    Specifications
    HS Code 659520
    Density 0.960 g/cm3
    Melt Flow Rate 8.0 g/10 min
    Tensile Strength At Yield 30 MPa
    Elongation At Break 500 %
    Flexural Modulus 1200 MPa
    Izod Notched Impact Strength 40 J/m
    Shore D Hardness 65
    Vicat Softening Temperature 125 °C
    Heat Deflection Temperature At 0 45 Mpa 80 °C
    Mold Shrinkage 1.5-2.0 %
    Water Absorption <0.01 %
    Melting Point 133 °C

    As an accredited TPC (Japan) HDPE KM693W factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing TPC (Japan) HDPE KM693W is supplied in 25 kg net bags, palletized; 1,000 kg jumbo bags are also available.
    Container Loading (20′ FCL) TPC (Japan) HDPE KM693W loaded in 20′ FCL: 25 kg bags, palletized, shrink-wrapped, stuffed, braced, and secured for sea transport.
    Shipping Shipping description: TPC (Japan) HDPE KM693W is a non-hazardous high-density polyethylene resin. It is typically packed in 25 kg bags or 500–1000 kg jumbo bags, palletized, stretch-wrapped, and shipped in dry containers. Keep dry, cool, ventilated, away from ignition sources and direct sunlight. No special hazardous-goods classification required.
    Storage Store TPC (Japan) HDPE KM693W in a cool, dry, well-ventilated warehouse away from direct sunlight, rain, heat, and ignition sources. Keep original bags closed, palletized, and protected from moisture, contamination, and excessive stacking. Maintain moderate temperature, avoid static buildup, and segregate from strong oxidizers. Follow local regulations and first-in-first-out stock rotation. Use appropriate PPE and avoid damaging packaging.
    Shelf Life No specific shelf life data available; stable under recommended cool, dry, well-ventilated storage away from sunlight and contaminants.
    Application of TPC (Japan) HDPE KM693W

    Industrial Packaging and UN-Certified Intermediate Bulk Containers

    For UN-certified industrial packaging, TPC (Japan) HDPE KM693W is processed on a monolayer accumulator-head extrusion blow molding line configured for parison programming; the programming points at the top, body, and bottom weld are set to compensate for parison sag, which becomes measurable after a drop time of 8–12 s. Melt temperature is maintained at 180–205°C, die gap at 1.2–2.0 mm, blow pressure at 0.6–0.8 MPa, and mold temperature at 10–25°C to control post-mold shrinkage. The accumulator head shot volume is matched to the part weight so that total cycle time is 120–180 s, and clamping force on the blow molds is maintained at 400–800 kN for 200 L drums to prevent flash at the parting line. The formulation additions are confined to a carbon black masterbatch let-down of 4–6 wt% from a 50 wt% carbon black masterbatch, yielding 2.0–2.5 wt% carbon black in the finished wall, plus hindered phenol antioxidant at 0.05–0.10 wt% and phosphite stabilizer at 0.05–0.10 wt%. Carbon black dispersion is checked by ISO 18553:2002, and environmental stress crack resistance is verified by ASTM D1693-15 Condition B; both tests are used because agglomerates and micro-defects at the pinch-off weld are the main initiators of drum sidewall fracture. Regulatory compliance is anchored to the UN Model Regulations ST/SG/AC.10/11/Rev.7 Chapter 6.1, ADR 6.1.5, the IMDG Code Part 6, ASTM D2561-17, and ISO 20848-1:2006. Finished parts are 200 L tight-head drums and 120 L open-head drums, plus 1000 L IBC inner bottles; the operational boundary is that post-consumer recyclate above 10 wt% reduces ESCR at the pinch-off weld and is not permitted in UN-certified hydrocarbon service.

    What Limits Permeation in Multi-Layer Fuel Tank Coextrusion?

