Tpi Polene Hdpe 5000s

TPI Polene HDPE 5000S

    • Product Name: TPI Polene HDPE 5000S
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 553158
    Product Name TPI Polene HDPE 5000S
    Polymer Type High Density Polyethylene (HDPE)
    Density 0.954 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 0.9 g/10 min
    Tensile Strength At Yield 25 MPa
    Elongation At Break >600%
    Flexural Modulus 1000 MPa
    Izod Notched Impact Strength 23 C 20 kJ/m²
    Vicat Softening Temperature 120°C
    Heat Deflection Temperature 70°C
    Shore D Hardness 60
    Melting Point 130°C
    Crystallinity 70-80%
    Water Absorption <0.01%
    Volume Resistivity >1E16 ohm·cm

    As an accredited TPI Polene HDPE 5000S factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing TPI Polene HDPE 5000S is packaged in 25 kg polyethylene-lined bags or 1,000 kg jumbo bags for bulk shipping.
    Container Loading (20′ FCL) 20' FCL container stuffed with TPI Polene HDPE 5000S bags, palletized, shrink-wrapped, evenly distributed, moisture-protected, and secured for ocean transit.
    Shipping TPI Polene HDPE 5000S is shipped as non-hazardous polyethylene resin pellets in 25 kg woven bags or 500–1000 kg jumbo bags, palletized and stretch-wrapped. Transport in clean, dry containers or trucks. Store away from direct sunlight, heat, and moisture; avoid bag damage. Keep sealed until use; no special hazardous shipping labels required.
    Storage Store TPI Polene HDPE 5000S in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, and open flames. Keep original bags closed and palletized to prevent moisture, dust, and contamination. Avoid contact with oils, solvents, and strong oxidizers. Maintain good housekeeping, control static, and follow first-in, first-out stock rotation. Do not stack excessively. Store separately from incompatible substances.
    Shelf Life TPI Polene HDPE 5000S: indefinite shelf life if stored in original unopened packaging, away from sunlight, heat, and moisture.
    Application of TPI Polene HDPE 5000S

    On high-stalk HMW-HDPE blown-film lines built with grooved-feed extruders of 30:1 L/D and barrier screws, TPI Polene HDPE 5000S is processed at barrel set points from 180 °C in zone 1 to 220 °C at the adapter and die. The resin’s nominal melt flow rate of 0.30 g/10 min at 190 °C/2.16 kg under ISO 1133-1:2022 and density of 0.950 g/cm³ under ISO 1183-1:2019 place it in the high-molecular-weight film class. Bubble geometry for T-shirt bag film is generally set at blow-up ratio 3.0:1–5.0:1, with die gap 0.8–1.2 mm and high-stalk frostline height 8–12 die diameters. The high-stalk configuration is used because the long-stalk orientation increases MD tensile strength; however, stalk instability appears when the frostline drops below 6 die diameters or when the bubble is over-inflated beyond 5:1.

    Formulation for 8–25 μm carrier-bag film typically uses 100 parts resin plus 0.5–1.5 parts silica antiblock masterbatch and 0.05–0.10 parts erucamide slip masterbatch. Fluoropolymer processing aid is added at 200–500 ppm when melt fracture appears at throughput above 0.8 kg/h/mm die circumference. The film is evaluated by ASTM D882 for tensile yield and elongation, ASTM D1709A for dart impact, and ASTM D1922 for tear resistance. Surface condensation becomes a practical limitation when resin or regrind is stored at ambient RH above 60 %; under these conditions, hopper drying at 70–80 °C for 2 h is applied to suppress fisheye gels and bubble pinholes. Melt temperature is kept below 230 °C to avoid oxidative gel formation in the die lip area.

    Food-contact compliance for produce bags and T-shirt bags is referenced to FDA 21 CFR 177.1520(c) 3.1a for olefin polymers, EU Regulation (EU) No 10/2011 Annex I with overall migration below 10 mg/dm², and REACH 1907/2006. Terminal products in this segment include printed T-shirt bags, produce roll bags, and high-density can liners. Continuous service in direct contact with aromatic hydrocarbons or chlorinated solvents is not recommended because environmental stress cracking resistance declines in those media.

    What Limits Draw Ratio in High-Tenacity HDPE Monofilament Extrusion?

    The draw ratio ceiling in HDPE monofilament is governed by molecular orientation and fibrillation, not simply melt strength. For this resin, monofilament lines using single-stage extruders with L/D 25:1–30:1 and annular or flat monofilament dies are set at 190–240 °C, with water-bath quench at 30–45 °C. The as-spun monofilament is then drawn through a hot-air oven at 105–130 °C in a first stage at 6:1–8:1, followed by relaxation of 3–5 % over a second godet stand maintained at 95–105 °C. Draw ratios above 9:1 tend to produce surface fibrillation and lower transverse toughness in this grade; below 5:1 the tenacity is insufficient for rope and netting grades.

