Tpc Japan Hdpe Kl880c

TPC (Japan) HDPE KL880C

    • Product Name: TPC (Japan) HDPE KL880C
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 562286
    Density 0.954 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 0.05 g/10 min
    Tensile Strength At Yield 25 MPa
    Tensile Strength At Break 30 MPa
    Elongation At Break 500%
    Flexural Modulus 1.10 GPa
    Notched Izod Impact Strength 0.15 J/cm
    Hardness Shore D 65
    Vicat Softening Point 123°C
    Heat Deflection Temperature 0 46 Mpa 70°C
    Brittleness Temperature -70°C
    Dielectric Constant 2.3
    Volume Resistivity 1e16 ohm·cm
    Water Absorption 0.01%
    Thermal Conductivity 0.40 W/m·K
    Coefficient Of Linear Thermal Expansion 1.2e-4 cm/cm/°C
    Specific Heat 2.30 J/g·°C
    Environmental Stress Crack Resistance Escr >1000 h
    Melting Point 130°C

    As an accredited TPC (Japan) HDPE KL880C factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing TPC (Japan) HDPE KL880C is supplied in 25 kg multiwall paper bags, 40 bags per pallet (1,000 kg).
    Container Loading (20′ FCL) 20′ FCL container loaded with TPC (Japan) HDPE KL880C, 25 kg bags, palletized, shrink-wrapped, seaworthy export packing for ocean transport.
    Shipping TPC (Japan) HDPE KL880C is a non-hazardous high-density polyethylene resin in pellet form. It is not classified as dangerous goods. Typically shipped in sealed 25 kg bags or jumbo bags, palletized, kept dry, and away from heat, sunlight, and contamination. General cargo handling applies.
    Storage Store TPC (Japan) HDPE KL880C indoors in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, and open flames. Keep original containers or bags tightly closed to prevent moisture, dust, and contamination. Use clean pallets, avoid excessive stacking, rotate stock, and keep away from strong oxidizing agents and incompatible chemicals. Follow local regulations and supplier SDS.
    Shelf Life Shelf life is typically 24 months when stored in original unopened packaging, cool, dry, and away from direct sunlight.
    Application of TPC (Japan) HDPE KL880C

    On accumulator-head shuttle blow moulding lines producing 20–30 L jerrycans, TPC (Japan) HDPE KL880C is processed through a 60 mm grooved-feed extruder with L/D 24–30 and a barrier screw. The melt temperature is held at 185–200 °C ahead of the die head; die head temperature is set at 190–195 °C. The parison die gap is 1.6–2.4 mm with a land length of 14–20 mm. A 10–20-point parison programmer increases wall thickness 20–35% at the neck and pinch-off zones. Preblow is initiated at 0.15–0.25 MPa, final blow at 0.6–0.8 MPa, into a mould cooled to 8–15 °C. Cooling time is governed by the 3–4 mm sidewall section. Demoulding is initiated when the outer surface reaches 55–65 °C. For dangerous-goods packagings, the moulded article is subjected to leakproofness, hydraulic pressure, and drop tests under UN Model Regulations Chapter 6.1. Environmental stress-crack resistance is assessed by ASTM D1693 Condition B, 100% Igepal CO-630, with lot acceptance normally specified as F50 greater than 600 h for chemical jerrycans; the supplier certificate of analysis remains the governing document. Food-contact articles require olefin polymer compliance under FDA 21 CFR 177.1520(c) and the overall migration limit of 10 mg/dm² under EU Regulation 10/2011 Annex I. End products include UN-rated 20–30 L jerrycans, IBC inner bottles, agricultural chemical containers, and multilayer barrier bottle outer layers. Pre-drying at 80 °C for 2 h is required if pellets have been stored at relative humidity above 60% because surface condensation produces splay and pinholes. Melt temperatures above 210 °C should be avoided due to parison sag and loss of wall-thickness control.

    What limits injection moulding cycle time when a fractional-melt HDPE is used in crate tooling?

