Tpc Japan Hdpe Kv165n

TPC (Japan) HDPE KV165N

    • Product Name: TPC (Japan) HDPE KV165N
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 341113
    Melt Flow Rate 190 C 2 16 Kg 0.05 g/10 min
    Density 0.955 g/cm3
    Tensile Strength At Yield 29 MPa
    Tensile Strength At Break 30 MPa
    Elongation At Break 700%
    Flexural Modulus 1300 MPa
    Vicat Softening Temperature 126 °C
    Brittleness Temperature -70 °C
    Environmental Stress Crack Resistance Escr >1000 h
    Hardness Shore D 66
    Melting Temperature 133 °C
    Coefficient Of Linear Thermal Expansion 1.5e-4 /°C

    As an accredited TPC (Japan) HDPE KV165N factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing TPC (Japan) HDPE KV165N supplied in 25 kg paper bags, 40 bags per pallet, totaling 1,000 kg net.
    Container Loading (20′ FCL) 20′ FCL container loading for TPC (Japan) HDPE KV165N: palletized 25 kg bags, shrink-wrapped, securely stuffed for export.
    Shipping TPC (Japan) HDPE KV165N is a high-density polyethylene resin, solid pellets, non-hazardous. Not regulated for transport (UN classification: none). Packed in 25 kg PE bags or 1,000 kg jumbo bags, palletized and stretch-wrapped. Ship in covered trucks/containers; store dry, away from heat, sunlight, and moisture. Handle with standard forklift.
    Storage Store TPC (Japan) HDPE KV165N in original, sealed bags or octabins in a cool, dry, well-ventilated warehouse. Protect from direct sunlight, UV, moisture, heat, and contamination. Keep away from ignition sources, strong oxidizers, and odorous materials. Stack pallets securely without crushing or puncturing packaging. Use first-in, first-out rotation, and avoid prolonged outdoor exposure or excessive stacking pressure.
    Shelf Life Stable under normal storage; no defined shelf life if kept cool, dry, and protected from UV, heat, and contamination.
    Application of TPC (Japan) HDPE KV165N

    On high-cavitation thin-wall injection moulding lines converting HDPE KV165N into disposable food-contact packaging, the starting let-down ratio is typically 96–98 wt% resin, 2–4 wt% white or custom masterbatch, and, where part release or surface slip is required, 0.5–1.0 wt% slip/antiblock masterbatch. For fatty and aqueous food simulants, compliance is predicated on FDA 21 CFR 177.1520 for olefin polymers and EU Regulation (EU) No 10/2011 Annex I, with specific migration testing under EN 1186-1 and GB 4806.7-2016 where destination markets require China GB assessment. The masterbatch carrier resin is not a neutral diluent in migration calculations, so the same food-contact designation must be documented for the entire let-down package. The production process is a high-speed, accumulator-assisted injection moulding operation. Melt temperatures are maintained at 190–230°C, and mould temperatures are held between 8°C and 30°C to freeze the high-flow melt into wall stocks of 0.4–1.2 mm. On a 350–500 t hydraulic machine with a 22:1 L/D general-purpose screw, fill times of 0.15–0.60 s and injection pressures of 80–140 MPa are common; hold pressure is set at 40–70 MPa with a switchover position adjusted for shot-to-shot melt viscosity variation of ±0.5 mm. Hot-runner valve-gate systems are preferred over cold sprue bushings because the increased gate vestige height in cold-runner systems creates a stress concentration at the base of dairy tubs and can reduce sidewall top-load resistance. The flow-length-to-wall-thickness ratio exceeds 180:1 in many designs, so gate placement, coolant line spacing of 25–40 mm and a minimum 3–5°C cooling-water temperature differential across the circuit are necessary to prevent warpage and sink marks. Pre-drying is generally not required when the resin is stored in sealed original packaging; if surface moisture exceeds 0.05 wt%, the material should be dried at 70–80°C for 2 h because trapped moisture in thin-wall sections produces surface streaks and voids. Terminal articles produced in this configuration include dairy spread tubs, opaque single-serve snack cups, frozen dessert containers and thin-wall lids. The key operational boundary is melt temperature: raising melt temperature above 230°C may improve fill in sub-millimetre sections but increases mould shrinkage towards 1.5–2.5% and can shift organoleptic risk if the masterbatch is not designed for high-temperature shearing. Converters should cap barrel residence time below 8 min and avoid melt stagnation in hot-runner dead spots.