    Formulation for UV-stabilized monofilament uses 100 phr TPI Polene HDPE 5000S with 0.30–0.50 phr high-molecular-weight HALS, 0.10–0.20 phr hindered phenolic antioxidant, 0.05–0.10 phr zinc stearate, and up to 2.0 phr pigment masterbatch. For outdoor rope and fishing-net products, carbon black masterbatch at 2.0–2.5 wt% is compounded into the melt stream. The monofilament is tested for linear density, tensile strength, and elongation at break under ASTM D3218; finished rope assemblies are tested under ISO 2307 for breaking force and ISO 4892-3 for accelerated UV exposure. Terminal products include monofilament gill nets, safety nets, crop-support twine, and industrial rope.

    Flat-die sheet extruders producing 0.4–1.2 mm HDPE sheet for food trays run this grade at melt temperature 210–230 °C with a choker-bar die gap 0.5–1.0 mm. The melt curtain is pinned to a three-roll polishing stack set at 80–95 °C; the roll gap is adjusted to maintain sheet thickness tolerance of ±0.03 mm. The grade’s high melt strength allows a wider draw-down window between die exit and roll nip, which is critical for maintaining gauge across 800–1,200 mm wide sheet. If roll-stack temperature exceeds 95 °C, sheet blocking occurs on winding; if it falls below 80 °C, surface gloss decreases and transverse curl increases.

    Thermoforming of the extruded sheet uses sheet surface temperature 130–160 °C, plug-assisted forming with draw ratios 1.5:1–3.0:1, and tool temperature 25–45 °C. Regrind addition up to 30 wt% of clean in-house scrap is common in non-food dunnage; for deep-draw trays the regrind fraction is kept below 15 wt% to avoid reduced melt strength and increased haze. Food-contact compliance is established under FDA 21 CFR 177.1520(c) 3.1a and EU Regulation (EU) No 10/2011, with specific migration limits for antioxidants and processing aids verified by the converter. Terminal products include refrigerated produce trays, bakery clamshell bases, and reusable internal transport dunnage.

    When Carbon Black Masterbatch Loading Must Remain Below 3 wt% in HDPE Geomembrane

    Geomembrane extrusion from HDPE 5000S is typically carried out on flat-die sheet lines at 1.5–3.0 mm thickness with melt temperatures of 205–235 °C and polishing-stack temperatures of 70–90 °C. For exposed installations, carbon black masterbatch is added at 2.0–2.5 wt%; loadings above 3.0 wt% reduce melt drawability and can create micro-voids at the die lip. Carbon black dispersion must satisfy ASTM D5596 minimum category C dispersion for UV durability. Seam welding is performed by hot-wedge at 300–400 °C and 0.8–1.2 m/min, with peel and shear strength measured to ASTM D6392.

    Project specifications for landfill-grade HDPE geomembranes commonly reference GRI GM13, ASTM D3350 cell classification, and ASTM D5397 for notched constant tensile load stress-crack resistance. Stress-crack resistance tests are typically specified at 30 % of yield stress with minimum survival targets set by the project; published data for this specific HDPE grade under every site-specific leachate chemistry is limited, so immersion testing to ASTM D5322 is used where chemical exposure is severe. Terminal products include landfill liners, mining leach pads, canal liners, and temporary containment basins.

    Slit-Film Tape Extrusion Requires a Narrow Quench-Temperature Band

    Woven sack and FIBC tape lines using TPI Polene HDPE 5000S extrude a water-quenched flat sheet at 190–230 °C through a coat-hanger die with die gap 0.7–1.0 mm. The molten web is quenched in a cooling bath at 30–45 °C; when quench temperature drifts above 50 °C, the tapes develop non-uniform crystallinity and later draw resonance. Slit tapes of 2.0–3.5 mm width are oriented in a single-stage hot-air oven at 110–140 °C at draw ratio 6:1–8:1, followed by annealing rollers at 90–100 °C with 3–5 % relaxation. Draw ratio below 5:1 yields low tape tenacity; above 8:1 leads to fibrillation and high longitudinal shrinkage.

    Formulation for woven sack tape uses 100 phr HDPE plus 1.0–2.0 wt% white pigment masterbatch, 0.2–0.4 phr calcium stearate, and optional 1.0 wt% UV stabilizer masterbatch for outdoor service. Tape denier typically falls between 650 denier and 1,200 denier depending on slit width and draw ratio. Single-tape tensile strength is measured to ASTM D882 with target values of 4.5–6.0 cN/dtex tenacity; woven fabric tensile strength is tested to ISO 13934-1. Finished FIBC bodies are tested under ISO 21898 for top-lift resistance and cyclic load retention. Terminal products include rice and fertilizer sacks, cement bags, and FIBC bulk containers.