    Cycle-time penalties in thick-wall HDPE crate moulding stem from differential shrinkage and slow heat transfer through 4–6 mm walls. The melt is injected at 200–250 °C, with peak injection pressure 80–120 MPa and holding pressure 50–70% of peak. Mould temperature is maintained at 10–30 °C, using turbulent-flow water channels of 8–10 mm diameter. Screw specifications for KL880C in injection moulding are L/D 20–24, compression ratio 2.5–3.0, and back pressure 0.5–1.5 MPa. Gates are placed to limit flow length to wall thickness ratio below 150:1; rib thickness is held at 50–60% of the nominal wall. Shrinkage is measured by ASTM D955 and typically falls in the range 1.8–2.5% parallel to flow for HDPE homopolymer. Warpage occurs when shrinkage differential between flow and transverse directions exceeds 0.5 percentage points; this is mitigated by balanced gate positioning and post-mould fixturing. Tensile yield is determined by ISO 527-2, flexural modulus by ISO 178, Izod impact by ISO 180/A, and deflection temperature by ISO 75-2 at 0.45 MPa. Compliance for returnable distribution crates and automotive component trays is established against RoHS 2011/65/EU Annex II homogeneous-material limits: lead < 1000 mg/kg, cadmium < 100 mg/kg, mercury < 1000 mg/kg, and hexavalent chromium < 1000 mg/kg. REACH candidate-list SVHC content above 0.1% by weight must be declared at article level. End products include returnable dairy crates, logistics totes, pallet boxes, and automotive kitting trays. Short shots may occur in thin-wall sections below 2 mm because KL880C is not an easy-flow injection grade; published data for spiral-flow length in this specific formulation is limited.

    Blown film bubble geometry and the control of stalk height

    In blown film lines running KL880C, a stalk bubble configuration is used because high-molecular-weight HDPE requires a longer melt relaxation distance before the frost line. A barrier screw extruder of L/D 30–33 feeds a 250–400 mm die with die gap 1.2–1.8 mm. The blow-up ratio is set at 3:1–4:1, stalk height at 6–8 die diameters, and frost-line height at 8–10 die diameters. Melt temperature at the die lip is held at 190–220 °C; lower temperatures increase melt fracture, while higher temperatures reduce bubble stability. Output rates on a 400 mm die may reach 300–400 kg/h depending on screw cooling and air-ring configuration. Film gauge is typically 8–25 µm. Tensile properties are tested by ISO 527-3, Elmendorf tear by ASTM D1922, dart drop by ASTM D1709 Method A, and coefficient of friction by ASTM D1894. Food-contact film requires FDA 21 CFR 177.1520(c) compliance and EU Regulation 10/2011 overall migration below 10 mg/dm². Packaging and packaging waste compliance under Directive 94/62/EC requires the sum of lead, cadmium, mercury, and hexavalent chromium to be below 100 mg/kg in the packaging article. End products include T-shirt bags, produce bags, industrial liners, and hygiene packaging overwrap. A common failure mode is bubble instability at high stalk height when ambient air velocity exceeds 1.5 m/s; the line should be shielded from cross-drafts.

    Before thermoforming, sheet extrusion from KL880C is constrained by sag and residual orientation in the machine direction. A 90–120 mm extruder with L/D 30–34 feeds a flat die of 900–1500 mm width. Melt temperature is kept at 200–225 °C, and the polish roll stack is set at 85–95 °C upper and 80–90 °C lower. Sheet thickness from 2–6 mm is produced for cut-sheet thermoforming. The sheet is reheated to 130–140 °C surface temperature in a tunnel oven with ceramic elements; plug-assisted vacuum forming uses an aluminium plug at 100–110 °C, with forming pressure of 0.5–0.8 MPa. Draw ratios are limited to 2:1–4:1 to prevent corner thinning below 60% of nominal wall. Density is verified by ISO 1183-1, tensile properties by ISO 527-2, Vicat softening temperature by ISO 306/A50, and Charpy impact by ISO 179-1. For automotive dunnage and material handling trays, flammability is assessed by FMVSS 302 or ISO 3795. End products include reusable transit trays, dunnage sheets, appliance liners, and automotive interior substrates. Pre-drying at 80 °C for 2 h is applied if outdoor storage in humid conditions is used. Roll temperatures above 100 °C cause sheet surface adhesion to the polished rolls and should be avoided.

