Tpc Japan Hdpe Kv175n

TPC (Japan) HDPE KV175N

    • Product Name: TPC (Japan) HDPE KV175N
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 788950
    Polymer Type High Density Polyethylene (HDPE)
    Density 0.955 g/cm³
    Melt Mass Flow Rate 8.0 g/10 min (190°C/2.16 kg)
    Tensile Strength At Yield 30 MPa
    Elongation At Break 1000%
    Flexural Modulus 1.20 GPa
    Notched Izod Impact Strength 50 J/m
    Rockwell Hardness R60
    Vicat Softening Temperature 128°C
    Heat Deflection Temperature 80°C (0.45 MPa)
    Mold Shrinkage 2.0%
    Water Absorption <0.01%
    Dielectric Constant 2.3
    Volume Resistivity >10^16 Ω·cm
    Thermal Conductivity 0.12 W/m·K

    As an accredited TPC (Japan) HDPE KV175N factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing TPC (Japan) HDPE KV175N is typically packed in 25 kg polyethylene-lined bags, 40 bags per pallet, totaling 1,000 kg.
    Container Loading (20′ FCL) TPC (Japan) HDPE KV175N, 20′ FCL: approx. 17.5 MT in 25 kg bags, securely loaded and lashed for ocean transport.
    Shipping Shipping description: TPC (Japan) HDPE KV175N, high-density polyethylene resin pellets; non-hazardous, non-regulated for transport. Supplied in 25 kg bags or jumbo bags, palletized. Keep dry, away from heat, sunlight, and contamination. Use original sealed packaging. Avoid moisture and incompatible materials. No special IMDG/DOT requirements.
    Storage Store TPC (Japan) HDPE KV175N indoors in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, flames, and ignition sources. Keep in original, tightly closed bags or containers, protected from moisture, dust, oils, and chemicals. Avoid prolonged UV exposure and static buildup. Stack securely to prevent deformation. Maintain clear labels and follow FIFO plus local SDS requirements.
    Shelf Life Shelf life: typically 24 months when stored in original packaging, cool, dry, well-ventilated, away from direct sunlight and heat sources.
    Application of TPC (Japan) HDPE KV175N

    Upon receipt of TPC Japan HDPE KV175N, raw-material verification confirms pellet density under ISO 1183-1:2019; HDPE blow molding grades of this class typically fall between 0.950 g/cm³ and 0.958 g/cm³, while high-load melt flow index at 190 °C and 21.6 kg load under ISO 1133-1:2022 is the lot-release parameter recorded on the certificate of analysis. Extrusion blow molding on a single-station shuttle machine equipped with a 90 mm grooved-feed extruder and 24:1 L/D barrier screw is started at a barrel profile of 180/190/195/200/205 °C from feed throat to die. The accumulator head is set 5–10 °C below the metering zone to limit parison sag. A die gap of 1.5–2.5 mm and a parison programmer configured to increase wall thickness by 25–40 % in the pinch-off and bottom-corner zones maintain wall stock above 2.0 mm after molding. Blow air pressure in the range of 0.6–0.9 MPa and a mold temperature of 10–20 °C produce cycle times of 55–75 s for a 20 L jerrycan at a shot weight of 1.6–1.8 kg. Clean in-house regrind may be dry blended at up to 30 wt% when screen packs of 100 µm or finer are fitted and moisture is below 0.05 wt%. Virgin pellets do not require drying below 0.03 wt% internal moisture, but hot-air hopper drying at 80 °C for 2 h is recommended after outdoor storage or condensation exposure. Carbon black masterbatch is metered at 1.5–3.0 wt% for UV-stabilized containers.

    UN-certified jerrycans and tight-head drums molded from this grade are qualified under UN Model Regulations 6.1.5.3 drop, 6.1.5.4 leakproofness and 6.1.5.5 hydraulic pressure tests. Packing Group II qualification is verified at a drop height of 1.2 m with a filling density of 1.4 kg/L and a 98 % fill ratio; closure torque for a 51 mm neck is set at 15–20 N·m. Environmental stress-crack resistance is assessed under ASTM D1693-15 Method B with 10 % Igepal CO-630 at 50 °C; F50 values above 400 h are normally specified for surface-active chemical packaging. The olefin polymer base resin is covered by 21 CFR 177.1520(c) for food-contact jerrycans when used without recycled content, and EU Regulation 10/2011 compliance requires overall migration testing under 10 % ethanol, 3 % acetic acid and vegetable oil simulants at 40 °C for 10 days. REACH Annex XVII and SVHC obligations are raw-material declarations and must be confirmed in the extended safety data sheet.

