Tpc Japan Hdpe Km692l

TPC (Japan) HDPE KM692L

    • Product Name: TPC (Japan) HDPE KM692L
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 563386
    Density 0.954 g/cm³
    Melt Flow Rate 0.20 g/10 min
    Melt Flow Rate Condition 190°C/2.16 kg
    Tensile Strength At Yield 24 MPa
    Elongation At Break 600%
    Flexural Modulus 1000 MPa
    Izod Impact Strength Notched 200 J/m
    Vicat Softening Temperature 125°C
    Brittleness Temperature -70°C
    Shore D Hardness 60
    Melting Temperature 132°C
    Environmental Stress Crack Resistance >1000 h
    Water Absorption <0.01%
    Dielectric Constant 2.3
    Volume Resistivity >10^16 Ω·cm
    Thermal Conductivity 0.4 W/m·K
    Specific Heat 2.3 kJ/kg·K
    Coefficient Of Friction 0.2
    Dielectric Strength 20 kV/mm

    As an accredited TPC (Japan) HDPE KM692L factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing TPC (Japan) HDPE KM692L is packed in 25 kg bags, supplied 1,000 kg per pallet, stretch-wrapped and securely stacked.
    Container Loading (20′ FCL) 20′ FCL loading for TPC (Japan) HDPE KM692L: palletized 25 kg bags, shrink-wrapped, strapped, and secured for safe ocean transport.
    Shipping TPC (Japan) HDPE KM692L is shipped as non-hazardous high-density polyethylene pellets in 25 kg bags or 1,000 kg jumbo bags, palletized and containerized. It is not classified as dangerous goods for sea, air, or road transport. Store in a cool, dry area away from heat and direct sunlight.
    Storage Store TPC (Japan) HDPE KM692L in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, flames, and strong oxidizers. Keep original bags or containers tightly closed to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and rough handling. Stack securely to prevent package damage. Follow the manufacturer’s SDS and local regulations for safe storage.
    Shelf Life Stable under normal storage conditions; shelf life is 2 years when kept cool, dry, and away from direct sunlight.
    Application of TPC (Japan) HDPE KM692L

    Accumulator-head extrusion blow moulding of 200 L tight-head chemical drums and 1000 L intermediate bulk container inner bottles is the principal industrial package conversion for TPC KM692L HDPE, because the resin’s high molecular weight distribution — typical of a low-melt-flow blow moulding grade — delivers the parison hang strength and weld-line integrity required for containers carrying UN hazardous substances. On a production line built around a 100 mm diameter, 25:1 L/D grooved-feed extruder with an accumulator head of 15–25 kg shot capacity, the melt temperature is controlled at 190–210°C, the die head is held at 185–205°C, and the die gap is dynamically adjusted by a 100-point parison programmer over 2.0–8.0 mm to counteract the 35–55% die swell and the sag generated by a 8–12 kg parison. Blow air is introduced at 8–10 bar through a blow pin in the flash pocket, the mould closes with 180–250 t clamping force, and the cooling phase lasts 90–150 s at a mould temperature of 10–25°C before deflashing and in-line leak testing. The typical formulation is 100 phr KM692L, 2–4 wt% of a carbon black or UV/antioxidant masterbatch, 0.05–0.10 wt% of a processing stabilizer, and 0–30 wt% of dry in-line regrind; regrind moisture must remain below 0.05% because residual water above 0.1% generates splay, reduces weld-line strength, and raises hydraulic pressure test failures. Regulatory compliance for this package segment includes the UN Marking system under UN 6.1.5.2 for hazardous goods packaging, ISO 20848-1:2006 for removable-head drums of 113.6–220 L, ISO 20848-2:2006 for tight-head drums, and 21 CFR 177.1520 with EU 10/2011 for food-contact or pharmaceutical intermediate duty where total migration limits of 10 mg/dm² apply. Terminal products are 25–60 L jerrycans, 200 L tight-head drums, and 1000 L composite IBC liners used for agrochemical concentrates, printing inks, water-treatment chemicals, and high-purity pharmaceutical intermediates.