    What Controls Torque Retention and Environmental Stress Crack Resistance in Injection-Moulded HDPE Closure Systems?

    The closure converter running HDPE KV165N on a 48- to 96-cavity hot-runner tool typically starts from a let-down ratio of 96–99 wt% resin, 1–4 wt% color masterbatch, and 0.05–0.2 wt% slip/antiblock additive; when the closure is intended for edible-oil or aggressive detergent environments, an additional 5–15 wt% LLDPE or metallocene polyethylene let-down is introduced to raise environmental stress crack resistance, but this also reduces top-load stiffness and should be qualified against the closure torque-retention specification. Compliance for food-contact closures is anchored to FDA 21 CFR 177.1520 and EU (EU) No 10/2011, while child-resistant closures are tested under ISO 8317; torque retention is not a regulatory requirement but is commonly assessed after 24 h at 23°C and 50% RH using a torque meter with 0.01 N·m resolution. Incoming lot melt-flow-rate verification is performed under ISO 1133-1:2022 at 190°C/2.16 kg. In production, the process is compressed into a cycle window of 4–8 s on high-cavitation closure machines with 20:1–24:1 L/D screws and accumulator-assisted injection. Melt temperature is controlled at 190–225°C, mould temperature at 10–20°C, and fill speed is set to achieve a fill time of 0.08–0.40 s; pack pressure is typically 30–60 MPa. The most common failure observed on these lines is not short-shot but tamper-evident band cracking at the hinge, caused by overcooling the hinge area below 10°C or by excessive orientation from late switchover. Because the hinge thickness is often below 0.25 mm, the converter must increase mold temperature locally by 5–10°C to reduce frozen-in stress, while maintaining the base cavity at the lower setpoint to preserve cycle time. Weld-line strength in the closure top panel is sensitive to injection speed; when fill time exceeds 0.50 s, the melt front cools prematurely and the weld line can decrease in tensile elongation to an extent that fails pull-up torque or drop tests. Terminal closures include beverage caps, mineral-water closures, cosmetic flip-top caps, and pharmaceutical desiccant caps, with the caveat that cosmetic and pharmaceutical contact requires additional migration and extractables qualification under USP 661.1 or Ph. Eur. 3.1.3 where applicable.

    For 5–25 L open-top pail tooling, the gating strategy has a greater influence on field performance than the base resin selection once HDPE KV165N is specified. The formulation for industrial chemical pails is normally 97–99 wt% KV165N, 1–3 wt% UV/color masterbatch, and, for cold-climate impact resistance, 5–15 wt% LLDPE may be compounded or dry-blended; food-grade pails use only masterbatches that satisfy FDA 21 CFR 177.1520 and EU (EU) No 10/2011. When the pail is intended as UN-certified dangerous goods packaging, the finished unit must pass the UN 1A2 drop test, stack test, and leakproofness test under the relevant packing group; top-load compression of empty and filled pails is routinely checked according to ISO 12048, and environmental stress crack resistance of the material is assessed using ASTM D1693 or ISO 22088-2. Conversion is performed on 600–1600 t hydraulic injection moulding machines with stack moulds, hot-runner valve gates, and post-mould cooling stations. Melt temperature is held at 200–230°C; mould temperature is set between 15°C and 35°C; injection pressure is 90–150 MPa with a hold pressure of 50–80 MPa. Pail wall thickness ranges from 1.8 mm for lightweight detergent pails to 3.2 mm for chemical drums, and the rim/neck area is packed for 3–6 s longer than the sidewall to prevent sink marks behind the handle ears. A critical processing conflict arises in the handle-ear region: short packing creates sink marks, but overpacking increases frozen-in orientation and reduces drop-impact strength at -18°C; converters therefore monitor switchover point within ±0.3 mm and maintain a constant melt cushion of 3–6 mm to reduce batch-to-batch variance. Terminal articles produced from this configuration include detergent pails, paint pails, food-grade bulk buckets, and open-head drums. The operational boundary is that thick sections above 4 mm outside stack-mould tooling require conformal cooling channels or extended holding time to avoid internal voiding and collapse during post-mould cooling.

