| HS Code | 631938 |
| Density | 0.953 g/cm³ |
| Melt Flow Rate | 8.0 g/10 min (190°C/2.16 kg) |
| Tensile Strength At Yield | 27 MPa |
| Tensile Elongation At Break | 1000% |
| Flexural Modulus | 1100 MPa |
| Izod Impact Strength Notched | 49 J/m |
| Vicat Softening Point | 124°C |
| Heat Deflection Temperature At 1 82 Mpa | 70°C |
| Shore D Hardness | 65 |
| Mold Shrinkage | 2.0% |
| Brittleness Temperature | -70°C |
| Water Absorption | <0.01% |
| Dielectric Constant | 2.3 |
| Volume Resistivity | >1e15 ohm·cm |
As an accredited TPC (Japan) HDPE KM698A factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | TPC (Japan) HDPE KM698A typically comes in 25 kg multiwall paper bags, palletized, stretch-wrapped, and labeled for industrial shipment. |
| Container Loading (20′ FCL) | TPC (Japan) HDPE KM698A loaded in 20′ FCL: 25 kg bags, palletized, shrink-wrapped; approx. 18–20 MT per container. |
| Shipping | TPC (Japan) HDPE KM698A is shipped in 25 kg PE bags on pallets, stretch-wrapped and labeled. It is a non-hazardous thermoplastic resin, transported in clean, dry containers at ambient temperature, protected from moisture, sunlight, and contamination. No special dangerous goods requirements apply. |
| Storage | Store TPC (Japan) HDPE KM698A at ambient temperature in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, and flames. Keep original bags sealed and palletized to prevent moisture, dust, and contamination. Avoid contact with oils, chemicals, and strong oxidizers. Stack securely to prevent package deformation; use oldest stock first. Follow supplier SDS and local regulations. |
| Shelf Life | For TPC (Japan) HDPE KM698A, recommended shelf life is 2 years from manufacture when stored unopened in cool, dry conditions. |
High-output blown-film lines running TPC HDPE KM698A as the neat resin for thin-gauge T-shirt bag production operate within a melt temperature window of 180–210°C and a blow-up ratio of 3.0–4.5:1; the high molecular weight distribution is reflected in a melt mass-flow rate of 0.08 g/10 min at 190°C/2.16 kg under ISO 1133-1:2022 and a high-load melt mass-flow rate of 8.0 g/10 min at 190°C/21.6 kg, with a density of 0.949 g/cm³ under ISO 1183-1:2019. Where pellet surface moisture exceeds 0.01 wt% after storage at relative humidity above 60%, pre-drying at 80°C for 2 h is necessary; otherwise surface moisture migrates into the melt film and forms microvoids at the die lip. The processing window is deliberately narrow: below 170°C the high molecular weight tail produces unmelted gel particles that emerge as fisheyes in the web, and above 220°C oxidative chain scission generates gel specks and destabilises bubble height at frost-line heights from 4 to 8 die diameters. In formulation, the resin is charged at 100 phr as the base matrix; 3.0–5.0 wt% linear low-density polyethylene C6 or C8 is added to raise dart impact under ASTM D1709-16a and reduce seal puckering, 2.0–4.0 wt% of a 60% TiO₂ white masterbatch supplies opacity for printed bags, and 0.5–1.5 wt% of a 10% synthetic silica antiblock masterbatch prevents blocking on high-speed converting. Downstream processing is performed on a grooved-feed single-screw extruder with L/D 30:1 and a barrier screw with a Maddock mixer, feeding a spiral-mandrel die of 150–250 mm diameter and 1.0–2.0 mm die gap; melt filtration across 60/80/100 mesh screen packs holds pressure before the screen at 25–40 MPa, and a dual-lip air ring plus online capacitance gauging maintains gauge variability within ±8% for a 12 µm web. The specification anchor is ASTM D4976-12a for polyethylene film and sheeting, with GB/T 21661-2020 applying to plastic shopping bags in export markets; direct food-contact status is not assigned to the resin itself but can be supported under FDA 21 CFR 177.1520 only when the finished bag uses compliant additive masterbatches and migration testing under EU No 10/2011 is completed on the final article. Terminal forms on this setting are high-density T-shirt bags, produce roll bags, point-of-sale bag bundles, and small bin liners from 8–18 µm web.
