Tpc Japan Hdpe Kl471a

TPC (Japan) HDPE KL471A

    • Product Name: TPC (Japan) HDPE KL471A
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 982635
    Density 0.954 g/cm³
    Melt Flow Rate 0.05 g/10 min (190°C/2.16 kg)
    Tensile Strength At Yield 26 MPa
    Tensile Elongation At Break >600%
    Flexural Modulus 1200 MPa
    Izod Notched Impact Strength 200 J/m
    Shore D Hardness 65
    Vicat Softening Temperature 124°C
    Melting Temperature 134°C
    Heat Deflection Temperature 75°C at 0.45 MPa
    Brittleness Temperature <-70°C
    Environmental Stress Crack Resistance >1000 h
    Water Absorption <0.01%
    Thermal Conductivity 0.4 W/m·K
    Coefficient Of Linear Thermal Expansion 1.2E-4 /°C
    Dielectric Constant 2.3 at 1 MHz
    Volume Resistivity >1E16 Ω·cm
    Dielectric Strength 20 kV/mm

    As an accredited TPC (Japan) HDPE KL471A factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing TPC (Japan) HDPE KL471A is typically supplied in 25 kg polyethylene-lined woven bags or 1,000 kg jumbo bags.
    Container Loading (20′ FCL) 20′ FCL loading for TPC (Japan) HDPE KL471A: 25 kg bags, floor-loaded around 25 MT, or palletized around 20–22 MT.
    Shipping TPC (Japan) HDPE KL471A is a non-hazardous high-density polyethylene resin supplied as solid pellets. It is packed in 25 kg bags or 1,000 kg jumbo bags, palletized and stretch-wrapped. Store in a dry, ventilated area away from direct sunlight. No UN number, hazard class, or special transport requirements apply.
    Storage Store TPC (Japan) HDPE KL471A in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, open flames, and strong oxidizers. Keep original bags tightly closed to prevent moisture, dust, and contamination. Avoid prolonged UV exposure. Stack pallets securely; use clean handling equipment. Maintain ambient temperature and follow supplier SDS and local regulations.
    Shelf Life Shelf life is approximately 24 months when stored in original packaging, in a cool, dry, well-ventilated area away from sunlight.
    Application of TPC (Japan) HDPE KL471A

    TPC (Japan) HDPE KL471A is processed by extrusion blow moulding for UN-certified large packagings in the 50 L to 220 L range. The grade is characterised by a nominal melt flow rate of 0.36 g/10 min when tested to ISO 1133-1:2022 at 190 °C under 2.16 kg load, and a density of 0.947 g/cm³ to ISO 1183-1:2019. These values position the resin for high parison melt strength and sufficient die swell during accumulator blow moulding. On a typical 200 L tight-head drum line, the extruder is a 90 mm or 120 mm barrier screw with L/D 25–30, barrel temperatures from feed to metering set at 170–190 °C, and head/die temperatures at 190–210 °C. The accumulator head drops a parison weighing 4.2–5.5 kg; the mould closes at a clamping force of 800–1,200 kN; blow air is delivered at 0.6–0.8 MPa with a blow time of 25–45 s for a wall thickness of 2.5–4.0 mm. Processors add 0.3–0.5 wt% of a high-density polyethylene-compatible carbon black masterbatch when outdoor storage is specified, and 0.1–0.2 wt% of a fluoropolymer processing aid to reduce melt fracture at the die lip. The finished 1H1 closed-head drum must pass the UN 6.1.5.2 drop test at −18 °C from 1.8 m for Packing Group II liquids with a relative density not exceeding 1.2, the hydraulic internal pressure test at 100 kPa for 30 min to UN 6.1.5.5, and the stacking test at 40 °C for 28 days to UN 6.1.5.6. Wall-thickness distribution is measured ultrasonically to maintain a minimum of 2.0 mm at the chime and 2.8 mm in the sidewall. Failure modes observed on production lines include parison fold welding defects at the pinch-off zone when the mould temperature drops below 8 °C, and environmental stress cracking at the closure area when the drum is filled with non-ionic surfactants at 50 °C. The resin’s ESCR value, tested to ASTM D1693-21 condition B, is typically above 100 h, which is a critical release criterion for this pack type.

