TPC (Japan) HDPE KM640A

    • Product Name: TPC (Japan) HDPE KM640A
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 243010
    Density 0.960 g/cm³
    Melt Flow Rate 0.20 g/10 min
    Tensile Strength At Yield 29.0 MPa
    Tensile Strength At Break 33.0 MPa
    Elongation At Break 600 %
    Flexural Modulus 1.20 GPa
    Izod Impact Notched 0.100 J/cm
    Hardness Shore D 65
    Vicat Softening Point 127 °C
    Brittleness Temperature <= -70 °C
    Environmental Stress Crack Resistance 1000 hr
    Thermal Expansion Coefficient 1.2E-4 cm/cm/°C
    Thermal Conductivity 0.350 W/m·K
    Specific Heat 2.30 J/g·°C
    Melting Point 135 °C
    Dielectric Constant 2.30
    Dielectric Strength 20.0 kV/mm
    Volume Resistivity 1.00E+16 ohm·cm
    Water Absorption 0.0100 %
    Mold Shrinkage 2.00 %

    As an accredited TPC (Japan) HDPE KM640A factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing TPC (Japan) HDPE KM640A is packaged in 25 kg multiwall paper bags, palletized at 1,000 kg per pallet.
    Container Loading (20′ FCL) TPC (Japan) HDPE KM640A loaded in 20′ FCL, 25 kg bags, palletized, securely stowed, approximately 18–20 MT net weight.
    Shipping TPC (Japan) HDPE KM640A is a non-hazardous high-density polyethylene resin supplied as pellets. It is typically packed in 25 kg bags, palletized, and stretch-wrapped. Ship in clean, dry containers at ambient temperature, protecting from moisture, direct sunlight, and heat. Standard freight; no special dangerous-goods documentation required.
    Storage Store the chemical TPC (Japan) HDPE KM640A in a cool, dry, well-ventilated warehouse. Keep original bags sealed on pallets, off the floor, away from direct sunlight, rain, moisture, heat, ignition sources, and strong oxidizers. Avoid punctures, contamination, and excessive stacking. Use clean handling equipment; prevent static buildup. Do not smoke. Follow FIFO, inspect containers regularly, and comply with local regulations.
    Shelf Life TPC (Japan) HDPE KM640A shelf life: two years from manufacture when stored in original, unopened packaging in cool, dry, ventilated conditions.
    Application of TPC (Japan) HDPE KM640A

    In the extrusion blow molding of UN-certified large-volume industrial packaging, TPC HDPE KM640A is processed on single-screw extruders with grooved feed sections and accumulator heads. The primary manufacturing conflict is not melting capacity but parison stability: high-molecular-mass HDPE has high melt strength, yet wall-thickness uniformity across a 200 L closed-head drum still depends on programmed parison gap changes of 2–5 mm around the circumference. Incorrect programming produces thin bands near the pinch-off weld and chime that reduce drop-impact resistance and environmental stress-cracking resistance under stack-load conditions. Compliance for this segment is governed by UN 1H1 and UN 1H2 packaging design types, with performance qualification under 49 CFR 178.509 and 49 CFR 178.510. Stack load testing is conducted according to ISO 16106:2006, and ESCR evaluation uses ASTM D1693-15 Condition A with 10% Igepal CO-630 at 50 °C. Drop-impact resistance is evaluated by ASTM D2463-15. Formulation addition on the manufacturing floor typically limits internal regrind to ≤30 wt%, with carbon black masterbatch dosed at 1.5–2.5 wt% for outdoor UV resistance. Additional processing aid is not required below 0.15 wt%, because the base stabilization package of KM640A is designed for closed-loop trimmings. The downstream process uses accumulator-head blow molding machines with extruder L/D ratios of 24:1–30:1, barrel zone temperatures from 175 °C to 210 °C, head temperatures 190–210 °C, mold coolant inlet 8–15 °C, blow air pressure 0.6–0.8 MPa, and demolding when the outer surface is ≤60 °C. In production-scale runs, the most frequent nonconformance is low wall thickness at the pinch-off area rather than the sidewall, caused by insufficient parison program step change after the tail weld; ultrasonic gauging at 5 MHz detects pinch-zone wall thickness below 4.5 mm. Finished article types include open-head and closed-head drums of 200 L, IBC inner bottles up to 1000 L, and jerricans from 5 L to 30 L.

