| HS Code | 197358 |
| Polymer Type | High Density Polyethylene (HDPE) |
| Density | 0.956 g/cm³ |
| Melt Mass Flow Rate 190 C 2 16 Kg | 8.0 g/10 min |
| Melting Point | 134 °C |
| Vicat Softening Temperature | 126 °C |
| Tensile Strength At Yield | 29 MPa |
| Tensile Strength At Break | 30 MPa |
| Elongation At Break | 1000 % |
| Flexural Modulus | 1180 MPa |
| Notched Izod Impact Strength | 40 J/m |
| Shore D Hardness | 65 |
| Mold Shrinkage | 1.5-3.0 % |
| Water Absorption | <0.01 % |
| Thermal Conductivity | 0.44 W/m·K |
| Volume Resistivity | >1E16 ohm·cm |
As an accredited TPC (Japan) HDPE KS178A factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | TPC (Japan) HDPE KS178A is supplied in 25 kg polyethylene-lined paper bags, with 1,000 kg jumbo bags available. |
| Container Loading (20′ FCL) | 20′ FCL loading: TPC Japan HDPE KS178A in 25 kg bags, palletized, shrink-wrapped, approximately 17–18 MT net per container. |
| Shipping | TPC (Japan) HDPE KS178A is a non-hazardous high-density polyethylene resin. It is not regulated for transport under DOT, IMDG, IATA, or ADR. Ship in original sealed 25 kg bags, palletized and shrink-wrapped. Keep dry, avoid heat, contamination, and oxidizers. No special labels or placards required; not a marine pollutant. |
| Storage | Store TPC (Japan) HDPE KS178A in a cool, dry, well-ventilated area, away from direct sunlight, heat, flames, and strong oxidizers. Keep original bags or containers closed, labeled, and off the floor on pallets. Prevent moisture, dust, and contamination. Avoid prolonged UV exposure and excessive stacking. Rotate stock and follow local regulations. Do not store near incompatible materials. Maintain good housekeeping. |
| Shelf Life | Shelf life is typically 12 months when stored unopened in original packaging, dry, cool, and away from direct sunlight. |
On a 500 mm twin-station shuttle blow molder producing 25 L tight-head HDPE jerrycans, the TPC (Japan) HDPE KS178A melt is maintained at a head temperature of 205–215°C, with feed-zone setpoint 170°C and die bushing 190–200°C. Parison programming shifts the die gap from 1.8 mm at the neck to 4.3 mm across the lower sidewall to counteract a measured hang-time sag of 12–16 mm/s; pre-blow air is 0.08–0.12 MPa and main blow air is 0.7–0.9 MPa. Mold coolant enters at 10–14°C and the overall cycle time is 58–72 s for a 2.7 kg shot. Pinch-off flash is held below 0.6 mm by trimming tool depth to reduce granule size variability in closed-loop regrind.
Formulation addition ratios are metered gravimetrically. The pellet is dry-blended with 2.0–3.0 wt% carbon black masterbatch, 0.05–0.15 wt% hindered phenolic antioxidant, 0.10–0.30 wt% antistatic concentrate for solvent packaging below 10-8 S/m surface conductivity, and 0.05–0.10 wt% calcium stearate as an acid scavenger. Regrind from tail flash and rejected containers is screened through 60/80/100 mesh and introduced at 15–30 wt%; the compound remains within the drop-tested melt strength band until regrind exceeds 40 wt%.
Regulatory compliance for dangerous-goods packaging follows 49 CFR 178.509, ADR 6.1.5, and the IMDG Code 6.1; food-contact applications are evaluated under FDA 21 CFR 177.1520 and EU Regulation (EU) No 10/2011. Sidewall thickness is verified by ultrasonic gauge at four quadrants with a tolerance of ±0.3 mm on the sidewall and ±0.5 mm at the pinch-off. Terminal products include 20 L and 25 L UN 1H2 jerrycans, 30 L narrow-mouth agricultural adjuvant containers, and 5–10 L handled bottles for water-based latexes where the grade has been qualified against ASTM D1693 environmental stress-crack resistance.