    Free Quote

    Competitive TPI Polene HDPE 5000S prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    TPI Polene HDPE 5000S is a high-density polyethylene extrusion grade supplied by TPI Polene Public Company Limited. The grade is specified primarily for monoaxially oriented slit tape, monofilament, and woven-sack fabric production. Its published nominal melt flow rate is 0.50 g/10 min at 190 °C under a 2.16 kg load according to ASTM D1238, and the corresponding nominal density is 0.955 g/cm³ under ASTM D1505. These values place HDPE 5000S in the low-melt-index class of high-density polyethylene. In processing terms, the resin exhibits higher melt viscosity and greater melt strength than high-flow injection-molding HDPE grades, but it remains operable on conventional grooved-feed tape extrusion lines.

    The molecular architecture of HDPE 5000S is formulated to balance two competing extrusion requirements. Sufficiently high average molecular weight is needed to stabilize the molten web during water-bath quenching and hot-air stretching, while the shear-thinning response must be strong enough to reduce apparent viscosity in the die-lip region. The published melt flow rate of 0.50 g/10 min should not be read as a direct extrusion-output index because the material is non-Newtonian. Capillary rheometry is required to quantify viscosity at the wall shear rates encountered in narrow tape dies, which commonly exceed 10³ s⁻¹. This shear-thinning behavior is the reason melt flow rate alone underestimates processability on a slit-tape line.

    Low-MFI extrusion hardware and thermal limits

    On production-scale equipment, HDPE 5000S is typically processed on a single-screw extruder with a grooved feed bushing and barrier screw. Common extruder diameters range from 65 mm to 150 mm; an L/D ratio of 30:1 or 33:1 is frequently selected for low-MFI HDPE because the longer screw improves melting uniformity without generating excessive residence time. Barrel temperature settings are generally ramped from 180 °C in the feed zone to 220–230 °C at the adapter and die. The die head is often held near 210 °C to reduce polymer buildup at the lips. Measured melt temperature should not exceed 250 °C, because oxidative chain scission can begin to reduce elongational viscosity and produce inconsistent tape draw characteristics.

    A water-cooled quench bath follows the die. For HDPE slit-tape lines, die gaps are generally set between 1.6 mm and 2.2 mm, and the cast web is quenched in a water bath held at 30–45 °C. If the quench temperature drops below 25 °C, the skin layer may cool too rapidly, producing a highly crystalline surface that can crack during later stretching. If the bath exceeds 55 °C, slower cooling can allow spherulitic growth that reduces tape clarity and tensile strength. These boundaries are operational starting points and must be validated on the specific line.

    What separates HDPE 5000S from blow-molding and film-grade HDPE in the same density range?

    HDPE 5000S occupies a mid-MFI position among high-density polyethylene products. Blow-molding grades used for detergent or personal-care containers frequently have melt flow rates near 0.2–0.4 g/10 min and densities near 0.952–0.958 g/cm³. Those grades provide excellent environmental stress crack resistance under ASTM D1693, but they may generate excessive melt pressure in a narrow tape die. High-molecular-weight film grades with melt flow rates from 0.04 g/10 min to 0.15 g/10 min are selected for bubble stability in large blown-film towers, yet their melt strength is often higher than needed for tape casting and may increase motor load. Injection-molding HDPE with melt flow rates above 20 g/10 min is not a process substitute because its low melt strength permits draw resonance and uneven neck-down under monoaxial stretching.

    The following nominal values are reproduced from published grade literature for TPI Polene HDPE 5000S. They represent typical lot data and are not specification limits. Lot-specific certificates of analysis take precedence where a purchase specification applies.

    PropertyNominal valueTest method
    Melt flow rate, 190 °C/2.16 kg0.50 g/10 minASTM D1238
    Density, 23 °C0.955 g/cm³ASTM D1505
    Tensile strength at yield, 50 mm/min29 MPaASTM D638
    Elongation at break, 50 mm/min>800 %ASTM D638
    Flexural modulus, 1 % secant1,100 MPaASTM D790
    Vicat softening temperature, 10 N125 °CASTM D1525
    Brittleness temperature<−70 °CASTM D746
    Hardness, Shore D64ASTM D2240

    The tensile properties reported under ASTM D638 are typically generated on compression-molded specimens and therefore represent resin benchmarks rather than finished tape properties. In oriented slit tape, machine-direction strength increases substantially with draw ratio while transverse ductility decreases. The resin supplier’s molded-specimen value is useful for lot-to-lot consistency control, but it cannot replace tensile testing of the final woven fabric under ISO 13934-1 or an equivalent fabric tensile method.

