Tpc Japan Hdpe Kl372a

TPC (Japan) HDPE KL372A

    • Product Name: TPC (Japan) HDPE KL372A
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 589569
    Density 0.954 g/cm3
    Melt Flow Rate 190 C 2 16 Kg 0.30 g/10 min
    Tensile Strength At Yield 25.0 MPa
    Tensile Strength At Break 30.0 MPa
    Elongation At Break 800 %
    Flexural Modulus 1.10 GPa
    Izod Impact Strength Notched 0.200 J/cm
    Shore D Hardness 66
    Vicat Softening Point 125 C
    Melting Point 133 C
    Brittleness Temperature -70.0 C
    Environmental Stress Crack Resistance >1000 hr
    Thermal Conductivity 0.44 W/m-K
    Coefficient Of Linear Thermal Expansion 1.2E-4 1/C
    Specific Heat Capacity 1.9 J/g-C
    Dielectric Constant 2.3
    Dissipation Factor 0.0002
    Volume Resistivity >1.0E15 ohm-cm
    Dielectric Strength 20 kV/mm

    As an accredited TPC (Japan) HDPE KL372A factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing TPC (Japan) HDPE KL372A is supplied in 25 kg multiwall paper sacks, palletized and stretch-wrapped for secure industrial delivery.
    Container Loading (20′ FCL) Standard Container Loading (20′ FCL) for TPC (Japan) HDPE KL372A: palletized 25 kg bags, shrink-wrapped, securely stowed for export.
    Shipping TPC (Japan) HDPE KL372A is a non-hazardous polyethylene resin, typically supplied in 25 kg bags or jumbo bags, palletized and stretch-wrapped. Ship in clean, dry containers or trucks at ambient temperature, avoiding moisture, direct sunlight, and excessive heat. Follow supplier SDS and local transport regulations.
    Storage Store TPC (Japan) HDPE KL372A in a cool, dry, well-ventilated warehouse. Keep away from direct sunlight, heat, flames, ignition sources, and strong oxidizers. Maintain sealed original bags or containers, stack on pallets off the floor, and prevent moisture, dust, and contamination. Avoid prolonged UV exposure. Follow local regulations and use first-in, first-out rotation. Inspect packaging regularly.
    Shelf Life TPC (Japan) HDPE KL372A typically has indefinite shelf life when stored dry, unopened, away from heat, sunlight, and contamination.
    Application of TPC (Japan) HDPE KL372A

    A 220 L tight-head blow-moulded drum body produced from TPC HDPE KL372A relies on a nominal density of 0.954 g/cm³ (ASTM D1505-20) and a melt flow rate of 0.07 g/10 min (ASTM D1238-20, 190 °C/2.16 kg) to maintain parison sag resistance at melt temperatures of 190–210 °C on accumulator-head extrusion blow-moulding machines with screw L/D ratios between 24:1 and 30:1. In this downstream production process, the high-molecular-weight fraction permits a programmed parison wall thickness of 3.5–5.0 mm in the body section, while the mould is held at 10–30 °C and inflated at 0.6–0.8 MPa; cooling time is typically 180–300 s before flash removal and automatic leak testing. The formulation addition ratio for UN-certified service allows clean internal regrind reincorporation at ≤30 wt% of the total shot weight, and carbon black masterbatch is metered at 2.0–2.5 wt% when opacity or outdoor weathering is specified; higher regrind levels require re-validation of drop impact and hydrostatic burst performance because the low-melt-flow base resin responds to regrind-induced viscosity reduction with measurable parison drawdown variation. Industry compliance is governed by UN Model Regulations Chapter 6.1 for plastics drums coded 1H1/Y1.8/250, requiring a hydrostatic pressure test at 250 kPa for 30 min, a 1.2 m drop test after conditioning at −18 °C, and a stack-load test at 40 °C for 28 days; material ESCR is verified under ASTM D1693-21 Condition B, 100 % Igepal, with values exceeding 1,000 h. The terminal finished product type is the UN-certified 220 L L-ring tight-head polyethylene drum used for liquid hazardous chemicals, fitted with 2 in and 3/4 in bungs and sealed with tamper-evident closures.

