| HS Code | 871381 |
| Product | TPC (Japan) HDPE KM592L |
| Polymer Type | High Density Polyethylene (HDPE) |
| Density | 0.958 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 0.45 g/10 min |
| Tensile Strength At Yield | 28 MPa |
| Tensile Strength At Break | 22 MPa |
| Elongation At Break | >600% |
| Flexural Modulus | 1200 MPa |
| Notched Izod Impact Strength 23 C | 10 kJ/m² |
| Vicat Softening Point | 126°C |
| Heat Deflection Temperature 0 46 Mpa | 70°C |
| Melting Point | 134°C |
| Hardness Shore D | 65 |
| Mold Shrinkage | 1.5-2.0% |
| Water Absorption | <0.01% |
| Environmental Stress Crack Resistance Escr | >1000 h |
| Volume Resistivity | >10^16 Ω·cm |
| Dielectric Constant 1 Mhz | 2.3 |
| Dielectric Strength | 20 kV/mm |
| Thermal Conductivity | 0.4 W/m·K |
| Coefficient Of Linear Thermal Expansion | 1.2E-4 /°C |
| Ul Flammability Rating | HB |
As an accredited TPC (Japan) HDPE KM592L factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | TPC (Japan) HDPE KM592L comes in 25 kg polyethylene-lined woven bags; 1,000 kg jumbo bags are also available. |
| Container Loading (20′ FCL) | Container loading of a 20′ FCL for TPC (Japan) HDPE KM592L, typically 25 kg bags, palletized, secured for ocean freight. |
| Shipping | TPC (Japan) HDPE KM592L is shipped as non-hazardous high-density polyethylene pellets, typically in 25 kg bags or jumbo bags on pallets. Use clean, dry containers; keep away from moisture, heat, and direct sunlight. Maintain cool, ventilated storage during transit. No dangerous goods classification or special transport requirements apply. |
| Storage | Store TPC (Japan) HDPE KM592L in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, flames, and oxidizing agents. Keep original bags closed, clean, and palletized to prevent moisture, dust, and odor contamination. Avoid prolonged UV exposure and excessive stacking. Store at ambient temperature. Use first-in, first-out stock rotation. Follow local regulations and the manufacturer’s safety data sheet. |
| Shelf Life | Shelf life: typically 24 months from manufacture when stored cool, dry, sealed in original packaging, away from direct sunlight. |
On accumulator-head extrusion blow moulding lines producing UN-rated 30 L jerricans, HDPE KM592L is charged as the sole thermoplastic base component without predrying when stored under dry cover; if exposed to relative humidity above 60%, surface moisture must be removed with a hot-air hopper dryer at 80°C for 2 h to prevent splay. The compliance envelope for this segment is set by the UN Model Regulations Chapter 6.1 for plastics packagings, comprising the 3H1/3H2 jerrican, 1H1/1H2 drum and 31HA1/Y composite IBC designations, with type approval testing under the UN Manual of Tests and Criteria Part III covering drop impact at -18°C, hydraulic pressure hold and stack load. Industrial producing plants operate to ADR/RID/IMDG Code multimodal requirements when the packaged product is classified dangerous goods. In production compounding, the standard letdown formulation is 98.0–99.0 wt% KM592L with 1.0–2.0 wt% colour or carbon black masterbatch for outdoor service, plus 0.05–0.15 phr external lubricant only where parison thickness control below ±0.3 mm is specified. Regrind from trimmed pinch-off and top flash is reintroduced at 10–25 wt%; exceeding 25 wt% has been observed on accumulator-head machines to reduce cold-temperature drop energy at the pinch-off weld because low-molecular-weight degradation products concentrate at the weld line. Processing on shuttle blow moulders with 80–120 mm screw diameters and 20:1–30:1 L/D ratios runs at melt temperature 180–205°C, blow pressure 0.6–0.8 MPa, mould temperature 20–40°C, and variable parison programming to compensate for the transition from the neck to the body. The terminal outputs are 20–30 L UN 3H1 jerricans, 120–220 L UN 1H2 open-head drums, and 1,000 L UN 31HA1/Y inner bottles for composite IBCs used for liquid agrochemicals, surfactants and water-treatment chemicals.