    Multi-layer fuel tank lines running TPC (Japan) HDPE KM693W are constrained primarily by the thermal degradation limit of EVOH barrier resins, which forces the HDPE melt temperature window to remain between 190°C and 220°C; below this range, the tie-layer adhesive shows viscosity mismatch and produces interfacial instability, while above this range EVOH gels form and contaminate the conductive inner layer. A six-layer coextrusion die with spiral mandrel distribution is fed by extruders having L/D ratios of 25:1–30:1; parison programming maintains 2.5–4.0 mm wall thickness in the body and 3.5–6.0 mm at the weld pinch area, because permeation failure concentrates at the pinch-off. Layer distribution is controlled by gravimetric feeders on the tie-layer and barrier extruders; a deviation of ±0.5 wt% in EVOH layer mass is sufficient to shift permeation outside the specified limit. Formulation splitting is critical: the inner conductive layer carries 8–12 wt% conductive carbon black to prevent electrostatic accumulation, the outer layer contains 2.0–2.5 wt% carbon black or colorant, the adhesive tie layer is 1.5–3.0 wt% of total wall mass, and the EVOH barrier layer is 1.5–3.0 wt% of total wall mass to limit hydrocarbon permeation. After molding, tanks are trimmed, hole-cut, and leak-tested at 20–30 kPa for 60 s. Compliance is verified by ECE Regulation No. 34, FMVSS 301, and SAE J1737; production audit rejects tanks with permeation above 0.5 g·mm/m²·day at 40°C. Finished part types are 40–80 L gasoline and diesel fuel tanks, including saddle tanks and hybrid fuel reservoirs. The primary incompatibility is zinc stearate carry-over above 0.01 wt%, which can deactivate the EVOH barrier and cause delamination at the tie-layer interface.

    When Agricultural Chemical Packaging Requires a Barrier Layer

    On coextrusion blow molding lines dedicated to agrochemical packaging, TPC (Japan) HDPE KM693W is processed with a polyamide or EVOH barrier core because the filled products often contain xylene, cyclohexanone, or emulsifiable concentrates that plasticize monolayer HDPE. The parison is extruded at 185–205°C, with a die gap of 1.5–2.5 mm and a drop time of 4–8 s; drop times beyond 8 s cause the barrier core to thin at the bottom weld and create permeation channels. In a three-layer bottle, the layer distribution is maintained at 70–75 wt% HDPE skin, 3–5 wt% polyamide or EVOH barrier, and 1–2 wt% tie-layer adhesive, with the remainder as regrind incorporated into the outer skin. Additives include 0.2–0.4 wt% hindered amine light stabilizer, 1.5–2.5 wt% carbon black in the outer layer, and 0.05–0.10 wt% processing stabilizer; fillers such as calcium carbonate are excluded because they reduce impact strength at the weld line. Post-mold handling includes deflashing of the pinch-off tail and a 24 h ambient conditioning period before xylene permeation testing, because barrier property equilibrium requires crystallinity stabilization. Compliance is governed by the UN Model Regulations ST/SG/AC.10/11/Rev.7, ADR Chapter 6.1, and 40 CFR Part 156 for pesticide container design in the United States; barrier performance is validated by xylene permeation testing under ASTM D2684-18 or equivalent. Finished products are 1 L, 5 L, 10 L, and 20 L containers marked UN 3H1 or UN 31H1, with leak testing at 20 kPa internal pressure before filling.