Six-extruder sequential coextrusion of 10 L multilayer jerrycans uses KS178A in the outer skin and in the regrind-containing carrier layers, with mass fractions of 12–18% outer HDPE, 35–50% regrind HDPE, 2–3% tie resin, 3–5% EVOH, 2–3% tie resin, and 15–20% inner HDPE. The outer layer is dry-blended with 2.0–4.0 wt% color masterbatch and 0.05–0.20 wt% antioxidant; the inner layer contains 1.5–2.5 wt% white masterbatch to provide visual contrast against the fill level. EVOH is pre-dried at 80°C for 4–6 h to a moisture content below 0.05 wt%, while KS178A requires hopper moisture below 0.05 wt% only when the ambient relative humidity exceeds 60%.
The die head is profiled from 220°C at the outer HDPE layer to 205°C at the EVOH layer to control viscosity mismatch and prevent interfacial waviness near the pinch-off. Blow air is 0.8–1.2 MPa and mold water is 8–15°C; the 10 L container cycle is 75–95 s. Wall thickness is fixed at 1.2–1.6 mm in the sidewall and 2.2–2.8 mm at the handle pinch area, with the EVOH layer thinned by 30–50% at weld lines but maintained above 1.5% of total wall in the top-load-bearing sections.
Dangerous-goods qualification for the multilayer container follows UN 3H2 design type testing under 49 CFR 178.509 and ADR 6.1.5; agrochemical compatibility is screened by comparing mass change and elongation loss under ASTM D543-21 after 30 days exposure at 40°C to xylene, cyclohexanone, and formulated emulsifiable concentrates. Food-contact status of the inner layer is assessed under FDA 21 CFR 177.1520 and EU Regulation (EU) No 10/2011. Terminal products include 5 L, 10 L, and 20 L multilayer jerrycans for solvent-based herbicides, emulsifiable concentrate pesticides, and adjuvants that require high oxygen barrier to prevent active ingredient oxidation.
A grooved-feed single-screw extruder with 33:1 L/D and a 200 mm barrier screw feeds a corrugator producing 300 mm outside diameter double-wall drainage pipe under a 180–210°C barrel profile, 190–210°C die temperature, and 0.6–0.9 bar corrugator vacuum. KS178A is dry-blended with 2.0–3.0 wt% carbon black masterbatch to meet the carbon black dispersion and ultraviolet resistance clauses of AASHTO M294 and EN 13476-1; the compound is checked by ISO 18553 dispersion rating before startup. The pipe is sized in a corrugated mold-block system with 10–25°C block cooling, and the inner liner is extruded in the same pass with a die lip gap of 1.2–2.0 mm. Terminal products include 300 mm double-wall road culverts, agricultural drainage lines, and cable duct where compliance with ASTM F2306/F2306M is required.
The one-stage injection blow process raises KS178A melt in the injection barrel to 205–225°C, fills a preform cavity at 80–120 MPa injection pressure, and transfers the preform at 145–155°C to the blow station before blowing with 0.6–1.2 MPa air into a mold held at 8–12°C. Preform neck temperature is held 10–15°C below the sidewall to preserve thread dimensional stability; blow air is introduced through a 0.8 mm orifice tip to reduce jetting and asymmetric inflation.
Formulation addition ratios for medicinal bottles are controlled by gravimetric dosing: 2.0–4.0 wt% white masterbatch with 60% TiO2, 0.05–0.15 wt% hindered phenolic antioxidant, and 0.05–0.15 wt% slip/antiblock concentrate. The target wall thickness is 0.4–0.9 mm for 30–100 mL bottles, with maximum deviation of ±0.10 mm in the seal area and ±0.15 mm in the sidewall measured by a vision wall-thickness gauge.