The shift from metal to plastic automotive fuel tanks is constrained by hydrocarbon permeation; monolayer HDPE walls can no longer meet China 6 and Euro 6 evaporative emission limits, so KM592L is positioned as the virgin outer and inner HDPE layers in a six-layer barrier structure. The controlling standards are ECE R34 Annex 5 for fire resistance, GB 18352.6-2016 for SHED testing, and OEM-specific permeation targets validated by sealed housing evaporative determination. In this structure the layer-weight distribution is a formulation constraint rather than a compound add-on: outer virgin HDPE 15–25 wt%, regrind HDPE 30–40 wt%, inner virgin HDPE 20–25 wt%, EVOH barrier 1.5–3.0 wt%, and adhesive tie layers 1.5–3.0 wt% of total wall thickness. Six extruders feed an accumulator head, with the HDPE and tie-layer temperature held at 190–210°C and the EVOH at 210–230°C to remain within its narrow melt-stability window; head tooling is designed with spiral mandrels to avoid dead spots. Axial parison programming uses wall-thickness feedback with tolerance ±0.3 mm. Finished tanks are subjected to cold impact at -40°C and pressure cycling; field failure analytics show that an increase in regrind above 30 wt% shifts the inner-layer melt-flow balance and generates gels that produce pinholing at the pinch-off seam. The terminal parts are 40–80 L fuel tanks for passenger cars and light commercial vehicles.
Instead of hydrocarbon permeation, SCR urea storage tanks are limited by a freeze-thaw stress-cracking mechanism: the working fluid is a 32.5 wt% aqueous urea solution that freezes and expands, so the HDPE wall must tolerate repeated phase change without cracking at the lower pinch-off weld. Material compatibility for DEF/AdBlue service is specified under ISO 22241-3:2019, which includes immersion testing of the polymer in the operating fluid at 50°C and evaluation of extractable behaviour that could degrade the SCR catalyst. In practice, KM592L is used at 99.0–100.0 wt% as the base, with 0–0.5 wt% blue or grey masterbatch and 0.10–0.30 wt% stabilizer masterbatch; copper phthalocyanine pigments are acceptable, but copper compounds must not be present as adventitious metal contaminants because Cu accelerates urea decomposition. The production process is extrusion blow moulding with parison programming, melt temperature 185–205°C, blow pressure 0.6–0.8 MPa, and mould temperature 20–35°C. The bottom pinch-off seam is the critical zone: after blowing, the part is trimmed with a heated clipping fixture at 40–50°C to reduce internal residual stress; each tank is then leak-tested with air at 20 kPa. Terminal products are 10–25 L DEF tanks for heavy-duty on-road and off-highway vehicles.
For outdoor non-potable water and chemical storage, KM592L is fabricated from extruded sheet by hot-gas and butt fusion welding rather than blow moulded; the long service requirement forces attention to UV stabilization and weld bead crystallinity instead of drop impact. The applicable standards are EN 12573-1:2000 for stationary welded thermoplastic tanks and DVS 2205-1 for calculation of tank walls and welds. To achieve outdoor service, the sheet is dry-blended with 2.0–2.5 wt% carbon black masterbatch, which should yield opacity and UV absorption; the dispersion quality is checked according to ISO 6964 with an aggregation index below 3. Sheet extrusion uses a barrier screw at 190–215°C, a polished roll stack at 60–80°C, and thickness control ±0.2 mm on 4–6 mm sheet. Hot-gas welding is executed at 210–230°C with 3–4 mm round nozzle distance and an inert gas purge to reduce oxidation; butt fusion joints are pressure-controlled at 0.12–0.18 MPa. Terminal outputs include 5–50 m³ cylindrical vertical storage tanks, scrubber bodies, dosing tanks and aquaculture containment units.
This segment is differentiated by thin-wall blow moulding with internal blow pin calibration and aggressive methanol/glycol exposure. OEM specifications generally require pressure-vacuum cycling at -30°C to 100°C and immersion in 50 vol% methanol/water at 60°C for 168 h per ASTM D471; the HDPE grade must retain elongation without environmental stress cracking at the pinch-off weld. KM592L is processed at 100 wt% with 0.5–1.0 wt% colour masterbatch and 0.10–0.20 wt% antioxidant masterbatch; silicone-based process aids may be added at 0.05–0.10 wt% to improve parison surface smoothness. Shuttle blow moulders with needle blow pins are used; parison pre-blow is set at 0.05–0.10 MPa and final blow pressure at 0.5–0.7 MPa, with mould temperature 20–30°C to maintain wall thickness 1.5–2.5 mm. The part is trimmed in a punch-and-die station, and weld seams are inspected by polarized light for residual stress. Terminal products are 2–5 L coolant recovery reservoirs and washer bottle assemblies.