    In closed-loop extrusion blow-moulding of 1,000 L composite intermediate bulk container inner bottles, TPC HDPE KL372A is processed at a melt temperature of 190–210 °C through an accumulator head with parison length control accommodating preform lengths of 1.5–1.8 m; the mould clamp unit is typically rated between 1,000 kN and 1,500 kN to maintain parting-line integrity during inflation at 0.6–0.8 MPa. The downstream production process uses a single-layer parison with programmed wall thickness distribution optimized for corner thinning, because the inner bottle must resist stack loads and hydraulic pressure without metallic overpack reinforcement. The formulation addition ratio allows clean internal regrind at ≤35 wt% of the total charge, while UV-stabilized masterbatch is dosed at 1.5–2.0 wt% when the composite IBC is intended for outdoor storage; any regrind source contaminated with hydrocarbon solvents or amines is excluded to avoid stress-cracking initiation in the discharge valve seat and sidewall bend zones. Industry compliance is evaluated under UN Model Regulations Chapter 6.5 for rigid plastics composite IBCs coded 31HA1/Y, with bottom drop tests from 1.2 m at −18 °C, top-lift and stack-load tests per the applicable UN test sequence, and dimensional verification of the inner receptacle interface before assembly into the steel cage. The terminal finished product type is the UN-certified 1,000 L composite IBC inner bottle, with an integrally moulded 150 mm top fill neck and a lower discharge valve seat compatible with 2 in butterfly or ball valve assemblies.

    What Limits Regrind Reincorporation in Six-Layer Automotive Fuel Tank Coextrusion?

    Six-layer fuel tank coextrusion places the highest demand on HDPE KL372A because the substrate skins must carry the parison during blow moulding while the EVOH barrier and tie layers remain continuous at total thicknesses below 10 mm. The process is run on a multi-layer accumulator-head blow-moulding machine with six extruders, melt temperatures of 210–230 °C for the HDPE skins and 200–220 °C for the tie and barrier layers, an annular die gap of 1.5–3.0 mm, and a mould close speed of 200–400 mm/s to limit fold-over defects at pinch-off seams. The formulation addition ratio positions TPC HDPE KL372A as the outer and inner skins at 70–80 wt% of the total tank mass; ethylene-vinyl alcohol copolymer is introduced at 1.5–3.0 wt%, maleic anhydride-grafted polyethylene tie layers at 2–3 wt% per layer, and clean plant regrind from the same six-layer scrap at 20–30 wt% of the HDPE fraction. Regrind content above 30 wt% produces measurable increases in parison sag and barrier layer thickness variation, which translates into elevated hydrocarbon permeation values on finished tanks. Industry compliance standards include UN ECE R34 Annex 5 for fire resistance and post-impact fuel leakage, hydrocarbon evaporative emission limits under EPA Tier 3 and CARB LEV III, SAE J2587 for permeation evaluation, and material-level tensile and ESCR testing under ASTM D638-14 and ASTM D1693-21 Condition B. The terminal finished product type is the automotive fuel tank for gasoline and oxygenated blends up to E10, with a six-layer wall structure and a nominal shell thickness of 6–10 mm depending on vehicle package space.

    Layer sequenceMaterialWeight fractionGoverning standard
    Outer skinTPC HDPE KL372A35–40 wt% of tank massASTM D1693-21
    Tie layerMaleic anhydride-grafted polyethylene2–3 wt% per layerSAE J2587
    Barrier layerEthylene-vinyl alcohol copolymer1.5–3.0 wt%ASTM D3985-17
    Tie layerMaleic anhydride-grafted polyethylene2–3 wt% per layerSAE J2587
    Inner skinTPC HDPE KL372A35–40 wt% of tank massASTM D1693-21
    Regrind fractionClean six-layer fuel tank scrap20–30 wt% of HDPE fractionASTM D1238-20

    When Carbon Black Masterbatch Extends UV Resistance in Moored Buoy Shells

    Outdoor moored buoy shells produced from TPC HDPE KL372A require compounded UV stabilization because the part must retain notched impact strength after multi-year exposure to saltwater, cyclic wave loading, and solar radiation. The downstream process is extrusion blow moulding on a twin-station accumulator-head machine with a melt temperature of 190–210 °C, a mould temperature of 10–30 °C, and a parison programming sequence that increases wall thickness to 8–15 mm at the top mooring eye and lower skirt attachment points. The formulation addition ratio for UV-stabilized buoy shells specifies a polyethylene-carrier carbon black masterbatch at 2.0–2.5 wt% to achieve a final carbon black content near 2.0 wt%, and a hindered amine light stabilizer masterbatch at 0.2–0.5 wt% when extended weathering resistance is specified; the masterbatch carrier is matched to high-molecular-weight HDPE to avoid melt-viscosity inversion during blending. Industry compliance for such components is not governed by a single mandatory global standard, so qualification is typically anchored to ASTM G154 Cycle 1 or ISO 4892-3 accelerated weathering, ASTM D638-14 tensile properties after 2,000–5,000 h exposure, and ASTM D1693-21 Condition B ESCR after environmental stress-cracking exposure; published data for this specific configuration is limited, and end users typically require Xenon arc or Florida outdoor exposure validation before acceptance. The terminal finished product type is the blow-moulded double-walled shell for moored navigation buoys, marker floats, and fender floats, filled with closed-cell polyurethane foam after moulding to prevent water ingress and maintain buoyancy after shell puncture.