    Downstream segmentRegulation / standardTest method / clauseTypical numerical criterion
    Blow-moulded food-contact containersFDA 21 CFR 177.1520(c)Olefin polymer extractable fractionMaximum extractable by end-use condition A–H
    Blow-moulded food-contact containersEU Regulation 10/2011 Annex IOverall migration10 mg/dm²
    UN-rated jerrycansUN Model Regulations Chapter 6.1Drop, stacking, leakproofnessNo leakage or rupture for packing group II
    Injection-moulded cratesRoHS 2011/65/EU Annex IIXRF screening / wet chemistryPb < 1000 mg/kg, Cd < 100 mg/kg
    Packaging filmDirective 94/62/ECHeavy-metal packaging limitSum Pb+Cd+Hg+Cr6+ < 100 mg/kg
    Drainage pipeEN 13476-1 / ASTM F2306Ring stiffness / creep ratioSN4 or SN8 at 3% deflection
    WPC deckingREACH 1907/2006SVHC article notification0.1% w/w per candidate-list substance

    When corrugated HDPE pipe substitutes reinforced concrete or PVC in drainage lines

    In buried drainage installations that replace 300 mm reinforced concrete pipe with corrugated HDPE profile, ring stiffness and creep ratio govern design. A 75 mm extruder with L/D 30–33 delivers melt at 190–210 °C to a corrugator with vacuum-forming mould blocks. The outer wall is 0.8–1.5 mm, the inner wall 0.6–1.2 mm, and the corrugation pitch is set to achieve the specified moment of inertia. Ring stiffness is tested by ISO 9969 and is specified as SN4 or SN8, corresponding to 4 kN/m² or 8 kN/m² at 3% deflection. Creep ratio is determined by ISO 9967; values above 4 trigger a downgrade in burial depth capacity. For the U.S. market, product is evaluated under ASTM F2306 for 10–30 in. corrugated HDPE pipe and AASHTO M294 for highway drainage. Environmental stress-crack resistance is measured by ASTM D1693 Condition A or B, with a minimum F50 often specified at 24 h for corrugated drainage profiles; published data for KL880C in this specific configuration is limited, and lot-specific high-load melt flow must be verified by ISO 1133-1:2022. End products include stormwater culverts, agricultural drainage laterals, cable duct sleeves, and leachate collection lines. Avoid melt temperatures above 220 °C because oxidative gel formation blocks the vacuum slots in the corrugator blocks.

    Drawing monofilament: quench bath kinetics and two-stage orientation

    For 1.0–1.2 mm monofilament, quench bath residence time is set at 8–15 s before the first draw stage. KL880C is extruded through a spinneret with hole diameter 0.8–1.6 mm at melt temperature 200–250 °C. The air gap is 20–50 mm, and the water bath is held at 30–40 °C. First-stage drawing at 4:1 is performed in hot water at 90–95 °C; second-stage drawing at 1.5–2.0:1 is performed in a hot-air oven at 105–110 °C. Total draw ratio is 7–10:1, followed by 5–8% relaxation in a heated annealing zone. Tensile tenacity and knot strength are evaluated by ISO 2307 or ASTM D2256. UV-stabilised formulations are assessed by ISO 4892-2 for accelerated weathering before use in aquaculture cage netting or safety nets. End products include Raschel knotless netting, safety nets, geogrid filaments, and agricultural support twine. The process is sensitive to quench-water temperature variation above ±2 °C; inconsistent cooling produces diameter variation that lowers draw consistency.

    Wood-plastic composite compounding with KL880C as the matrix phase begins with moisture control, not melt temperature. Wood flour at 50–60 wt% is pre-dried to below 1% moisture before feeding into a co-rotating twin-screw extruder of L/D 44–48 and screw diameter 75–92 mm. KL880C comprises 30–40 wt% of the formulation; maleated polyethylene coupling agent is added at 2–3 wt%, and zinc stearate or PE wax lubricant at 1–2 wt%. Melt temperature is held at 170–190 °C to limit thermal degradation of lignocellulosic filler. Venting is run with vacuum below -0.08 MPa at two ports to strip moisture and volatiles. Extruded profiles are cooled in a spray calibration tank at 15–25 °C and cut. Flexural modulus is tested by ASTM D790, water absorption by ASTM D570, and creep response by ISO 899-2. For deck boards, ASTM D7031 and EN 15534-1 provide the specification framework. Flame performance for interior use is assessed by EN 13501-1; most unfilled HDPE/WPC formulations achieve Euroclass E without fire retardants. Compliance with REACH 1907/2006 requires SVHC content below 0.1% w/w, and RoHS 2011/65/EU applies to electrical and electronic equipment housings if the profile is used as a component. End products include deck boards, railing profiles, fencing slats, and automotive interior substrates. Avoid amine-based lubricants in this compound because amine groups can compete with the maleated coupling agent for wood-fibre surface sites and reduce interfacial adhesion.

