Tpc Japan Hdpe Km590l

TPC (Japan) HDPE KM590L

    • Product Name: TPC (Japan) HDPE KM590L
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 949869
    Density 0.958 g/cm³
    Melt Flow Rate 0.35 g/10 min (190°C/2.16 kg)
    Tensile Strength At Yield 28.0 MPa
    Tensile Strength At Break 35.0 MPa
    Elongation At Break 800%
    Flexural Modulus 1.20 GPa
    Shore D Hardness 65
    Notched Izod Impact Strength 80 J/m
    Vicat Softening Temperature 124 °C
    Heat Deflection Temperature At 0 46 Mpa 75 °C
    Heat Deflection Temperature At 1 8 Mpa 45 °C
    Brittleness Temperature -70 °C
    Melting Point 133 °C
    Thermal Conductivity 0.40 W/m·K
    Coefficient Of Linear Thermal Expansion 1.2e-4 /°C
    Specific Heat Capacity 1.9 J/g·°C
    Dielectric Constant 2.3
    Dissipation Factor 0.0005
    Dielectric Strength 20 kV/mm
    Volume Resistivity 1e16 Ω·cm
    Water Absorption 0.01%

    As an accredited TPC (Japan) HDPE KM590L factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing TPC (Japan) HDPE KM590L is supplied in 25 kg multiwall paper bags, palletized with 40 bags per pallet (1,000 kg).
    Container Loading (20′ FCL) Container loading (20′ FCL) of TPC (Japan) HDPE KM590L, 25kg bags, palletized, shrink-wrapped, and securely stowed for ocean export shipment.
    Shipping Shipping description: TPC (Japan) HDPE KM590L is a non-hazardous high-density polyethylene resin. Not classified as dangerous goods under IMDG/IATA/ADR. Pack in 25 kg moisture-resistant bags or bulk containers, palletized and shrink-wrapped. Store cool, dry, away from heat, sunlight, and ignition sources. Handle with normal industrial hygiene; avoid dust generation and static discharge.
    Storage Store TPC (Japan) HDPE KM590L in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, and flames. Keep original bags sealed, palletized, and off the floor to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and excessive stacking. Use first-in, first-out stock rotation. Maintain clean, dry handling areas and follow local regulations. Store at ambient temperature.
    Shelf Life Stable under proper storage; recommended shelf life about 12 months in original unopened packaging, dry, cool, away from direct sunlight.
    Application of TPC (Japan) HDPE KM590L

    Pressure pipe extrusion with HDPE KM590L is anchored by the long-term hydrostatic design basis established under ISO 9080:2012. Where lot certification confirms PE100 classification, the compound demonstrates a minimum required strength of 10.0 MPa at 50 years and 20 °C; the allowable design stress is 8.0 MPa with a design coefficient of 1.25 under ISO 4427-1:2019. Extrusion on grooved-feed single-screw lines with L/D 30:1 to 36:1 and a barrier screw maintains melt temperature at 190 °C to 210 °C. Typical barrel profile is feed zone 170 °C to 180 °C, compression 190 °C to 200 °C, metering 200 °C to 210 °C; melt pressure before screen pack is held at 200 bar to 350 bar with a 60/100/60 mesh pack to remove contaminants and raise back pressure. The adapter and spiral mandrel die are held at 195 °C to 210 °C to avoid melt fracture while retaining hoop strength. Vacuum calibration at -0.2 bar to -0.6 bar and cooling water at 15 °C to 25 °C stabilise outer diameter and wall thickness. Field failure modes on production lines include internal die-lip deposits, surging from insufficient grooved-feed pressure, and wall-thickness eccentricity above ±0.2 mm when spider-leg temperature differentials exceed 5 °C. Potable water pipes are specified in SDR 17, SDR 13.6, SDR 11, and SDR 7.4 dimensions, corresponding to nominal pressure ratings of PN 10, PN 12.5, PN 16, and PN 25 for water at 20 °C; gas distribution lines under ISO 4437:2014 are commonly extruded in SDR 11. Slow crack growth resistance is verified through the notched pipe test of ISO 13479:2009 at 80 °C and 4.6 MPa hoop stress, with failure typically required beyond 500 h for PE100 compounds. Butt fusion welding is qualified under ISO 21307:2017; joint geometry, bead size, and interfacial pressure must follow the pipe manufacturer’s approved ranges. Where black pipe is produced, carbon black masterbatch is added at 2.0 wt% to 2.5 wt% and dispersion is assessed according to ISO 18553:2002. HDPE KM590L should not exceed 230 °C melt temperature during processing; higher temperatures accelerate oxidative degradation and shift the long-term hydrostatic strength regression curve.