    Blow-moulded selective catalytic reduction urea tanks manufactured from TPC HDPE KL372A are produced by monolayer extrusion blow moulding or by coextruding a carbon black outer skin over a natural or black inner layer, with melt temperatures of 190–210 °C, mould temperatures of 10–30 °C, and programmed parison wall thicknesses of 3–6 mm to support ultrasonic welding bosses and heating element brackets. The formulation addition ratio restricts non-contaminated plant regrind to ≤20 wt% of the total shot weight because higher levels reduce environmental stress-cracking resistance after prolonged exposure to 32.5 wt% aqueous urea solution; carbon black masterbatch is dosed at 2.0–2.5 wt% for opacity and UV resistance, while amine-based processing aids are excluded due to the risk of extractable nitrogen species migrating into the fluid. Industry compliance is evaluated under ISO 22241-1:2019 for diesel exhaust fluid AUS 32 quality and ISO 22241-3:2017 for materials compatibility and storage, with long-term immersion testing in AUS 32 at 60 °C for 3,000 h used to screen resin suitability; published data for this specific KL372A configuration is limited, so formal qualification against the vehicle manufacturer's material specification is required. The terminal finished product type is the SCR urea solution tank for heavy-duty diesel and off-road aftertreatment systems, fitted with a 50–100 mm filler neck, level sensor port, and heated suction line boss.

    Free Quote

    Competitive TPC (Japan) HDPE KL372A prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    TPC (Japan) HDPE KL372A is a grade designation for a high-density polyethylene resin supplied by TPC in Japan. The designation identifies the supplier, country of origin, polymer family, and grade code; it does not by itself define the melt flow rate or density. High-density polyethylene resins are predominantly linear ethylene polymers with a density above 0.940 g/cm³ as determined by ISO 1183-1. KL372A is intended for conversion operations in which melt strength, solid-state stiffness, and environmental stress crack resistance are balanced against processability. Because open-literature values specific to KL372A are limited, the controlling property range should be obtained from the supplier lot certificate rather than transferred from generalized HDPE data.

    What specification framework governs KL372A?

    The resin is characterized by standard polyethylene test methods. Melt flow rate is measured at 190 °C under a 2.16 kg load using ISO 1133-1:2022 or ASTM D1238-23. Density is reported after conditioning or annealing according to ISO 1183-1. Tensile yield stress and elongation at break are determined by ASTM D638-14 at a test speed of 50 mm/min. Flexural modulus is measured by ASTM D790-17, and notched Izod impact is measured under ASTM D256-23. Thermal properties are evaluated by ISO 11357-3 for melting peak temperature and ISO 306 for Vicat softening point. Environmental stress crack resistance is tested according to ASTM D1693-15. The following matrix summarizes the relationship between test method, typical high-density polyethylene ranges, and the need to confirm grade-specific values for KL372A.

    PropertyTest methodTypical HDPE rangeKL372A verification basis
    DensityISO 1183-10.941–0.970 g/cm³supplier lot certificate
    Melt flow rateISO 1133-1:2022 / ASTM D1238-230.2–50 g/10 mingrade-specific certificate
    Tensile yield stressASTM D638-1420–32 MPagrade-specific certificate
    Elongation at breakASTM D638-14100–1000%grade-specific certificate
    Flexural modulusASTM D790-17800–1600 MPagrade-specific certificate
    Notched Izod impactASTM D256-2320–200 J/mgrade-specific certificate
    Vicat softening pointISO 306120–130 °Cgrade-specific certificate
    Environmental stress crack resistanceASTM D1693-1510–1000 hgrade-specific certificate

    Because the melt flow rate of KL372A is not provided in open public literature, conversion settings derived from typical high-density polyethylene grades must be adjusted after receiving the lot-specific melt flow rate and density values. A melt flow rate below 1.0 g/10 min generally indicates higher average molecular weight and greater melt strength, while a melt flow rate above 5 g/10 min reduces fill pressure but can lower environmental stress crack resistance and dart impact. These relationships are indicative and do not replace the lot certificate.