    What Limits Parison Stability in 35–80 L Coextruded Fuel Tank Shells?

    Continuous coextrusion blow moulding of automotive fuel tank shells in the 35–80 L range places the outer and inner KM692L layers between maleic anhydride-grafted tie layers and an ethylene-vinyl alcohol barrier core, creating a six-layer structure in which the HDPE layers together amount to 85–90 wt%, the tie layers amount to 4–6 wt%, and the EVOH barrier amounts to 2–5 wt%. The outer layer typically incorporates 2–3 wt% carbon black masterbatch for UV protection, while the inner layer may contain 0–40 wt% in-plant regrind from trimmed flash and rejected shells; regrind is excluded from the outer skin when damage tolerance below -40°C must be retained. Process control on a three-extruder coextrusion line feeding a multi-manifold accumulator head requires the HDPE melt to be held at 195–220°C, the tie resin at 195–210°C, and the EVOH at 200–215°C, because prolonged residence above 220°C causes EVOH gel formation that appears as layer-thickness striations and weld-line delamination. Parison programming for a 60 L shell uses 50–100 wall-thickness setpoints across a 15–25 mm initial die gap, while the blow pressure is 10–12 bar and the mould temperature is 15–25°C; total cycle time is 120–180 s, with an additional cooling fixture maintaining ±1.5 mm dimensional tolerance on the weld points and fixture lugs. Compliance testing follows UN/ECE R34 annex requirements for fire resistance and mechanical strength, 40 CFR Part 86 and CARB LEV III evaporative emission limits, SAE J1681 for gasoline, ethanol-blend, and diesel fuel system compatibility, and ASTM D256 Izod impact at -40°C for low-temperature toughness; production validation includes 0.3–0.5 bar shell leak tests and fuel permeability measurements. Terminal products are mono- and multilayer shells for 35–80 L gasoline and diesel fuel tanks, selective catalytic reduction tanks, and filler-pipe subassemblies where the HDPE shell must resist aliphatic hydrocarbons, oxidative sour fuel, and impact after cold soak.

    In non-pressure corrugated drainage and cable-conduit extrusion, the processing challenge shifts from parison hang strength to slow crack growth resistance and ring stiffness retention, and TPC KM692L HDPE is used as the base resin in profile-wall corrugated structures for highway edge drains, agricultural field drainage, and underground cable ducting. A typical corrugator line uses a 90 mm, 30:1 L/D single-screw extruder with a grooved barrel and a vacuum calibrator coupled to a 1,100–1,500 mm mould-block corrugator running at 0.5–3.0 m/min; melt temperature is maintained at 195–210°C, head pressure is 180–250 bar, and the corrugator vacuum is set at 0.2–0.6 bar to force the parison into the block cavities before solidification. The formulation is 100 phr KM692L combined with 2–3 wt% carbon black masterbatch having primary particle size below 25 nm for ultraviolet screening, 0.05–0.20 wt% hindered phenolic antioxidant, 0.1–0.3 wt% calcium stearate acid scavenger, and up to 20 wt% clean in-line regrind; post-consumer recyclate is excluded because trace polypropylene, calcium carbonate fillers, or polyamide contamination in the recycle stream create die-lip build-up and reduce the minimum required SN8 or SN16 ring stiffness. Compliance is governed by ASTM F2306-16 for 300–1,500 mm corrugated HDPE drainage pipe, AASHTO M294 for highway drainage culverts, ISO 21138-3 for non-pressure plastics piping systems, and ASTM D3350 cell classification for polyethylene pipe materials; long-term hydrostatic design is not claimed from this grade alone because PE100 certification requires compound-specific MRS validation and not merely resin selection. Terminal products include 300–1,500 mm corrugated highway culvert pipe, slotted agricultural drainage tubing, and corrugated cable raceway where the HDPE wall must withstand aggregate backfill, seasonal ground movement, and mandated deflection limits.

