TPC (Japan) HDPE KM640L

    • Product Name: TPC (Japan) HDPE KM640L
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 155485
    Density 0.964 g/cm³
    Melt Flow Rate 0.30 g/10 min
    Tensile Strength At Yield 30.0 MPa
    Tensile Strength At Break 20.0 MPa
    Elongation At Break 500%
    Flexural Modulus 1.30 GPa
    Izod Impact Strength Notched 0.100 J/cm
    Hardness Shore D 65
    Vicat Softening Temperature 125 °C
    Heat Deflection Temperature At 0 46 Mpa 75.0 °C
    Melting Point 135 °C

    As an accredited TPC (Japan) HDPE KM640L factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing TPC (Japan) HDPE KM640L is supplied in 25 kg net multi-wall bags, palletized for industrial transport and storage.
    Container Loading (20′ FCL) 20′ FCL container loading: TPC (Japan) HDPE KM640L, typically 25 MT net in 25 kg bags, securely stowed for dry ocean transport.
    Shipping TPC (Japan) HDPE KM640L is shipped as non-hazardous high-density polyethylene pellets, typically in 25 kg PE bags or bulk liners, palletized and stretch-wrapped. Transport in clean, dry containers; protect from moisture, direct sunlight, heat, and contamination. Store in a cool, dry, ventilated area. No special dangerous goods classification required.
    Storage Store TPC (Japan) HDPE KM640L in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, and ignition sources. Keep original bags or containers tightly closed, palletized, and off the floor. Protect from moisture, oils, acids, and contaminants. Avoid prolonged UV exposure and excessive stacking. Maintain good housekeeping; follow the manufacturer’s SDS and local regulations.
    Shelf Life Shelf life approximately two years when stored in original, unopened packaging in a cool, dry, ventilated area away from sunlight.
    Application of TPC (Japan) HDPE KM640L

    On single-station shuttle blow moulders converting 25 L UN-certified jerricans, TPC HDPE KM640L is processed with an 80 mm extruder, 25D L/D, and an accumulator head shot capacity of 3.0–3.5 kg. Melt temperature at the die exit is maintained between 190 °C and 205 °C; head and die zones are held at 195–210 °C; mould circuits run at 12–18 °C. Blow pressure is set at 0.7–0.9 MPa, with a pre-blow delay of 1.0–1.8 s. Parison programming controls the wall thickness through a die gap range of 1.2–2.8 mm. Container body weight for a 25 L jerrican is specified at 1.1–1.35 kg. The low melt flow index of KM640L under ISO 1133-1:2022 at 190 °C/2.16 kg sits within the extrusion blow moulding control range of 0.3–0.5 g/10 min; density under ISO 1183-1:2019 is 0.950–0.960 g/cm³. Finished jerricans are qualified under UN 1H1/Y1.9/250, with stack load testing at 40 °C for 28 days and drop testing at −18 °C after conditioning for 24 h. ESCR measured under ASTM D1693 condition B exceeds 600 h; this is the controlling property for packaging 20% acetic acid, 5% sodium hypochlorite, and 30% hydrogen peroxide in vented jerricans. Carbon black masterbatch is added at 2.0–3.5 wt% for UV stabilization. Post-industrial regrind from the same production line is limited to 30 wt% to maintain ESCR and notched drop-impact margins. The grade is not qualified for concentrated nitric acid above 30% at ambient temperature, and amine-based antistatic surface coatings are avoided because they can reduce downstream fluorination adhesion.

    How Does EVOH Layer Instability Limit Automotive Fuel Tank Coextrusion?

