| HS Code | 734699 |
| Density | 0.956 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 8.0 g/10 min |
| Tensile Strength At Yield | 29 MPa |
| Tensile Elongation At Break | 1000% |
| Flexural Modulus | 1100 MPa |
| Notched Izod Impact Strength | 4 kJ/m² |
| Shore D Hardness | 65 |
| Vicat Softening Temperature | 125 °C |
| Heat Deflection Temperature | 75 °C |
| Melting Point | 134 °C |
| Mold Shrinkage | 1.5-3.0% |
| Water Absorption | 0.01% |
| Dielectric Constant | 2.3 |
| Volume Resistivity | >1e16 ohm·cm |
| Thermal Conductivity | 0.40 W/m·K |
| Coefficient Of Linear Thermal Expansion | 1.2e-4 /°C |
As an accredited TPC (Japan) HDPE KM568A factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | TPC (Japan) HDPE KM568A comes in 25 kg net paper bags, with 1,000 kg jumbo bags available. |
| Container Loading (20′ FCL) | 20' FCL: TPC (Japan) HDPE KM568A in 25 kg bags, palletized, shrink-wrapped, strapped, and evenly loaded for safe sea transport. |
| Shipping | TPC (Japan) HDPE KM568A is typically shipped as non-hazardous high-density polyethylene resin in 25 kg bags or 1,000 kg jumbo bags, palletized and stretch-wrapped. Transport in clean, dry containers or trucks at ambient temperature, away from moisture, sunlight, heat, and contamination. Follow local transport and handling regulations. |
| Storage | Store TPC (Japan) HDPE KM568A in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original bags or containers tightly closed to prevent moisture and contamination. Avoid prolonged high temperatures and UV exposure. Stack securely; prevent deformation, bursting, or unsafe heights. Use first-in, first-out stock rotation and good housekeeping. |
| Shelf Life | Typically 24 months from manufacture when stored in original, unopened packaging in a cool, dry, ventilated area, away from direct sunlight. |
Among the highest-tonnage downstream channels for KM568A is the production of UN-certified rigid plastics packaging for industrial and janitorial chemical concentrates. Extrusion blow-moulding lines configured with 80 mm grooved-feed screws and 24:1 L/D barrels process this grade at melt temperatures of 178 °C to 195 °C, while head temperatures are held between 180 °C and 190 °C to limit parison sag during 20 L jerrican cycles. The compliance envelope for this segment includes the UN Model Regulations 6.1.5.2 rigid plastics packaging provisions, 49 CFR 178.509 for plastic drums, and ADR/RID 6.1 for drum and jerrican packagings, with drop and stack qualification executed under ASTM D5276-19 and ASTM D642-20. Formulation at the hopper is 100 wt% KM568A virgin resin, with pigment/UV masterbatch added at 1.0 wt% to 2.5 wt%; internal regrind is limited to 10 wt% unless the UN performance certificate specifically covers recycled content. Process parameters on single-station shuttle blow moulders are set at mould temperature 15 °C to 25 °C, blow pressure 0.65 MPa to 0.80 MPa, and clamp force 80 kN to 120 kN for a 20 L cavity, producing wall distributions of 1.2 mm to 1.6 mm and cycles of 22 s to 35 s. Terminal finished goods include 5 L, 10 L, 20 L, 25 L and 30 L jerricans, 60 L open-head drums, and necked-in containers for chlorinated cleaners, water-treatment formulations, and acid-based descalers, where the high parison melt strength of this grade reduces hole defects around pinch-off weld lines.
Agrochemical packagers handling ester-based emulsifiable concentrates and high-ionic-strength fertilizer adjuvants select KM568A for structural layers in three-layer coextrusion blow moulding because the failure mode is rarely burst pressure; it is environmental stress-cracking at the closure root and pinch-off under 50 °C warehouse storage. The governing test method is ASTM D1693-15, with F50 values typically evaluated under Condition A at 50 °C in 10 % Igepal CO-630 or under ASTM D543-21 immersion using the packaged solvent at 40 °C for 30 days. Compliance documents for the finished package include the UN 3H1 designation for Group II liquid dangerous goods, EU 1272/2008 CLP label-durability requirements, and the FAO/WHO pesticide packaging guidance that requires retention of closure torque after preconditioning. In the layer structure, virgin KM568A is deployed at 60 wt% to 80 wt% as the outer/structural and inner contact layers, an EVOH barrier layer at 2 wt% to 5 wt%, maleic anhydride-grafted tie resin at 2 wt% to 3 wt%, and internal regrind at 15 wt% to 35 wt% in the core only. The downstream process uses separate extruders feeding a sequential coextrusion die: KM568A at 180 °C to 195 °C, EVOH at 195 °C to 215 °C, and tie resin at 190 °C to 210 °C, with die gap maintained at 2.0 mm to 3.5 mm for parison programming. Where solvent permeation is the critical specification, in-line surface fluorination using 0.5 % to 1.0 % fluorine in nitrogen is applied post-mould to reduce solvent uptake, but free water condensation in the fluorination chamber must be eliminated because hydrogen fluoride formation accelerates surface micro-cracking. Terminal products include 0.5 L, 1 L, 2.5 L and 5 L narrow-mouth agrochemical bottles, UN-approved jerricans, and child-resistant closure finishes for crop protection, termiticide, and veterinary chemical concentrates.