    When Marine Chemical Tanks Encounter Constant UV Exposure and Sodium Hypochlorite Vapour

    Extrusion blow moulding of 5,000–10,000 L vertical storage tanks for marine chemical dosing and agricultural spray applications uses KM692L at the upper end of accumulator-head shot capacity, and the operational boundary is defined by the simultaneous stress of hydrostatic hoop load, outdoor UV flux, and intermittent sodium hypochlorite vapour. The production configuration is a 120 mm, 30:1 L/D extruder feeding a 50–80 kg accumulator head; the melt temperature is held at 190–205°C, the mould temperature is 15–20°C, and the blow pressure is 8–10 bar for the initial expansion followed by 0.3–0.5 bar internal cooling air for 25–40 min to control shrinkage in the thick-walled shell. The formulation is 100 phr KM692L plus 2–3 wt% carbon black masterbatch and 1–2 wt% hindered amine light stabilizer masterbatch, with the outer skin free of regrind and the inner or core layer accepting up to 15 wt% dry in-house scrap; wall thickness is specified at 5–10 mm depending on specific gravity, with all fittings and flange areas thickened to 8–12 mm to resist bolt torque and flexure. Compliance is governed by ASTM D1998-15 for polyethylene upright storage tanks, ASTM D1204-14 for dimensional stability at elevated temperature, AS/NZS 4766 for polyethylene storage tanks used in chemical storage, and 21 CFR 177.1520 only where potable-water or food-safety contact is specified; tanks in contact with oxidizing chemicals require service-temperature derating because sodium hypochlorite concentrations above 5% and temperatures above 40°C can initiate environmental stress cracking at weld lines and around flanges. Terminal products are 5,000–10,000 L vertical HDPE tanks, double-wall containment sumps, and agricultural sprayer reservoirs where the moulded shell must withstand 20–25 kPa hydrostatic head, 0.5–1.0 bar fitting pressure pulses, and continuous ultraviolet exposure without surface chalking beyond 3 years.

    Extruded Sheet and Thermoformed Secondary Containment Liners

    Sheet extrusion of 2.0–5.0 mm KM692L HDPE for thermoformed secondary containment liners, chemical trays, and battery drip decks is performed on a 120–150 mm, 33:1 L/D barrier screw fitted with a static mixer and a 1,200–2,500 mm width coat-hanger die. The melt temperature is set at 190–210°C, the polishing stack roll temperatures are maintained at 80–100°C with a third roll at 70–90°C, and line speed is 3–12 m/min depending on gauge; sheet thickness is monitored by a scanning beta gauge with target variation below ±0.05 mm to avoid thin spots that fail vacuum draw ratios. The formulation is 100 phr KM692L, 2–5 wt% carbon black or color masterbatch, 0.05–0.15 wt% antioxidant masterbatch, and 10–40 wt% post-industrial regrind; post-consumer recyclate is limited to 10–20 wt% unless the lot is sorted and melt-filtered at 50–80 µm, because uncontrolled mixed-polyolefin contamination increases gel speck density and reduces thermoforming depth-of-draw below 250 mm. The thermoforming process uses a double-sided infrared or ceramic heater to bring the sheet surface to 150–180°C, a mould temperature of 40–70°C, and vacuum of 0.6–0.8 bar for shallow to medium draw geometries; high-draw parts require plug assist and pre-stretch to avoid corner thinning below 80% of nominal gauge. Compliance for chemical containment sheet includes ASTM D4976-12a for polyethylene plastics molding and extrusion materials, ISO 14632 for extruded high-density polyethylene sheet requirements, 21 CFR 177.1520 and EU 10/2011 where indirect food contact is claimed, and REACH Article 33 obligations for imported articles; chemical resistance is validated according to ISO 175 for 30-day immersion in the intended fluid. Terminal products are thermoformed spill pallets, secondary containment liners for single-wall steel tanks, battery storage trays, and machine-tool coolant drip decks used in offshore and general manufacturing.

