Tpc Japan Hdpe Kz145n

TPC (Japan) HDPE KZ145N

    • Product Name: TPC (Japan) HDPE KZ145N
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 589026
    Manufacturer TPC (Japan)
    Product HDPE KZ145N
    Polymer Type High Density Polyethylene (HDPE)
    Density 0.956 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 0.05 g/10 min
    Tensile Strength At Yield 29 MPa
    Tensile Strength At Break 30 MPa
    Elongation At Break 600%
    Flexural Modulus 1.2 GPa
    Notched Izod Impact Strength 0.20 J/cm
    Shore D Hardness 66
    Vicat Softening Point 127°C
    Melting Point 135°C
    Brittleness Temperature -70°C
    Deflection Temperature At 0 46 Mpa 78°C
    Environmental Stress Crack Resistance >1000 h
    Mold Shrinkage 0.02 cm/cm
    Thermal Expansion Coefficient 1.2E-4 /°C
    Dielectric Constant 2.3
    Dissipation Factor 0.0002
    Volume Resistivity 1E17 ohm·cm
    Dielectric Strength 20 kV/mm

    As an accredited TPC (Japan) HDPE KZ145N factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing TPC (Japan) HDPE KZ145N is typically supplied in 25 kg net paper bags, palletized and stretch-wrapped for industrial handling.
    Container Loading (20′ FCL) 20′ FCL container loaded with TPC Japan HDPE KZ145N resin bags, palletized, shrink-wrapped, and securely stowed for ocean transport.
    Shipping TPC (Japan) HDPE KZ145N is shipped as a non-hazardous polyethylene resin, typically in 25 kg bags on pallets, stretch-wrapped and loaded into 20 ft or 40 ft containers by sea. Store in a cool, dry, ventilated area, away from moisture, direct sunlight, and contamination. No special dangerous goods handling required.
    Storage Store TPC (Japan) HDPE KZ145N in a cool, dry, well-ventilated warehouse, away from direct sunlight, rain, moisture, heat, and ignition sources. Keep original bags or containers tightly closed and palletized. Prevent contamination, dust, and physical damage. Avoid prolonged high temperatures and UV exposure. Use first-in, first-out stock rotation; stack safely to prevent deformation. Observe local regulations.
    Shelf Life TPC (Japan) HDPE KZ145N has a shelf life of approximately 24 months when stored in original packaging, cool, dry, and away from sunlight.
    Application of TPC (Japan) HDPE KZ145N

    In UN 3H1 tight-head jerrican production, KZ145N from TPC (Japan) is processed on a single-station shuttle blow moulding machine with a 90 mm/25 L/D grooved-feed extruder and a 4 L accumulator head. Melt temperature is held at 190–210°C, die temperature at 170–190°C, and mould shell temperature at 12–20°C. Pre-drying is not required unless condensation has formed; at RH above 70%, a hopper dryer at 60°C for 1–2 h prevents surface splay. Blow pressure is set at 0.6–0.8 MPa, with pre-blow delay 0.3–0.6 s and exhaust time 1.2–2.0 s. The parison programmer adds 15–20% wall thickness at the shoulder pinch-off and 10–15% at the bottom weld to maintain top-load strength after hot fill at 60°C. For Packing Group II qualification, 20 L and 25 L containers are drop-tested at 1.2 m onto a rigid steel plate at 18°C in accordance with UN 6.1.5.3, then subjected to internal hydraulic pressure at 100 kPa for 5 min under UN 6.1.5.5. Carbon black masterbatch is introduced at 2.0–2.5 wt%; UV exposure is assessed under ASTM G154-23 Cycle 1. End-use parts include 10 L, 20 L, and 25 L UN-rated jerricans for petroleum distillates, brake fluids, and coolant concentrates.

    What Coextrusion Limits Govern HDPE Skin Layers in Automotive Fuel Systems?

