and double-station shuttle blow molding machines equipped with 65 mm, 24:1 L/D grooved-feed extruders at barrel zone setpoints of 170 °C–195 °C in the feed and compression sections, rising to 200 °C–210 °C at the metering section and die head. Observed melt temperatures at the die exit on continuous production lines typically register between 195 °C and 205 °C, a processing window that preserves parison melt strength for container volumes up to 1 L. Monolayer detergent bottle formulations are compounded at 96.5–98.0 wt% neat HDPE 5604F combined with 2.0–3.5 wt% pigment masterbatch; no supplemental processing aids are required under ambient conditions with relative humidity below 60 %. Above that threshold, pre-drying of the masterbatch at 80 °C for 2–4 h is implemented to prevent surface splay defects. Environmental stress crack resistance (ESCR) constitutes the critical performance criterion for liquid detergent packaging containing anionic and nonionic surfactant systems formulated at alkaline pH values of 8.5–11.0. Published ESCR data for HDPE blow molding grades in the 0.955–0.956 g/cm³ density band typically indicate F50 values exceeding 100 h under ASTM D1693 immersion in 100 % Igepal CO-630 at 50 °C, although grade-specific published data for 5604F in aggressive hypochlorite-based cleaners remains limited. A documented processing boundary exists at melt temperatures above 220 °C: oxidative chain scission accelerates antioxidant depletion, and ESCR retention has been measured to degrade by 30–50 % on blow-molded bottle shoulder and pinch-off zones when residence time exceeds 8 min at that temperature. Production-scale experience on accumulator-head machines indicates that die head tooling with 0.5–1.5 mm die gaps and 15-point parison programmers are necessary to maintain wall thickness variance below ±0.15 mm at container shoulder, sidewall, and base transition radii. Industry compliance for this downstream track is anchored to REACH Regulation (EC) No 1907/2006 Annex XVII restrictions, RoHS Directive 2011/65/EU for heavy-metal colorant content, and the United Nations Globally Harmonized System (GHS) label durability requirements under UN Recommendation 12. Terminal blow-molded product types include 500 mL–1 L laundry detergent bottles, multi-surface cleaner trigger-spray bodies, bleach-containing household chemical containers, and fabric softener bottles with integrated dosing chambers. The clean compatibility profile of HDPE 5604F with chlorine-releasing agents at concentrations below 5 wt% active hypochlorite is supported by field data from detergent packaging facilities, where annual reject rates attributable to stress-cracking at flash-line pinch-off zones remain below 0.5 % when cooling air temperature at the mold is controlled between 8 °C and 12 °C.\[\begin{array}{|c|c|c|c|c|}\hline\textbf{Test Condition} & \textbf{ASTM Method} & \textbf{Condition Detail} & \textbf{Typical Result for HDPE Blow Molding Grade (0.955 g/cm³)} & \textbf{Application Relevance} \\\hline\text{ESCR F50} & ASTM D1693 & 100 % Igepal CO-630, 50 °C & > 100 h & Detergent bottle shelf-life \\\hline\text{Tensile Strength at Yield} & ASTM D638-14, Type IV specimen & 50 mm/min crosshead & 26–28 MPa & Bottle compression resistance \\\hline\text{Elongation at Break} & ASTM D638-14, Type IV specimen & 50 mm/min crosshead & > 800 % & Drop-impact energy absorption \\\hline\text{Melt Flow Index} & ASTM D1238-20, 190 °C/2.16 kg & — & 0.4–0.7 g/10 min & Parison sag control \\\hline\text{Density} & ASTM D1505-18, gradient column & 23 °C & 0.955–0.956 g/cm³ & Stiffness and ESCR balance \\\hline\end{array}\]
What Governs Parison Stability in Pharmaceutical Bottle Blow Molding?