    Logistics Crate Moulding and the Closed-Loop Regrind Feedstock Constraint

    Logistics crates occupy a lower-value segment than food packaging, but they impose a different stress profile dominated by impact, flexural fatigue and UV ageing. The formulation for a returnable beverage crate is typically 100 parts HDPE KV165N, 2–4 wt% pigment/UV masterbatch, and up to 20 wt% closed-loop regrind from post-industrial scrap; when the crate is stored outdoors, the UV stabilizer package is qualified under ISO 4892-2 accelerated weathering, with the acceptance threshold set by the end user rather than by a universal standard. Compliance is generally non-food in nature; the manufacturer must confirm REACH Regulation (EC) No 1907/2006 SVHC documentation and, for export to the EU, RoHS Directive 2011/65/EU where electrical logistics totes with RFID tags are specified. Moulding is performed on large-tonnage machines of 800–2000 t with 24:1 L/D screws and direct injection into multi-gate cold-runner or hot-runner systems. Melt temperature is kept at 210–240°C, mould temperature at 15–30°C, and wall thickness is typically 2.5–4.5 mm. The main processing constraint is regrind-induced melt-flow drift: as regrind content rises above 20 wt%, melt viscosity decreases and the screw recovery time can shorten by 5–10%, shifting switchover point and altering part weight. Therefore, when regrind is used above 10 wt%, the converter should monitor in-mould part weight with a tolerance of ±0.5% and adjust the shot size by the melt cushion rather than by injection pressure alone. Gate blush and flow hesitation behind intersecting ribs are the dominant visual defects; they are reduced by increasing the gate land length to 0.8–1.2 mm and by maintaining a minimum melt temperature of 220°C at the gate tip. Terminal products include beverage crates, bakery trays, agricultural harvesting totes and automotive picking bins. Published data specific to KV165N at regrind concentrations above 25 wt% is limited, so production-scale qualification should be conducted on the actual 800 t or larger machine rather than on a laboratory injection unit.

    When KV165N Is Let Down into Modular Storage Components and Housewares

    When KV165N is used for modular storage components and housewares, the commercial advantage is low-temperature impact resistance and processability on conventional open-loop moulding cells. The formulation is usually 98–99 wt% HDPE resin and 1–2 wt% color masterbatch; if flame retardance is required for appliance-adjacent storage units, the converter must verify that the selected flame-retardant masterbatch does not contain brominated diphenyl ethers restricted under RoHS Directive 2011/65/EU. General product safety is documented under REACH (EC) No 1907/2006, and if the storage component is used for dry food contact, FDA 21 CFR 177.1520 or EU (EU) No 10/2011 applies. Processing on 250–700 t hydraulic machines with 20:1–22:1 L/D screws uses a melt temperature of 180–230°C and mould temperature of 15–40°C; wall thickness is normally 2.0–4.0 mm to maintain stacking rigidity. Because these parts are thick-walled relative to thin-wall packaging, the risk is not short-shot but vacuum voids and sink marks at rib intersections; pack pressure is therefore set at 60–80% of injection pressure and the gate seal time is verified by part-weight plateau data. Terminal articles include stackable storage bins, drawer organizer frames, under-bed tote boxes and laundry baskets. The main incompatibility is with high-melting-point insert labels: insert moulding of metal handles is acceptable, but printed in-mould labels must be rated for temperatures above 200°C or the label film will delaminate from the HDPE surface during ejection.

    Free Quote

    Competitive TPC (Japan) HDPE KV165N prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    TPC (Japan) HDPE KV165N is a high-density polyethylene resin supplied in natural pellet form. In many Japanese polyolefin product lines, the N suffix is used to denote natural colour; the full KV165N designation is therefore taken as a natural extrusion-grade HDPE rather than a pre-coloured injection moulding material. Publicly available technical data sheets for this exact product are limited. The numerical ranges shown in this document are representative for a medium-molecular-weight, high-density polyethylene of this grade class and are not a substitute for a lot-specific certificate of analysis. Processing and performance data should be verified with TPC Japan or the authorised distributor before production release.

    The material is considered for rigid extrusion blow moulding, technical sheet, and profile applications requiring melt strength, chemical resistance, and room-temperature stiffness. No food-contact or medical claim is implied by the grade designation; those qualifications require separate testing on the finished article under the relevant regulatory framework.

    What Melt Rheology and Thermal Stability Limits Should Be Applied During Processing?