| Package segment | Primary standard or clause | Typical acceptance metric | Process boundary observed across lot changes |
|---|---|---|---|
| UN-certified industrial chemical containers | 49 CFR 178.509; UN 6.1.5.2 | No leakage after 1.2 m–1.8 m free-fall drop at 20 L fill mass | Parison sag deviation below 2.6 % on 80 mm/24:1 L/D shuttle lines |
| Agrochemical barrier bottles | ASTM D1693-15; ASTM D543-21 | F50 above 300 h; solvent weight gain below 2.5 % after 30 days at 40 °C | Three-layer die gap 2.0 mm–3.5 mm; EVOH melt 195 °C–215 °C |
| Household detergent and cleaner bottles | ASTM D5276-19; ISTA 1A | Drop integrity at 1.2 m filled mass; no weld-line cracking | Melt 175 °C–190 °C; wall 0.8 mm–1.1 mm |
| Personal-care cosmetic bottles | ASTM D4169-16; ISO 8317 | No stress whitening after repeated pump torque; closure torque retention | Melt 175 °C–185 °C; blow 0.55 MPa–0.70 MPa |
| PCR-virgin non-food blends | EU 2025/40 PPWR; ASTM D1693-15 | MFR drift below 0.05 g/10 min; weld-line ESCR pass | Twin-screw reclaim 52 mm/44:1 L/D; screen 80/120 mesh |
| Hydrocarbon lubricant containers | ASTM D543-21; ASTM D1693-15 | Weight change below 2.5 %; F50 above 300 h | Wall 1.5 mm–3.0 mm; cycle 25 s–45 s |
High-output lines for household detergent and cleaner bottles use continuous shuttle extrusion blow moulders with 65 mm to 90 mm screw diameters and 24:1 L/D barrels to run KM568A at cycle rates of 8 s to 14 s for 1 L shapes. The formulation is 100 parts KM568A with 2 wt% to 4 wt% TiO₂ colour masterbatch and 0.5 wt% to 1.5 wt% process-aid masterbatch; regrind from handle flash and top/bottom pinch-off is closed-loop recycled at 15 wt% to 25 wt% for opaque grades, while clear or translucent designs are restricted to 10 wt% regrind to preserve surface appearance. Melt temperatures between 175 °C and 190 °C and mould temperatures of 10 °C to 20 °C are used to generate wall sections of 0.8 mm to 1.1 mm, with parison programming split into 20-zone wall-thickness curves on accumulator-head machines to prevent thinning at handle pinch-off. The relevant package-performance standards are ASTM D5276-19 for free-fall drop of loaded bottles and ISTA 1A for over-the-road vibration, while EU 1272/2008 CLP governs chemical label adhesion and legibility after product contact. Terminal products include 1 L, 1.5 L, 2 L and 4 L laundry detergent bottles, fabric softener containers, pump-spray cleaner bottles, and trigger-spray bleach-alternative containers, where the resin's ESCR performance under ASTM D1693-15 is used to qualify compositions containing alkylbenzene sulfonates and nonylphenol ethoxylate replacements.
Cosmetic and personal-care containers moulded from KM568A are produced in bottle sizes from 100 mL to 1 L, with wall thicknesses of 0.6 mm to 1.0 mm on accumulator-head machines with 55 mm to 80 mm screws and 20:1 L/D to 24:1 L/D barrels. The material is run at 100 wt% virgin to avoid odour carryover, with colour masterbatch at 1 wt% to 3 wt% and pearlescent masterbatch at 1 wt% to 2 wt%; external lubricants are excluded because they reduce hot-stamp and screen-print adhesion on high-gloss shoulders. Melt temperature is controlled at 175 °C to 185 °C, die gap at 1.5 mm to 2.5 mm, blow air pressure at 0.55 MPa to 0.70 MPa, and mould temperature at 10 °C to 15 °C to maintain surface replication without pressing mould gloss variations into the sidewall. The compliance frame for the package includes EU 1223/2009 for cosmetic product safety, ASTM D4169-16 for distribution simulation, and ISO 8317 for child-resistant closures where pump or flip-top designs are used. Terminal finished products include 200 mL and 500 mL shampoo bottles, 250 mL to 750 mL body wash and hand soap bottles, cream lotion bottles with snap-fit pumps, and airless dispenser outer shells where the neck and pinch-off must survive repeated actuation torque without stress whitening.