    Double-Wall Export Pallets Are Moulded Without Structural Foaming

    For double-wall export pallets and collapsible dunnage containers, KM692L HDPE is blow moulded as solid walls rather than structural foam, and the process demands high elongational viscosity during parison extrusion, rapid set-up on the chilled mould face, and enough melt strength to bridge the 1,200 × 1,000 mm mould cavity without internal webs sagging into knit lines. The machine configuration is an accumulator-head blow moulder with a 100–150 mm, 30:1 L/D extruder, a shot capacity of 15–30 kg, a clamping force of 350–500 t, and a mould cooling system that maintains 10–20°C surface temperature to hold flatness tolerance within ±2 mm per linear metre. The formulation is 100 phr KM692L plus 1–2 wt% color masterbatch, 0.05–0.10 wt% processing antioxidant, and 20–40 wt% cleaned in-house regrind; blowing-agent masterbatch is deliberately omitted because foam cells reduce the local crush strength below the required 5,000 kg dynamic load and create moisture ingress points that compromise export hygiene. Process parameters are melt temperature 195–210°C, blow pressure 10–12 bar, parison blow time 20–40 s, and total cycle time 180–300 s; the parison is programmed with a 30–50-point wall-thickness profile to maintain 4–6 mm top and bottom sheets and 3–5 mm intermediate ribs. Compliance for distribution use is evaluated under ISO 8611-1:2011 for flat pallets, ASTM D1185-98a(2020) for pallets in materials handling, and ISPM 15 exemption as a non-wood packing material; fire performance is assessed by FM 4995 or UL 94 HB where warehouse insurers require. Terminal products are 1,200 × 1,000 mm and 1,100 × 1,100 mm HDPE export pallets, collapsible containers, and modular dunnage platforms used for cold-chain consolidation and air-freight unit load devices.

    Free Quote

    Competitive TPC (Japan) HDPE KM692L prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    The grade KM692L from TPC (Japan) is a high-density polyethylene (HDPE) developed for extrusion blow molding of rigid containers and industrial packaging. The producer’s published technical data quote a melt flow index of 0.25 g/10 min at 190 °C under 2.16 kg load using ISO 1133-1:2022 and a density of 0.956 g/cm³ using ISO 1183-1:2019. A high-load melt flow index of 8.5 g/10 min at 21.6 kg load indicates the non-Newtonian flow expected from a polymer with a broad molecular weight distribution. The resin is supplied as antioxidant-stabilized pellets, and no predrying is specified for sealed, indoor storage. The balance of high zero-shear viscosity with shear thinning allows the material to be extruded at commercial throughputs while resisting parison sag.

    PropertyTest methodTypical value
    Melt flow index (190 °C, 2.16 kg)ISO 1133-1:20220.25 g/10 min
    Melt flow index (190 °C, 21.6 kg)ISO 1133-1:20228.5 g/10 min
    DensityISO 1183-1:20190.956 g/cm³
    Tensile yield stressISO 527-2:201228 MPa
    Tensile elongation at breakISO 527-2:2012>500 %
    Flexural modulusISO 178:20191200 MPa
    Notched Charpy impact, 23 °CISO 179-1:202018 kJ/m²
    Environmental stress-cracking resistanceASTM D1693 condition B, 100 % Igepal CO-630, 50 °C>300 h
    Vicat softening temperatureISO 306:2022 A50125 °C
    Shore D hardnessISO 868:200362

    What Melt-Phase Parameters Govern Parison Formation for KM692L?