    KM640L is employed in six-layer coextruded diesel and gasoline fuel tanks where the HDPE inner and outer layers require a combination of low mould-in stress and high ESCR. The coextrusion line typically uses 60–70 mm primary extruders for HDPE, a 45 mm extruder for EVOH, and 35 mm extruders for maleic anhydride-grafted polyethylene tie layers. Melt temperatures for KM640L are held at 200–215 °C; EVOH is processed at 210–230 °C; tie layers are held at 195–220 °C. The viscosity mismatch between KM640L and EVOH at shear rates of 10–100 s⁻¹ governs layer distribution stability. Layer thickness ratios must be maintained within ±0.5% of target to avoid hydrocarbon permeation above 2.0 g/m²-day per EPA 40 CFR Part 86 evaporative emission requirements. Pre-blow and parison programming are set to keep the EVOH layer unruptured; a blow-up ratio of 1.8:1–2.2:1 and mould temperature of 10–20 °C are standard. Compressed air for blow pressure is supplied at 0.8–1.1 MPa with a supply dew point below −40 °C to prevent bubble formation in the barrier layer. The maximum allowable regrind inclusion from post-industrial fuel tank flash is 35 wt% in the core layer only; beyond this, parison curl and layer disorientation become measurable on die exit cameras. Published data for KM640L in direct fluorinated monolayer fuel tanks is limited; converter trials with 5–8 mm parison thickness suggest that surface fluorination at 0.5–1.5 g/m² fluorine reduces permeation, but batch-to-batch variance remains a production bottleneck.

    Generic six-layer structure for KM640L-based automotive fuel tanks
    Layer sequenceMaterialNominal thickness shareMelt temperature
    1 outerKM640L + 2.5 wt% carbon black30%200–215 °C
    2 tieMaleic anhydride-grafted PE2.5%195–220 °C
    3 barrierEVOH3%210–230 °C
    4 tieMaleic anhydride-grafted PE2.5%195–220 °C
    5 regrind coreKM640L + process flash32%200–215 °C
    6 innerKM640L30%200–215 °C

    Agrochemical bottle production for organophosphate and pyrethroid formulations exploits the high ESCR of KM640L. The conversion line is configured with a 60 mm extruder, 24D L/D, and a continuous shuttle mould of 2+2 cavities for 1 L and 5 L bottles. Melt temperature is held at 180–195 °C, die temperature at 190–200 °C, mould temperature at 12–16 °C, and blow pressure at 0.6–0.8 MPa. ESCR testing under ASTM D1693 condition A in 10% Igepal CO-630 exceeds 1000 h; under condition B it is used to qualify bottle lots for xylene and cyclohexanone mixtures at ≤5% concentration. Bottles for fenthion and chlorpyrifos formulations require a fluorinated internal surface at 0.3–0.7 g/m² fluorine to reduce solvent absorption, while cypermethrin emulsifiable concentrate bottles rely on the base ESCR without fluorination. Closures are not injection moulded from KM640L; high-torque polypropylene closures are specified. In-mould labelling is precluded when wall thickness is below 1.2 mm because parison cooling rate variance causes label delamination. Post-consumer recyclate is not permitted in this segment under UN 3H1/Y1.4/100 chemical packaging certification.

    Large-Volume Storage Tank Liners and IBC Conversion

    For 220 L L-ring drums and 1000 L IBC liners, a 120 mm extruder with 30D L/D and an accumulator head shot capacity of 12–18 kg is required. KM640L is processed at a melt temperature of 190–205 °C; die head temperature is 200–210 °C; parison programming with 5–10 points compensates for parison sag over a 1.8–2.5 m hang length. For 220 L drums, body weight is fixed at 10.0–11.5 kg to meet UN 1H2/Y1.8/150 stack-load testing at 40 °C for 28 days. Mould cooling time of 180–300 s controls side-wall sink and top flange flatness. Stress cracking resistance is verified under ASTM D1693 condition B in 100% Igepal, with F50 values above 500 h; this supports storage of nonylphenol ethoxylate-based surfactants and glycol ethers at 40 °C. The primary limitation is the hydraulic clamp force of at least 600–800 kN on dual-station shuttle machines.