    When KL372A is processed by blown film and sheet extrusion

    If the grade is directed to blown film processes, pre-drying is generally unnecessary when pellet moisture remains below 0.05 wt%; however, condensation in outdoor silos can introduce surface moisture. A hot-air hopper dryer set at 70–80 °C for 1–2 h may be used when visual splay, pinholes, or bubble defects appear. For monolayer high-molecular-weight HDPE film, a grooved-feed extruder with a barrier screw and L/D ratio of 25:1–30:1 is commonly employed. The die gap is set between 0.8 mm and 1.2 mm, and the melt temperature is maintained in the range of 190–230 °C as measured by an immersion thermocouple at the adapter. Blow-up ratio is typically held at 2:1–4:1, with frost line height controlled at 5–8 die diameters to stabilize the bubble. On production-scale lines, bubble instability is observed when the stalk length is too short or when die lip exit velocity exceeds the melt strength of the resin.

    On a three-layer coextrusion blown film line with die diameter 250 mm and die gap 1.2 mm, the use of HDPE in the core layer instead of LLDPE reduces bubble sag but raises the frost line height required for crystallization. The primary process conflict is the narrow window between the melt temperature required to eliminate melt fracture and the upper temperature at which surface oxidation becomes visible. For high-density polyethylene, melt fracture is often observed as shark-skin surface roughness at die shear rates above 1000–1500 s⁻¹; increasing die gap or reducing output is preferred over raising melt temperature above 240 °C. If a wider die gap is not available, a fluoropolymer processing aid masterbatch at 300–500 ppm may lower apparent melt viscosity at the die wall without altering bulk rheology. These ranges are equipment-dependent and do not replace the resin supplier’s processing recommendation.

    Film property verification should be performed on samples conditioned at 23 ± 2 °C and 50 ± 5% RH for at least 40 h according to ASTM D618. Dart impact is measured by ASTM D1709-16a with a 66 cm drop height; Elmendorf tear by ASTM D1922-15; tensile properties by ASTM D882-18. Haze is determined by ASTM D1003-21, and specular gloss by ASTM D2457-13. These procedures are essential when comparing KL372A film with LLDPE or MDPE because differences in frost line crystallization and surface finish are not captured by resin melt flow rate alone.

    In injection molding of KL372A, the injection unit should use a general-purpose polyolefin screw with L/D ratio 18:1–22:1 and compression ratio 2.2:1–2.8:1. The barrel temperature profile from feed throat to nozzle is typically 180 °C, 200 °C, 210 °C, and 220 °C, with the nozzle at 220–240 °C. Mold temperature is held at 10–30 °C to promote rapid solidification and short cycle times. Injection pressure is adjusted between 70 MPa and 110 MPa based on melt viscosity and part geometry. The shot size should remain between 30% and 70% of barrel capacity to limit residence time. Parallel-platen clamp force can be estimated from cavity pressure and projected area; HDPE typically requires 300–500 kN/m² of projected area for thin-wall applications. High-density polyethylene exhibits mold shrinkage of 1.5–3.0%, and anisotropic shrinkage is more pronounced in grades with higher molecular weight and orientation.

    For injection molded caps and closures, a hot-runner mold with gate diameter 2.0–2.5 mm and cooling time 8–12 s is used. The packing pressure profile is set to 60–80% of peak injection pressure for 3–5 s to limit sink marks. In production trials, inadequate packing leads to voids in thick sections and increases part weight variation to ±0.15%. HDPE crystalline shrinkage begins during the mold-open phase and continues for 24–48 h after demolding; therefore, dimensional inspection should be delayed. The mold temperature should be uniform within ±5 °C; differential cooling causes bow and warpage in flat closures. If melt temperature is raised above 250 °C to reduce viscosity, discoloration and odor can appear, particularly in hot-runner systems with long residence times.

    Twin-screw compounding effects on melt viscosity and additive dispersion

    For conversion operations requiring masterbatch dilution or additive incorporation, KL372A can be compounded on a co-rotating twin-screw extruder with L/D 40:1 or greater. The screw configuration should include kneading blocks and distributive mixing elements to break down agglomerates without generating excessive viscous heating. At constant throughput, feed rate variations of ±2% can produce torque deviations of 5–10% on a 40 mm co-rotating twin-screw machine; these deviations are process-related and do not necessarily indicate resin inconsistency. Melt temperature at the die plate should be kept below 240 °C to avoid thermal-oxidative chain scission and discoloration. When adding peroxide for rheology modification, the peroxide concentration must be limited to the supplier’s prescribed range because uncontrolled free-radical chain scission shifts melt flow rate and reduces high-load melt strength. Published data for KL372A in peroxide-modified systems is limited; therefore, pilot-scale evaluation is recommended before production deployment.