    Pressure pipe design and test matrix for HDPE KM590L
    ParameterStandard / methodCondition or target
    Minimum required strengthISO 9080:201210.0 MPa at 50 years / 20 °C
    Design stress waterISO 4427-1:20198.0 MPa with coefficient 1.25
    Slow crack growthISO 13479:200980 °C, 4.6 MPa, > 500 h
    Melt temperature windowproduction control190 °C–210 °C
    Carbon black loadingISO 18553:20022.0 wt%–2.5 wt%

    What Limits Parison Sag During Extrusion Blow Moulding of KM590L?

    On an accumulator head line running HDPE KM590L, stable parison formation is recorded when melt temperature is held between 190 °C and 210 °C, die gap is set at 1.5 mm to 2.5 mm, and die swell is allowed to compensate for part radius rather than being suppressed by excessive drawdown. Large-part extrusion blow moulding of 25 L to 120 L open-head and tight-head drums, jerry cans, and intermediate bulk container liners uses parison programming with 10 to 50 axial points; wall thickness at the pinch-off zone is typically increased by 20% to 40% relative to the sidewall to offset thinning. Blow air pressure is set at 0.6 MPa to 0.8 MPa, and mould temperature is maintained at 10 °C to 20 °C for sufficient cooling. Cycle time for a 120 L drum falls in the range of 90 s to 180 s depending on wall thickness and post-cooling. Parison sag, not melt flow rate, is the limiting rheological defect; heavy preforms show observable necking when melt temperature drifts above 215 °C or when shot size exceeds the accumulator by more than 15% of nominal capacity. Transport packaging produced from HDPE KM590L is tested for dangerous goods under the UN Model Regulations, with design type qualification according to stacking, drop, and hydraulic pressure tests. Food-contact containers fall under FDA 21 CFR 177.1520 and EU 10/2011, but migration testing must be completed on the actual blow-moulded article. Stress crack resistance is specified by ASTM D1693-15 condition B; UN-certified containers for aggressive hydrocarbons and oxidising liquids require higher ESCR values and chemical compatibility testing. Pre-drying at 80 °C for 2 h to 4 h is recommended when resin has been stored at relative humidity above 60%, otherwise surface splay and pinhole defects appear. Colour concentrates at 1 wt% to 3 wt% must use a high-density polyethylene carrier; carriers based on low-molecular-weight waxes or incompatible LLDPE reduce impact toughness and ESCR.

    In landfill liner and heap leach pad construction, HDPE KM590L is extruded into 1.50 mm and 2.00 mm smooth or textured geomembrane on wide flat-die calender lines. The resin is compounded with carbon black masterbatch to achieve 2.0 wt% to 3.0 wt% carbon black content by ASTM D4218, with dispersion evaluated by ISO 18553:2002; poor dispersion creates localised oxidation sites and reduces stress crack resistance. Melt temperature at the flat die is held at 200 °C to 230 °C, calender roll temperatures are set at 60 °C to 90 °C, and haul-off tension is controlled to maintain dimensional tolerance within ±5% of nominal thickness. Wrinkles, gauge bands, and calender release marks are plant-observed defects traced to incorrect nip pressures, roll temperature differences exceeding 5 °C, or insufficient back tension. Geomembrane specification is governed by GRI-GM13 for landfill and mining applications. The compliance matrix includes density, carbon black content, oxidative induction time, tensile properties, tear resistance, and stress crack resistance. Welding on site uses hot-wedge fusion at 300 °C to 400 °C and is qualified by peel and shear tests under ASTM D6392 or ASTM D4437; field seams are traced by air-channel testing. HDPE KM590L should be stored out of direct sunlight and UV-protected packaging should remain intact until extrusion to preserve antioxidant package performance.