    Marine Float Blow Molding Exposes KM693W to Prolonged Thermal Oxidation

    Because marine float walls exceed 4 mm and cooling cycles extend beyond 180 s, TPC (Japan) HDPE KM693W is subjected to prolonged thermo-oxidative conditions during parison formation, and the stabilizer package must be adjusted accordingly. The formulation for UV-stabilized service includes 2.0–2.5 wt% carbon black, 0.20–0.50 wt% hindered amine light stabilizer, 0.10–0.30 wt% UV absorber, and 0.05–0.15 wt% phenolic antioxidant; when a non-black float is specified, carbon black is replaced by titanium dioxide at 1.0–2.0 wt% and the hindered amine light stabilizer loading is raised to 0.30–0.50 wt%. The blow molding process uses an accumulator head with a melt temperature of 180–200°C, mold temperature of 5–15°C to increase skin crystallinity, and a post-mold annealing step at 80°C for 4 h to relieve bosses and insert stresses. Mold closing speed is reduced to 0.3–0.5 m/s during the final 20 mm of travel to avoid knit-line stress at insert bosses. Weathering performance is assessed by ASTM D4329-21 fluorescent UV exposure; published data for this specific configuration is limited, so tensile elongation retention above 50% after 3000 h is adopted as a batch release criterion from HDPE outdoor exposure data rather than a supplier-reported marine float datasheet. Impact resistance is verified by ISO 8256 instrumented puncture. Finished parts are mooring buoys, fenders, and modular floating dock cells with wall thickness not less than 4 mm at any point.

    In twin-parison clamshell molding of industrial pallets, TPC (Japan) HDPE KM693W is processed within a narrow window because two parisons are extruded simultaneously; any length mismatch between the parisons produces rib fusion defects that can reduce racking strength by more than 30%. The extrusion blow molding machine is fitted with a twin-parison accumulator head, L/D of 25:1–30:1, melt temperature of 185–205°C, and mold closing force of 800–1500 kN; internal air pressure of 0.5–0.7 MPa is applied after the mold closes to fuse the upper and lower decks at the rib intersections. Cycle time for a 1100×1100 mm pallet is 180–240 s, with mold cooling at 10–20°C; demolding before core solidification creates deck bowing. The formulation contains 2.0–2.5 wt% carbon black, 0.10–0.20 wt% hindered phenol antioxidant, and 0.15–0.30 wt% hindered amine light stabilizer; no glass fiber or mineral filler is used because filler reduces environmental stress crack resistance in cold-storage conditions. Load performance is tested under ISO 8611-1:2021, dimensional conformity under ISO 6780:2003, and hygienic food-contact pallets are validated under FDA 21 CFR 177.1520 and EU Regulation (EU) No 10/2011. Finished product types include rackable 1100×1100 mm pallets, 1200×1000 mm export pallets, and hygienic closed-deck pallets for meat and dairy cold chains. Regrind content above 30 wt% is the operational limit because melt pressure variation and rib void formation increase on production-scale accumulator machines.

    Within the 20–60 L potable water container segment, TPC (Japan) HDPE KM693W is processed on single-station blow molding machines with a melt temperature of 180–200°C, a parison die gap of 1.0–1.8 mm, and blow pressure of 0.6–0.7 MPa; the mold is cooled to 10–20°C to limit warpage of flat side panels. The formulation is restricted to food-contact-approved additives: 0.05–0.10 wt% hindered phenol antioxidant, 0.05–0.10 wt% phosphite stabilizer, and, where a blue tint is required, 0.5–1.0 wt% phthalocyanine blue masterbatch. Carbon black is excluded because extraction testing under EU Regulation (EU) No 10/2011 becomes more complex, and the container must meet an overall migration limit of 10 mg/dm². The container wall is designed to a minimum thickness of 0.8 mm at the thinnest point, and the pinch-off tail is trimmed hot to prevent a notch that would initiate stress cracking under repeated filling. Drop testing is conducted at 5°C with filled containers from 1.2 m onto a concrete floor; the acceptance criterion is no leakage after three drops. Potable water contact compliance is established under FDA 21 CFR 177.1520, EU Regulation (EU) No 10/2011 Annex I, and NSF/ANSI/CAN 61. Finished products are 20 L carboys, 40 L portable water storage containers, and 60 L dispenser bottles. The material should not be used for continuous hydrostatic pressure service above 50°C, because creep resistance declines and the base pinch-off may distort.