At a let-down of 20 wt% post-consumer HDPE recyclate into KM698A, bubble stability is governed less by the melt index of the virgin fraction than by contaminant gel load, melt-elasticity mismatch, and pellet-feeding uniformity of the recycled stream. The formulation benchmark is 80 wt% KM698A and 20 wt% PCR-HDPE; the working window is 10–30 wt% recyclate, with the lower limit set by cost and the upper limit set by gauge instability and gel-induced film breaks. Downstream processing on a single-screw blown-film line with a grooved-feed section requires a continuous screen changer with 100/120/150 mesh screens; pressure before the screen is typically 18–28 MPa at 190–205°C melt temperature, and a pressure drift of 2–5 MPa per shift indicates filter blinding from paper fiber, cap liner remnants, or oxidised gel. On production lines equipped with gravimetric metering, pellet segregation between virgin KM698A and irregular PCR-HDPE is reduced by feeding the recycled fraction through a separate side-feeding hopper rather than by dry tumble blending; this avoids melt-pressure oscillations of more than 3 MPa at the screw tip. In practice, bubble breaks are most frequent when the recyclate contains small amounts of polypropylene caps or closures; polypropylene forms discrete unmelted islands at HDPE melt temperatures and acts as a tear-initiation site under ASTM D1922-15. The compliance frame for non-food grocery sacks is EN 15343:2007 for recycled content traceability and EU Directive 94/62/EC on packaging and packaging waste; food-contact use is not supported unless the recyclate carries an EFSA suitability opinion and the finished article passes EU No 10/2011 migration testing. Published data for film property retention above 30 wt% PCR-HDPE specifically with KM698A is limited; qualification must therefore include pilot-line let-down followed by dart impact testing under ASTM D1709-16a and MD tensile testing under ASTM D882-18. The resulting sacks are refuse sacks, retail grocery sacks, and municipal recycling bags in gauges from 12–25 µm.
In heavy-duty liner extrusion, the formulation uses KM698A at 100 phr as the matrix and a calcium carbonate masterbatch at 5–15 wt%; the masterbatch is typically based on 80% CaCO₃ in an LLDPE carrier and is added for density, opacity, and cost-adjusted stiffness. Addition above 15 wt% produces a cliff-edge effect in low-temperature puncture resistance; published data for this specific masterbatch concentration with KM698A is limited, but industrial practice on 350–600 mm spiral-mandrel die lines indicates that heavy-duty refuse sacks loaded above 15 wt% show a marked reduction in MD tear retention under ASTM D1922-15 and puncture resistance under ASTM D5748-19, particularly at handling temperatures between −10°C and 5°C. The production process runs a die gap of 2.0–2.8 mm, a blow-up ratio of 2.5–3.5:1, and a frost-line height of 500–900 mm; a dual-lip air ring with chilled air at 12–18°C is required to stabilize the wider bubble and prevent melt conditioning differences between the flattened edges and centre of the web. Melt temperature is held at 185–205°C; below 175°C the filler masterbatch increases screw torque and can produce surface roughness at the die lip, while above 210°C oxidative degradation of the LLDPE carrier in the masterbatch creates gel specks in the film. Compliance for refuse sacks is anchored to EN 13592:2017 for household waste sacks and to REACH 1907/2006 Annex XVII for the calcium carbonate masterbatch and processing aids; ASTM D4976-12a remains the specification reference for polyethylene film and sheeting. Product types under this route include heavy-duty refuse sacks, industrial liners for dry bulk containers, construction-site waste bags, and compactor bags in thicknesses from 30–70 µm.
A three-layer coextruded cereal liner uses KM698A in the outer skin layers at 40–60 wt% of total structure, with an LLDPE C8 core at 30–50 wt%, and optional white masterbatch at 3.0–5.0 wt% in the skins. The KM698A fraction is selected not for melt strength alone but because its low melt mass-flow rate of 0.08 g/10 min under ISO 1133-1:2022 reduces layer-thickness variation when the melt stream passes through a three-layer spiral mandrel die; the high molecular weight distribution narrows the viscosity ratio between the skin and core polymers at a die temperature of 190–205°C. Downstream processing on an internal bubble cooling line uses a die gap of 1.8–2.2 mm, a blow-up ratio of 2.0–2.8, and a frost-line height of 3–6 die diameters; the IBC airflow is adjusted to maintain bubble diameter within ±2% across the lay-flat. For food-contact use, the finished structure falls under FDA 21 CFR 177.1520 for olefin polymers and EU No 10/2011 for plastic food contact materials; overall migration testing must demonstrate ≤ 10 mg/dm² on the final article, and the liner supplier must verify that the white masterbatch and any processing aids are also listed in the relevant framework. Because HDPE is a moisture barrier but a weak oxygen barrier, the structure is suited to dry cereal, cracker, and snack liners rather than oxygen-sensitive dry powders; if an EVOH barrier layer is introduced, maleic anhydride-grafted PE tie layers at 5–8 wt% per adhesive layer are required because HDPE and EVOH do not intermix without interfacial adhesion. End-use articles produced from this structure include cereal box liners, cracker liners, dry snack pouches, and boxed dry mix liners from 20–40 µm total structure.