In pharmaceutical container production, the 5604F resin is run on injection blow molding (IBM) platforms and continuous extrusion blow molding lines dedicated to cleanroom operation under ISO 14644-1 Class 8 conditions. The melt temperature at the die exit is maintained between 190 °C and 200 °C, a deliberately narrower band than detergent-grade processing to minimize low-molecular-weight degradation species that would appear as extractables during USP <661.1> testing. Formulation for monolayer pharmaceutical containers consists of 99.0–100 wt% neat HDPE 5604F; if coloration is specified, masterbatch loadings are capped at 2.0 wt% using only pigment chemistries listed in FDA 21 CFR 178.3297 for indirect food and drug contact. The production process for tablet bottles typically employs a three-station IBM machine cycle: injection of the preform at 220 °C–240 °C barrel temperature, transfer to the blow station for container formation at a blow ratio not exceeding 2.0:1, and ejection with automated closure fitment verification. Compliance is governed by USP <661.1> for plastic packaging systems, European Pharmacopoeia Chapter 3.2.2 for polyethylene containers, and ICH Q3D for elemental impurities in container contact surfaces. Batch-to-batch variance in parison length is documented on IBM lines when ambient temperature fluctuation exceeds ±3 °C during a production shift; the resulting wall thickness deviation at the container base requires mold temperature compensation of ±2 °C. Terminal product types include 60 mL–240 mL tablet containers with child-resistant closure-compatible neck finishes, 100 mL–500 mL syrup bottles graduated for oral dosing, nasal spray bodies with tight bore tolerances of ±0.05 mm at the delivery orifice, and ophthalmic solution containers where drop-count consistency depends on sidewall compression modulus exceeding 700 MPa in the hoop direction. The ESCR performance of 5604F in pharmaceutical packaging is evaluated under ASTM D1693 conditions and additionally under simulated formulation exposure testing per USP <661.1> protocols using model solvents including ethanol-water mixtures and buffered solutions at pH 2.0 and pH 10.0.The conversion of HDPE 5604F into food-contact containers proceeds on accumulator-head extrusion blow molding machines rated for 20–30 kg/h throughput when processing containers in the 250 mL–2 L volume range. The resin is introduced without pre-drying at relative humidity below 60 %; above that threshold, a 2 h desiccant dryer cycle at 80 °C is inserted upstream of the hopper to eliminate surface moisture that produces splay on pinch-off weld lines. Compliance for food packaging applications derives from FDA 21 CFR 177.1520(c) defining permitted olefin polymers for food contact, EU Regulation (EU) No 10/2011 with an overall migration limit of 10 mg/dm² for all food simulants, and GB 9685-2016 for positive-list additives in the Chinese market. The formulation is strictly constrained: neat HDPE 5604F is used at 99.0–100 wt%, with any antioxidant or neutralizer content predetermined by the resin manufacturer's stabilization package and not modified by the converter. Addition ratios for food-contact masterbatch, when color is required, do not exceed 1.5 wt% and must comply with the dual-use additives list in FDA 21 CFR 177.1520(b). Production process parameters for food jars differ from detergent bottle lines in one critical respect: mold cooling channels are operated at 5 °C–10 °C lower than detergent container production to accelerate crystallization kinetics and reduce residual monomer or oligomer diffusion to the food-contact surface. Terminal product types include 500 g–1 kg honey containers requiring barrier performance against moisture ingress at the 0.03 g/m²·day threshold at 23 °C and 85 % RH, spice jars with extended neck profiles, condiment squeeze bottles rated for repeated flexural fatigue of 50,000 cycles without sidewall whitening, and aseptic dairy portion cups where the blow molding flash line must be trimmed with automated deflashing systems achieving dimensional tolerances of ±0.1 mm.Table 2 below consolidates the compliance matrix for 5604F across food-contact applications:\[\begin{array}{|c|c|c|c|c|}\hline\textbf{Compliance Domain} & \textbf{Standard/Regulation} & \textbf{Specific Clause/Test} & \textbf{Limit/Requirement} & \textbf{Verification Frequency} \\\hlineUS Food Contact & FDA 21 CFR & §177.1520(c) & Olefin polymers allowed for food contact & Per formulation change \\\hlineEU Migration & Regulation (EU) No 10/2011 & Annex I, OML & 10 mg/dm² total migration & Per production campaign \\\hlineCanada Food Contact & HPFB/Health Canada & Section 2, Polyethylene & No objection letter required & Per resin lot \\\hlineChina Positive List & GB 9685-2016 & Additive appendix & Listed additives only & Per masterbatch batch \\\hlineSensory Testing & ISO 13302:2003 & Odor and taste transfer & No objectionable taint & Per new application \\\hline\end{array}\]Cosmetic Container Wall Thickness Distribution Across Blow Ratios