    Six-layer blow moulding of 45–80 L fuel tanks uses KZ145N in the outer and inner HDPE skins, typically at 40–50 wt% combined virgin HDPE split between the two skins, 35–45 wt% regrind, and the remaining thickness occupied by two maleic anhydride tie layers and one EVOH barrier layer. Melt temperature at the die inlet is held at 205–215°C; die temperature is 185–195°C on spiral mandrel heads with an annular diameter of 420–560 mm. Shear rate in the die gap is maintained below 250 s-1 to avoid flow-induced sharkskin on the inner skin. Blow air pressure of 0.7–1.0 MPa is applied after a 0.4–0.8 s pre-blow step, with mould temperature controlled at 10–20°C. Permeation is measured according to SAE J1737. Published data for KZ145N in this specific six-layer configuration is limited; end-use qualification must include vehicle-level evaporative emission testing. Carbon black is dosed at 2.0±0.2 wt%. End products include passenger car, SUV, and marine outboard fuel tanks requiring low permeation and high drop-impact resistance.

    1000 L IBC Liner Weld-Line Integrity and Stacking Load Transfer

    In 1000 L and 1250 L composite IBC bottles blow moulded from KZ145N, the critical process defects are bottom pinch-off weld thinning and sidewall melt striations that later enlarge into environmental stress cracks in the bottom radius. A single-head long-stroke accumulator machine with 120 mm/25 L/D extruder and 20 kg shot capacity is used. Melt temperature is set between 185°C and 200°C; barrel profile steps from 170°C at the hopper to 190°C at the metering zone. Mould temperature is held at 15–25°C, and cooling time for a 10 kg parison is 240–360 s. Blow air is introduced at 0.5–0.7 MPa following a 1.0–1.5 s pre-inflation delay to minimize melt draw. The integrally moulded discharge outlet is programmed with 20–30% additional wall thickness relative to the nominal sidewall. Qualification includes a hydraulic pressure test at 100 kPa for 10 min under ADR Chapter 6.5 and a stacking load of 2,400 kg over 28 days at 40°C per ISO 2234. End-use parts include 1000 L IBC liners for demineralized water, hydraulic oil, and non-hazardous detergent concentrates.

    Agricultural crop-protection pack closures and blow-moulded bottles made from KZ145N require resistance to aggressive adjuvants and hydrocarbon solvents in the 5–15% aromatics range. Compliance follows FAO/WHO Guidelines for the packaging and storage of pesticides, supplemented by UN drop and stack tests. Sidewall compounds are dry-blended with 2.0–3.0 wt% carbon black and 0.10–0.20 wt% hindered amine light stabilizer before feeding. A two-layer coextrusion blow moulding line with 70 mm/24 L/D primary extruder and 35 mm/24 L/D second-layer extruder produces 1 L and 5 L bottles with a black outer surface and a natural inner surface to reduce additive migration into the liquid. Melt temperature is 190–205°C, mould temperature 10–25°C, and blow pressure 0.6–0.8 MPa. The bottles are evaluated under ASTM D1693-25 Condition B at 50°C in 10% Igepal CO-630; lot acceptance is generally linked to zero failure after 200 h, though published data for KZ145N in this specific formulation is limited and must be confirmed against the supplier certificate. Drop impact at 0°C is measured per ASTM D2463-15. End-use: 1 L, 5 L, and 10 L containers for glyphosate, paraquat, and synthetic pyrethroid formulations in export markets.

    When Wave Impact Stress Crack Propagation Dictates Buoy Shell Design

    After long-term saltwater immersion, cyclic flexural stress at the mooring eye insert of marine marker buoys blow moulded from KZ145N drives low-stress environmental stress cracking. The parison is blown in a 20–60 L single-cavity mould using an 80 mm/24 L/D extruder with melt temperature 190–205°C and die temperature 175–185°C. Mould cooling is set to 10–20°C; cycle time is 90–150 s for 5–8 kg parts. A 2.0–2.5 wt% carbon black masterbatch is included, and the outer surface is texturized to 0.8–1.2 mm depth to mask impact scuffing. Mooring eye inserts are ultrasonically welded after moulding. Salt fog exposure under ASTM B117-19 for 1,000 h and tensile impact retention per ASTM D1822-13 are used to qualify lot stability. Drop testing from 3 m onto concrete at -20°C per ASTM D2463-15 identifies low-temperature brittle fracture at the bottom weld. End-use parts include navigation buoys, fishing net floats, and fender buoys in nearshore service.