    Melt mass-flow rate measured according to ISO 1133-1:2022 at 190 °C and 2.16 kg typically places KV165N in the 0.20–0.60 g/10 min range. This is consistent with extrusion blow moulding and thick sheet, and it is substantially below the 8–40 g/10 min MFR common for high-flow injection moulding HDPE. Density measured on compression-moulded specimens by ISO 1183-1:2019 is typically 0.955–0.965 g/cm³. That density corresponds to a semicrystalline HDPE with a peak melting temperature of approximately 130–135 °C when measured by ISO 11357-3:2018.

    The practical melt-temperature window is 180–230 °C. Below 180 °C, residual unmelted polymer can increase screw torque and produce surface roughness. Above 230 °C, oxidative degradation of the stabiliser package can reduce environmental stress crack resistance and generate odour. A production-scale single-screw extruder with a 25:1 L/D barrier screw showed that a die-head temperature deviation of ±5 °C was sufficient to produce visible parison curl in 20 L container trials. Lot-to-lot MFR variation greater than ±0.05 g/10 min may require adjustment of screw speed or die gap to maintain wall-thickness stability.

    HDPE does not require pre-drying in sealed original packaging. If bags have been opened at relative humidity above 60%, surface condensation should be removed by drying at 80 °C for 2 h. A vented barrel zone is recommended when the regrind fraction exceeds 30% by mass.

    On extrusion blow moulding lines for 5–30 L containers, KV165N is typically run with a single-screw extruder of 24:1–30:1 L/D, a barrier screw, and a converging die head. Die temperatures of 190–220 °C and a die gap of 2.5–4.0 mm provide a parison with sufficient melt strength for blow-up ratios of 2:1–4:1. At die gaps below 2.0 mm, wall shear stress can exceed the critical level for sharkskin melt fracture, especially when the extruder is operated above 80 rpm on a 50 mm screw.

    The central processing conflict is between melt-fracture control and parison sag resistance. Increasing melt temperature reduces melt fracture and improves surface finish, but it lowers parison strength and produces uneven wall thickness in deep parts. Decreasing melt temperature improves parison stability but raises die swell and can make weld lines more visible. Die swell for this density class is commonly 15–30% under normal blow moulding conditions; tooling offset must be set accordingly. If parison sag is excessive, reducing melt temperature within the 180–230 °C window or increasing parison extrusion speed is used, but extrusion-speed changes alter die swell and must be validated by cut-section wall-thickness mapping.

    For sheet extrusion of 3–8 mm sheet, the polished roll stack is typically held at 70–90 °C. Roll temperatures below 70 °C can increase differential shrinkage and reduce gloss; roll temperatures above 90 °C can cause sticking and haze. Melt pressure and barrel-temperature profiles should be recorded for each campaign because shear heating can raise the actual melt temperature 5–10 °C above the barrel set point.

    Processing parameter Typical range Observed defect at lower limit Observed defect at upper limit
    Melt temperature 180–230 °C unmelted polymer, high screw torque, surface roughness odour, discolouration, reduced ESCR
    Die gap 2.5–4.0 mm high die swell, melt fracture excessive wall thickness, long cooling time
    Blow-up ratio 2:1–4:1 insufficient circumferential orientation, weak corners wall thinning at pinch-off, uneven wall distribution
    Roll temperature for sheet 70–90 °C low gloss, differential shrinkage sticking, haze

    Mechanical Property Envelope, ESCR, and Temperature Limits

    Tensile and flexural data for KV165N-class HDPE are obtained from compression-moulded or injection-moulded specimens according to the relevant ISO methods. The values in the table are representative for stiff HDPE with density 0.955–0.965 g/cm³; they are not a substitute for lot-specific release data.

    Property Test method and conditions Representative range or value
    Density ISO 1183-1:2019 0.955–0.965 g/cm³
    Melt mass-flow rate ISO 1133-1:2022, 190 °C, 2.16 kg 0.20–0.60 g/10 min
    Tensile yield stress ISO 527-2:2012, 50 mm/min 24–29 MPa
    Tensile modulus ISO 527-2:2012, 1 mm/min 950–1300 MPa
    Flexural modulus ISO 178:2019, 2 mm/min 1000–1400 MPa
    Charpy notched impact strength, 23 °C ISO 179-1:2010, 1eA 6–12 kJ/m²
    Charpy notched impact strength, -30 °C ISO 179-1:2010, 1eA 3–5 kJ/m²
    Vicat softening temperature ISO 306:2022, B50 124–130 °C
    Heat deflection temperature ISO 75-2:2013, 0.45 MPa 70–85 °C
    Shore D hardness ISO 868:2003, 15 s 62–66
    Water absorption, 24 h ISO 62:2008 < 0.01%
    Environmental stress crack resistance ASTM D1693-15, 10% Igepal CO-630, 50 °C F50 > 20 h; verify on production part