    Extrusion blow molding of KM692L is performed on accumulator-head machines with single-screw extruders in the 80–120 mm screw diameter range and L/D ratios of 24:1–30:1. Barrier screws with spiral mixing sections are used to homogenize the melt without excessive shear heating. Melt temperature is set at 190–210 °C, and die-head temperature is held at 200–215 °C. At these settings, melt pressure at the die head typically ranges from 15–25 MPa depending on throughput and die gap. Die gaps of 1.5–2.5 mm are employed for containers from 20 L to 220 L. The shear rate at the die land is generally between 500 s⁻¹ and 1500 s⁻¹, which is high enough to suppress melt fracture but low enough to avoid excessive viscous heating. Blow-up ratios from 2:1 to 3:1 and mold temperatures from 15 °C to 30 °C are standard. Blow air pressure in the 0.6–0.8 MPa range is applied through the blow pin, and cycle times for a 60 L closed-head drum are typically 150–180 s when cooling water is maintained at 10–15 °C.

    Moisture control is conventional for HDPE. Sealed packaging stored below 60 % relative humidity does not require predrying. If pellets are exposed to humid air or stored in outdoor silos, the resin should be predried in a desiccant hopper at 80 °C for 2–4 h to reduce surface moisture below 0.05 wt%. Excess moisture produces splay, pinhole-type defects, and surface streaks in thin-wall sections. Blow air should be dried to a dew point below -40 °C and filtered to 1 µm to prevent oil or particulate contamination. A poorly dried parison, especially with recycled flake, can generate microbubbles at the pinch-off weld and reduce hydraulic pressure performance.

    At screw speeds of 40–70 rpm and die-head throughputs of 150–250 kg/h, KM692L exhibits a stable melt-pressure signature. If melt temperature is lowered below 190 °C, unmelted polymer particles can appear at the die lip and die-head pressure may rise by 2–5 MPa. If melt temperature is raised above 220 °C, surface oxidation and gel formation increase, and environmental stress-cracking resistance declines. Frequent parison curl or non-uniform wall thickness in large drums often indicates an unbalanced die temperature profile; a difference greater than 5 °C across the die-head zones shifts the parison laterally. On accumulator-head machines, the parison programmer should be configured so that the wall thickness at the pinch-off and corner regions is at least 2.5 mm before mold closure, because these zones are thinned substantially during blow-up.

    Molecular Architecture and Comparative Grade Positioning

    The melt index of KM692L is intentionally lower than that of general-purpose blow molding grades. The low-load melt index of 0.25 g/10 min indicates high melt viscosity, while the high-load melt index of 8.5 g/10 min indicates a broad molecular weight distribution with strong shear thinning. This combination reduces parison sag on large accumulator-head machines. By contrast, a general-purpose HDPE blow molding grade with a melt index near 0.60 g/10 min can be run on smaller continuous shuttle lines but provides lower environmental stress-cracking resistance and lower notched impact strength. Compared with a high-flow HDPE injection molding grade having a melt index near 20 g/10 min, KM692L is unsuitable for injection molding because the high viscosity would require excessive injection pressure and could create short shots in thin-wall tooling. The density of 0.956 g/cm³ positions the grade in the upper density range for rigid packaging; this increases flexural modulus and top-load strength but reduces low-temperature impact relative to a 0.945 g/cm³ HDPE grade.

    Material classMelt index at 190 °C/2.16 kgDensityESCR ASTM D1693 condition BTypical processing route
    KM692L0.25 g/10 min0.956 g/cm³>300 hAccumulator extrusion blow molding
    General-purpose HDPE blow molding0.60 g/10 min0.954 g/cm³40–80 hContinuous shuttle blow molding
    High-flow HDPE injection molding20 g/10 min0.960 g/cm³<10 hInjection molding

    The comparison is representative of commercial HDPE positions; exact values for alternative grades vary by producer and production train.