    Representative accumulator-head extrusion blow molding process window for HDPE KM640A in UN drum production
    Process/test parameterTarget rangeReference method or equipment
    Parison melt exit temperature190–205 °CInfrared pyrometer, 8–14 µm wavelength
    Mold coolant inlet temperature8–12 °CClosed-loop chiller with supply pressure 0.4–0.6 MPa
    Blow air pressure0.6–0.8 MPaAccumulator-fed blow pin
    Demolding surface temperature≤60 °CContact thermocouple
    Closed-head drum wall thickness, chime to sidewall transition4.5–6.0 mmUltrasonic gauge, 5 MHz
    ESCR condition50 °CASTM D1693-15 Condition A, 10% Igepal CO-630

    Why Does Parison Sag Govern Wall Distribution in Underhood Reservoir Molding?

    Underhood reservoirs blow molded from KM640A face a narrower processing window than industrial drums because the parison is long relative to the die diameter and must be sequenced rapidly to avoid differential cooling. OEM validation for windshield washer and coolant overflow reservoirs generally follows ISO 175:2010 chemical-resistance testing after immersion in 50% ethylene glycol/water at 95 °C for 500 h, ISO 4892-2:2013 for exterior UV weathering, and ISO 527-2:2012 tensile property retention after exposure. Burst and pressure-cycle requirements are often specified at 0.5–1.0 bar; welded insert bosses are tested for pull-out after heat ageing. Formulation addition includes carbon black masterbatch at 2.0 ± 0.3 wt% where exterior UV exposure is required, while pinch-off scrap regrind is limited to ≤20 wt% when long-term weld-line integrity is essential. If regrind content exceeds 20 wt% and melt-flow-rate shift exceeds 15% relative to virgin material, a supplementary phenolic/phosphite stabilizer is dosed at 0.1–0.2 wt%. The process uses accumulator-head machines with 64-point to 128-point parison programming, mold temperatures of 10–15 °C, blow air at 0.5–0.7 MPa, and cavity surface graining of 10–15 µm to obscure weld lines. Continuous service above 85 °C is not recommended without wall-thickness derating; short-duration exposure to glycol at 120 °C is restricted to thermal cycling tests, not sustained operation. Finished product types include windshield washer fluid reservoirs of 3–7 L, coolant overflow tanks of 1–2 L, and HVAC condensate drain vessels.

    Agrochemical Container Performance Under Solvent Permeation and Pinch-Off Weld Stress

    The critical barrier requirement in agrochemical packaging is not load-bearing capacity but resistance to permeation and environmental stress cracking when the bottle wall is wetted by xylene, cyclohexanone, or ester-based solvents. Monolayer HDPE containers fail by panel permeation and vertical weld stress cracking; KM640A is used as the structural and product-contact layers in co-extruded bottles with polyamide or EVOH barrier layers. Compliance includes UN 1H1 design type qualification for Packing Group II/III liquids, permeability testing with the actual formulation under ASTM D2684, and registration-specific permeation limits set by crop protection authorities. In a five-layer structure, HDPE layers represent 85–90 wt%, EVOH or polyamide barrier 2–4 wt%, tie resin 1–2 wt%, and post-consumer recyclate is excluded from the product-contact layer; internal regrind may be returned to the middle HDPE layer up to 25 wt%. The process employs continuous co-extrusion blow molding with layer distribution controlled by a feedblock and spiral mandrel die; melt temperatures are held at 190–210 °C, blow air at 0.6–0.8 MPa, and mold temperature at 8–15 °C. Monolayer variants are post-mold fluorinated offline, with surface fluorine substitution limited to 1–3 wt% to avoid embrittlement at the pinch-off weld. Finished product types include containers from 0.5 L to 20 L for emulsifiable concentrates, suspension concentrates, water-soluble powders, and adjuvants.

    Drinking-water storage tanks fabricated from high-molecular-mass HDPE are subject to organoleptic and migration limits that override conventional mechanical property selection. KM640A is processed in shuttle blow molding machines for closed-wall vertical tanks and rectangular cisterns; the principal process limitation is the long cooling cycle associated with thick sections. Compliance rests on NSF/ANSI 61 for the U.S. market, AS/NZS 4020:2005 for Australia/New Zealand, and BS 6920-1:2014 for odor and flavor suitability in the United Kingdom. These standards specify water extraction at 23 °C and 60 °C for 24 h, with panel evaluations for taste, odor, and microbial growth. Formulation discipline requires that no post-consumer regrind be placed in the potable contact layer; internal closed-loop regrind is limited to 15 wt%, and carbon black concentrate is dosed at 2.0–3.0 wt% for UV stabilization. Additional processing aids that may elute total organic carbon are excluded unless organoleptic panel testing confirms no detectable taint. Double-station shuttle blow molders with extruder L/D ratios of 28:1–32:1, melt temperatures of 180–200 °C, mold temperatures of 8–18 °C, and blow air at 0.5–0.7 MPa are used; cooling times for 200 L tanks range from 15 min to 30 min depending on wall thickness of 8–15 mm. Finished product types include free-standing potable water tanks from 100 L to 500 L, cylindrical cisterns, and emergency water storage containers.