    Environmental stress crack resistance is not always included in the published grade datasheet for HDPE 5000S. Converters handling surfactants, agrochemicals, or lubricating-oil packaging should request a lot-specific F50 value under ASTM D1693. The test is geometry-sensitive; notched constant-strain specimens can produce interlaboratory variation, so the minimum F50 requirement should be agreed between buyer and supplier before production. Published data for this specific property is limited when it is not declared on the certificate of analysis.

    When monoaxial orientation is pushed past 10:1, the failure mode becomes fibrillation

    Slit-tape lines using HDPE 5000S commonly operate at draw ratios between 6:1 and 10:1. In that window, the oriented tape develops sufficient molecular alignment to carry denier-specific tensile strength without excessive surface fibrillation. Above 10:1, the failure mode changes: surface fibrils begin to separate from the tape core under low strain, and the tape can split during weaving. This response is not unique to HDPE 5000S; it is a general behavior of low-MFI HDPE tape grades under excessive orientation. On a 90 mm grooved-feed extruder running a 1.8 mm die gap, splitting is often first observed at the tape edges because quench temperature and die-lip shear are highest in those positions. Reducing draw ratio or raising the water-bath temperature above 35 °C may suppress edge fibrillation, but only within the range where tape stiffness and tensile strength remain acceptable.

    Draw resonance and neck-in instability are additional limits. Because the melt flow rate is low, the molten web retains orientation; if draw ratio is changed too quickly during start-up, the web can oscillate in width and thickness, producing periodic denier variation. Closed-loop denier-control systems on modern tape lines use laser gauges to hold basis weight within ±5 % of target. A stable web with HDPE 5000S is typically reached after an equilibration period of 10–20 min once barrel temperatures stabilize. Die-lip thermocouple placement is critical because temperature gradients greater than 5 °C across the die width produce slit-tape denier variation that cannot be corrected by draw ratio alone.

    For outdoor woven sacks and flexible intermediate bulk containers, HDPE 5000S requires additional ultraviolet stabilization. The virgin resin is not inherently UV-resistant. A hindered amine light stabilizer system is typically compounded at 0.10–0.30 wt% or added as masterbatch. Accelerated weathering is commonly assessed under ASTM G154 Cycle 1 with UV-A 340 lamps; an agricultural sack specification may use a tensile strength retention threshold of 70 % after 1,000 h. Published data for the specific durability of HDPE 5000S under this protocol is limited, so verification should be performed on the finished woven article rather than extrapolated from typical resin datasheets.

    Moisture absorption is low, and pre-drying of virgin pellets is generally not required when the resin is stored below 40 °C in closed containers. If calcium carbonate masterbatch is added for cost reduction or matte surface, the masterbatch should be dried to less than 0.05 % moisture before letdown. Entrapped water can produce microvoids that become visible as tape brittleness after orientation. Regrind addition is possible, but the maximum letdown should be limited to 20 wt% unless extrusion speed and melt temperature are reduced, because repeated heat history lowers melt strength and increases the probability of web breaks on high-speed looms.

    For food-contact packaging, HDPE 5000S may be supplied with a food-contact declaration when requested. Under United States regulations, polyethylene homopolymer with density above 0.94 g/cm³ is referenced in FDA 21 CFR 177.1520, but the finished article must meet the extraction limits and end-use restrictions applicable to the specific food type and temperature condition. In the European Union, overall migration testing under EU Regulation (EU) No 10/2011 and its amendments is required for plastic materials intended for food contact. Converters must also verify compliance with REACH Article 33 notification duties for any substances of very high concern introduced by masterbatches or processing aids. For non-food industrial sacks, RoHS Directive 2011/65/EU is generally limited to electrical and electronic equipment applications and does not apply to polyethylene woven fabrics unless the fabric is integrated into covered equipment.

    ReferenceScopeConverter verification
    ASTM D1238Melt flow rate at 190 °C/2.16 kgLot acceptance and incoming QC
    ASTM D1505Density measurementResin density verification
    ASTM D638Tensile properties of molded specimensLot-to-lot consistency
    ASTM D1693Environmental stress crack resistanceSpecify minimum F50 for aggressive service
    FDA 21 CFR 177.1520Olefin polymer food-contact requirementsObtain grade-specific food-contact declaration
    EU Regulation (EU) No 10/2011Plastic food-contact material migration limitsOverall migration and specific migration tests
    ASTM G154Accelerated UV weathering practiceFinished-article weathering protocol

    Storage should minimize prolonged exposure to ultraviolet light and temperature excursions above 40 °C. Repeated exposure to sunlight can consume the phenolic antioxidant package before processing, shifting the melt flow rate upward and causing yellowing in the extruded web. Pellets should be kept in original packaging or closed silos. Purging with a lower-viscosity HDPE is recommended before shutdown to prevent plugging of narrow die lips. During start-up after shutdown, die-lip polymer deposits should be removed with brass tools only; steel tools can scratch the die surface and create streaks in the cast web.