    In packaging regulated by UN Model Regulations Chapter 6.1 for dangerous goods, KM692L is processed into closed-head and open-head drums with capacities from 20 L to 220 L. Closed-head drums of 60 L are produced on accumulator-head machines with parison programmer control and mold cooling circuits capable of holding a mold temperature of 15–30 °C. Top-load strength for stacked storage is supported by the flexural modulus near 1200 MPa, while drop impact at -18 °C is supported by the high-molecular-weight fraction. However, drop-test performance is strongly influenced by wall thickness distribution; a wall thickness variation exceeding ±0.3 mm in the corners or handle pinch-off can produce brittle failure at low temperature. Therefore, parison programming is critical.

    Chemical compatibility follows the general HDPE hierarchy: aliphatic hydrocarbons, aqueous salt solutions, and many dilute acids and alkalis are contained at ambient temperatures, but aromatic hydrocarbons, chlorinated solvents, strong oxidizing acids, and amine-bearing formulations can promote environmental stress cracking or softening. For filled-container validation, immersion testing under ASTM D543-21 and container performance after contact with the packaged liquid should be conducted. Published data for KM692L under specific aggressive chemical configurations are limited; converter-specific permeation and ESCR testing is required.

    When a Closed-Head Drum Specification Requires High ESCR at Reduced Wall Thickness

    When part mass is reduced, the failure mode shifts from top-load yielding to slow crack growth. KM692L exhibits an environmental stress-cracking resistance above 300 h under ASTM D1693 condition B using 100 % Igepal CO-630 at 50 °C. This property is not a direct predictor of all container failures; constant-strain bent-strip testing should be supplemented with ISO 16770:2019 slow crack growth measurements or ASTM F2136-18 notched constant ligament-stress testing for thin-wall parts. In converter reports and producer technical bulletins, the high-molecular-weight tail of KM692L has been reported to permit down-gauging of large containers when the replacement grade is a conventional monomodal HDPE, but the magnitude of down-gauging varies with tool geometry, pinch-off design, and chemical fill. Published data for this specific configuration are limited; therefore, any wall thickness below 2.0 mm must be qualified by drop testing and stacking tests under the intended shipping temperature range.

    Dimensional Control in KM692L Requires Stable Mold Temperature and Controlled Regrind Fraction

    Dimensional stability after blow molding is governed by crystallization kinetics and process-dependent orientation. Mold shrinkage in KM692L is typically 1.5–2.5 % in the machine direction and 1.0–2.0 % in the transverse direction. These ranges are produced at mold temperatures of 15–30 °C; higher mold temperatures reduce residual stress but increase post-mold shrinkage and cycle time. Blow molds with inadequate cooling produce weld-line distortion and non-uniform stack top load. Weld-line integrity in handle areas is improved by maintaining uniform melt temperature and preventing cold slugs from the breaker plate. A mold temperature differential greater than 5 °C between the mold halves can produce differential shrinkage and warpage in large panels.

    Clean dry regrind is routinely incorporated at levels up to 30 wt% in extrusion blow molding of KM692L on accumulator-head lines. Each regrind pass raises the melt index by approximately 0.02–0.05 g/10 min due to thermomechanical chain scission and reduces the high-molecular-weight fraction that supplies ESCR. Regrind flake moisture should be held below 0.05 wt%, and the flake should be free of paper labels, adhesive residues, and incompatible polymer fines. At regrind levels above 30 wt%, notched impact and ESCR must be re-evaluated because the proportion of the original high-molecular-weight fraction is diluted and oxidative degradation products can accelerate stress cracking.

    Food-contact use of natural KM692L is possible only when the converter validates the finished article under FDA 21 CFR 177.1520(c) conditions of use A–H and confirms that all colorants, antioxidants, and processing aids meet the applicable positive lists. For electrical and electronic equipment housings, a converter-applied audit of the formulation against Directive 2011/65/EU as amended is required. Unstabilized natural HDPE does not provide long-term UV resistance; outdoor service in sunlight requires carbon black or UV stabilizer concentrates, which must be verified for each application by weathering tests such as ISO 4892-2:2013.