    Geomembrane compliance matrix for HDPE KM590L
    PropertyMethodControl target
    ThicknessASTM D51991.50 mm or 2.00 mm minimum average
    DensityASTM D1505≥ 0.940 g/cm³
    Melt flow indexISO 1133-1:2022<1.0 g/10 min at 190 °C/2.16 kg
    Carbon black contentASTM D42182.0 wt%–3.0 wt%
    Oxidative induction timeASTM D3895> 100 min at 200 °C

    Heavy-Gauge Sheet Thermoforming and the Melt Sag Window

    During heavy-gauge sheet extrusion of HDPE KM590L on a 120 mm single-screw line with a 2.4 m wide polished roll stack, melt temperature is maintained at 200 °C to 220 °C and roll stack temperatures are set from 60 °C to 90 °C. Sheet thickness ranges from 3 mm to 10 mm for thermoformed dunnage trays, automotive returnable packaging, and industrial cutting boards. HDPE KM590L sheet enters the vacuum forming station at a surface temperature of 165 °C to 185 °C; above 190 °C, heavy-gauge HDPE exhibits objectionable sag, non-uniform wall thickness, and webbing in deep-draw cavities. Female moulds are held at 80 °C to 100 °C to prevent premature freeze-off. Processors record cycle times of 60 s to 120 s for 4 mm sheet depending on draw ratio and plug assist settings. Regrind from skeleton trim is mixed back at up to 20 wt%; higher levels reduce Charpy impact strength and can shift thermoforming temperature downward. Food-contact applications require compliance with FDA 21 CFR 177.1520 and EU 10/2011; industrial returnable packaging is specified by load capacity, drop resistance, and stacking tests rather than food-contact standards. Moisture-related defects are uncommon but pre-drying at 80 °C for 2 h to 4 h is applied when exposed to relative humidity above 60%. Low-gloss or textured surfaces are obtained with embossed roll stacks; deep embossing reduces thickness at pattern bases and should be accounted for in the initial sheet gauge.

    When Carbon Black Masterbatch Dispersion Governs UV Service Life in Above-Ground Piping

    Because outdoor exposure adds ultraviolet oxidation to the normal 50-year design load, carbon black masterbatch at 2.0 wt% to 2.5 wt% is dispersed into HDPE KM590L for above-ground mining slurry lines, tailings overland pipes, and firewater ring mains. The particle size must be below 25 nm, and dispersion is rated under ISO 18553:2002; agglomerates larger than 60 μm create stress concentrations and reduce slow crack growth resistance. Accelerated weathering is evaluated under ISO 4892-2 or ISO 4892-3 with exposure to 0.51 W/m² at 340 nm and 60 °C black-panel temperature; retention of elongation at break after 3000 h is used to compare formulations rather than to predict service life. On production lines, inconsistent masterbatch feeding at the extruder throat causes alternating grey and black bands visible on the pipe surface; these bands correlate with reduced weathering resistance and are rejected by visual inspection. Mechanical design for above-ground HDPE KM590L pipe follows the same pressure rating as buried pipe but adds support spacing, thermal expansion restraints, and UV stabilisation. Thermal expansion is calculated at 0.15 mm/m·K to 0.20 mm/m·K; longitudinal expansion loops or slide supports are required for temperature swings above 20 °C. Hydrostatic design stress at elevated service temperatures is reduced by the derating factors of ISO 4427-1:2019; continuous service above 40 °C requires a shift to the appropriate SDR or a lower operating pressure. The finished pipe is joined by butt fusion under ISO 21307:2017, and electrofusion under ISO 12176-2. Published data for KM590L-specific weathering profiles in all global UV regimes is limited; outdoor service life must be confirmed by site-specific UV exposure and hydrostatic regression testing.

    Unlike tubular film grades in the 0.7 g/10 min to 1.2 g/10 min melt flow range, HDPE KM590L demands a high-stalk bubble configuration when coextruded as the stiffening core layer in heavy-duty industrial sacks and FIBC liners. Melt temperature at the die is held at 200 °C to 220 °C, blow-up ratio is set from 2:1 to 3:1, and frost line height is raised to 6 to 10 die diameters to stabilise the bubble. The HDPE layer, typically 20% to 30% of total film thickness, contributes flexural modulus and creep resistance to the coextruded structure; outer layers of LLDPE or mLLDPE provide dart impact and seal integrity. Dart impact is tested by ASTM D1709-16a, Elmendorf tear by ASTM D1922-15, and tensile modulus by ISO 527-3:2018. Published data for this specific configuration with HDPE KM590L is limited; film converters should qualify the grade on the target coextrusion line before final structure lock.