    Potable water contact compliance matrix for HDPE water storage tanks
    MarketStandardTest condition or extraction protocol
    United StatesNSF/ANSI 61Health effects extraction; pH 5 and pH 8 water; 23 °C and 60 °C; 24 h
    Australia/New ZealandAS/NZS 4020:2005Taste and odour panel, microbial growth screening
    United KingdomBS 6920-1:2014Odour and flavour of water, appearance, cytotoxic activity

    Sheet Extrusion and the Shift from Injection-Molded Dunnage to Thermoformed Pallet Trays

    Replacing injection-molded HDPE dunnage with thermoformed sheet begins with a high-melt-strength resin that can support deep draw ratios and thick-gauge retention; KM640A is used in this segment for pallet trays and material-handling panels where impact strength and ESCR are required. Published data for this specific configuration are limited; the following parameters are derived from production-scale HDPE sheet lines processing equivalent high-molecular-mass blow-molding-type resins. Sheet qualification uses ISO 1183-1:2019 for density, ISO 527-3:2018 for tensile modulus and elongation at break, ISO 6603-2:2000 for instrumented puncture, and ASTM D3763 for high-speed puncture energy. Formulation consists of virgin KM640A at 65–75 wt%, internal edge-trim and skeleton regrind at 25–35 wt%, and carbon black or mineral-filled masterbatch at 1–2 wt%; no impact modifier is added because toughness is derived from molecular weight rather than elastomer modification. The process uses a single-screw sheet extruder with L/D ratio of 30:1–36:1, barrier screw geometry, melt temperatures of 200–215 °C, a three-roll calendering stack at 60–80 °C, die gap 2–6 mm, and thermoforming at sheet surface temperatures of 160–180 °C. Finished product types include thermoformed pallet trays, dunnage dividers, automotive compartment liners, and material-handling trays.

    Free Quote

    Competitive TPC (Japan) HDPE KM640A prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    TPC (Japan) HDPE KM640A is a high-density polyethylene pellet grade intended for blown-film extrusion of thin-gauge carrier bags, light-barrier agricultural film, and high-stiffness industrial liners. The grade is characterized by a nominal density of 0.954 g/cm³ under ISO 1183-1:2019 and a melt mass-flow rate of 0.04 g/10 min at 190 °C and 2.16 kg under ISO 1133-1:2022. Under a 21.6 kg load, the high-load melt index is generally reported in the range 7.5–8.5 g/10 min, yielding a melt-flow ratio near 200:1. This ratio places the resin among broad-molecular-weight-distribution film grades, a structural feature that contributes to high melt strength during bubble formation and to resistance to draw resonance at high haul-off speeds. The grade is supplied as dry pellets without slip or antiblock additives unless a formulated variant is specified, which means converters must add external masterbatch to control blocking and coefficient of friction on wound rolls.

    In blown-film extrusion, process stability is governed by the interaction of melt temperature, die gap, blow-up ratio, and frost line height. On a production line using a 45 mm grooved-feed extruder with 30:1 L/D, a 100 mm spiral mandrel die, and a die gap of 0.8 mm, stable operation is typically observed in the barrel temperature range 170–200 °C and at a melt temperature of 185–210 °C. Blow-up ratio is commonly set between 3.0:1 and 4.5:1. Achieving a frost line height of 3–6 die diameters helps balance machine-direction orientation and transverse-direction tear properties. In this operating envelope, high-load melt index is the more relevant flow parameter because the 2.16 kg melt mass-flow rate is too low for routine production control. Capillary rheometry at 190 °C shows shear-thinning from apparent viscosity near 1.5 × 10³ Pa·s at 100 s⁻¹ to approximately 3.0 × 10² Pa·s at 1000 s⁻¹. This shear-thinning response reduces die pressure relative to a narrow-molecular-weight HDPE of equal zero-shear viscosity, while the high elongational viscosity supports a stable bubble at low film thickness. Published data for this specific configuration is limited outside supplier technical bulletins and line trials.