Extrusion blow molding of cosmetic bottles from HDPE 5604F is executed with accumulator-head machines fitted with adjustable die gaps from 0.75 mm to 2.0 mm and multi-zone parison programmers capable of 30 discrete wall thickness points. The critical production challenge in cosmetic packaging is the interplay between blow ratio and wall thickness uniformity: increasing blow ratio beyond 2.5:1 degrades sidewall thickness variance beyond ±0.2 mm and generates visible stress whitening at the transition between container body and shoulder geometry. The formulation for opaque cosmetic bottles comprises 97.0–99.0 wt% neat HDPE 5604F with 1.0–3.0 wt% pigment masterbatch selected for lightfastness per ISO 105-B02 Blue Wool Scale ratings of 6 or higher; pearlescent or metallic finishes require an additional 0.5–1.0 wt% effect pigment dispersion, which simultaneously increases melt viscosity by 5–10 % and requires die temperature adjustment of +3 °C to +5 °C to restore parison surface smoothness. Compliance anchors for cosmetic packaging include EU Regulation (EC) No 1223/2009 Annex II prohibition verification for cosmetic container materials, ISO 17744:2004 for determining migration of substances from plastic packaging into cosmetic products, and FDA 21 CFR Part 700 where cosmetic containers sold in the US market are evaluated under the Federal Food, Drug, and Cosmetic Act Section 602. The production process is characterized by a specific cooling efficiency requirement: cosmetic bottle wall thickness of 0.6–1.2 mm necessitates mold cooling times between 9 s and 14 s per station cycle, and mold temperature is held at 12 °C–18 °C to achieve the surface gloss associated with premium cosmetic branding without inducing internal stress that would later manifest as base creep under vertical stacking loads exceeding 10 kPa. Terminal product types include 50 mL–500 mL lotion bottles with pump closure neck finishes, cream jars with internal lip diameters machined to ±0.05 mm, serum dropper bottles requiring precise sidewall flexibility for controlled drop dispensing, and compact powder stacking jars where the vertical compression strength under a 200 N top load must be maintained without permanent deformation. Production experience on Bekum BM-304 and Kautex KEB-series machines documents that 5604F exhibits consistent parison hang buoyancy at barrel residence times up to 6 min, permitting interrupted production schedules without excessive gel accumulation in the die head.For industrial chemical and agrochemical container production, HDPE 5604F is processed on accumulator-head blow molding machines with maximum shot capacities from 2 L to 10 L for containers requiring UN dangerous goods certification. The resin is compounded at 96.0–98.0 wt% with 2.0–4.0 wt% carbon black masterbatch when ultraviolet stabilization against outdoor storage is specified, or with 1.5–2.5 wt% pigment masterbatch for color-coded chemical class identification systems mandated by internal plant safety protocols. Chemical compatibility for containers used with agricultural pesticide formulations, solvent-based industrial cleaners, and petroleum-derived additive concentrates requires ESCR testing beyond standard ASTM D1693 conditions. Containers manufactured for Roundup-type glyphosate formulations and organophosphate-based pesticide concentrates are typically evaluated under ASTM D2561 (bottle ESCR under hoop stress) at 60 °C, with documented failure thresholds below 48 h indicating unacceptable environmental stress crack initiation at the internal stress concentration point at the container base flash line. Compliance for this application track is anchored to the United Nations Recommendations on the Transport of Dangerous Goods, Model Regulations (UN RTDG), specifically Chapter 6.1 for packaging construction and testing, supplemented by ADR (European Agreement Concerning the International Carriage of Dangerous Goods by Road) and IMDG Code requirements where maritime transport is specified. Production process parameters for industrial containers demand higher melt temperatures of 205 °C–215 °C at the die exit to reduce parison sag during long-shot extrusion for volumes exceeding 5 L; however, this elevated temperature band compresses the thermal degradation margin, and residence time must be capped at 5 min to prevent antioxidant depletion below the critical threshold of 0.04 wt% remaining concentration. Terminal product types include 1 L–5 L agrochemical containers with UN certification marking, 2 L–10 L industrial solvent containers with integrated bung closures, laboratory reagent bottles rated for corrosive liquid handling under ISO 4796, and fuel additive bottles where the container wall must maintain vapor transmission rates below 0.5 g/m²·day at 40 °C for aromatic hydrocarbon mixtures. The compatibility of HDPE 5604F with petroleum-based solvents used in automotive additive formulations is documented through immersion testing per ASTM D543-14, where weight gain typically remains below 1.5 % after 7 days of immersion in diesel fuel at 23 °C.Multilayer Barrier Requirements Shift Small-Container Design