    Free Quote

    Competitive TPC (Japan) HDPE KM590L prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    TPC (Japan) HDPE KM590L is an extrusion blow-molding grade of high-density polyethylene intended for large containers, automotive fuel tanks, industrial packagings, and other thick-section applications in which environmental stress-cracking resistance and parison stability are primary constraints. Supplier technical literature identifies the resin by a nominal density of 0.955 g/cm³ and a high-load melt index of 5.9 g/10 min at 190 °C under 21.6 kg, measured in accordance with ISO 1133-1:2022. The L-suffixed stabilization package separates KM590L from general-purpose HDPE grades when long-term heat aging and repeated chemical contact are specified. In comparison with standard unimodal blow-molding HDPE of similar density, KM590L is differentiated by higher melt strength, longer environmental stress-cracking resistance, and a more restrictive thermal history requirement on accumulator-head machines. Typical product forms are natural or black pellets. All values stated in this document are representative supplier literature values and must be checked against the lot-specific certificate of analysis before production release.

    What Distinguishes KM590L from General-Purpose HDPE Blow-Molding Grades

    General-purpose HDPE blow-molding grades with comparable density often have high-load melt index values below 3.0 g/10 min and are aimed at small bottles or low-parison-weight parts. KM590L raises high-load melt index to 5.9 g/10 min without eliminating the high molecular weight fraction responsible for parison tension and weld-line integrity. This is achieved by a broad molecular-weight distribution and short-chain branch placement that arrests slow crack growth at the base weld and along the parting line. Grades with higher density above 0.958 g/cm³ may offer greater top-load stiffness but typically show shorter failure times in the bent-strip environmental stress-cracking test. At 0.955 g/cm³, KM590L retains sufficient crystallinity for top-load strength while maintaining F50 failure above 1000 h under ASTM D1693-21 condition B. Using the two-phase density model, this density corresponds to a crystalline volume fraction of approximately 65–70% when referenced to 1.000 g/cm³ for the crystalline phase and 0.852 g/cm³ for the amorphous phase.

    Representative property profile of TPC (Japan) HDPE KM590L from supplier technical literature
    Property Test method Representative value
    Density ISO 1183-1:2019 0.955 g/cm³
    High-load melt index, 190 °C/21.6 kg ISO 1133-1:2022 5.9 g/10 min
    Tensile stress at yield ISO 527-2:2012 27 MPa
    Tensile elongation at break ISO 527-2:2012 >600 %
    Flexural modulus ISO 178:2019 1200 MPa
    Notched Izod impact, 23 °C ISO 180:2019/A 25 kJ/m²
    Shore D hardness ISO 868:2003 63
    Vicat softening point, A50 ISO 306:2022 128 °C
    Brittleness temperature ASTM D746-20 < -80 °C
    Environmental stress-cracking resistance, 10% Igepal CO-630, condition B, F50 ASTM D1693-21 > 1000 h

    These values are representative; no single-point table can replace part-scale testing because blow molded wall thickness, weld-line orientation, and incorporated regrind shift final performance. The ASTM D1693-21 condition B value is especially sensitive to molded-in stress and specimen thickness, so chemical-contact service life should be confirmed on the final container geometry.

    On accumulator-head blow molding lines with 70–90 mm grooved-barrel extruders and 24:1–30:1 L/D barrier screws, the melt temperature should be profiled from 180 °C at the feed section to 200 °C at the die. The operating melt-temperature window is 190–210 °C. Extended residence time above 220 °C for more than 10 min can degrade the high molecular weight fraction and reduce pinch-off strength. If surface moisture exceeds 0.05 wt%, pre-drying at 80 °C for 4 h in a desiccant hopper dryer is recommended, especially when regrind content is above 20 wt%. Regrind addition should be validated for high-load melt index shift and contamination because accumulator shot-to-shot repeatability depends on consistent melt viscosity.

    Parison programming is mandatory for containers above 60 L. The parison should be programmed with a thicker section at the pinch-off zone and a thinner section near the moil to compensate for radial die swell and longitudinal sag. Die gap set points cannot be taken directly from capillary viscosity data because die swell and sag are strongly tooling-dependent; published data for this specific configuration is limited. Production settings should therefore be developed on the actual accumulator head and mold, using wall-thickness scanning of sectioned parts.