Small rigid containers for liquid pharmaceuticals and cosmetics demand low-extractable HDPE and documented regulatory compliance. KM592L meets the polymer identity and extractable limits of FDA 21 CFR 177.1520(c), and finished packaging is screened under USP <661.1>/USP <661.2> for pharmaceutical use, with EU food-contact migration evaluated under EU 10/2011. Cosmetic packaging adds organoleptic restrictions that require testing for odour and taint via ASTM E462-84 or internal sensor panels. Unlike industrial articles, this segment excludes regrind entirely; the feed is 100 wt% KM592L, often with 0.5–1.0 wt% low-extractable white masterbatch. External lubricants such as zinc stearate are limited to < 0.1 wt% to avoid excessive extractables. The process uses intermittent extrusion blow moulding with filtered blow air (0.22 μm) and melt temperature 180–200°C. Mould cooling is maintained at 20°C; dimensional stability is checked by leak testing at 10 kPa. Published dynamic mechanical data for KM592L under concentrated surfactant solutions is limited; qualification programmes should replicate the intended product matrix before commercial use. Terminal products are 50–1000 mL bottles for liquid pharmaceuticals, mouthwashes and cosmetic emulsions.
Competitive TPC (Japan) HDPE KM592L prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
TPC (Japan) HDPE KM592L is a high-density polyethylene resin whose designation appears in industrial resin listings for blow moulding, sheet and profile extrusion, and rigid packaging applications. The grade is not represented by a universal ISO 1872-1 nomenclature string; the KM592L suffix is a manufacturer-specific code. A converter should therefore separate the general HDPE classification, which requires a density above 0.940 g/cm³ under ISO 1183-1:2019, from the grade-specific certified values for melt-mass flow rate, mechanical properties, and additive content. Published data for this specific configuration is limited, so all downstream process windows should be validated against the TPC certificate of analysis for the actual lot.
The KM592L designation does not inherently disclose density, melt viscosity, or molecular weight distribution. The standard verification matrix for a high-density polyethylene of this class includes density, melt-mass flow rate, tensile yield stress, elongation at break, flexural modulus, Charpy or Izod impact resistance, softening point, and environmental stress-crack resistance. Each property must be tied to its controlling test method and specimen conditioning history; otherwise cross-lot comparison is not technically meaningful. Conditioning should follow ISO 291:2008 class 2, at 23 °C and 50% relative humidity, unless the manufacturer’s certificate states otherwise.
For food-contact applications, converter review should require a written statement of compliance under FDA 21 CFR 177.1520(c) for olefin polymers, with attention to the density and extractives limitation applicable to the finished part. REACH compliance requires a separate safety data sheet and confirmation that the substance or mixture does not contain a listed candidate substance above the applicable threshold. RoHS obligations are not normally relevant for unfilled polyethylene packaging unless the part is integrated into electrical or electronic equipment, in which case the supplier must confirm the absence of restricted flame-retardant or heavy-metal additives.
Processing of HDPE KM592L on an accumulator-head blow moulding line should begin with a melt-temperature profile established from the lot-specific melt-flow rate. On a 90 mm grooved-barrel extruder with a 25:1 L/D ratio and a barrier screw, high-molecular-weight HDPE grades typically require barrel zones between 180 °C and 220 °C, with the head and die held within 200 °C to 230 °C. The exact profile for KM592L must be derived from the manufacturer’s recommended melt temperature and the measured head pressure. Excessive hold time above 240 °C should be avoided because thermo-oxidative chain scission can reduce parison melt strength and shift the solid-state impact response. If surface moisture is present from storage at relative humidity above 60%, a desiccant hopper set at 70 °C for 2 h is sufficient; HDPE is not hygroscopic in bulk, and prolonged drying at high temperature can promote pellet softening or fusion.
Die swell and parison sag must be characterised on the actual KM592L lot using a capillary rheometer under ISO 11443:2021. Shear viscosity should be mapped from 10 s⁻¹ to 1000 s⁻¹ at 190 °C, 210 °C, and 230 °C. High-melt-strength HDPE grades used in large-part blow moulding typically show a measurable swell increase when the die land length is shortened or the melt temperature is lowered; the resulting parison dimensions affect pinch-off weld integrity and container wall uniformity. Published data for this specific configuration is limited, so production-scale swell ratios should not be extrapolated from a general HDPE datasheet.
Environmental stress-crack resistance is not a single intrinsic value; it depends on comonomer type and placement, molecular weight, tie-molecule concentration, and the severity of the stress-cracking fluid. For rigid packaging and industrial containers, the bent-strip test under ASTM D1693-21 in a surface-active solution at 50 °C is a common sorting method, but lot acceptance for aggressive fluids should use slow crack growth data generated under ISO 16770:2019 at defined stress levels. A high-molecular-weight HDPE with a broad or bimodal molecular weight distribution may exhibit longer failure times at a given stress than a unimodal grade of similar density because the high-molecular-weight fraction increases the number of load-bearing tie molecules between lamellae. The KM592L datasheet should therefore be reviewed for molecular architecture indicators such as rheological ratio, bulk density, and the ratio of high-load melt index to standard melt-mass flow rate.