Compliance for pharmaceutical use follows USP <661.1> and USP <661.2> extractables testing, Ph. Eur. 3.1.3, FDA 21 CFR 177.1520, and elemental impurity limits under ICH Q3D. Steam autoclaving above 121°C is not recommended for this HDPE grade; terminal products are therefore limited to 30 mL oral dosing bottles, 100 mL syrup bottles, and 10 mL ophthalmic dropper bottles that are sterilized by ethylene oxide or gamma irradiation at 25 kGy, where published data for this specific configuration is limited and requires lot-specific oxidative induction time testing.
A 120 mm single-screw extruder with L/D 30:1 and a barrier flight section feeds a 3.5 m flat sheet die for 1.5 mm smooth HDPE geomembrane. Barrel temperatures are set 195–220°C, die temperature 220–235°C, and the three-roll stack is held at 85–105°C to minimize residual stress; screen changer uses 40/60/80 mesh packs to remove gels. The KS178A pellet is dry-blended with 2.0–3.0 wt% carbon black masterbatch, 0.20–0.50 wt% antioxidant package, and 0.01–0.05 wt% fluoropolymer process aid. Carbon black dispersion is verified by ISO 18553 and by microtome inspection at 20× magnification before wound rolls are released.
Compliance with landfill liner specifications follows GRI-GM13 for smooth 1.5 mm HDPE geomembrane: nominal density under ASTM D1505 is typically above 0.940 g/cm³, tensile break strength under ASTM D6693 is expected to exceed 27 kN/m, elongation at break exceeds 700%, and stress-crack resistance under ASTM D1693 Condition C is evaluated for ≥500 h in the sheet machine direction and transverse direction. Thickness tolerance is maintained at ±5% by a beta gauge feedback loop. Terminal products include 1.0–2.5 mm geomembrane rolls for landfill basal liners, mining heap leach pads, and pond liners where low-temperature flexibility at −20°C is qualified by ASTM D1790-based brittleness testing.
Multi-layer coextrusion blow molding of 10 L fuel tanks places KS178A in the outer and inner HDPE layers with an EVOH barrier layer at 2–4% of total wall thickness and tie layers at 1.5–2.5%. The outer layer is dry-blended with 1.5–2.5 wt% carbon black masterbatch and 0.15–0.30 wt% UV stabilizer; the inner layer contains 0.05–0.15 wt% acid neutralizer to reduce fuel oxidation by-product attack. Melt temperature is 205–225°C, die head 220–230°C, mold coolant 6–10°C to increase cooling stress at pinch-off and improve low-temperature drop-impact resistance.
Permeation compliance for small off-road engine fuel tanks is tested under EPA 40 CFR Part 1054 or CARB EVAP using fuel C at 28°C and 40°C; the EVOH layer must remain continuous at corners and pinch-off, with minimum wall in EVOH of 0.5% of total wall thickness. Drop-impact qualification is performed on filled 10 L tanks at −40°C from 1.2 m onto a concrete impact surface; failure at the sidewall-thread interface occurs when local wall thickness falls below 1.5 mm. Terminal products include 5–20 L fuel tanks for lawnmowers, generator sets, outboard engines, and compact construction equipment.
Competitive TPC (Japan) HDPE KS178A prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
TPC (Japan) HDPE KS178A is a pelletized high-density polyethylene grade in which the suffix KS178A designates a specific polymerization and stabilization profile within the producer’s blow molding range. The material is defined not by filler content or by a single additive package, but by its melt rheology, molecular weight distribution, and comonomer distribution. Because the manufacturer’s certificate of analysis is the controlling document for any given lot, incoming inspection at converters may verify melt mass-flow rate under ISO 1133-1:2022 at 190 °C with 2.16 kg load, density under ISO 1183-1:2019, and moisture content by volumetric Karl Fischer titration. Published data for this specific configuration is limited; resin certification should not proceed without the product technical datasheet and lot release values.