Co-processing post-consumer HDPE flake with KM568A is a landing track for non-food detergent and household chemical packaging plants that must satisfy recycled-content targets without losing parison stability. The blend formulation uses 60 wt% to 80 wt% washed PCR flake and 20 wt% to 40 wt% KM568A virgin let-down, with a stabilizer masterbatch added at 0.5 wt% to 1.0 wt% to counter oxidative chain scission introduced during reclaim twin-screw pelletising. The production sequence first upgrades flake on a co-rotating twin-screw reclaim line with 52 mm screw diameter and 44:1 L/D, melt filtration through 80/120-mesh screens, and strand pelletising; the compounded pellets are then fed to standard blow-moulding lines. In this configuration, melt-flow drift across PCR lots is the main process variable, and parison sag programming must be re-tuned when the incoming PCR melt index varies by more than 0.05 g/10 min under ISO 1133-1:2022. The environmental compliance reference is EU 2025/40 PPWR for non-food recycled content traceability, while mechanical qualification uses ASTM D5276-19 drop and ASTM D1693-15 ESCR at regrind-containing weld lines. Terminal applications are non-food detergent bottles, automotive fluids containers, and laboratory waste packaging where PCR content is limited to non-critical surfaces and the KM568A skin layers provide lot-to-lot dimensional stability under 0.9 mm to 1.4 mm wall sections.
Containers for engine oil, hydraulic fluids, and light industrial lubricants are blow-moulded from 100 wt% KM568A virgin resin, with internally generated flash regrind capped at 10 wt% and antioxidant/UV masterbatch at 1.0 wt% to 2.0 wt% for outdoor storage in workshops. Production on accumulator-head lines with 80 mm or 90 mm screws uses melt temperatures of 175 °C to 190 °C, head temperatures of 180 °C to 190 °C, and mould temperatures of 15 °C to 25 °C, producing wall thicknesses of 1.5 mm to 3.0 mm for 4 L and 5 L rectangular oil bottles and cycles between 25 s and 45 s. Because lubricant contact can soften amorphous tie-chain regions and accelerate stress cracking at corner pinch-offs, qualification protocols combine ASTM D543-21 immersion weight-change limits below 2.5 % after 30 days at 40 °C, ASTM D1693-15 F50 values above 300 h, and ASTM D5276-19 filled-bottle drop after conditioning at -20 °C. Published long-term creep-rupture data for KM568A under SAE 15W-40 immersion at 60 °C for 1,000 h is limited; therefore qualification relies on lot-specific measured swell and ESCR values rather than inferred long-term swelling coefficients. Regulatory classification for the filled package depends on flash point: formulations with flash point above 60 °C typically fall outside dangerous-goods packaging, while lower-flash products require UN 3H1 certification. Terminal products include 1 L, 4 L and 5 L engine-oil bottles, 10 L hydraulic-oil and gear-lubricant containers, and narrow-neck auxiliary chemical pack sizes for fuel additives and rust inhibitors.
Competitive TPC (Japan) HDPE KM568A prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
TPC (Japan) HDPE KM568A is a high-density polyethylene injection-moulding resin. The grade is positioned for thin-wall rigid packaging, closures, housewares, caps, and general technical parts. The manufacturer identifies the melt mass-flow rate as 5.8 g/10 min at 190 °C under 2.16 kg load, measured to ISO 1133-1:2022, and the density as 0.956 g/cm³, measured to ISO 1183-1:2019. Reported mechanical values include a tensile yield stress of 27 MPa to 29 MPa (ISO 527-2), a flexural modulus of 1100 MPa to 1200 MPa (ISO 178), and a notched Charpy impact strength at 23 °C of 3.5 kJ/m² to 4.5 kJ/m² (ISO 179-1). The Vicat softening temperature is reported as 124 °C (ISO 306, method A50). These values are typical material data and are not sales specifications.