| Verification parameter | Standard method | Review objective for KM592L |
|---|---|---|
| Density | ISO 1183-1:2019 | Confirm HDPE class and crystallinity-related stiffness. |
| Melt-mass flow rate | ISO 1133-1:2022, 190 °C, 2.16 kg | Set extrusion and injection process severity. |
| High-load melt index | ISO 1133-1:2022, 190 °C, 21.6 kg | Estimate melt strength and parison sag resistance. |
| Tensile yield stress | ISO 527-2:2012 | Verify short-term load-bearing capacity. |
| Flexural modulus | ISO 178:2019 | Assess bending stiffness in large panels or sheets. |
| Notched Charpy impact | ISO 179-1:2010 | Detect low-temperature brittleness risk. |
| ESCR | ASTM D1693-21 or ISO 16770:2019 | Qualify for detergents, agrochemicals, or wetting agents. |
| Ash content | ISO 3451-1:2019 | Confirm additive loading and contamination limits. |
If KM592L is used for intermediate bulk containers or UN-certified packagings, the resin lot should also be tested with the finished-part drop and stack protocols required by the transport regulation. Resin-level ESCR data do not replace drop testing under ISO 2248:1985 or its current equivalent, hydraulic pressure testing for closures, and stack-load testing at elevated temperatures. The processing history at the converter can reduce slow crack growth resistance if weld-line cooling is too rapid or if regrind is incorporated beyond the qualified proportion. Regrind additions above 20 wt% should be revalidated because repeated shear and thermal exposure can shift the high-molecular-weight tail and alter the lot-to-lot viscosity profile.
HDPE KM592L is likely to be compared with linear low-density polyethylene and conventional unimodal HDPE when a converter selects a resin for a large rigid container, automotive duct, or industrial tank. The choice between HMW-HDPE and LLDPE is governed by stiffness, melt strength, chemical resistance, and low-temperature impact. High-density polyethylene provides a higher flexural modulus than LLDPE at equivalent thickness because of higher crystallinity, but it may exhibit lower puncture propagation resistance at freezer temperatures. For applications requiring stack strength at ambient or elevated temperature, the higher softening point of HDPE is normally advantageous. For applications requiring deep-point impact after sharp-edge abuse, an LLDPE-rich layer may be favoured unless the HDPE grade has a sufficiently high molecular weight and comonomer distribution to retain slow crack growth resistance.
| Material class | Density range | Typical flexural modulus range | Processing behaviour |
|---|---|---|---|
| TPC HDPE KM592L class | 0.940 to 0.967 g/cm³ depending on lot | High; verify with ISO 178:2019 | High melt strength; suitable for large parisons when MFR is low. |
| LLDPE | 0.915 to 0.925 g/cm³ | Lower; more flexible | Higher dart impact; lower modulus; may require wider die gap. |
| Unimodal HDPE injection grade | 0.950 to 0.965 g/cm³ | High; moderate toughness | High MFR; limited parison melt strength. |
In accumulator-head blow moulding, the decisive variable is often parison sag resistance after the accumulator discharge. A high-molecular-weight HDPE grade with low standard MFR and a broad molecular weight distribution can support longer parison lengths without excessive thinning. That property must be confirmed with the KM592L high-load melt index and not inferred from density alone. A converter running a 250 L open-head drum on a shuttle blow moulder may require a melt temperature high enough to maintain a smooth parison surface but low enough to prevent draw-down. If the KM592L lot shows a narrower processing window than the incumbent grade, the die gap, accumulator fill rate, and mould closing speed should be adjusted before increasing melt temperature, because higher melt temperature reduces parison integrity and increases cycle time.
Chemical compatibility of HDPE KM592L must be validated against the service fluid, not assumed from the generic polyethylene name. HDPE retains useful resistance to many aqueous acids, alkalis, and polar solvents at ambient temperature, but swelling or stress cracking may occur in aromatic hydrocarbons, chlorinated solvents, and some oxygenated hydrocarbons under sustained stress. The relevant immersion or stress-cracking exposure should follow ISO 22088-2:2006 or ASTM D543-21 with the chemical at the upper service temperature. If the part is used in a closed-loop mould-cooling application with glycol or detergent residues, testing should include the actual diluted mixture rather than a single reference surfactant. Published data for this specific configuration is limited, so a chemical compatibility study on the finished KM592L part is required before changing the service fluid.
Feedblock purging from a previous polypropylene campaign must be sequenced with an HDPE-compatible purge material. Contamination from propylene-based residues can reduce weld-line strength in large blow-moulded parts even when the bulk melt appears clear. The purge procedure should include a viscosity-matched HDPE purge, followed by a minimum residence-time soak at the recommended KM592L melt temperature, and then a visual verification of the melt stream together with melt-pressure stabilisation. A melt-pressure fluctuation greater than 2% after the breaker plate may indicate residual incompatible material or a partially blocked screen pack; the screen pack should be inspected when the head pressure rises above the lot-specific upper control limit.