    Free Quote

    Competitive TPC (Japan) HDPE KL880C prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    TPC (Japan) HDPE KL880C is a high-molecular-weight high-density polyethylene extrusion resin specified for corrugated drainage pipe, buried non-pressure conduit, and structural sheet. The grade is supplied as a carbon-black-stabilized compound with a nominal density of 0.958 g/cm³ determined to ISO 1183-1:2019. The melt mass-flow rate at 190°C and 5 kg is 0.28 g/10 min, and the high-load melt mass-flow rate at 190°C and 21.6 kg is 8.5 g/10 min, both tested to ISO 1133-1:2022. The resulting melt flow ratio of approximately 30:1 indicates a broad molecular weight distribution. Carbon black content is controlled in the range 2.0–2.5 wt% by ISO 6964, which contributes to ultraviolet resistance in above-ground sections of drainage systems. The product is not characterized by spiral-flow length or thin-wall injection-moulding behavior; its release basis is extrusion rheology rather than high-shear injection viscosity alone.

    In corrugated pipe extrusion, the 21.6-kg high-load melt flow rate is more informative than the 5-kg value because it applies higher shear stress to the high-molecular-weight fraction. A shift of ±0.5 g/10 min in the 21.6-kg value can produce measurable changes in die-head pressure and parison sag. On a 150 mm grooved-feed single-screw extruder, the pressure change is typically 5–10%, requiring a screw-speed correction of 2–5 min⁻¹ to maintain constant mass throughput. A value above 9.5 g/10 min is treated as a wall-thickness sag risk during the mold-block vacuum phase, while a value below 7.5 g/10 min is evaluated for excessive screw torque and melt-temperature rise.

    Slow crack growth resistance of KL880C is assessed by environmental stress cracking resistance to ASTM D1693-21 in 10% Igepal CO-630 at 50°C. Manufacturer-published data list an F50 exceeding 1000 h, although published data for this specific configuration are limited and should be confirmed on the production lot. This ESCR level is relevant because corrugated drainage pipe develops stress concentrations in the root of each corrugation; a lower-ESCR unimodal HDPE can exhibit root cracking under long-term soil load. High ESCR in KL880C is associated with a broad molecular weight distribution and controlled comonomer placement rather than low crystallinity alone. The density of 0.958 g/cm³ is high enough to retain ring stiffness after the pipe is formed.

    Why does high-load melt flow rate exert more control over corrugated pipe wall thickness than density alone?

    The corrugator vacuum pulls the melt into the mold block; if the high-molecular-weight fraction is too low, the parison thins at the corrugation roots before cooling. Density controls bulk stiffness but does not control this extensional-flow behavior. The 5-kg value of 0.28 g/10 min is below the practical resolution limit of some laboratories because of the long measurement interval, so the 21.6-kg value of 8.5 g/10 min is used as the production control. The ratio of the two values is used to detect cross-contamination with a blow-moulding or film grade. If the 5-kg value rises above 0.35 g/10 min while density remains inside specification, the melt flow ratio drops below 24:1 and the material is quarantined for cap-layer trials rather than structural pipe extrusion. This is not a cosmetic issue; it indicates loss of the high-molecular-weight fraction and a measurable reduction in ASTM D1693 F50.

    For large-diameter corrugated drainage pipe, KL880C is run on grooved-feed single-screw extruders with screw diameters of 120–200 mm and L/D ratios of 30:1–36:1. Barrel zone temperatures are typically 180–210°C from feed to metering, with die zones at 195–215°C and measured melt temperature 199–213°C. Back pressure is maintained between 20 MPa and 30 MPa. Screen packs of 40/60/80/40 mesh are common. Pre-drying is not required when the resin is stored below 60% RH; if ambient relative humidity exceeds 70% RH, surface moisture can generate micro-voids and die-face streaking. A desiccant hopper with a dew point of −40°C or lower is used for moisture-sensitive jobs. Pipe wall thickness is controlled to ±0.2 mm at normal line speeds. Melt temperature above 220°C can increase die-lip build-up and carbon black dispersion defects; below 195°C, the melt may show poor mold-block filling and high amperage.