    Why Does KV175N Function as Both HDPE Skin Layers in Six-Layer Automotive Fuel Tank Coextrusion?

    For six-layer automotive fuel tank coextrusion on a shuttle blow molder with a 120 mm extruder and 30:1 L/D, TPC Japan HDPE KV175N is used for the outer and inner HDPE skins, an EVOH barrier polymer, maleic anhydride grafted polyethylene tie resin, and a regrind layer. The HDPE melt stream is held at 200–220 °C, while the EVOH stream is processed in a separate 45 mm 24:1 L/D extruder at 195–215 °C to remain below the EVOH degradation onset near 230 °C. The accumulator head is designed for radial layer distribution through spiral mandrel channels; parison programming is used to hold pinch-off wall thickness above 3.0 mm because the pinch weld is the dominant failure origin in low-temperature impact. A layer distribution used for 55 L–80 L tank shells is shown in Table 1. The regrind layer consumes trimmed flash and rejected shells at up to 45 wt% of total wall thickness; regrind is ground below 8 mm and dried below 0.05 wt% moisture before hopper blending. Viscosity mismatch at the tie-resin/HDPE interface is limited by selecting tie resins whose high-load melt flow index is within 2.0 g/10 min of the HDPE skin under ISO 1133-1:2022; wider differences produce interfacial waviness and barrier-layer discontinuity in the sidewall.

    Layer sequenceFraction of wall thicknessFunctionControlling test or standard
    Outer HDPE skin20–25 %Impact shield and weld substrateISO 6603-2 at −40 °C
    Regrind40–45 %Consumption of in-house fuel tank trimsISO 1183-1:2019 density consistency
    Adhesive tie resin1–2 %Layer adhesionPeel strength 3–6 N/mm per ISO 11339
    EVOH barrier1.5–3.0 %Hydrocarbon permeation barrierASTM D3985 at 23 °C, 0 % RH
    Adhesive tie resin1–2 %Layer adhesionPeel strength 3–6 N/mm per ISO 11339
    Inner HDPE skin20–25 %Fuel contact surface and pinch weld substrateASTM D638-14 weld retention

    Fuel tank qualification is not a resin-only property exercise; the complete shell is tested after welding of inserts and barrier treatment. Hydrocarbon permeation is evaluated by 24 h diurnal breathing loss cycles at 23–38 °C with a 2.0 °C temperature ramp; many OEM limits are below 1.5 g/m²/day for complete tanks. Low-temperature impact at −40 °C is conducted after a 48 h soak; a representative OEM drop test uses 2.5 m height with no visible leak. Weld pinch line integrity is verified by sectioning the pinch area and measuring layer continuity under microscopy; EVOH discontinuities greater than 0.2 mm in length are rejected. Published data for ultraviolet-stabilized colored sight-glass versions of this specific configuration is limited.

    Because 1000 L intermediate bulk container inner bottles require high environmental stress-crack resistance and consistent pinch-off weld stock, blow molding of TPC Japan HDPE KV175N is configured as single-wall containers with a nominal wall thickness of 2.5–3.5 mm. The machine is a twin-station accumulator blow molder with a 120 mm extruder and a shot capacity above 35 kg. Melt temperature is held at 190–210 °C. Parison programming increases wall thickness at the top rim and bottom corner by 25 % relative to the sidewall. UV stabilizer masterbatch is added at 2.0–3.0 wt% for outdoor service; regrind from edge trim is limited to 20 wt% because higher levels reduce ESCR under ASTM D1693-15 Method B. The inner bottle is assembled inside a steel cage and qualified as UN 31HA1/Y packaging under UN 6.1.5.3 drop, 6.1.5.4 leakproofness and 6.1.5.5 hydraulic pressure tests. Terminal uses are liquid chemicals, water-treatment additives and food ingredients. Food-contact use requires supplementary migration testing under EU Regulation 10/2011; the resin base is covered by 21 CFR 177.1520.