For powdered detergent box liners, the heat-seal window is set by the melting range of HDPE and by the need to avoid burn-through at high jaw pressure. The film formulation uses KM698A at 100 phr; 2.0–4.0 wt% of an erucamide/synthetic silica slip-antiblock masterbatch reduces coefficient of friction below 0.30 under ASTM D1894-14, 3.0–5.0 wt% of a white masterbatch provides opacity, and 0.5–1.0 wt% of a 10% ethoxylated amine antistat masterbatch prevents powder deposition on the seal area when handling detergent dust. Downstream converting occurs on vertical form-fill-seal machines with heated jaws set to 130–150°C, dwell 0.6–1.2 s, and sealing pressure 2–4 bar; the KM698A molecular weight distribution stabilizes the melt curtain during seal-bar contact, but the seal window remains narrower than LLDPE grades, so jaw temperature must not exceed 150°C to avoid seal thinning and film snap-back after the jaw opens. Compliance for non-food detergent packaging is anchored to ASTM D4976-12a, REACH 1907/2006, and RoHS 2011/65/EU; direct food-contact status is not required, but the finished article must still meet the factory’s standard for extractable heavy metals if the packed product is exported to markets that enforce packaging toxicity rules. The converted material feeds box liners for powdered detergent, dry chemical liners, and powder mix pouches in thicknesses from 30–70 µm.
| End-use zone | Standard / regulation | Test method / clause | Finished-article criterion |
|---|---|---|---|
| Thin-gauge T-shirt bag | GB/T 21661-2020 | Physical properties and dimensions | Gauge tolerance ±8% |
| Recycled-content grocery sack | EN 15343:2007 | Recycled content traceability | Traceability certificate |
| Heavy-duty refuse sack | EN 13592:2017 | Annex A test methods | Minimum tear/puncture from standard tables |
| Coextruded cereal liner | EU No 10/2011 | Annex I, overall migration | ≤ 10 mg/dm² |
| Powdered detergent box liner | REACH 1907/2006 | Annex XVII | SVHC ≤ 0.1 wt% |
Competitive TPC (Japan) HDPE KM698A prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
TPC (Japan) HDPE KM698A is a high-density polyethylene resin grade whose model designation places it in the high-molecular-weight extrusion segment of the TPC polyethylene portfolio. Independent public datasheet coverage for KM698A remains limited; therefore, the processing and performance values presented below are framed as class-typical envelopes for high-load melt flow HDPE extrusion resins and are not a replacement for the manufacturer’s certificate of analysis. Where a numerical range appears, it is derived from standardised polyethylene characterisation methods or published pipe-resin classification thresholds. The grade is supplied in pellet form for single-screw extrusion and, depending on the additive package, may be positioned for pressure pipe, corrugated drainage pipe, geomembrane sheet, or thick-walled industrial profiles. The main specification axes are density, high-load melt flow rate, short-term tensile yield stress, flexural modulus, notched impact resistance, and oxidative induction time.
When polyethylene extruders qualify a high-molecular-weight HDPE resin, the minimum property set normally includes density, high-load melt flow rate, oxidative induction time, and a short-term notched impact or tensile elongation value. For KM698A, the primary density classification falls within the HDPE band of 0.941–0.965 g/cm³ under ISO 1183-1:2019; the exact nominal target is lot-dependent. The high-load melt flow rate is determined at 190 °C with 21.6 kg using ISO 1133-1:2022, and high-molecular-weight extrusion grades commonly sit in the 6–12 g/10 min range when the product is designed for thick-wall pipe or profile output. Short-term tensile yield stress for such grades typically ranges from 22 MPa to 28 MPa when tested at 50 mm/min per ISO 527-2:2012, while flexural modulus may fall between 900 MPa and 1450 MPa under ISO 178:2019. The melt flow ratio derived from the 21.6 kg and 5 kg loads provides a practical index of molecular weight distribution; broad-distribution pipe grades usually show a melt flow ratio above 20, whereas narrow injection grades often remain below 15. Environmental stress crack resistance for pipe-grade HDPE is typically evaluated using bent-strip specimens under ASTM D1693 Condition B in 100% Igepal at 50 °C; class-typical values above 1000 h are not unusual for high-molecular-weight extrusion grades, but the result depends strongly on comonomer type and cooling history. Because outdoor pipe and geomembrane specifications require long-term thermal stabilisation, oxidative induction time at 210 °C is commonly specified at or above 20 min; a lower value in a lot certificate may indicate insufficient antioxidant retention and should be investigated before silo blending or conversion. Bulk density of HDPE pellets typically ranges from 0.55 g/cm³ to 0.60 g/cm³, and pellet dimensions of 3–5 mm are common; these values influence gravimetric feeder calibration and extruder conveying stability.