In extrusion blow molding, the grade is directed toward rigid containers in which parison melt strength and environmental stress crack resistance determine service life. Typical applications for HDPE blow molding resins of this class include jerry cans, industrial drums, agricultural chemical bottles, and intermediate bulk container liners. The grade may be run on accumulator-head machines and continuous shuttle blow molders. It differs from injection-molding HDPE in that its molecular architecture is selected for parison integrity at low melt flow rather than for high injection flow and short cycle time.
Differentiation from other products is established through molecular architecture and melt rheology rather than nominal density alone. Injection-moulding HDPE grades are typically designed for high flow and short cycle times, with melt mass-flow rates above 20 g/10 min under ISO 1133-1:2022 conditions. Blown-film HDPE grades often occupy a melt mass-flow rate near 1.0 g/10 min, with narrow molecular weight distribution to control bubble stability. Blow molding HDPE grades such as KS178A are generally positioned in a lower melt mass-flow rate band, commonly between 0.20 g/10 min and 0.80 g/10 min, to provide sufficient melt strength during parison hang. These values are not product-specific releases; the KS178A certificate of analysis defines the actual lot value. The combination of medium-to-high molecular weight and controlled comonomer distribution affects extensional viscosity, parison sag, and post-extrusion swell, which in turn determines die design and pinch-off seam quality.
On accumulator-head blow molding lines, parison quality is sensitive to melt temperature at the die exit, die gap profile, and fill rate. HDPE blow-molding grades similar to KS178A are usually processed at melt temperatures between 170 °C and 210 °C. Exceeding 230 °C can initiate oxidative chain scission, lower molecular weight, and reduce environmental stress crack resistance; continuous melt temperature monitoring at the die exit is therefore standard. Die head tooling is programmed to produce a thickness profile that compensates for wall thinning at the pinch-off zone and the lower sidewalls of large containers. On accumulator heads with shot capacity above 5 L, parison drop times typically remain below 20 s; longer drop times require high melt strength and can be validated by capillary rheometry under ISO 11443:2021. Published data for KS178A-specific parison sag rates is limited, so initial line trials on the target tooling are required before production release.
Clamp force and pinch pressure should be established from part projected area and mold construction. For industrial drums, hydraulic clamp systems with capacity above 200 kN are common, but the required force is calculated from mold dimensions and melt viscosity. Mold temperature control between 10 °C and 30 °C is typical for HDPE blow molding to stabilize part cooling and minimize warpage. Slower cooling of thick pinch-off seams can produce sink marks and dimensional drift; post-molding dimensional checks under ISO 6603-1 or customer-specific gauging are used.
When the part is down-gauged below 0.5 mm nominal wall thickness, melt fracture and parison instability can dominate. For high molecular weight HDPE blow molding grades, the shear rate at the die lip is calculated from parison velocity and die gap. At shear rates above 500 s⁻¹ on certain die geometries, melt fracture may produce rough parison surfaces. Reducing die gap or increasing melt temperature within limitations can shift the shear rate; however, higher temperature accelerates sag. In such cases, dynamic rotational rheometry or capillary rheometry is used to identify critical shear stress. For high molecular weight HDPE, critical shear stress for melt fracture is often close to 0.20 MPa to 0.40 MPa, though the exact value is grade-dependent. Thin-wall blow molding therefore requires a narrow processing window, and published data for this specific configuration is limited.
On production-scale shuttle blow molding lines, a recurring failure mode for high molecular weight HDPE is pinch-off flash delamination when mold closing speed is too high or melt temperature is too low. Adjustment of mold close speed and pinch design to maintain a minimum flash thickness of 0.1 mm to 0.3 mm prevents cold consolidation defects. Another observed issue is wall-thickness variation caused by parison curl after die exit; this is reduced by die centering, uniform melt temperature, and parison programming.