In small-volume personal care extrusion blow molding, particularly for travel-size shampoo, conditioner, and body wash containers, HDPE 5604F is run on continuous shuttle machines with single-cavity or double-cavity molds at cycle times from 8 s to 12 s depending on container wall thickness and cooling air supply at the mold face. The production bottleneck encountered on high-cavitation shuttle lines is not melt delivery but rather mold cooling capacity: when cycle time is compressed below 8 s on 500 mL containers with 0.8 mm nominal wall thickness, post-ejection deformation at the base pinch-off zone has been documented as the primary rejection category, exceeding 1.5 % of total production. The formulation approach for this application track is unique in that HDPE 5604F serves as the structural layer in two-layer coextruded constructions, with ethylene-vinyl alcohol (EVOH) or polyamide barrier layers introduced at 3–5 wt% of total container mass when fragrance retention or water vapor barrier enhancement is required. Adhesion between the HDPE 5604F structural layers and the barrier core is achieved through maleic anhydride grafted polyethylene tie resins dosed at 2–4 wt% of total formulation. Compliance requirements for personal care products mirror those of cosmetic packaging under EU Regulation (EC) No 1223/2009, with additional durability expectations defined by the International Air Transport Association (IATA) dangerous goods regulations for travel-size products sold at duty-free terminals. Production process considerations center on the coextrusion die temperature differential: the barrier layer channel is maintained at 200 °C–210 °C while the HDPE 5604F channels operate at 190 °C–200 °C to compensate for the higher melt strength of the polyamide layer and prevent interfacial instability at the die confluence point. Terminal product types include 30 mL–100 mL travel-size bottles with tamper-evident closure compatibility, 250 mL–500 mL hotel amenity containers with silk-screened branding surfaces, pump-action body wash bottles requiring neck finish tolerances of ±0.1 mm for pump collar sealing, and coextruded fragrance bottles where sensory threshold testing per ISO 13302:2003 is executed on every production lot to verify absence of odor carryover from the barrier resin system.In small-volume industrial packaging for specialty chemical distribution, 5604F is converted on single-station blow molding lines dedicated to short-run production of 500 mL–2 L containers for laboratory reagent suppliers and specialty chemical formulators. The processing window deviates from high-volume detergent bottle production in that accumulator head shot capacity is deliberately oversized by 25–30 % relative to container final weight to accommodate the extended parison programming necessary for containers with eccentrically positioned neck offsets or insert-molded handle geometries. Melt temperature is held between 195 °C and 205 °C, and the parison extruder screw speed is reduced to 30–50 % of maximum rated throughput to extend residence time and stabilize parison diameter uniformity, which is critical for containers where the neck opening diameter relative to body diameter exceeds 60 %. Compliance anchors are derived from ISO 17712 for tamper-evident container sealing mechanisms, the United Nations RTDG for small-volume chemical packaging when products are classified as dangerous goods, and ISO 9001:2015 production traceability requirements where each container lot is traced to a specific resin batch certificate. Terminal product types include 500 mL–1 L laboratory reagent containers with chemical compatibility verified against a 45-exposure panel of common laboratory solvents including acetone, methanol, and diethyl ether, 1 L semiconductor-grade chemical containers where ionic extractables must be below 1 ppb total leachable sodium, and specialty catalyst delivery containers where wall thickness at the container base must remain above 2.5 mm to prevent puncture during vacuum-assisted transfer operations.When Blow Molding Replaces Injection Molding in Horticultural and Pool Chemical Packaging