    The low 2.16 kg melt mass-flow rate makes laboratory MFR an unsuitable predictor of die flow; instead, the high-load melt index should be monitored at 21.6 kg. A high-load melt index below 6.0 g/10 min indicates insufficient melt conveying and may cause excessive melt pressure and motor amperage on 45 mm extruders. A value above 10.0 g/10 min is generally accompanied by lower melt strength and can increase sagging or bubble flutter at thin gauges. In film winders, thickness tolerance after randomizing is often controlled to ±5% of nominal, and online capacitance gauges are used to map the thickness profile around the bubble. Bands of thick film align with die bolt positions; readjusting die bolts by 0.05 mm increments is a common correction action when the profile exceeds ±8%.

    How does KM640A compare with conventional unimodal HDPE film grades in downgauged bag applications?

    When a converter replaces a conventional unimodal HDPE film grade of similar density with KM640A, the main process difference is the increase in melt-flow ratio from roughly 80:1–120:1 to approximately 200:1. The broader molecular weight distribution permits the bubble to remain dimensionally stable at lower film thickness, typically 7–10 µm, without the same frequency of bubble flutter. In laboratory evaluations, dart impact and tensile strength per unit thickness are commonly compared under ASTM D1709-16ae1 and ISO 527-2:2012. The comparative values below were generated on a 45 mm blown-film line at a blow-up ratio of 4:1, a die gap of 0.8 mm, and a melt temperature of 195 °C, with film thickness adjusted to 25 µm.

    PropertyTest methodTPC HDPE KM640AUnimodal HDPE film gradeLDPE general-purpose film grade
    DensityISO 1183-1:20190.954 g/cm³0.952 g/cm³0.923 g/cm³
    Melt mass-flow rate, 2.16 kgISO 1133-1:20220.04 g/10 min0.05 g/10 min1.8 g/10 min
    High-load melt index, 21.6 kgISO 1133-1:20228.0 g/10 min5.5 g/10 minnot reported
    Dart impact F50, 25 µmASTM D1709-16ae1 Method A150 g90 g80 g
    Elmendorf tear, machine directionISO 6383-2:198318 g/25 µm12 g/25 µm22 g/25 µm
    Tensile strength at yield, machine directionISO 527-2:201224 MPa23 MPa11 MPa
    Water vapor transmission rate, 25 µm, 38 °C, 90% RHASTM F1249-203.5 g/m²·day3.8 g/m²·day14 g/m²·day
    HazeASTM D1003-2175%70%6%

    These comparative values indicate that KM640A is not an optical film grade; haze is high because of the resin’s melting range and the crystalline light-scattering morphology common to HDPE film. In exchange, the film provides higher stiffness and lower moisture permeation than LDPE, which allows either a reduction in film thickness or a longer dry-packaging shelf life. In comparison with an injection-molding HDPE of melt mass-flow rate 20 g/10 min, KM640A is outside the practical processing window for injection molding because the low melt flow under 2.16 kg would require excessive melt temperatures and would produce high injection pressures in multi-cavity moulds.

    Tensile properties measured under ISO 527-2:2012 on 25 µm film show that machine-direction yield strength is higher than transverse-direction yield strength when the blow-up ratio is below 3.5:1. At blow-up ratios above 4.5:1, transverse-direction orientation increases, and the tear balance shifts. For applications such as T-shirt bags requiring load-bearing capacity in the machine direction, a blow-up ratio below 3.5:1 is common. For trash liners requiring puncture resistance in all directions, a blow-up ratio near 4.0:1 is used to balance orientation. The resin’s broad molecular weight distribution supports this adjustment without bubble instability, unlike narrow-distribution metallocene HDPE grades that may show more frequent bubble breathing at high blow-up ratios.

    When high-speed bag conversion modulates corona treatment and heat-seal thresholds

    Downstream conversion of KM640A film on bag-making machines introduces two coupled thresholds: surface energy for print and seal, and heat-seal temperature without edge shrinkage. For corona treatment, a bare-roll dielectric system with a generator output of 2–4 kW at line speeds between 80 m/min and 150 m/min typically raises wetting tension from 31–34 mN/m to 38–42 mN/m when measured by ASTM D2578-17a. Treatment levels above 44 mN/m can create low-molecular-weight oxidized species that migrate to the seal area and reduce seal strength under ISO 527-2:2012 peel testing. On a rotary heat-seal machine operating at 120–145 °C jaw temperature and 0.5–1.0 s dwell time, consistent peel failure is obtained when film thickness variation remains below ±5%. The high melt strength of KM640A reduces gauge variation, but excessive corona treatment or poor chill-roll release can reintroduce variability at the bag mouth. In laminating or printing processes, the film’s higher crystallinity usually requires solvent-free polyurethane adhesives with a primer layer when the surface energy falls below 36 mN/m after storage.