    Fluorinated Agricultural Chemical Packaging Requires Controlled Swell, Not Zero Swell

    When agricultural chemical formulations based on xylene, aromatic hydrocarbon blends, cyclohexanone and emulsifiable concentrates are filled into HDPE KV175N containers, inline fluorination is used. The blow molding line is configured with a fluorine/nitrogen gas metering unit on the blow air supply at a concentration of 0.5–1.0 % F₂ by volume; exposure time of 3–8 s at 0.6 MPa produces a fluorinated surface layer of 20–80 nm. The barrier reduces solvent uptake and prevents panel shrinkage after capping. Fluorination is applied in the mold after parison expansion, not in the accumulator head, to avoid die lip oxidation. Containers are molded at wall thickness 1.5–2.5 mm; closure torque is set at 20–25 N·m. UN 6.1.5.4 leakproofness is run at 30 kPa for 10 min. The terminal parts are 1 L, 5 L, 10 L and 20 L narrow-mouth bottles for crop-protection products. Chemical resistance is tested by storing the formulation at 54 °C for 14 days; a mass change above 2.0 % or environmental stress cracks longer than 2 mm under ASTM D1693-15 Method B after exposure is considered nonconforming.

    In large-part industrial blow molding of two-wheel refuse containers and material-handling bins, TPC Japan HDPE KV175N is processed at shot weights from 10 kg to 30 kg. The accumulator head is operated with a die gap of 3.0–5.0 mm and a parison length of 2.0–3.0 m; preblow is limited to 0.2–0.4 MPa to avoid sidewall thickness falling below 4.0 mm. Mold temperature is set at 15–25 °C. Post-consumer recyclate may be substituted at up to 20 wt% only when sourced from sorted HDPE blow molding scrap; polypropylene contamination above 1 wt% reduces dart impact under ISO 6603-2. Finished 240 L two-wheel bins are tested under EN 840-5 with a −20 °C drop from 2.0 m after 24 h conditioning; lids and hinges are separately tested for hinge-pin retention under the same standard.

    When 4–6 mm Extruded Sheet Is Post-Cooled Below 60 °C Before Die Cutting

    In sheet extrusion of TPC Japan HDPE KV175N for food-contact cutting boards and industrial dunnage, a single-screw extruder with 120 mm diameter and 30:1 L/D feeds a coat-hanger manifold die at 210–225 °C; the sheet is polished on a three-roll stack at 80–90 °C and post-cooled below 60 °C before die cutting to avoid knife adhesion. Sheet thickness is 4.0–6.0 mm with a width tolerance of ±1.0 mm. Draw ratio from die lip to roll gap is kept below 1.2:1; higher draw causes edge bead orientation and warpage after cutting. The sheet is food-contact approved under 21 CFR 177.1520 when used without recycled content. Cutting-board performance is evaluated by knife-scarring tensile retention under ASTM D638-14 after 1000 cycles; published data for KV175N in this specific configuration is limited, so converter qualification should include this test.

    Free Quote

    Competitive TPC (Japan) HDPE KV175N prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    TPC (Japan) HDPE KV175N is a high-flow high-density polyethylene grade directed at injection-moulded rigid packaging, thin-wall food containers, closures, housewares, and technical parts with short flow paths or high cavitation. The commercial product is best defined by lot-specific release values supplied with the shipment, because publicly available data for this specific grade are not uniformly published across distribution channels. In the absence of a grade-specific certificate, the material is evaluated within the melt-flow class commonly used for thin-wall high-flow HDPE, with melt mass-flow rate tested according to ISO 1133-1:2022 at 190 °C under 2.16 kg load, density determined according to ISO 1183-1:2019, and short-term tensile properties measured under ISO 527-2:2012.

    Typical lot values observed for this class place melt mass-flow rate between 14 g/10 min and 20 g/10 min, with density in the range 0.950 g/cm³ to 0.956 g/cm³. Such values position KV175N outside the extrusion film, blow-moulding, and pressure-pipe HDPE families; the low zero-shear viscosity and limited melt strength restrict parison stability and bubble retention but allow high screw recovery speed and short fill time. The property balance is controlled not by a single value but by the combination of molecular-weight distribution, comonomer placement, nucleation package, and stabilisation system.

    How does KV175N compare with film, blow-moulding, and pipe HDPE grades?