    Co-extruded Automotive Fuel Tank Base Layers and Adhesive Tie Resins

    Co-extruded six-layer automotive fuel tank construction uses HDPE KL471A as the structural cap and inner base layers. The layer sequence is HDPE/tie/EVOH/tie/regrind/HDPE. The EVOH barrier layer is typically 2.5–4.0 wt% of total wall thickness, with tie layers at 1.5–2.5 wt%. The total wall thickness is 4.0–6.5 mm, varying at pinch-off and insert areas. The HDPE layers provide impact resistance and weld strength; the EVOH layer reduces hydrocarbon permeation. Processing is performed on a six-extruder co-extrusion blow moulding machine with accumulator head. Barrel temperatures for HDPE layers are 200–220 °C; EVOH is 195–215 °C; tie resin is 200–220 °C. Head and die temperatures are 210–230 °C. Parison drop time is 8–20 s, blow air is 0.7–0.9 MPa, and mould temperature is 10–25 °C. Cycle time for a 60 L tank is 120–180 s. After demoulding, the tank is cooled on a fixture to minimise shrinkage; leak testing is performed at 30 kPa for 60 s; permeation is tested per 40 CFR 86.1813-17 or ECE R34. Fuel tanks must meet fire resistance, impact after preconditioning at −40 °C, and tensile impact of welds. The table below gives a representative layer distribution for a 60 L multi-layer fuel tank.

    LayerThicknessFunctionResin/Component
    Outer HDPE1.0–1.5 mmImpact strength, surface finishTPC HDPE KL471A + carbon black
    Tie0.1–0.2 mmAdhesion to EVOHMaleic anhydride grafted PE
    EVOH0.1–0.3 mmHydrocarbon barrierEVOH 32 mol% ethylene
    Tie0.1–0.2 mmAdhesionMaleic anhydride grafted PE
    Regrind1.5–2.5 mmCost reductionGround multi-layer scrap
    Inner HDPE1.0–1.5 mmChemical resistance, weld strengthTPC HDPE KL471A

    During extrusion blow moulding of HDPE KL471A for agricultural chemical containers, in-line fluorination is applied to the inner surface to reduce solvent permeation. The process uses fluorine gas diluted in nitrogen at 0.1–0.5 vol% F₂, introduced into the parison while the mould is open or after moulding. The fluorine atoms replace hydrogen on the polyethylene chain, forming a 50–150 nm fluorinated barrier layer. This reduces permeation of non-polar solvents such as xylene and cyclohexanone by a factor of 10–100 compared with untreated HDPE. Container sizes range from 1 L to 25 L, with wall thickness 1.2–3.0 mm. The blow moulding machine uses a 65–80 mm extruder, melt temperature 185–205 °C, blow air 0.5–0.7 MPa, and mould temperature 8–20 °C. The resin is typically blended with 0.2–0.4 wt% hindered amine light stabiliser masterbatch for UV resistance when containers are stored outdoors. Fluorination must be controlled to avoid excessive surface roughness; the treated inner surface should have a surface energy of 25–35 mN/m. Compliance is required to UN 6.1.5.2.1 for Packing Group II and III liquids, EPA FIFRA container standards, and FAO/WHO guidelines where relevant. The finished containers are bottom-gripped in drop tests at −18 °C from 1.2 m. Production bottlenecks include fluorine gas feed pulsation causing uneven barrier thickness, and parison weld lines at the handle area failing at low temperatures.

    HDPE KL471A is extruded into sheet of 2.0–10.0 mm thickness for thermoformed secondary containment basins and chemical tank liners. The sheet line uses a 90–120 mm single-screw extruder with L/D 30–33, a flat die with adjustable lip, and a three-roll stack at 70–90 °C. Melt temperature at the die is 195–215 °C. Sheet is then thermoformed at 130–150 °C surface temperature with plug assist into basins of 0.5–2.0 m³ capacity. Welding of sheet sections is performed by hot-gas or extrusion welding with HDPE welding rod at 220–240 °C melt temperature. The finished liner is tested for spark testing at 15–30 kV to detect pinholes and hydrostatic leak testing for 24 h to EN 13361:2018 or ASTM D4437/D4437M-16 for geomembranes. Chemical compatibility is determined by immersion testing in 98% sulfuric acid and 30% sodium hydroxide at 23 °C for 7 days with change in tensile properties less than 10%. Processing addition: 1.5–2.5 wt% carbon black masterbatch is added when the liner is used in outdoor installations to meet ISO 16871 weathering. End product is used as secondary containment under chemical storage tanks, with a design leak rate below 1 × 10⁻⁶ m³/m²/day. Failure modes include weld cracking at the corner folds when the sheet is thermoformed below 120 °C, and environmental stress cracking in contact with wetting agents when the liner is under constant strain.

    What Limits Parison Wall Uniformity in 1,000 L IBC Inner Bottle Moulding?