    When KL880C is evaluated as a direct substitute for a conventional unimodal blow-moulding HDPE in structural sheet, where do the processing boundaries appear?

    In structural sheet and thick-walled corrugated board applications, KL880C differs from a generic unimodal blow-moulding HDPE with similar density by exhibiting higher melt strength and lower shear thinning. The melt curtain retains width stability at wider die gaps, but the extruder screw recovery characteristics are different. The 21.6-kg flow of 8.5 g/10 min is not directly substitutable for a blow-moulding resin with the same 21.6-kg value if the 5-kg value is 0.40 g/10 min; the latter will have lower head pressure and may require a different screw temperature profile. Comparative data for this equipment-specific substitution are limited, and tooling tryouts are required before conversion. In blow-moulding accumulator heads, KL880C can produce higher die swell and longer parison hang time, which may require a reduction in head temperature of 5–10°C to match container wall-thickness distribution.

    Systematic comparative matrix for KL880C, PE100 pressure pipe resin, and unimodal blow-moulding HDPE
    ParameterTPC HDPE KL880CPE100 pressure pipe resinUnimodal blow-moulding HDPE
    Nominal density, ISO 1183-10.958 g/cm³0.949–0.953 g/cm³0.950–0.954 g/cm³
    High-load MFR, 190°C, 21.6 kg, ISO 1133-18.5 g/10 min8.0–12.0 g/10 min5.0–10.0 g/10 min
    MFR, 190°C, 5 kg, ISO 1133-10.28 g/10 min0.25–0.35 g/10 min0.30–0.45 g/10 min
    ESCR F50, 10% Igepal, ASTM D1693>1000 h>1000 h200–500 h
    Pressure rating to ISO 4427-1Not ratedPE100Not rated
    Primary processing windowCorrugated pipe, sheet extrusionExtrusion pressure pipeBlow moulding, large containers

    The comparative matrix identifies the central difference: KL880C is not a pressure-pipe resin. It is not assigned an MRS class under ISO 4427-1:2019 and must not be used for potable water or gas distribution under continuous hydrostatic pressure. In contrast, a PE100 resin with similar high-load MFR is designed for 10.0 MPa minimum required strength at 50 years and 20°C. KL880C is specified for non-pressure drainage and conduit applications where soil deflection and long-term ring stiffness, rather than internal pressure, govern lifetime. In buried corrugated pipe manufactured to EN 13476-2 or ASTM F2306, the product is selected for root-cracking resistance and crush strength.

    Compliance and regulatory status matrix for KL880C
    Regulatory or standard referenceApplicabilityVerification requirement
    EU 10/2011Food-contact plasticsNot provided as a routine release; lot-specific migration testing required
    FDA 21 CFR 177.1520Olefin polymers for food contactNot automatically granted for carbon-black pipe grades; verify finished article
    REACH (EC) No 1907/2006Registration and SVHC disclosureRequired at material level
    RoHS 2011/65/EUHomogeneous materials in electrical and electronic equipmentPolymer matrix usually below restricted limits; lead, cadmium, mercury, chromium VI not deliberately added
    EN 13476-2Corrugated drainage pipeFinished pipe performance depends on processing and design
    ISO 4427-1Pressure pipeNot applicable to KL880C

    Material handling at the conversion site affects whether KL880C performs at the stated ESCR and ring-stiffness levels. The carbon-black-stabilized pellets should be stored in a dry area at 20–30°C; prolonged storage above 40°C can oxidize pellet surfaces and increase gel content. Regrind from corrugated pipe can be blended at 10–20 wt% without loss of root-wall integrity when the regrind is dry and screen-filtered through a 40/60 mesh pack. Higher regrind levels, especially with wet regrind or fine dust, produce variable carbon black dispersion and lower slow crack growth resistance. The operational boundary is set by retention of ASTM D1693 F50 relative to virgin pellets; if a plant trial falls below the established lot-specific retention threshold, the blend ratio is reduced or the regrind is diverted to non-structural conduit.