    When Recycled HDPE Regrind Is Reintroduced into KM640L Bottle Production

    Regrind reintroduction changes the melt rheology and ESCR of KM640L containers. On a continuous shuttle line producing 2 L bottles, addition of 30 wt% post-industrial flash from the same grade does not significantly shift die pressure below 180 °C, as measured by melt pressure at 12–16 MPa at the adapter; however, ESCR under ASTM D1693 condition B falls from 600 h to 350–450 h when regrind content reaches 35 wt%. The critical control point is moisture content of the blend. Published data for this specific configuration is limited; plant practice requires pre-drying of post-consumer flake at 80–90 °C for 4 h when ambient relative humidity exceeds 60%. Melt filtration through 80–120 mesh stainless steel woven screens is specified to remove gel particles from heat history. A gravimetric hopper blender maintains regrind ratio within ±2 wt%. The use of post-consumer recyclate in direct food-contact containers is outside the grade’s normal qualification unless enclosed by a virgin KM640L functional barrier of at least 0.5 mm. Recycled content claims are verified under ISO 14021:2016.

    In portable marine fuel storage, fluorinated monolayer tanks are converted on small accumulator-head machines with 50 mm extruders and 22D L/D. KM640L is selected because its melt strength allows blow-up ratios up to 2.5:1 without localized thinning when the mould shape includes deep draw corners. The tank body weight for 12 L portable marine tanks is 0.85–0.95 kg. Inline fluorination is performed after blow moulding at 0.5–1.0 g/m² fluorine to reduce hydrocarbon permeation. The outer surface is pigmented with UV masterbatch at 3.0 wt%. Impact resistance at −20 °C is validated under ISO 6603-2:2023 or ASTM D3763. The limiting processing condition is the narrow die gap of 0.8–1.5 mm, which increases backpressure above 20 MPa when melt temperature is below 190 °C; therefore, start-up is executed with a heated die soak at 200 °C for 30 min to prevent freeze-off at the accumulator head.

    Free Quote

    Competitive TPC (Japan) HDPE KM640L prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    TPC (Japan) HDPE KM640L is a high-density polyethylene grade formulated for thick-walled extrusion blow moulding, industrial container production, and sheet extrusion where high melt strength, environmental stress crack resistance, and pinch-off weld integrity control part acceptance. The designation belongs to the manufacturer’s high-molecular-weight HDPE portfolio; the pelletised product is typically supplied as a natural or colour-compounded extrudate with a stabiliser package suitable for melt processing at conventional blow moulding temperatures. The figures presented below are representative of this resin class and must be checked against the official certificate of analysis for each production lot.

    The property window commonly reported for high-molecular-weight HDPE blow moulding resins in the 0.944–0.950 g/cm³ density class is summarised in Table 1. Individual lots of KM640L may depart from these values because pelletising, additive loading, and comonomer distribution shift the measured responses.

    Property Test method Nominal range or value Processing or service significance
    Melt flow rate, 190 °C/2.16 kg ISO 1133-1:2022, procedure A 0.25–0.40 g/10 min Controls extrusion pressure, parison drawdown, and accumulator fill time.
    Density ISO 1183-1:2019 0.944–0.950 g/cm³ Governs stiffness, permeability, and slow crack growth resistance.
    Tensile yield stress ISO 527-2:2012, type 1B 22–26 MPa Short-term load-bearing capacity of container walls.
    Elongation at break ISO 527-2:2012 >600% Ductile response beyond the yield point.
    Flexural modulus ISO 178:2019 850–1050 MPa Container stacking stiffness and wall rigidity.
    Charpy notched impact, 23 °C ISO 179-1/1eA:2010 20–30 kJ/m² Ambient puncture and drop-impact resistance.
    Charpy notched impact, −30 °C ISO 179-1/1eA:2010 8–14 kJ/m² Low-temperature toughness for cold-climate transport.
    Vicat softening point, A50 ISO 306:2022 122–126 °C Short-term heat resistance during filling or washing.
    Hardness, Shore D ISO 868:2003 60–64 Surface scratch and abrasion response.
    Environmental stress crack resistance, F50, condition B ASTM D1693-15 ≥600 h Resistance to slow crack growth in surfactant-bearing service fluids.
    Oxidative induction time, 200 °C ISO 11357-6:2018 ≥20 min Indicates stabiliser activity after melt processing.
    Peak melting temperature ISO 11357-3:2018 128–132 °C Thermal transition relevant to hot-fill exposure.