    In blow moulding of 1,000 L IBC inner bottles, the limiting process variables are parison sag, die swell, and accumulator head pressure. HDPE KL471A provides a melt flow rate of 0.36 g/10 min to ISO 1133-1:2022, which maintains parison integrity over the 1,000–1,400 mm parison length. The accumulator head on a 120–150 mm extruder delivers a shot weight of 12–18 kg in 8–15 s; head pressure is 25–35 MPa. The mould clamping force is 3,000–6,000 kN; blow air is 0.6–0.8 MPa; mould temperature is 10–20 °C. Wall-thickness programming adjusts die gap from 1.0 mm at the top to 6.0 mm at the bottom corners. The finished inner bottle has a nominal wall thickness of 1.5–3.5 mm and a weight of 10–14 kg. Dimensional stability is checked by 3D scanning; the bottom outlet boss must remain within ±2 mm of true position. Compliance for composite IBCs is UN 31H1 for intermediate bulk containers; the inner bottle is drop-tested inside its steel cage from 1.2 m after conditioning at −18 °C. Hydraulic internal pressure test is performed at 70 kPa for 10 min to UN 6.5.4.8.5. Processing difficulties arise when the parison temperature drops below 185 °C at the lower edge, causing weld-line thinning at the bottom pinch-off; this is controlled by maintaining die exit temperature at 205–215 °C and closing the mould within 12 s of parison drop. Published data for this specific configuration is limited for some accumulator head geometries.

    Free Quote

    Competitive TPC (Japan) HDPE KL471A prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    The resin grade TPC (Japan) HDPE KL471A is positioned within the high-density polyethylene family produced from ethylene copolymerized with a minor alpha-olefin content. The comonomer insertion reduces crystallinity relative to homopolymer grades and improves slow crack growth resistance, which is a design-critical property in pressure-bearing thick-wall sections. Procurement of KL471A should distinguish whether the designation represents natural, uncompounded resin or a fully compounded black pipe material. In black pipe configurations, carbon black loading is normally maintained between 2.0 wt% and 2.5 wt%, with dispersion quality controlled to at least ISO 18553 grade 3 to provide ultraviolet stabilization and reduce agglomerate-initiated fracture. General food-contact status for high-density polyethylene is addressed under FDA 21 CFR 177.1520 and European Union Regulation (EU) No 10/2011, but product-specific conformity for KL471A must be obtained from the supplier’s certificate of conformity because stabilizer packages and carbon black may be subject to regional additive restrictions.

    How Is KL471A Differentiated from HDPE Film and Injection Molding Grades?

    The differentiation is primarily rheological and molecular. Injection molding grades are typically designed for high melt flow at 190°C/2.16 kg, often above 10 g/10 min, to fill thin-walled tooling at moderate clamp force. KL471A is not formulated around that processing objective. Its utility lies in low-melt-flow extrusion where molecular weight remains high enough to produce hydrostatic strength and slow crack growth resistance. Film grades, by contrast, are controlled for narrow molecular weight distribution and reduced melt elasticity to stabilize blown-film bubble geometry. Such a distribution would be inappropriate for thick-wall pipe tooling because it lowers melt integrity and sag resistance. Compared with commodity blow molding grades, KL471A is expected to display higher viscosity and a broader molar mass distribution when supplied as a pipe-extrusion resin, although published product-specific molar mass data for this designation is limited in public trade literature. Batch-to-batch verification should therefore rely on the lot certificate of analysis rather than on generic class descriptions.

    Reference property envelope for high-molecular-weight HDPE pipe-extrusion families Typical range or value Test method
    Density of natural resin 0.945–0.952 g/cm³ ASTM D1505 / ISO 1183-1
    Melt flow rate at 190°C/5 kg 0.20–0.40 g/10 min ISO 1133-1:2022 / ASTM D1238
    Tensile yield stress 22–26 MPa ISO 527-2 / ASTM D638
    Tensile elongation at break >600% ISO 527-2
    Flexural modulus 800–1100 MPa ISO 178 / ASTM D790
    Charpy notched impact at 23°C No break typical or >20 kJ/m² ISO 179-1
    Environmental stress crack resistance, F50 >1000 h ASTM D1693-15 condition B
    Carbon black content, black compound 2.0–2.5 wt% ISO 6964 / ASTM D1603
    Carbon black dispersion ≤ grade 3 ISO 18553

    For single-screw pipe extrusion, the material should be processed on a grooved-feed extruder with L/D 30:1–36:1 and a barrier screw or high-performance mixing section. Feed and compression zone temperatures are commonly maintained between 180°C and 210°C, while head and die temperatures are held from 200°C to 220°C. The target melt temperature at the die entry is generally kept below 240°C; sustained operation above this threshold accelerates antioxidant consumption and can reduce hydrostatic strength before visible gel formation appears. Melt filtration through a 60/80/100 mesh screen pack removes carbon agglomerates and incidental contamination, but screen-pack pressure drop must be logged continuously. A rising pressure trend at constant screw speed can indicate carbon black dispersion failure, gel accumulation, or contamination in the feedstock. Interruption of extrusion with melt held above 230°C for more than 20 min is an operational boundary for high-molecular-weight HDPE because oxidative chain scission generates microgel defects that are not removed by standard melt filtration.