    Free Quote

    Competitive TPC (Japan) HDPE KZ145N prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    TPC (Japan) HDPE KZ145N is a high-molecular-weight high-density polyethylene film resin supplied for thin-gauge blown film packaging. Producer technical bulletins list a nominal density of 0.945 g/cm³ when determined under ISO 1183-1, and a melt mass-flow rate of 0.14 g/10 min at 190 °C and 2.16 kg under ISO 1133-1. Film tensile data cited in producer literature include a tensile stress at yield of 23 MPa and an elongation at break of 800 % under ISO 527-3. Dart drop impact at 25 μm film thickness is reported as 180 g under ISO 7765-1/A. These values are nominal and subject to lot-to-lot variation within producer release limits.

    The grade is specified in grocery sacks, side-gusseted bags, freezer liners, refuse sacks, and heavy-duty liners where puncture resistance, tear balance, and seal integrity are the primary design requirements. It is not supplied for injection molding, pipe extrusion, or blow molding; its melt-flow and molecular-weight design are specific to blown film.

    Representative producer-published properties for KZ145N
    PropertyTest methodUnitValue
    Density at 23 °CISO 1183-1g/cm³0.945
    Melt mass-flow rateISO 1133-1g/10 min0.14
    Tensile stress at yieldISO 527-3MPa23
    Elongation at breakISO 527-3%800
    Dart drop impact, 25 μm filmISO 7765-1/Ag180
    Vicat softening temperatureISO 306/A50°C124

    In blown film conversion, the grade is processed on grooved-feed extruders equipped with barrier screws and L/D ratios of 30:1 or higher. Typical melt-temperature setpoints are 190 °C to 220 °C, with die temperatures of 200 °C to 210 °C. The die gap is normally set between 1.2 mm and 1.8 mm. The resin is used in high-stalk bubble configurations with blow-up ratios of 2.5:1 to 4.0:1; this window permits a balance between machine-direction tear and transverse-direction impact. At blow-up ratios below 2.0:1, machine-direction orientation increases and tear anisotropy becomes more pronounced. At blow-up ratios above 5.0:1 with small dies, bubble oscillation and gauge variation are frequently observed. Frost-line height is typically set between 2 and 5 die diameters, depending on ambient air temperature and cooling-ring capacity.

    What Processing Constraints Govern Thin-Gauge Film Extrusion of KZ145N?

    Because the melt mass-flow rate is 0.14 g/10 min, the material has higher melt viscosity than a 0.30 g/10 min general-purpose HDPE film resin. This increases screw torque, die pressure, and melt-temperature generation by viscous dissipation. The extruder should maintain melt temperature below 250 °C; above this threshold, thermo-oxidative chain scission creates gel particles and yellowing. Long residence time at 220 °C in stagnant die-lip zones can also produce carbonaceous deposits. Purging with LDPE or a commercial purging compound before shutdown is used to control die buildup. Output rate is limited more by bubble stability and heat removal than by extruder capacity. In thin-gauge films below 15 μm, melt strength must be retained by keeping the die exit temperature at the upper end of the window and by avoiding excessive drawdown from a large die gap. Because KZ145N has a high molecular weight, melt fracture can appear as a rough film surface if the die gap is too narrow or the die land is too short. A die land ratio between 10:1 and 15:1 and die entry angles of 45–60 degrees are typical for high-molecular-weight film dies. The resin is generally not predried for routine film conversion, but surface condensation from storage at relative humidity above 60 % should be removed with a hopper dryer at 60–80 °C for 2–4 h to prevent surface streaking and bubble instability.

    Heat seal response in KZ145N bags is influenced by film orientation, thickness, and additive package rather than pellet lot alone. For lower-density HDPE blown films, heat seal initiation temperatures typically fall in the 120 °C to 135 °C range at sealing pressures of 0.5 N/mm² to 1.5 N/mm² and dwell times of 0.5 s to 1.5 s. Hot-tack data specific to KZ145N are limited in published sources; converter trials on impulse and constant-heat sealers are required for high-speed bag conversion. Without slip and antiblock additives, the film coefficient of friction can exceed 0.4 under ISO 8295, making web transport difficult. Erucamide-type slip agents migrate to the film surface over 24–72 h after conversion; the final coefficient of friction depends on masterbatch dilution and corona treatment level. Excessive corona above 45 mN/m may oxidize the surface and reduce seal strength. At film thicknesses below 10 μm, seal strength is dominated by seal-bar temperature control and film-gauge uniformity.