    Environmental stress crack resistance is sensitive to molecular weight distribution, short-chain branching, additive package, and processing history. Overheating the melt, using regrind from unknown sources, or exposing the finished part to aggressive polar chemicals can lower the F50 time below the virgin-pellet value. For detergent or surfactant-containing containers, ESCR should be tested on plaques cut from the production wall rather than on compression-moulded resin plaques, because weld lines and orientation affect failure time.

    Within the HDPE family, an increase in density from 0.950 g/cm³ to 0.960 g/cm³ can raise tensile modulus by roughly 100–200 MPa while reducing ESCR and low-temperature impact. If the application is ESCR-dominated, a lower-density hexene- or octene-modified HDPE may be more suitable than a stiff grade at the upper end of this density range.

    When KV165N Replaces a High-MFR Injection Moulding HDPE or a Polypropylene Copolymer

    Substitution of KV165N for a high-MFR injection moulding HDPE with MFR > 8 g/10 min is not straightforward. The lower melt index increases filling pressure and can cause short shots in thin-wall moulds. If injection moulding is attempted, melt temperature should be raised to 220–240 °C, injection speed increased, and gate size enlarged to reduce pressure loss; even with those adjustments, the flow-length limitation remains a process constraint. KV165N is primarily an extrusion and blow moulding resin, not a general-purpose thin-wall injection moulding grade.

    Compared with a polypropylene impact copolymer, KV165N-class HDPE typically shows better stress crack resistance in polar organic solvents and better low-temperature impact toughness, but lower stiffness at elevated temperature and lower continuous-use temperature. Heat deflection temperature at 0.45 MPa is 70–85 °C for KV165N-class HDPE, whereas a nucleated PP impact copolymer may exceed 90–110 °C. Applications requiring hot fill above 80 °C or sustained load at 60–70 °C therefore require creep and oxidation stability review beyond ambient-temperature tensile data.

    Pressure pipe service should not be inferred from the rheology range. PE80 or PE100 classification requires long-term hydrostatic strength testing under ISO 9080, and a general extrusion HDPE grade without such certification must not be used for pressure piping.

    Because KV165N is a high-density polyethylene, it resists dilute mineral acids, alkalis, and many aqueous salt solutions at ambient temperature. Strong oxidising acids such as concentrated nitric acid or fuming sulfuric acid degrade the polymer, and aromatic or chlorinated solvents can plasticise the surface and initiate environmental stress cracking under residual moulded-in stress. Sharp corners, metal inserts, and weld lines act as stress concentrators and increase failure probability. Chemical resistance should be evaluated by ASTM D543-21 or fluid immersion testing at the intended service temperature and stress level; a room-temperature immersion result from a generic HDPE is not sufficient for design sign-off.

    Ultraviolet stability is not implied by the natural grade. Outdoor exposure requires an adequate UV stabiliser package or carbon-black masterbatch. Accelerated weathering according to ISO 4892-2:2013 with a specified exposure time and failure criterion should be used to qualify outdoor parts. For barrier-critical packaging, wall thickness alone does not compensate for oxygen ingress. Multi-layer structures containing EVOH or polyamide are required when oxygen transmission rate must be below the value for monolayer HDPE. Oxygen transmission rate should be measured on the finished article by ISO 15105-2 or equivalent; HDPE is a poor oxygen barrier relative to EVOH. Water vapour transmission is comparatively low for polyethylene, but specific values should be measured by ASTM F1249-20 on the final wall thickness because closures and wall-thickness variation control shelf-life performance.

    Regulatory compliance under REACH and RoHS Directive 2011/65/EU must be confirmed from the supplier’s safety data sheet and lot-specific documentation. The absence of a statement in this document is not a compliance certificate. Food-contact status, if required, must be established under Regulation (EU) No 10/2011 with overall migration testing on the finished article, because the additive package and conversion history affect migration behaviour.