    When Carbon Black Dispersion Limits Hydrostatic Service Life

    In black HDPE pressure pipe, poorly dispersed carbon black agglomerates act as stress concentrators under sustained internal pressure. The consequence is not primarily aesthetic; it is a reduction in slow crack growth resistance and long-term hydrostatic performance. Pipe extrusion operations evaluate dispersion by compression-molding a thin specimen and comparing the size and population of visible agglomerates against the reference micrographs in ISO 18553. A dispersion rating worse than grade 3 should trigger lot quarantine because such material can pass short-term burst tests yet fail long-duration hydrostatic testing. When KL471A is supplied as natural resin and carbon black masterbatch is added at the pipe plant, high-shear twin-screw compounding is preferred over simple dry blending. Gravimetric feeding is required to maintain carbon black content within 2.0–2.5 wt%, and the final ashing result should be verified against ISO 6964 or ASTM D1603. Published hydrostatic regression data specific to KL471A are limited in public trade sources; therefore the appropriate pressure-pipe classification must be carried by the compound or pipe manufacturer rather than inferred from a density or melt flow rate certificate alone.

    Melt Rheology, Process Control Ranges, and Equipment Boundaries

    Die swell and sag resistance are governed by molecular weight, molecular weight distribution, and comonomer placement along the polyethylene chain. Capillary rheometry at 190°C for high-molecular-weight HDPE pipe families commonly shows shear viscosity between 10,000 Pa·s and 30,000 Pa·s at 10 s⁻¹, although KL471A-specific capillary data should be requested from the compound supplier because minor formulation adjustments can shift the viscosity curve. Melt elasticity controls circumferential wall-thickness uniformity in pipe extrusion and is evaluated through extrudate swell at fixed die length-to-diameter ratio. Excessive swell increases die-lip deposit and creates wall-thickness variation when calibration sleeve vacuum is insufficient. Pipe lines should monitor haul-off speed, melt pressure before the screen pack, and die temperature independently. Melt pressure instability greater than ±1.0 MPa at constant throughput generally indicates feed instability, inconsistent regrind particle size, or slugging of carbon black masterbatch.

    Compliance for potable water pressure pipe is not established solely by the resin datasheet. European pipe applications require classification of the compound under ISO 4427-1 and EN 12201, with long-term hydrostatic strength evaluated according to ISO 9080 and material classification under ISO 12162. A PE100 designation is a pipe-compound classification and not a resin property that can be assumed from a single melt flow or density value. In North American practice, ASTM D3350 cell classification and PPI TR-4 hydrostatic design basis listings provide the pressure-pipe design framework. The pipe manufacturer’s listing for NSF/ANSI 61 or equivalent potable water contact certification must reference the specific compound and not only the base resin. For regulatory conformity, the supplier should provide documentation showing compliance with REACH, RoHS 2011/65/EU, and any applicable national food-contact measures.

    Compliance boundary Scope Evidence required for KL471A-containing systems
    ISO 4427-1 / EN 12201 Polyethylene piping systems for water supply and pressure service Compound classification and hydrostatic test documentation from pipe manufacturer
    ISO 9080 / ISO 12162 Long-term hydrostatic strength and PE material classification Regression data and minimum required strength classification
    ASTM D3350 Polyethylene pipe and fitting material cell classification Cell class from compound supplier
    FDA 21 CFR 177.1520 Olefin polymers for food-contact use Supplier certification of formulation compliance
    EU Regulation (EU) No 10/2011 Plastic materials and articles intended for food contact Migration test report or supplier declaration
    NSF/ANSI 61 Drinking water system components Listing by compound or pipe trade designation
    RoHS 2011/65/EU Lead, cadmium, mercury, hexavalent chromium, PBB, PBDE limits Test report or material declaration

    High-humidity storage above 60% RH can introduce surface moisture on cold feedstock, and rapid heating in thick-wall extrusion can produce surface pitting even when the bulk resin remains dry. Predrying is therefore specified for cold feedstock handled in such environments, even though high-density polyethylene is generally hydrophobic. Recycled content used in pipe or large-part extrusion must comply with traceability and quality requirements such as EN 15343, and potable-water applications impose additional migration and odor restrictions that may limit post-industrial or post-consumer recyclate inclusion. Incompatibility with amine-based additive carriers and certain phenolic antioxidant combinations should also be evaluated before changing masterbatch suppliers, because additive interactions can alter discoloration behavior and long-term stabilization. Processors converting KL471A should maintain lot-level records of melt pressure, melt temperature, carbon black dispersion, and screen-pack change intervals because these variables control consistency in service-critical pipe and extrusion applications.