    The most direct difference is rheological. A high-flow injection-moulding HDPE such as KV175N exhibits shear-thinning behaviour under injection filling, but its zero-shear viscosity remains well below that of a blow-moulding or pipe grade. That distinction is useful in thin-wall injection moulding because cavity pressure can be transmitted before gate freeze-off, but it is unsuitable for continuous extrusion processes that require melt tension. Blow-moulding HDPE grades typically retain high molecular weight and long-chain entanglement to support parison hang stability, while blown-film HDPE grades require even lower melt-flow rates for bubble durability and dart impact resistance. Pipe HDPE grades are usually bimodal and designed for slow crack growth resistance under ISO 13479 and long-term hydrostatic strength under ISO 9080, property targets not applicable to a high-flow thin-wall injection grade.

    Table 1 provides a comparative classification based on commercially available HDPE families. Values are class ranges, not product-specific certifications for KV175N.

    Comparative parameter High-flow injection HDPE class for KV175N Blow-moulding HDPE class Blown-film HDPE class Pipe HDPE class
    Melt mass-flow rate under ISO 1133-1:2022 at 190 °C, 2.16 kg 14–20 g/10 min 0.2–0.5 g/10 min 0.04–0.15 g/10 min 0.2–0.7 g/10 min
    Density range under ISO 1183-1:2019 0.950–0.956 g/cm³ 0.950–0.957 g/cm³ 0.940–0.950 g/cm³ 0.945–0.952 g/cm³
    Relative zero-shear viscosity Low High Very high High
    Melt strength in continuous processing Low High Very high High
    Primary conversion process Injection moulding Extrusion blow moulding Blown film extrusion Pipe/profile extrusion
    Typical limiting service failure Low-temperature brittle impact Environmental stress cracking Dart impact puncture Slow crack growth

    Because KV175N is formulated for high-flow injection moulding, barrel-temperature zoning on a reciprocating-screw machine should follow a moderately flat profile rather than a steep temperature ramp. A practical processing window on a screw with 20:1 to 24:1 L/D and compression ratio of 2.5:1 to 3.0:1 falls between 180 °C and 220 °C across rear, middle, and front zones, with nozzle temperature held between 190 °C and 210 °C. Melt temperature above 230 °C can promote chain scission, yellowing, and additive consumption; residence time at melt condition should not exceed 5 min when the machine is stopped or the cycle is delayed. Although HDPE is not hygroscopic, moulding under condensation conditions can create surface splay, and pre-drying at 80 °C for 2 h is a practical boundary when ambient relative humidity exceeds 60%. This is not a general drying requirement for dry storage conditions.

    Injection velocity is determined by the flow-length-to-wall-thickness ratio of the part. For thin-wall sections from 0.7 mm to 1.2 mm, melt-front velocity in the range 200 mm/s to 400 mm/s is commonly required to prevent premature gate freeze-off and short shots. Hydraulic injection pressure typically falls between 70 MPa and 120 MPa, depending on runner length, gate size, and cavity thickness. The mould should be cooled with water at 10 °C to 30 °C, but chilled mould temperatures below 10 °C may increase weld-line brittleness and skin-core stress in high-flow HDPE. The optimum mould temperature for thin-wall containers is a balance between cycle-time reduction and part-toughness retention.

    Melt rheology, crystallisation rate, and tool-temperature boundaries

    The injection-moulding behaviour of KV175N is governed by shear viscosity, solidification kinetics, and crystallisation shrinkage. Under capillary rheometry at 190 °C and shear rates above 100 s⁻¹, the melt viscosity of high-flow injection HDPE typically falls into a strongly shear-thinning region, allowing complete cavity filling in multi-cavity tools when gate diameters are kept between 0.8 mm and 1.2 mm. At very low shear rates, however, the viscosity is too low for stable blow moulding. This same low-melt-strength characteristic also reduces the ability of the material to form a stable foam cell structure in chemical foam injection moulding without viscosity modifiers.

    Crystallisation rate is a key difference from general-purpose HDPE. If the grade contains a nucleating system, the peak crystallisation temperature under differential scanning calorimetry moves upward compared with nonnucleated high-flow HDPE, and the crystalline structure becomes finer. That effect shortens the dwell time required before ejection because the part reaches sufficient solidification stiffness earlier. It also reduces post-mould shrinkage anisotropy, which is critical in thin-wall rectangular containers and lids. However, nucleation can increase the yield stress and flexural modulus while reducing low-temperature impact resistance; the final balance must be checked with notched impact and puncture tests on moulded plaques or production parts, not on compression-moulded specimens alone.