The application of HDPE 5604F to horticultural and swimming pool chemical container production is driven by a cost-to-performance substitution equation: blow molding eliminates the multi-drop mold complexity of injection molding while preserving the chemical barrier and ESCR properties required for aggressive oxidizer formulations. Production is executed on accumulator-head machines with shot capacities from 1 L to 5 L, operating at melt temperatures between 190 °C and 205 °C and mold cooling water at 8 °C–10 °C to maximize surface hardness against stacking loads. Formulation for this application track adds 0.05–0.15 wt% calcium stearate as an acid scavenger when the container is specified for trichloroisocyanuric acid or calcium hypochlorite granule storage; the acid scavenger neutralizes trace chlorine degradation products that would otherwise attack the polyethylene chain at elevated warehouse temperatures. Compliance requirements are anchored to United Nations RTDG for oxidizing substances (Class 5.1) packaging, ISO 16103:2005 for packaging of dangerous goods, and ASTM D543-14 immersion testing using 10 % sodium hypochlorite solution at 40 °C for 7-day exposure. The production process for pool chemical pails involves a specific pinch-off zone challenge: containers with base diameters exceeding 150 mm develop flash-line internal stress concentrations that are mitigated by local mold temperature elevation of +5 °C at the pinch-off region, a modification that reduces stress whitening events by approximately 40 % compared to uniform mold temperature control. Terminal product types include 1 kg–5 kg pool disinfectant containers with moisture barrier requirements below 0.1 g/m²·day at 38 °C and 90 % RH, horticultural fertilizer containers with low-temperature drop-impact resistance maintained to -10 °C per ASTM D5276-19, and granular garden chemical containers where sidewall compression strength under a 400 N vertical load must not exhibit permanent deformation exceeding 1 mm. The ESCR behavior of 5604F in the presence of chlorine-releasing pool chemicals is a non-linear function of formulation concentration: containers exposed to chlorinating agents above 65 wt% active chlorine exhibit accelerated surface micro-cracking at internal stress points, whereas concentrations below 50 wt% active chlorine produce ESCR retention exceeding 80 % of virgin resin performance after 90 days of accelerated aging at 60 °C.
Free Quote
Competitive TPI Polene HDPE 5604F prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at
+8618005193850
or mail to
sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Inquiry
Get Free Quote of Ascent Petrochem Holdings Co., Limited
Flexible payment, competitive price, premium service - Inquire now!
Certification & Compliance
-
TPI Polene HDPE 5604F is manufactured under an ISO 9001 quality system and complies with relevant regulatory requirements.
-
COA, SDS/MSDS, and related certificates are available upon request.
For certificate requests or inquiries, contact: sales8@ascent-chem.com.
More Introduction
At a melt flow rate of 0.04 g/10 min under ASTM D1238 and a nominal density of 0.956 g/cm³ under ASTM D1505, TPI Polene HDPE 5604F is placed in the high-molecular-weight, high-density polyethylene film segment. The grade is intended for blown-film conversion in which thin-gauge stiffness, creep resistance, and bubble melt strength are specification targets, including T-shirt bags, grocery sacks, carrier bags, and high-speed packaging films. The melt flow rate is determined under a 2.16 kg piston load at 190 °C; a value below 0.05 g/10 min indicates that melt viscosity is high and that processing routes requiring low-viscosity flow, such as injection moulding and extrusion coating, are not appropriate. In blown-film practice, the high viscosity of HDPE 5604F supports an extended bubble stalk and draw distance before crystallisation, but it also increases screw torque and die-head pressure compared with lower-molecular-weight film resins. Manufacturer-published datasheet values and lot-specific certificates of analysis should be consulted because density and melt flow rate are controlled within production tolerances. Gel count and oxidation induction time are not part of the base datasheet and require separate certification for sensitive film applications.
Typical film structures use HDPE 5604F as a stiffness layer in monolayer or coextruded formats. Film tensile properties are commonly measured under ASTM D882 rather than the rigid-specimen method ASTM D638; converter specifications frequently require machine-direction and transverse-direction tensile strengths above 20 MPa and elongation at break above 400% at thicknesses between 8 µm and 25 µm. Dart impact resistance under ASTM D1709 Method A declines with downgauging and must be correlated with bag-drop performance on the target conversion line. Because HDPE 5604F has a higher density and crystallinity than linear low-density polyethylene, blocking behaviour and coefficient of friction differ; slip and antiblock additives are usually introduced by the converter rather than supplied in the base resin. Published data for structures below 10 µm is limited, so production-line validation is required.