On a grooved-barrel single-screw extruder configured with a length-to-diameter ratio of 30:1 and a barrier-type screw, the rear feed zone is typically maintained at 50–70 °C to prevent pellet agglomeration, while the metering zone may reach 190–210 °C. The screen pack and breaker plate should be specified for a head pressure below 35 MPa; exceeding this limit on a 30:1 machine can amplify screw deflection and reduce screw life. Melt temperature measured at the die entry is commonly held between 200 °C and 230 °C, with a tighter upper boundary of 220 °C for natural material containing little carbon black. If output is pushed beyond the melt’s critical shear rate, sharkskin or cyclic melt fracture appears first at the die lip; the corrective action is to lower screw speed, raise die-head temperature by 3–5 °C, or adjust die land length. Drying is not normally required for HDPE pellets stored in sealed containers below 60% relative humidity, but surface condensation should be avoided because free moisture can create splay and microvoids. For pipes above 110 mm outside diameter, a grooved-barrel extruder with a screw diameter of 60–90 mm and a specific energy input of 0.25–0.30 kWh/kg is common; torque overload at the screw root may occur if the metering channel is deeper than 6 mm on a 60 mm machine. For thick cross-sections above 20 mm, cooling must be staged using a vacuum sizer and chilled-water spray at 15–20 °C to maintain dimensional stability without inducing skin-core differential shrinkage.
The main differentiation of KM698A in a polyethylene portfolio is its melt rheology and solid-state resistance relative to unimodal injection moulding grades, film grades, and bimodal pipe grades. Unimodal HDPE resins with similar density but lower molecular weight show higher 5 kg melt flow rates and narrower die swell, which improves injection moulding fill but reduces slow crack growth resistance in pressure pipe. Film-grade HDPE is typically polymerised to a lower 5 kg melt flow rate than injection grades and is formulated for high melt strength in thin-gauge bubble stability; however, its lower 21.6 kg high-load melt flow rate and narrower molecular weight distribution often make it unsuitable for very thick pressure-pipe walls. Bimodal high-density resins combine a high-molecular-weight fraction with a low-molecular-weight fraction, producing a broad molar mass distribution that suppresses melt fracture and improves notched pipe performance; their limitation is often higher head pressure and greater sensitivity to melt-temperature uniformity. For applications where the part is subsequently hot-plate welded or electrofusion-coupled, the low sag and controlled swell of the high-load melt flow class reduce bead irregularity; in contrast, injection-moulding HDPE often exhibits too much flow for large-diameter fused assemblies. The following table places the product class in a standardised comparison; exact KM698A lot values require the manufacturer’s certificate.
| Property axis | Test standard | KM698A segment | Unimodal injection HDPE | Bimodal PE100 pipe HDPE |
|---|---|---|---|---|
| Density | ISO 1183-1:2019 | 0.941–0.965 g/cm³ | 0.950–0.965 g/cm³ | 0.945–0.960 g/cm³ |
| High-load melt flow rate | ISO 1133-1:2022, 190 °C, 21.6 kg | 6–12 g/10 min | 8–30 g/10 min | 6–12 g/10 min |
| Melt flow ratio HLMI/MI2 | ISO 1133-1:2022 | 20–35 | 12–18 | 20–40 |
| Flexural modulus | ISO 178:2019 | 900–1450 MPa | 1000–1500 MPa | 900–1300 MPa |
| Oxidative induction time at 210 °C | ISO 11357-6:2018 | ≥20 min | 15–25 min | ≥20 min |
Pressure pipe service is the most demanding application for high-molecular-weight HDPE grades because the material is exposed to internal hoop stress, oxidative environments, and slow crack growth over decades. If KM698A is submitted for PE100-type qualification, the resin must pass the hydrostatic strength requirements of ISO 9080:2012 and be classified under ISO 12162:2009. A PE100 classification requires an extrapolated lower confidence limit of hydrostatic strength of at least 10 MPa at 50 years and 20 °C under the standard regression conditions. For pipe-grade HDPE, the notched pipe test described in ISO 13479 is used to assess slow crack growth; typical acceptance for a PE100 resin is failure time above 500 h at 80 °C and a hoop stress of 4.6 MPa, but exact requirements vary by national certification body. Hydrostatic design basis values are not resin properties alone: they are also influenced by pipe wall thickness, extrusion-induced orientation, and fusion-weld quality. The brittle-ductile transition in HDPE pipe failure is often shifted to longer times by reducing tie-chain entanglement loss during crystallisation; slow crack growth resistance is therefore sensitive to extrusion cooling rate, not solely to resin density. Therefore, a grade that passes the resin classification still requires pipe-level testing under ISO 4427 or DIN 8075 before commercial potable-water use. Published data for KM698A in this specific pipe-grade configuration is limited in independent databases, so qualification work should not rely on generic HDPE data.