    Comparative Film-Resin Property Balance

    The position of KZ145N relative to other polyolefin film resins is defined by its density, melt-flow rate, and molecular weight distribution. A comparison of mainstream resin classes is shown in Table 2. The density of 0.945 g/cm³ is lower than that of a stiff 0.952–0.955 g/cm³ HDPE, which reduces flexural modulus and improves stress-crack resistance in bent or folded packages. The melt-flow rate of 0.14 g/10 min keeps melt strength high enough for large-bubble stability but is higher than that of very high-molecular-weight HDPE grades used for ultra-thin can liners. Compared with a 0.30 g/10 min film resin, KZ145N produces higher dart impact and better bubble-carrying capacity but may require 10–15 % lower gravimetric output on a given extruder due to higher die pressure. Compared with an MDPE of 0.934 g/cm³, KZ145N offers higher modulus and better heat resistance but lower clarity and higher seal initiation temperature.

    Typical resin-class comparison for film extrusion
    Resin classDensityMelt mass-flow rateFilm property emphasis
    KZ145N0.945 g/cm³0.14 g/10 minBalanced dart, tear, and environmental stress-crack resistance
    General-purpose HDPE film0.950–0.954 g/cm³0.25–0.60 g/10 minHigher stiffness, easier drawdown
    Very high-molecular-weight HDPE film0.949–0.955 g/cm³0.04–0.10 g/10 minMaximum dart impact, high back-pressure
    MDPE film0.934–0.940 g/cm³0.50–1.00 g/10 minLower seal initiation, higher clarity

    In multi-layer coextruded film, KZ145N is used in core or outer layers to provide toughness while LDPE or LLDPE skin layers supply seal performance. The melt-temperature differentials between adjacent layers should not exceed 10 °C to avoid interfacial instabilities. If a polyamide barrier layer is included, a tie-layer based on maleic anhydride-grafted polyolefin is required. Edge trim and start-up scrap from KZ145N can be re-pelletized and dry-blended at up to 15 wt% without significant loss of film impact, provided the reclaim is not thermally degraded. Higher reclaim levels increase gel count and may lower bubble stability.

    When KZ145N Replaces a 0.952 g/cm³ HDPE in Bag Conversion

    Replacement of a 0.952 g/cm³ HDPE with KZ145N on an existing blown film line requires adjustment of melt temperature, die gap, and blow-up ratio. Because KZ145N has a lower melt-flow rate, melt pressure rises, and the screw speed required for a set gravimetric output may be 8–15 % higher. The die gap is usually opened by 0.2 mm to 0.4 mm to reduce die pressure and improve bubble stability. Blow-up ratio may need to be increased from 2.2:1 to 3.0:1–3.5:1 to restore transverse-direction impact balance after film gauge is reduced. The frost-line height is lowered to maintain a more symmetrical bubble and to prevent excessively rapid quenching that can reduce dart impact. Puncture resistance and seal strength are typically evaluated against the incumbent film using ISO 7765-1, ISO 6383-1, and a calibrated heat-seal peel test under ASTM F88. When barrier performance is critical, the lower density of KZ145N should be accounted for; water vapour transmission rate rises relative to a 0.952 g/cm³ film, with published permeability coefficients indicating a 10–20 % increase per 0.008 g/cm³ density reduction.

    Regulatory positioning for KZ145N follows the producer's product stewardship documentation. For food-contact use in the United States, the resin is covered by olefin polymer provisions of 21 CFR 177.1520, subject to end-use condition of use. For European Union food-contact applications, compliance with Regulation (EU) No 10/2011 and its amendments is demonstrated by migration testing in the intended food simulant; overall migration limits depend on film thickness and food category. The unfilled polyolefin grade is typically supplied without heavy-metal stabilizers; the producer can provide REACH SVHC and RoHS statements when required. Operational boundaries include avoidance of melt temperatures above 250 °C, storage away from aromatic or halogenated solvents, and protection from ultraviolet light unless a UV-stabilized version is specified. Polyethylene exposed to extended outdoor service without 2–3 wt% carbon black or hindered-amine stabilizer undergoes chain scission, gloss loss, and embrittlement. The grade should not be blended with polar adhesive polymers or strongly acidic flow agents without converter trial, because dispersed polar phases can reduce film tear strength and seal integrity.

    Top