What melt-flow and density boundaries impose torque and pressure limits on this grade?
The rheological behaviour of HDPE 5604F is dominated by low melt flow and high molecular weight, resulting in high shear viscosity at low shear rates. On a single-screw extruder with L/D 30:1 and a grooved-feed section, the grade generates higher die-head pressure than a 0.2 g/10 min blow-moulding HDPE when processed at the same melt temperature and die gap. A barrier screw with mixing elements is preferred for homogenisation because simple conveying screws can produce melt-temperature heterogeneity. Back-pressure at the screen changer should be monitored with a pressure transducer; progressive screen clogging raises head pressure and destabilises bubble geometry. Melt temperature should be kept below 220 °C to limit oxidative degradation and gel formation. If the melt temperature falls below 190 °C, the high viscosity can overload the extruder drive and create excessive shear heating.
The melt index ratio between 21.6 kg and 2.16 kg conditions under ASTM D1238 is a process-relevant indicator of shear thinning. For high-molecular-weight film HDPE grades, the ratio is commonly above 20:1. Capillary rheometry at 190 °C across shear rates from 10 s⁻¹ to 1000 s⁻¹ provides better die-pressure prediction than single-point melt flow rate. The power-law index of high-molecular-weight HDPE film grades typically falls in the range 0.25–0.40 over that shear-rate interval. Published data for this specific grade under full rheometric characterisation is limited; lot-specific rheometry is recommended for critical thin-gauge lines.
The property envelope of HDPE 5604F is not fully defined by density and melt flow rate. Converter specifications typically include film tensile properties under ASTM D882, dart impact under ASTM D1709, and tear strength under ASTM D1922. The following table summarises representative nominal ranges drawn from published high-density polyethylene film grade data; current certificates of analysis should be consulted for exact lot values.
| Property |
Test method |
Unit |
Published nominal range |
| Density |
ASTM D1505 |
g/cm³ |
0.955–0.957 |
| Melt flow rate at 190 °C, 2.16 kg |
ASTM D1238 |
g/10 min |
0.035–0.045 |
| Tensile yield strength |
ASTM D638 |
MPa |
28–31 |
| Elongation at break |
ASTM D638 |
% |
600–900 |
| Flexural modulus |
ASTM D790 |
MPa |
1000–1200 |
| Vicat softening point |
ASTM D1525 |
°C |
124–127 |
When high-stalk bubble geometry is applied to HDPE 5604F
High-stalk bubble configurations separate melt orientation from crystallisation and improve gauge uniformity. In this mode, the melt exits the die at 200–215 °C, is drawn into a stalk of 6–8 die diameters height, and then expands at the frost line. The low melt flow of HDPE 5604F provides sufficient melt strength to stabilise the stalk under moderate variations in extrusion rate and crosswind. If the die gap is below 0.8 mm, high shear at the die lip can initiate sharkskin melt fracture. Increasing the die gap to 1.0–1.2 mm and raising die temperature to 210 °C reduces surface defects. Frost-line height must be controlled within ± 50 mm; excessive height produces gauge bands and blocking. On production-scale lines, air-ring configuration and internal bubble cooling become critical when output exceeds 80 kg/h on a 65 mm die. Published data for this specific configuration is limited, but start-up records generally show that edge creasing and gauge bands originate from unbalanced air flow rather than resin deficiency.
Thickness control at 10 µm is more sensitive to melt-temperature uniformity than at 25 µm. Melt-temperature variation across the die circumference above ± 3 °C produces gauge bands and lowers dart impact under ASTM D1709. The high viscosity also increases residence time in the adapter; die-lip deposits may form if barrel wall temperatures exceed 220 °C. Periodic purging with high-viscosity HDPE or a commercial purging compound after 8 h of continuous operation is common if gels appear.
Corona treatment is required for print adhesion. Untreated polyethylene film has surface energy below 32 dyn/cm; corona treatment typically raises the surface energy to 38–42 dyn/cm. The treatment decays over time, so winding tension and storage time must be controlled. HDPE 5604F does not contain a built-in surface modifier, so treatment stability depends on the converter’s additive package and storage conditions. Water-based and solvent-based inks require different dyne retention; published data for this specific configuration is limited.