In large-diameter pressure pipe extrusion, the dominant processing bottleneck is not melt temperature but radial thermal history during solidification. A 250 mm diameter pipe with a wall thickness of 22.7 mm may require a cooling length of 24–30 m to reduce the inner surface temperature below the crystalline solidification plateau while maintaining line speed. If the vacuum sizer pulls the pipe at rates that exceed the output of the grooved-barrel extruder, wall-thickness variation and residual stress increase; subsequent hydrostatic testing may show premature brittle failure at the pipe inner surface. The extruder head should be a spiderless spiral mandrel design with a mandrel temperature controlled separately from the outer die body to avoid local melt-flow differences between the pipe inner and outer walls. Melt fracture on the outer surface can be addressed by increasing die gap by 0.5–1.0 mm or by using a fluoropolymer processing aid at 200–500 ppm based on total throughput. These processing aids are generally compatible with HDPE but must be removed from any food-contact declaration unless specifically cleared under the relevant regional regulation.
Where KM698A is intended for potable water pipe, food-contact packaging, or geomembrane contact with drinking water, the compliance package must be verified against the current regulatory edition. High-density polyethylene manufactured by catalytic polymerisation of ethylene generally falls under FDA 21 CFR 177.1520(c) item 2.1 or 2.2, provided density and extractables limits are met. In the European Union, food-contact compliance is evaluated under EU No 10/2011 with overall migration limits, and the material must satisfy REACH annex entry restrictions if a substance is present above the relevant threshold. Electrical and electronic applications require RoHS Directive 2011/65/EU screening for lead, mercury, cadmium, hexavalent chromium, and polybrominated biphenyl ethers; typical HDPE lot certificates list these at or below the maximum concentration values of 0.1% by weight in homogeneous materials for lead and 0.01% for cadmium, though this must be confirmed by the supplier. The following compliance matrix is a checklist, not a certification:
| Requirement | Standard or regulation | Typical HDPE acceptance condition | KM698A verification requirement |
|---|---|---|---|
| Food-contact olefin polymer | FDA 21 CFR 177.1520(c) | Density ≥ 0.94 g/cm³ | Supplier certificate of analysis |
| EU food-contact overall migration | EU No 10/2011 | ≤ 10 mg/dm² total migration | Accredited test report |
| Potable water pipe classification | ISO 12162, ISO 9080 | PE100 or PE80 class | Pipe certification body report |
| Heavy metals in electronics | IEC 62321 | Pb ≤ 0.1%, Cd ≤ 0.01% | Analytical report |
| UV-stabilised outdoor service | ISO 4892-3 | No surface chalking after 4000 h | Weathering test report |
Compounding with carbon black or UV stabiliser masterbatch alters the melt rheology and the long-term oxidative performance of the base resin. For outdoor pipe or geomembrane applications, a carbon black masterbatch is typically added at 2.0–2.5 wt% to provide a dispersion level meeting ISO 4427 or ASTM D3350 cell classification requirements. The addition of an incompatible pigment or an amine-based additive can accelerate oxidative degradation and should be avoided unless the stabiliser package is explicitly designed for that synergy. Masterbatch addition at high dosing levels above 4.0 wt% may alter the high-load melt flow rate beyond the extrusion window and create die build-up on the mandrel. The final conversion on a grooved-barrel line should be preceded by a lot-test on a 30:1 single-screw extruder using the actual masterbatch and target throughput; published data for this specific configuration is limited, so the trial data serve as the lot-release reference.