    Rheological Boundaries on Accumulator-Head Lines

    High-load melt index alone is a single-point quality-control value; it does not define the shear-thinning slope or elongational behavior of KM590L. The ratio of high-load melt index to low-load melt flow rate is used by processors as a qualitative indicator of molecular-weight distribution breadth. A lower low-load melt flow rate at a given HLMI indicates higher viscosity at low shear rates, which supports parison stability during hang times. Supplier technical bulletins do not always publish full capillary flow curves. Where those data are unavailable, the processor should characterize the grade at production rates using the actual die and accumulator head rather than extrapolating from ISO 1133-1:2022 data.

    In practical terms, barrel temperatures below 170 °C can produce excessive head pressure, melt fracture, and frost-line defects; temperatures above 220 °C accelerate parison drawdown and increase the risk of local gel formation at die stagnation points. A production tolerance of ±5 °C across the die circumference is required for uniform parison thickness. Die swell for high-molecular-weight HDPE grades commonly ranges from 35% to 60% depending on die land length, shear rate, and melt temperature; published data for this specific configuration is limited. Blended material outside an HLMI window of 5.4–6.4 g/10 min should not be used in dangerous-goods packaging without requalification, because wall-thickness variation and pinch-off inconsistency can exceed 10% on large parts.

    Color and additive packages affect the rheological and environmental stress-cracking response. Black concentrates containing carbon black above 2.0 wt% can increase stiffness and slightly reduce weld-line impact. Custom colors should be pre-dispersed in a compatible HDPE carrier; direct addition of liquid colorants can plasticize the melt and alter die swell. Masterbatch let-down ratios above 4 wt% should be validated for HLMI shift, because many carrier resins have higher melt flow than KM590L and will reduce parison stability.

    When Chemical-Contact Service Life Exceeds Standard HDPE Ratings

    Standard high-density blow-molding grades with density 0.952–0.954 g/cm³ often show environmental stress-cracking failure between 100 h and 500 h under ASTM D1693-21 condition B. KM590L is specified where the same test must exceed 1000 h because the container is exposed to surfactants, agricultural chemicals, stack loading, or outdoor storage. The improvement is not an elimination of stress cracking; it is a delay in crack initiation caused by a higher population of tie molecules and by comonomer units that resist disentanglement at weld lines. For strong oxidizing acids, aromatic hydrocarbons, or chlorinated solvents, compatibility must be validated on the final molded article, because processing orientation, weld-line geometry, and wall thickness dominate service life.

    Operational boundaries apply. Continuous service above 80 °C in oxidizing media is outside the normal design envelope. KM590L is not normally qualified as a PE100 pressure pipe resin and should not be substituted into pipe applications requiring ISO 9080 hydrostatic strength data. Avoid combinations with copper-based flame retardants or free-radical-generating additives beyond supplier-recommended concentrations, because these can consume the stabilizer package and reduce long-term heat aging. Food-contact use is typically addressed under FDA 21 CFR 177.1520 for olefin polymers, subject to extractive and additive limitations; EU food-contact verification should be performed on the final article under Regulation (EU) No 10/2011.

    In a 200 L tight-head industrial drum application, KM590L is selected not because it is the highest-stiffness HDPE but because the pinch-off weld retains impact strength and environmental stress-cracking resistance after molding. Compared with a lower-density HDPE film grade, KM590L has lower branch density and higher crystallinity, which increases top-load capacity and lowers permeation. Compared with a high-flow HDPE injection-molding grade, KM590L shows a much lower melt flow rate under 2.16 kg and a high molecular weight fraction that prevents parison drawdown and short-shot hesitation. Compared with a low-HLMI blow-molding grade, KM590L can be processed at moderate melt temperatures and is better matched to large shot sizes, but it requires stricter control of regrind and melt temperature to maintain parison uniformity. These differences are measurable in density, high-load melt index, and environmental stress-cracking failure time.

    Multilayer automotive fuel tank structures often use KM590L as the HDPE layer in combination with an EVOH barrier. Adhesion layers are required; the HDPE layer cannot be coextruded with EVOH without tie resin. Processing temperature of the tie resin and EVOH must not exceed the KM590L upper limit of 220 °C. The parison programming sequence should account for the higher melt strength of the HDPE layer relative to the tie resin and EVOH layers to avoid layer thinning at the pinch-off zone. Published data for this specific configuration is limited, so layer distribution must be verified by sectioning fuel tank walls and measuring barrier-layer thickness across the parting line.