    Specification Benchmarks and Lot-Release Parameters

    The high-load melt flow rate measured at 190 °C under 21.6 kg is typically reported in the 20–35 g/10 min range for this resin class, yielding an MFR ratio of roughly 70–110 when divided by the 2.16 kg value. This ratio indicates a broad molecular-weight distribution that provides shear thinning during extrusion and parison inflation while retaining enough low-shear viscosity to limit sag. Batch-to-batch variation in the 21.6 kg/2.16 kg ratio is more useful than single-point melt flow rate for detecting lot drift.

    The processing latitude of KM640L is governed by molecular architecture rather than by density alone. Medium-density comonomer placement and a low melt flow rate shift the failure mode under sustained stress from brittle slow crack growth to ductile yielding. A higher-density unimodal HDPE with the same 2.16 kg melt flow rate commonly exhibits shorter ASTM D1693-15 condition B failure times, because the thicker lamellae raise yield stress but reduce tie-molecule density. In practical terms, the resin is selected where containers are exposed to detergents, agricultural chemicals, or temperature cycles that generate internal stress at pinch-off and flash regions.

    Capillary rheometry on high-molecular-weight HDPE blow moulding grades of this class shows a pronounced shear-thinning transition between 10 s⁻¹ and 1000 s⁻¹; apparent viscosity at 100 s⁻¹ is typically one order of magnitude lower than at 1 s⁻¹. This response allows the accumulator to fill without excessive pressure while maintaining parison integrity. During parison inflation, extensional viscosity dominates; broad molecular-weight distribution contributes strain hardening that reduces local thinning. Processors should monitor melt pressure before the die rather than screw speed alone; a progressive pressure increase at constant screw speed often signals screen-pack plugging from recycled content or gel formation, not a change in melt flow rate.

    What Differentiates KM640L from Narrow-MWD Injection Moulding HDPE?

    The primary contrast is not chemical resistance but melt rheology and long-term failure behaviour. An injection-moulding HDPE with a melt flow rate of 12–25 g/10 min can fill a thin-wall tool at high shear; KM640L at 0.25–0.40 g/10 min cannot follow that filling path without excessive pressure and shear heating. Conversely, the low melt flow rate of KM640L allows a parison to hold its shape before inflation, whereas a 15 g/10 min injection grade would draw down excessively in a 30 L container tool. Die swell, typically 25–45% for this high-molecular-weight class compared with 10–20% for a narrow-MWD injection grade, also changes the required die gap and pinch-off trim.

    Under ASTM D1693-15 condition B, injection-moulding HDPE grades often record failure at 10–50 h, while the high-molecular-weight blow moulding class is specified above 600 h. That gap is not visible in ordinary tensile strength or flexural modulus, but it dominates selection for containers holding aggressive surfactant solutions. However, KM640L is not interchangeable with a PE100 pipe grade: its density is lower, its hydrostatic creep resistance is lower, and its 21.6 kg melt flow index is higher than typical bimodal pipe resins designed for long-term pressure rating.

    Colour masterbatches should use an HDPE or LLDPE carrier with a melt flow rate below 2.0 g/10 min to maintain viscosity matching at the accumulator. Letdown ratios above 4 wt% for high-titanium-dioxide white concentrates can increase die deposits and reduce impact in unpigmented weld zones. Antistatic or slip concentrates should be validated by ESCR testing because migrating additives can plasticise the amorphous phase and shorten ASTM D1693-15 condition B failure time in ways not visible in standard melt flow or density data.