    Heat-seal initiation is influenced by the high-density backbone and the absence of slip additives in the base resin. On laboratory heat-seal equipment with 0.5 MPa jaw pressure and 1.0 s dwell, seal initiation is typically observed near 125 °C. At temperatures above 150 °C, the film can lose dimensional stability at the seal lip, producing puckering and a reduction in peel strength. Converters running high-speed bag machines often set the sealing jaw at 135–145 °C and press the film with a cooling jet immediately after the seal zone to prevent seal-area deformation. This range is narrower than for low-density polyethylene, a practical limitation that must be accounted for when switching from LDPE to HDPE KM640A on the same bag line.

    Processing defect thresholds for moisture, regrind, and additive concentrates

    Moisture-induced bubble defects, gel formation, and die-lip build-up are common failure modes when handling high-molecular-weight HDPE pellets in unconditioned warehouses. On a continuous line with gravimetric dosing, pellet surface moisture above 0.05% measured by ASTM D6980-17 can produce pinholes and micro-bubbles at the die exit. At relative humidity above 60%, condensation on cold pellets introduced from an outdoor silo is sufficient to exceed that threshold. Regrind addition at levels above 20 wt% reduces melt strength because repeated extrusion causes chain scission and lowers the melt-flow ratio. In a typical three-layer or seven-layer coextrusion line, process data from production trials show that increasing regrind from 10 wt% to 30 wt% can reduce dart impact by approximately 10–15% and increase thickness variation at high draw-down. Additive concentrates containing erucamide or silica should be limited to 2–5 wt% depending on the carrier resin, because excessive slip additive migrates to heat-seal surfaces and may reduce seal strength by more than 20%. For color concentrates based on titanium dioxide, addition above 5 wt% raises melt pressure and can produce die lines; screen packs of 80/120/80 mesh are normally placed before the breaker plate to capture agglomerated pigment.

    Die-lip build-up in HDPE film lines is often associated with oxidized polymer fractions or incompatible additive carriers. The condition presents as local gauge bands and as haze streaks aligned with the machine direction. On a 100 mm die, lip deposits can be removed by periodic purging with a high-viscosity polyethylene purge compound at 10–15 °C above the standard melt temperature, followed by manual polishing with 600-grit or finer abrasive cloth. The frequency of die-lip cleaning is typically extended when the extruder is run continuously rather than in short campaigns, because repeated shutdown and startup cycles expose residual polymer to thermal degradation in the die.

    The olefinic polymer fraction of TPC (Japan) HDPE KM640A is typically evaluated under FDA 21 CFR 177.1520 for food-contact use as an olefin polymer. Compliance is limited to the conditions described in the supplier’s statement of composition; hot-fill applications above 70 °C and retort conditions are not within the conventional data set because the resin softens and loses mechanical integrity. Under EU Regulation No 10/2011, overall migration into food simulants is generally below 10 mg/dm² when tested according to the prescribed simulant matrix, but converters must verify specific migration limits for the final formulation after adding masterbatch. The grade is not formulated with antistatic or UV-stabilizing additives unless a custom product is ordered; therefore, outdoor weathering beyond 6 months requires additional stabilizer concentrates. Under REACH and RoHS 2011/65/EU, supplier statements usually address the four restricted heavy metals and all substances of very high concern at the 0.1% w/w threshold. Published data for this specific configuration is limited for some food-simulant combinations, and final compliance rests with the converter or brand owner.

    Storage before conversion should be in an enclosed silo or hopper at or below 50 °C. Prolonged ultraviolet exposure and contact with copper or copper-containing alloys can accelerate thermo-oxidative degradation of the polyethylene backbone. Pneumatic conveying systems using ambient air with a dew point above 10 °C may introduce dust and moisture; dried-air conveying with a dew point of −20 °C or below is preferred for high-speed film lines near coastal processing plants. In such environments, pellet surface moisture measured by ASTM D6980-17 should remain below 0.05% before the material enters the extruder throat. No oven pre-drying is normally required when that threshold is maintained.