    Free Quote

    Competitive TPC (Japan) HDPE KM693W prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    TPC (Japan) HDPE KM693W is a high-density polyethylene grade referenced in conversion specifications for close-tolerance extrusion blow moulding, thick-sheet extrusion, and industrial container production. The grade designation is supplier-controlled, and the suffix W does not have a universal ISO meaning; lot-level properties must therefore be taken from the manufacturer’s current product datasheet and certificate of analysis. Published data for this specific configuration is limited, so the values below are HDPE class-level ranges for preliminary specification only, not replacements for KM693W lot certificates. The material falls within the thermoplastics classification framework of ISO 17855-1 and JIS K 6922-1. For unmodified HDPE, density is classed between 0.940 g/cm³ and 0.970 g/cm³. In blow-moulding and high-melt-strength film grades, the melt mass-flow rate at 190 °C and 2.16 kg is typically below 1.0 g/10 min; injection-moulding HDPE grades of similar density may exceed 20 g/10 min.

    Because the conversion behaviour of HDPE KM693W cannot be inferred from a single melt flow rate, the following methods should be applied during lot acceptance: melt mass-flow rate by ISO 1133-1 or ASTM D1238, density by ISO 1183-1 or ASTM D1505, tensile yield stress and elongation by ISO 527-2 or ASTM D638, flexural modulus by ISO 178, and impact resistance by ISO 179-1 or ASTM D256. Class-level HDPE tensile yield stress is commonly between 20 MPa and 32 MPa, while flexural modulus is commonly between 800 MPa and 1,600 MPa. The actual values for KM693W may sit at specific points within these ranges and should be verified for structural calculations.

    The primary differentiation of KM693W from narrow-molecular-weight-distribution injection-moulding HDPE is expected in its shear-thinning response and low-shear melt strength. Dynamic frequency sweeps under ISO 6721-10 provide a more useful specification than melt flow rate alone: a high-melt-strength grade displays a lower crossover frequency and a longer terminal relaxation time. On a capillary rheometer operated at 190 °C with a 30/1 die, blow-moulding HDPE shear viscosity at 100 s⁻¹ is commonly above 1,000 Pa·s, whereas injection-moulding grades may fall below 200 Pa·s at the same rate. This difference determines die swell, parison sag resistance, and the stability of long parisons in large-part blow moulding.

    What Limits the Processing Window in Extrusion Blow Moulding of KM693W?

    The limiting factor is not usually the extruder drive but the parison melt strength and the thermal-oxidative stability of the stabiliser package. On reciprocating-screw blow moulders with screw diameters from 60 mm to 90 mm and L/D ratios of 24:1 to 36:1, the feed zone is often maintained below 180 °C, the compression zone between 180 °C and 210 °C, and the die head between 190 °C and 220 °C. Melt temperature at the die entry should remain below 240 °C for general-purpose HDPE; above this temperature, antioxidant consumption accelerates and gel particles may appear in the wall. Residence time at maximum melt temperature should be kept below 5 min during stoppages. Breaker-plate pressure in high-molecular-weight HDPE typically falls between 15 MPa and 35 MPa. If pressure exceeds 40 MPa, a blocked screen pack, undersized die gap, or an overshear condition should be suspected.

    Mould temperature for blow moulding is usually held between 8 °C and 20 °C to control cycle time; for sheet extrusion, roll-stack temperatures are adjusted to 70–95 °C to reduce differential crystallinity and warpage. Cooling time for thick-wall HDPE containers increases with wall thickness squared, making mould-channel Reynolds numbers and coolant flow rates more important than coolant temperature alone. In a narrow-MWD HDPE, surface melt fracture onset can shift with melt-temperature changes of only ±5 °C; broader-MWD grades such as high-melt-strength blow-moulding types generally show a more gradual onset. The die gap should be set in relation to parison length and swell: excessive die gap widens the parison wall and increases sag, while an undersized gap can produce melt fracture at the lip.