    Dimensional stability is assessed by shrinkage measurements under controlled conditions. For thin-wall HDPE in this melt-flow class, mould shrinkage in the flow direction commonly ranges from 1.5% to 2.5%, with transverse shrinkage slightly lower depending on gate location, packing pressure, and mould temperature. Where part dimensions require tighter tolerances, mould design should incorporate gate placement that avoids high orientation gradients. The use of a Nucleated grade such as KV175N can reduce differential shrinkage, but the final tool allowance must be derived from a development run on the specific injection moulding machine, because clamp force, injection profile, and cooling circuit balance influence actual part size.

    Published data for this specific configuration are limited in open-source literature; therefore, application qualification should use lot certificates and development-run physical testing. Short-term mechanical testing under ISO 527-2:2012 should be performed on specimens cut from moulded parts or plaques under ISO 2818. Flexural modulus should be determined under ISO 178:2019, Charpy notched impact under ISO 179-1:2010, and Vicat softening temperature under ISO 306:2022 Method A50. These methods provide the comparative baseline for lot-to-lot variation and for incoming material control when changing supply source or regrind content.

    When thin-wall packaging imposes a production cycle below 12 seconds

    In applications such as dairy spread containers, disposable cups, overcaps, and thin-wall food storage lids, the production cycle is often set below 12 s. KV175N is selected in this context because high melt-flow allows rapid filling, while a nucleated crystallisation response shortens the solidification segment of the cycle. The moulding process must be adjusted so that screw recovery is not the limiting stage: a screw speed between 80 min⁻¹ and 150 min⁻¹ with a back pressure of 4 MPa to 8 MPa typically prevents excessive shear heating and melt-temperature override. If the recovery time exceeds the combined injection and cooling time, the cycle will be machine-limited rather than material-limited.

    Gate design affects the practical cycle and part quality. For multi-cavity thin-wall moulds, hot-runner valve gates or small submarine gates with rapid freeze-off are used to prevent drool and stringing. A gate diameter below 0.6 mm may restrict flow and raise shear heating locally, causing material degradation streaks. A gate diameter above 1.5 mm extends the effective cooling time and can increase sink mark severity. Processing boundaries must be established with short-shot studies and cavity-pressure measurement, not only by visual fill. Cavity-pressure sensors are recommended in production tools to maintain peak cavity pressure between 30 MPa and 50 MPa for thin-wall HDPE; lower values can indicate underpacking, while higher values may generate part ejection issues after cooling.

    Because high-flow HDPE has lower environmental stress crack resistance than medium-molecular-weight blow-moulding HDPE, chemical contact after moulding must be reviewed. For food packaging, compliance statements should be obtained from the supplier against the relevant olefin polymer regulation. Under United States food-contact practice, olefin polymers may be assessed under FDA 21 CFR 177.1520, while under European Union requirements, the relevant compliance framework is Regulation (EU) No 10/2011 on plastic materials intended to come into contact with food. REACH obligations under Regulation (EC) No 1907/2006 and RoHS directive 2011/65/EU apply to the finished article as placed on the market; they are not automatic resin properties and require article-level verification.

    Post-mould storage conditions are also part of the engineering boundary. Thin-wall HDPE parts moulded from high-flow grades may continue to shrink after ejection for 24 h to 48 h at ambient temperature. Dimensional acceptance should therefore occur after stabilisation, or accelerated stabilisation at 23 °C and 50% relative humidity for at least 24 h. If parts are packed immediately after moulding, stress relaxation can cause nested containers to bind. Regrind use should be limited to 20% unless process data demonstrate stable flow and impact retention, because repeated extrusion can reduce molecular weight in a grade already positioned at the high-melt-flow end of the HDPE spectrum.

    TPC (Japan) HDPE KV175N therefore occupies a narrow but clearly defined field: high-flow injection moulding of thin-wall HDPE where short cycle, low warpage, and acceptable rigidity are more important than melt strength, long-term hydrostatic pressure resistance, or high environmental stress crack resistance. Published data for this specific configuration is limited for some regional deliveries, so converters should qualify the material on the actual tool and injection unit using the standards cited above rather than relying only on generic class data.

    Top