Heat sealing of HDPE 5604F requires higher seal temperatures than linear low-density polyethylene films. Heat-seal strength is commonly measured under ASTM F88; the seal initiation temperature of high-density polyethylene films typically lies between 125 °C and 135 °C, depending on thickness and seal-bar dwell. Coextruded LLDPE skins lower the seal initiation temperature and improve seal-through-contamination performance on bag lines. The higher density of HDPE 5604F also narrows the sealing window relative to lower-density film grades; converter trials must define the upper seal temperature to avoid seal distortion.
Water-vapour transmission rate under ASTM E96 is lower than that of linear low-density polyethylene films of comparable thickness because higher density reduces free volume. Oxygen transmission rate under ASTM D3985 remains high relative to polar barrier polymers; HDPE 5604F is not a barrier resin for oxygen-sensitive goods. It is therefore used in packaging where moisture stiffness and mechanical strength are more important than oxygen barrier. Converting lines that require high oxygen barrier use coextrusion or lamination with EVOH or metallised film; compatibility of the HDPE layer with tie resins should be confirmed.
Comparative selection against LLDPE film and HDPE blow-moulding grades
Relative to butene- or hexene-LLDPE film grades with density 0.918–0.923 g/cm³ and melt flow rate 0.8–1.2 g/10 min, HDPE 5604F raises tensile modulus and yield strength but lowers dart impact and tear propagation resistance under ASTM D1922. A monolayer HDPE 5604F film has a higher secant modulus than an equivalent LLDPE film; the trade-off is a more brittle puncture failure mode. For high-speed bag lines, coextruding a thin LLDPE skin with a HDPE 5604F core increases puncture resistance while retaining stiffness. In comparison with conventional HDPE blow-moulding grades, HDPE 5604F has a lower melt flow rate and is specified for film rather than bottle wall thickness control; blow-moulding grades are formulated for higher environmental stress crack resistance and different shear-rate flow. The selection boundary is therefore set by flow path: HDPE 5604F is not appropriate for injection moulding or blow moulding because its melt viscosity prevents adequate mould filling at standard clamp force settings. Published data for direct substitution of HDPE 5604F in blow-moulding tools is limited.
The grade’s comparative position within the supplier’s film portfolio is defined by melt flow rate and film-grade stabilisation rather than density alone. When downgauging from 20 µm to 12 µm, the loss in dart impact can be partially offset by blending with LLDPE, but the blend ratio must be confirmed by film testing under ASTM D1709 and ASTM D882. A processing advantage of lower-density film resins is lower energy input per kilogram; HDPE 5604F increases head pressure and motor torque, so screw speed and barrel temperature profiles must be adjusted accordingly. If the target line is a high-output coextrusion line with tight gauge tolerance, the resin should be evaluated at full output because melt-pressure and bubble-stability behaviour change with rate.
From a regulatory perspective, HDPE 5604F falls within olefin polymer provisions for food-contact film. A supplier statement under FDA 21 CFR 177.1520 is usually available, but the converter remains responsible for finished-article compliance under end-use extraction conditions. The grade should not be exposed to strong oxidising acids, aromatic solvents, or chlorinated hydrocarbons at elevated temperatures, because swelling and environmental stress cracking may occur. Storage should be in a covered, ventilated warehouse below 50 °C. Sustained relative humidity above 60% may require drying; if pellet surface moisture is evident, a desiccant hopper dryer at 80 °C for 4 h is recommended. Clean regrind up to 20 wt% is usually acceptable if free of LLDPE, LDPE, and paper fines, but physical properties under ASTM D1709 and ASTM D882 must be revalidated on the target line. Published data for this specific regrind configuration is limited.
The compliance matrix below identifies the main certification routes used for food-contact film and overall regulatory documentation.
| Standard or regulation |
Scope |
Verification pathway |
| FDA 21 CFR 177.1520 |
Olefin polymers for food-contact articles |
Supplier food-contact statement and end-use extraction testing under intended conditions of use |
| EC 1935/2004 |
Food contact materials and articles |
Overall migration testing under EN 1186 on finished film |
| REACH |
Registration and SVHC communication |
Article 33 declaration for substances of very high concern above 0.1 wt% |
| RoHS 2011/65/EU |
Restriction of hazardous substances |
Supplier declaration and X-ray fluorescence screening of heavy metals |