    Batch-to-batch variation in granule size and stabiliser content should be monitored by bulk density and additive extraction. Blow-moulding operations commonly report that lot-to-lot melt-pressure variation above ±5 % at fixed screw speed indicates a change in molecular weight distribution. Under such conditions, barrel profile, die gap, or screw speed should be adjusted only after confirming that the material was not contaminated with a higher-melt-flow HDPE. For pigmented KM693W, high-shear dispersion of organic pigments in a twin-screw compounding line with L/D ratios of 32:1 or higher is required before letdown; inadequate dispersion can create specks and reduce environmental stress crack resistance.

    HDPE KM693W generally does not require pre-drying unless surface condensation has occurred. If silo storage cycles below dew point at relative humidity above 60 %, hopper heating at 70–80 °C for 2 h is sufficient to remove surface moisture. Drying temperatures above 90 °C should be avoided because pellet surface tack may develop. Avoid continuous exposure to strong oxidising acids above 60 °C and to chlorinated solvents. Amine-based antistatic concentrates should not be combined with KM693W unless stress-crack resistance is validated under ASTM D1693, because amine antistats can accelerate environmental stress cracking in thin-wall HDPE containers.

    When Aromatic Hydrocarbon Contact Requires Barrier-Grade Validation

    When the intended application involves agricultural chemicals, paint thinners, fuel components, or aggressive detergent systems, HDPE KM693W must be validated against the specific chemical mixture. High-density polyethylene is resistant to aqueous salt solutions and many dilute acids, but aromatic hydrocarbons and chlorinated solvents lower the critical stress for environmental stress cracking. Stress-crack resistance should be tested under ASTM D1693 condition B or C and ISO 22088-3. The flexural modulus of HDPE decreases as comonomer addition reduces crystallinity; therefore a high-ESCR inner layer or cap layer may be required if the outer layer is optimised for top-load strength and stacking rigidity. Barrier performance against hydrocarbons is not a strength of unmodified HDPE: permeation rates for aromatic and aliphatic hydrocarbons are substantially higher than those of nylon or fluorinated multilayer structures. If the product is intended for fuel-system components, KM693W should be considered only after permeation testing according to the relevant SAE or OEM specification, because a generic HDPE datasheet will not supply the required hydrocarbon permeation coefficient.

    Compared with isotactic polypropylene, HDPE has lower heat deflection temperature under ISO 75-2 method B at 0.45 MPa, often below 80 °C, while PP homopolymer may exceed 100 °C. However, HDPE typically retains impact resistance at low temperatures below -40 °C and may be preferred for freezer-grade containers and cold-climate service. Against linear low-density polyethylene, HDPE offers higher modulus and lower gas permeability but lower dart impact resistance and tear resistance. Against medium-density polyethylene, HDPE provides higher top-load strength and better chemical resistance, but reduced slow-crack-growth resistance in some pipe-like geometries. KM693W should therefore be differentiated from other HDPE products by its intended melt-strength class and by the supplier’s lot-specific density, not by the HDPE label alone.

    Compliance Verification Matrix for Food-Contact and Automotive Under-Hood Conditions