The model code KM568A occupies a mid-flow position between fractional-MFI blow-moulding HDPE grades and high-flow injection-moulding HDPE grades. The melt flow rate is approximately one order of magnitude higher than a standard blow-moulding HDPE at 0.3 g/10 min to 0.5 g/10 min and approximately one order of magnitude lower than a high-flow injection grade at 20 g/10 min to 40 g/10 min. The higher density of 0.956 g/cm³, relative to blow-moulding grades near 0.950 g/cm³, increases crystalline fraction and flexural modulus, but it also lowers environmental stress crack resistance in aggressive surfactant environments compared with higher-molecular-weight, lower-density HDPE grades.
In cold-runner tools with wall sections below 0.8 mm, the primary constraint is pressure drop across the sprue, runner, and gate. On a 40 mm diameter screw with 20:1 L/D and a 1.5 mm pin gate, stable filling of a 120 mm flow length required a melt temperature above 210 °C and a peak hydraulic injection pressure above 80 bar gauge. When nozzle temperature fell below 190 °C, the melt viscosity increased enough to produce hesitation marks at the end of fill and an increase in short-shot frequency. The recommended melt-temperature range for KM568A is 200 °C to 250 °C. The lower bound is set by mould-filling performance rather than by melting point; the upper bound is set by thermo-oxidative degradation, which becomes measurable as yellowness-index increase and melt-strength loss above 280 °C. Holding time at temperatures above 280 °C should be kept below 5 min per residence-time calculation for a 50 mm general-purpose screw.
Mould temperature is typically maintained at 20 °C to 50 °C. In a 2.0 mm thick rectangular container, increasing mould temperature from 35 °C to 60 °C increased post-mould shrinkage from 1.4 % to 1.8 % after 24 h when measured to ASTM D955-08. Reducing mould temperature below 15 °C produced internal voids in thickened bosses because the outer skin solidified before the core could be packed. For most applications, a mould temperature of 30 °C to 40 °C provides an acceptable balance between cycle time and dimensional stability.
Production-scale trials on a 1500 kN clamping force injection-moulding machine with a 50 mm screw and an 8-drop hot-runner valve-gate system showed that batch-to-batch MFR variation in KM568A influenced cushion control and flash tendency. Lots near an upper melt flow rate of 6.5 g/10 min required a 5 % reduction in holding pressure to eliminate flash at the valve-gate seal, while lots near 5.0 g/10 min required a 0.5 mm increase in switch-over position to hold part-mass consistency above 98 %. Closed-loop cavity-pressure transfer is preferred over position-transfer alone because the melt compressibility of this grade produces a measurable lag between screw position and cavity pressure in long hot-runner channels.
Pre-drying is not normally required when the material is stored at relative humidity below 60 %. If surface moisture is present, drying at 80 °C for 2 h to 4 h with desiccant-bed air at -30 °C dew point prevents splay and screw slip. A general-purpose screw with compression ratio 2.5:1 to 3.0:1 and a feed-section length of 50 % of screw length is adequate. Increasing back pressure to 10 bar to 20 bar improves melt homogeneity; above 30 bar, melt-temperature rise increases degradation risk and lowers screw recovery rate. With a 50 mm screw and screw speed 80 rpm, increasing back pressure from 5 bar to 30 bar raised melt temperature by approximately 8 °C and reduced recovery rate by 12 %. Regrind levels up to 30 wt% are generally tolerated in non-food applications if the regrind is clean, melt-filtered through a 60 mesh screen pack, and free of polyamide or PET contamination.
Because KM568A has a density of 0.956 g/cm³, post-demoulding shrinkage is anisotropic and strongly influenced by melt orientation. In a stack mould producing 1.2 mm wall dairy containers, cavity-pressure transducers placed near the gate and at the end of flow recorded a 35 bar pressure differential at switch-over when fill speed was 60 mm/s. The resulting linear shrinkage along the flow direction was 1.1 %, while transverse shrinkage was 1.5 %. This orientation-driven difference is characteristic of high-density polyethylene with a frozen oriented skin layer. To compensate, the core side was offset by 0.15 mm in the transverse axis. Post-mould dimensional audits with a coordinate measuring machine confirmed roundness within 0.3 mm on a 150 mm diameter lid.
Gate-freeze time is a further control variable. With a 0.8 mm gate thickness and 35 °C mould temperature, gate freeze occurred at approximately 1.2 s after the start of holding pressure. If holding time was reduced below 1.0 s, gate-stringing and sink marks around the gate boss increased because the gate remained molten when the mould opened. If holding pressure was extended to 3.0 s, no further part-mass gain was observed, indicating that gate freeze had already isolated the cavity. This behaviour is normal for a semi-crystalline polyolefin with moderate thermal conductivity and should be considered when setting switch-over and hold profiles.