Conversion of HDPE KS178A on single-screw extruders with barrier screws and Maddock mixing sections is standard. Extruder length-to-diameter ratios of 24:1 to 30:1 and screen packs configured at 20/40/60 mesh are used on similar HDPE blow molding grades to remove incidental fines and improve melt homogenization. Higher shear mixing may increase melt temperature; therefore, screw speeds on continuous extrusion lines are often kept below 60 rpm for large parison outputs, though the limit is a function of screw diameter and back pressure. Back pressure below 15 MPa is a practical starting point for resin with high molecular weight, but line-specific optimization is required.
Pre-drying of unopened HDPE pellet containers is not normally required in controlled indoor storage. However, extended outdoor storage at high relative humidity can introduce surface moisture that appears as splay or surface defects. In such cases, desiccant drying at 80 °C for 2 h to 4 h is used to bring moisture below 200 ppm before extrusion. The resin should not be dry-blended with amine-based processing aids if acid-neutralizing stabilizer interactions are a concern, because premature additive reaction can shift melt pH and tooling corrosion behavior. Batch-to-batch variability in melt flow rate for HDPE blow molding grades can be observed as a shift of 0.05 g/10 min to 0.10 g/10 min within certified limits; processing adjustments include parison programming and die gap changes.
Relative to low-density polyethylene, HDPE KS178A is characterized by a higher crystalline fraction and lower permeability to water vapor under ASTM E96/E96M-22; however, the grade’s opacity and lower clarity prevent use in transparent film. Relative to polypropylene, HDPE blow molding grades typically exhibit better environmental stress crack resistance in detergent environments but lower continuous service temperature; polypropylene may be selected where hot-fill above 100 °C is required. The choice between HDPE, LDPE, and PP is therefore specific to the stress-cracking environment and geometry, not solely to cost.
| Property | Test designation | Unit | Typical use in resin certification |
|---|---|---|---|
| Melt mass-flow rate | ISO 1133-1:2022 | g/10 min | Lot release and processability |
| Density | ISO 1183-1:2019 | g/cm³ | Rigidity and crystallinity |
| Tensile yield stress | ISO 527-2:2012 | MPa | Wall strength design |
| Flexural modulus | ISO 178:2019 | MPa | Top-load and sidewall stiffness |
| Charpy impact strength, notched | ISO 179-1:2010 | kJ/m² | Low-temperature toughness |
| Environmental stress crack resistance | ASTM D1693-21 | h | Detergent and chemical compatibility |
| Vicat softening temperature | ISO 306:2022 | °C | Heat resistance for hot-fill |
| Oxidation induction time | ISO 11357-6:2018 | min | Stabilization package verification |
Regional compliance is evaluated separately from mechanical performance. Food-contact suitability is assessed under FDA 21 CFR 177.1520(c), EU Regulation 10/2011 Annex I, and applicable Japan positive-list frameworks, depending on jurisdiction. Migration testing uses food simulants defined in EU Regulation 10/2011 chapter 2.1 for aqueous, acidic, alcoholic, and fatty food types; converters must validate final article surface-to-volume ratios. For industrial dangerous goods packaging, UN certification under ADR/RID chapter 6.1 is required, including leakproofness and stack-load resistance. These certifications are product- and design-specific, not intrinsic to the resin alone.
In agricultural chemical packaging, resin performance is assessed through environmental stress crack resistance testing under ASTM D1693-21 and by weight-loss permeation cups according to ASTM E96/E96M-22 for water vapor transmission. If contact with amines or oxidizing agents is anticipated, chemical compatibility testing is required because oxidative degradation can reduce the effective service life of the container. Grade-specific data for KS178A in these aggressive environments is often not disclosed in public technical data sheets; application-specific testing on molded containers remains necessary. When surfactant-filled containers are conditioned at 50 °C for 48 h, the absence of visible cracking is a minimum screening criterion, but extension to 168 h or longer is required for aggressive formulations.