    Specification review map for TPC (Japan) HDPE KM693W lot acceptance
    PropertyMethodClass-level HDPE rangeProcessing implication
    DensityISO 1183-1 / ASTM D15050.940–0.970 g/cm³Higher density raises modulus and barrier but reduces impact and ESCR
    Melt flow rateISO 1133-1 / ASTM D12380.03–1.0 g/10 min for blow-moulding classLower MFR increases melt strength but raises torque
    Tensile yield stressISO 527-2 / ASTM D63820–32 MPaUsed for top-load and burst calculations
    Flexural modulusISO 178800–1,600 MPaStiffness for stacking and hoop rigidity
    ESCRASTM D1693 / ISO 22088-3Class-dependent; request lot F50 valueCritical for detergent and surfactant packaging
    Vicat softening temperatureISO 306 method A50120–130 °C class rangeShort-term heat exposure benchmarks
    Regulatory documentation matrix for TPC (Japan) HDPE KM693W
    Legislation/standardReferenceRequired supplier documentationTypical boundary
    EU chemical registrationREACH 1907/2006Safety data sheet and Article 33 declarationSVHC content below 0.1 % w/w per article
    EU hazardous substancesRoHS 2011/65/EU Annex IISupplier statementLead 0.1 %; cadmium 0.01 %; mercury 0.1 %; hexavalent chromium 0.1 %
    US food contactFDA 21 CFR 177.1520Extraction testing or supplier letterOlefin polymer specification for intended food type
    EU food contactEU 10/2011Migration testingOverall migration 10 mg/dm² or 60 mg/kg
    Plastics classificationISO 17855-1 / JIS K 6922-1Designation blockPE-HD classification

    On production-scale accumulator-head machines, defects specific to HDPE blow moulding include parison curvature, die lines, and pinch-off weld weakness. Die lines can arise from degraded polymer buildup at the die lip, causing localised melt fracture. Weld-line strength in the pinch-off area is governed by melt temperature, mould closing speed, and pinch design; low melt temperature or excessive parison length can produce a cold weld. In thick-sheet extrusion, poor roll cooling or excessive roll gap can induce warpage because differential crystallinity develops across the sheet thickness. These defects are not unique to KM693W, but they become more visible in high-density grades with high melt strength because parison sag is reduced and die-swell variation is more readily seen in thick-wall parts.

    For food-contact and automotive under-hood uses, additive migration kinetics in the polymer matrix must be considered. Nonylphenol-free stabilisers and low-migration organoleptic-neutral additives are relevant for food-contact HDPE. When recycled content is introduced, the resulting melt flow stability, odour, and impact properties must be revalidated because post-consumer HDPE may reduce drop impact and increase lot-level variability. The material should not be assumed to comply with food-contact requirements solely on the basis of the HDPE classification; supplier documentation must confirm the specific grade, additive package, and compliance boundary.

    In end-use service, HDPE KM693W should not be specified for continuous exposure to strong oxidising acids above 60 °C, aromatic solvents, or chlorinated hydrocarbons without testing. For outdoor applications, UV resistance must be confirmed; the W suffix does not automatically indicate carbon black or hindered amine light stabiliser content. Surface cracking in detergent reservoirs, coolant expansion tanks, and agricultural containers is a more reliable indicator of ESCR deficiency than tensile elongation at yield. The appropriate test is therefore ASTM D1693 or ISO 22088-3 under the end-use chemical environment, not a general-purpose immersion test.

    The difference between KM693W and other HDPE grades is also expressed in processing equipment selection. High-melt-strength HDPE requires a screw with deeper feed-channel geometry and a compression ratio suitable for high-molecular-weight material, typically between 2.0:1 and 3.5:1. A shallow, high-compression screw designed for injection moulding can overheat the material and generate gel particles. Accumulator-head machines with volumetric shot capacity above 10 L are commonly used for large industrial containers; the melt must have adequate sag resistance over the open drop time. If the parison elongates more than 10 % before mould closing, the grade may be unsuitable for the part geometry, regardless of its density and melt flow rate.

    The value of KM693W in a product specification depends on its match to the conversion route. For thick-wall containers requiring high top-load strength, stiffness, and chemical resistance, an HDPE grade with class-level density above 0.945 g/cm³ and low melt flow rate is typically considered. For thin-wall packaging requiring high speed and low melt temperature, a higher-melt-flow HDPE may be preferable. The selection should be confirmed through rheological testing, ESCR testing, and full-scale trials on the intended accumulator-head or continuous-extrusion machine. Because grade-specific KM693W data are supplier-controlled, all numerical specification limits should be written against the certificate of analysis rather than against class-level HDPE tables.

    Top