    On a grooved-barrel single-screw blow moulder with L/D 30:1 and an accumulator head, typical processing starts with feed-zone temperatures of 60–90 °C, compression-zone temperatures of 180–200 °C, and die-head set points of 190–210 °C. The actual melt temperature at the die should remain within 190–210 °C; below 180 °C surface melt fracture and die lines may appear, while above 240 °C thermo-oxidative degradation accelerates and can generate gel particles and yellowing. Blow air pressure is normally set at 0.6–0.8 MPa, with mould temperatures between 10 °C and 20 °C for thin-wall surface finish. For thick-walled industrial parts above 5 mm nominal wall, a mould temperature of 20–30 °C is sometimes used to reduce residual stress and improve pinch-off strength at the expense of cycle time.

    HDPE is not hygroscopic, and predrying is unnecessary if the resin is stored in sealed containers at low humidity. When sacks or octabins have been exposed to condensation or relative humidity above 60%, surface moisture can produce splay; desiccant drying at 80 °C for 2–4 h with a dew point equal to or below −40 °C restores a stable feed. Clean in-house regrind from the same grade can be incorporated at up to 20 wt% without statistically significant loss in ESCR in production-scale studies on similar high-molecular-weight HDPE grades; higher regrind fractions increase gel count, dust, and parison tear sensitivity at the flash line.

    When Large-Part Extrusion Blow Moulding Demands Melt Strength

    Large-part blow moulding exposes the resin to two principal failure mechanisms: parison sag before mould closure and stress cracking at the pinch-off weld. KM640L is selected where the part mass exceeds roughly 1 kg and wall thickness in the flash vicinity must remain uniform after parison inflation. In accumulator-head machines, the parison is dropped at low shear rate; a low melt flow rate limits drawdown, while broad molecular-weight distribution reduces the tendency for the parison to tear at the die exit.

    Reported application areas for this grade class include 20–30 L industrial jerry cans, agricultural chemical containers, automotive windscreen washer reservoirs, and large multi-trip packaging. Monolayer containers made from this resin are not normally considered sufficient for automotive fuel systems because hydrocarbon permeation limits under evaporative emission regulations require fluorination, sulfonation, or multilayer EVOH construction. Published data for KM640L in monolayer fuel-tank service are limited; the resin is suitable for aqueous and non-fuel hydrocarbon containers unless a barrier treatment has been validated.

    In production-scale trials on similar HDPE grades, wall-thickness variation is controlled by adjusting accumulated shot size, die gap, and parison programming rather than by raising melt temperature. Excessive melt temperature to improve surface gloss will produce parison sag and thin sidewalls; excessive blow pressure can create undercuts and increases pinch-off flash. A programmed parison with a thicker section at the top and bottom is used when the blow ratio exceeds 2.5:1 or when the projected part length exceeds 600 mm.

    Regulatory status for KM640L depends on the final formulation and colour package. Natural high-density polyethylene grades that meet the extractables and end-use conditions of 21 CFR 177.1520(c) are used in food-contact articles under the conditions of use specified in 21 CFR 176.170(c). For the European market, compliance is assessed under Regulation (EU) No 10/2011, with overall migration limits of 10 mg/dm² for food-contact plastics. Under REACH Regulation (EC) No 1907/2006, a substance of very high concern is not expected in the neat resin at or above 0.1 wt%, but the downstream user must verify finished-article status. RoHS Directive 2011/65/EU restrictions apply to homogeneous materials and are usually satisfied by natural unfilled HDPE; colour concentrates and recycled content may alter lead, cadmium, mercury, hexavalent chromium, PBB, or PBDE results.

    Service limitations should be observed. The resin is not intended for continuous exposure to strong oxidising acids, chlorine gas, or aromatic solvents; gasoline and aggressive solvent blends require barrier treatment. The natural stabiliser package is not a UV system; outdoor weathering requires carbon black or a UV-stabilised variant. Sustained mechanical load at temperatures above 60 °C should be supported by creep rupture data for the specific part geometry and stress state.