    Comparative architecture and property limits across polyethylene families

    The primary differences between KL372A and other polyethylene families arise from density, short-chain branching, and melt rheology. High-density polyethylene has fewer short-chain branches than linear low-density polyethylene and lacks the long-chain branching typical of high-pressure low-density polyethylene. These structural differences affect processing and end-use performance. The following table compares the general classes; KL372A belongs to the HDPE row, with the caveat that exact density and melt flow rate must be confirmed from the lot certificate.

    Polyethylene classDensity rangeBranching architectureTypical processing methodCharacteristic limitation
    LDPE0.915–0.935 g/cm³long-chain branchedblown film, extrusion coatinglower stiffness, lower temperature resistance
    LLDPE0.910–0.940 g/cm³linear with short-chain branchesblown and cast filmlow melt strength, draw resonance in extrusion
    MDPE0.926–0.940 g/cm³linear, intermediate densityrotomolding, pipeintermediate stiffness, slower crystallization
    HDPE including KL372A0.941–0.970 g/cm³predominantly linear, low branchingblown film, sheet, injection moldinglower clarity, higher orientation-induced anisotropy

    Compared with general-purpose injection-molding HDPE grades, KL372A is expected to show a lower melt flow rate if it is positioned for film or high-molecular-weight applications. That lower melt flow rate increases melt strength and bubble stability in blown film but raises injection pressure and may reduce surface gloss in molded parts. Compared with LLDPE film resins of the same thickness, HDPE film generally shows higher tensile modulus and lower dart impact and tear propagation resistance. These differences are evaluated by ASTM D1709 for dart drop, ASTM D1922 for Elmendorf tear, and ASTM D882 for thin-film tensile properties. If KL372A is used in high-stiffness packaging or industrial liners, the transition to HDPE should be validated on the target blown film line because bubble geometry and downgauging limits differ from LLDPE.

    Within the supplier’s high-density polyethylene portfolio, grade differentiation is usually based on melt flow rate, density, molecular weight distribution, and comonomer type. Without the supplier’s full grade map, direct grade-to-grade claims for KL372A cannot be verified from public sources. However, a low-melt-flow film grade will typically differ from a high-flow injection grade in the following manner: film grade has higher molecular weight, broader molecular weight distribution, greater melt strength, and improved bubble stability, while high-flow injection grade has lower pressure drop, shorter cycle time, and reduced environmental stress crack resistance. The selection between KL372A and another HDPE grade should be made on the basis of ISO 1133-1:2022 melt flow rate, ISO 1183-1 density, and ASTM D1693-15 ESCR, not on nominal resin type alone.

    Storage conditions affect processing stability. The resin should be stored in sealed, clean containers away from direct sunlight and moisture ingress. Bulk silo temperature should not exceed 40 °C to avoid pellet blocking and additive migration. In tropical climates with relative humidity above 60%, condensation on cold pellets transferred into a warm manufacturing hall can introduce surface moisture; a hopper dryer at 70–80 °C for 1 h is an accepted corrective action. Additive bloom may occur if the resin is stored for extended periods above 30 °C; the mechanism involves migration of antistatic or slip agents to the pellet surface and can reduce printability of film.

    Food-contact applicability for polyolefin resins is typically evaluated under FDA 21 CFR 177.1520 or the corresponding JIS K 6922 Japan Hygienic Olefin Standards. A specific grade such as KL372A may be manufactured to food-contact status only if the supplier’s certificate states that the monomer and additive composition comply with the relevant positive list. For industrial film and sheet applications, REACH registration and RoHS Directive 2011/65/EU do not automatically apply to all heavy-metal limitations; the grade should be verified against the supplier’s safety data sheet. Antimicrobial or UV-stabilized articles should be evaluated under the appropriate end-use-specific standard before commercial use.

    KL372A should not be processed above 260 °C for extended hold-ups because thermal degradation can generate low-molecular-weight species and reduce elongation at break. Outdoor service without adequate UV stabilization typically produces surface cracking and loss of tensile properties within months, especially in thin films; a carbon black loading of 2–2.5 wt% or a hindered amine light stabilizer package is required for multi-year exposure. The resin should not be combined with amine-based additives if peroxide crosslinking is intended, because amine interference can alter the peroxide half-life and reduce gel content. For extruder shutdown, a purge with low-melt-index polyethylene or commercial purging compound reduces black specks during start-up; repeated shutdowns without purging can increase gel particle levels. In twin-screw compounding, high shear rates above 2000 s⁻¹ may cause local melt temperature spikes that are not detected by the die melt thermocouple.

    Top