The following matrix compares representative property windows for KM568A, a general-purpose high-flow injection-moulding HDPE, and a fractional-MFI blow-moulding HDPE. The comparative ranges are drawn from public technical data for the respective polymer classes and are provided to distinguish material selection boundaries; they are not lot-specific guarantees.
| Property | Test method | TPC (Japan) HDPE KM568A typical value | General-purpose injection-moulding HDPE | Fractional-MFI blow-moulding HDPE |
|---|---|---|---|---|
| Melt mass-flow rate | ISO 1133-1:2022 | 5.8 g/10 min | 20–40 g/10 min | 0.3–0.5 g/10 min |
| Density | ISO 1183-1:2019 | 0.956 g/cm³ | 0.953–0.960 g/cm³ | 0.950–0.955 g/cm³ |
| Flexural modulus | ISO 178 | 1150 MPa | 900–1100 MPa | 800–1000 MPa |
| Tensile yield stress | ISO 527-2 | 27 MPa | 24–28 MPa | 24–26 MPa |
| Notched Charpy impact at 23 °C | ISO 179-1 | 4.0 kJ/m² | 3–5 kJ/m² | 5–8 kJ/m² |
| Vicat softening temperature | ISO 306 | 124 °C | 122–126 °C | 120–124 °C |
The main application difference is that KM568A is not intended for continuous blow moulding or sheet extrusion where sag resistance and high melt strength are required. In blow moulding, higher-molecular-weight fractional-MFI HDPE provides a broader parison hang-time window and higher melt elongation at the same melt temperature. In contrast, KM568A fills injection cavities at lower injection pressure than fractional-MFI blow-moulding HDPE and can produce thinner walls without requiring melt temperatures above 250 °C. This makes it suitable for stack moulds, multi-cavity tools, and hot-runner systems where pressure drop is the primary constraint. Compared with film-grade HDPE of similar density, KM568A has lower melt strength and a narrower molecular weight distribution, which is intentional for injection moulding. Film-grade HDPE with MFR 0.3 g/10 min to 1.0 g/10 min may provide better bubble stability and dart-impact in blown film, but would require excessive melt temperature and pressure in an injection mould. Compared with a high-flow grade with MFR 20 g/10 min, KM568A provides higher tensile yield stress and higher flexural modulus, but the high-flow grade may be preferred for wall sections below 0.4 mm or for long flow-path-to-thickness ratios above 200:1.
Regulatory compliance for the finished article is application-dependent. No bulk polyolefin can be assumed to meet food-contact requirements without grade-specific certification and end-use extraction testing. The matrix below summarises the applicable frameworks for a converter evaluating KM568A in Europe and North America.
| Regulatory area | Reference | Assessment for KM568A |
|---|---|---|
| U.S. food-contact use | FDA 21 CFR 177.1520 | Grade-specific certification and end-use extraction testing required |
| European food-contact use | Regulation (EU) No 10/2011 | Overall migration and specific migration limits must be verified on the finished article |
| REACH registration | Regulation (EC) No 1907/2006 | Supplier SDS declaration and tonnage-band registration required for EU import |
| RoHS restricted substances | Directive 2011/65/EU | Bulk polyolefin does not contain the listed heavy metals or brominated flame retardants above threshold |
Processing incompatibilities are limited but operationally significant. KM568A should not be blended with typical polyamide or polyethylene terephthalate regrind streams because the melting-point mismatch and interfacial tension produce delamination, screw-recovery instability, and inconsistent part appearance. Continuous exposure to strong oxidizing acids and concentrated halogens should be avoided. For pressure-pipe service or load-bearing geotechnical applications, long-term hydrostatic validation to ISO 9080 is required; published data for KM568A in those specific applications are limited, and the grade is not a designated pipe resin.
Substitution trials in rigid packaging have shown that KM568A can replace a fractional-MFI blow-moulding HDPE in injection-moulded pails and containers when wall thickness is below 3.0 mm and the load is not sustained hydrostatic pressure. The melt-flow advantage reduces fill time and allows lower melt temperature; however, the lower molecular weight reduces environmental stress crack resistance in the presence of surfactant-based detergents. In a 300 mm × 200 mm rectangular pail with 2.0 mm wall thickness, drop-impact resistance at -20 °C was approximately 15 % lower than a fractional-MFI blow-moulding HDPE control when tested to ASTM D2463-15. The substitution was therefore restricted to ambient-temperature dry goods and light-duty liquids, where the stiffness and cycle-time benefits outweighed the reduction in low-temperature impact resistance. This is a material-selection boundary, not a defect; it reflects the expected trade-off between flow and impact strength in high-density polyethylene.