| HS Code | 485356 |
| Density | 0.953 g/cm³ |
| Melt Flow Rate | 8.0 g/10 min |
| Tensile Strength At Yield | 28 MPa |
| Tensile Strength At Break | 22 MPa |
| Elongation At Break | 500% |
| Flexural Modulus | 1.10 GPa |
| Notched Izod Impact Strength | 0.100 J/cm |
| Shore D Hardness | 65 |
| Vicat Softening Point | 123 °C |
| Heat Deflection Temperature At 0 46 Mpa | 75 °C |
| Thermal Expansion Coefficient | 1.2E-4 cm/cm/°C |
| Thermal Conductivity | 0.40 W/m·K |
| Specific Heat | 1.9 J/g·°C |
| Dielectric Constant | 2.3 |
| Volume Resistivity | 1E16 ohm·cm |
| Water Absorption | <0.01% |
| Ul Flammability | HB |
| Melting Point | 131 °C |
| Processing Temperature | 200-260 °C |
| Mold Temperature | 20-60 °C |
As an accredited TPC (Japan) HDPE KL371A factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | TPC (Japan) HDPE KL371A packaging: 25 kg polyethylene-lined bags, available in 1,000 kg jumbo bags. |
| Container Loading (20′ FCL) | TPC (Japan) HDPE KL371A is securely loaded in 20′ FCL containers with standard export packing for safe, compliant ocean transport. |
| Shipping | TPC (Japan) HDPE KL371A is a non-hazardous high-density polyethylene resin. Ship as general cargo, not regulated by DOT/IMDG/IATA. Typically packed in 25 kg bags or jumbo bags on pallets. Store cool and dry, away from heat and direct sunlight. No UN number required. |
| Storage | Store TPC (Japan) HDPE KL371A in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, and flames. Keep bags or containers sealed to prevent moisture, dust, and contamination. Separate from strong oxidizers. Avoid prolonged UV exposure and extreme temperatures. Stack securely to prevent package damage. Observe local regulations and the manufacturer’s SDS. Use appropriate PPE when handling. |
| Shelf Life | TPC (Japan) HDPE KL371A shelf life: 24 months when stored dry, cool, ventilated, away from direct sunlight in original packaging. |
The most frequently observed downstream route for TPC (Japan) HDPE KL371A is single-layer extrusion blow molding of household and institutional chemical containers in the 0.5–5 L range. Typical certificate values include a nominal melt mass-flow rate of 0.35 g/10 min at 190 °C/2.16 kg (ISO 1133-1:2022) and a nominal density of 0.956 g/cm³ (ISO 1183-1:2019). On shuttle accumulator machines using 60–90 mm screws at 24:1–30:1 L/D, melt temperature is held between 185 °C and 205 °C; a die gap of 1.2–2.0 mm and parison programming with 10–30 points are used to counter sag on hang lengths of 150–250 mm. Production-scale experience shows that when parison sag exceeds 15 mm over 10 s, the lower pinch-off weld thickens and downstream tail-trimming load increases; die-head temperature variation must remain within ±3 °C to avoid shear-induced melt fracture at throughputs above 80 kg/h. Blow air pressure of 0.55–0.70 MPa, mold temperature of 8–15 °C, and a pre-blow delay of 0.2–0.4 s are typical for a 1 L bleach bottle at 38–42 g shot weight. The base formulation for monolayer containers is 76–98 wt% virgin KL371A, 2–4 wt% colorant masterbatch, and 0–20 wt% same-grade post-industrial regrind; for aggressive oxidizer service, regrind content is reduced to 0 wt% and virgin KL371A is increased accordingly because oxidatively degraded regrind contributes carbonyl by-products. Regulatory compliance is anchored to UN ST/SG/AC.10/11/Rev.8 dangerous goods packaging tests, ADR 6.1.3 for land transport, and Regulation (EC) No 1272/2008 for classification and labelling of filled products. Terminal products are 0.5 L, 1 L, 2 L, and 5 L bottles for sodium hypochlorite, quaternary ammonium disinfectants, laundry detergent, and acid-based toilet cleaners.
| Parameter | Range or condition | Equipment or reference |
|---|---|---|
| Melt temperature at die head | 185–205 °C | IR pyrometer on accumulator head |
| Screw speed | 35–55 rpm | 60 mm 24:1 L/D grooved-feed extruder |
| Blow air pressure | 0.55–0.70 MPa | Calibrated blow air circuit |
| Mold cooling water | 8–15 °C | Chiller setpoint with 0.3–0.5 MPa flow |
| Pre-blow delay | 0.2–0.4 s | Machine PLC timer |
| Regrind level | 0–20 wt% | Same-grade post-industrial flake |
| Colorant masterbatch | 2–4 wt% | LLDPE carrier, feeder hopper |
| Dry cycle time for 1 L | 11–14 s | Shuttle machine with 1+1 cavity |
Continuous wheel extrusion blow molding of personal care containers differs from shuttle operations primarily in parison contact time and cooling uniformity. KL371A runs on 16–24-cavity wheel machines when the die-head temperature is maintained at 180–200 °C, because continuous extrusion removes the hang-time instability observed on accumulator equipment. The formulation is normally modified with a slip/antistatic concentrate at 0.5–1.0 wt% of total compound to allow downstream filling-line feeding; colorant masterbatch is added at 1–3 wt%, and regrind from the same product family is limited to 15 wt% because higher ratios lower surface gloss and increase the coefficient of friction to values above 0.25 as measured by ASTM D1894. The process uses blow pin pressure of 0.6–0.8 MPa and mold cooling water at 8–12 °C; post-mold flame or corona treatment is specified when the surface energy target is 38–42 mN/m for label adhesion and silk-screen decoration. Cosmetic packaging compliance rests on EU Regulation (EC) No 1223/2009 safety documentation and producer REACH declarations under EC 1907/2006; it is not automatically a food-contact clearance. Terminal parts are 100 mL–1 L bottles for shampoo, conditioner, body wash, and lotion closures.
Single-layer food bottles made from KL371A require converter verification of olefin polymer compliance under FDA 21 CFR 177.1520 paragraph (c) extractive limits, and Commission Regulation (EU) No 10/2011 with an overall migration limit of 10 mg/dm² in food simulant D1 or D2 depending on oil type. The formulation ratio for the food-contact layer is 100 wt% virgin KL371A; regrind is excluded from the inner layer because it introduces oxidation by-products that shift organoleptic thresholds, and only food-grade white masterbatch is allowed at 1–2 wt% after migration testing. Extrusion blow molding is conducted at 180–195 °C, lower than the household chemical range, to limit thermal degradation of the low-molecular-weight fraction; blow air is passed through 0.01 μm coalescing filters to reduce odor carryover, and molds are buffed to an SPI B-2 finish to avoid micro-roughening that traps oil residues. The downstream parts are 500 mL, 1 L, 2 L, and 5 L bottles for soybean oil, sunflower oil, vinegar, and soy sauce, with cap torque retention verified according to ASTM D2063 under simulated distribution cycles.
UN-rated containers for pesticide, herbicide, and solvent distribution impose design-type approval tests that override ordinary commercial dimensional tolerances. KL371A is processed on accumulator-head machines with 80–90 mm screws and 24:1–30:1 L/D to produce a programmed parison for 5–20 L jerrycans; wall-thickness programming maintains a minimum sidewall of 1.2 mm, while the handle area is reinforced to 2.0–2.5 mm. The formulation uses 100 wt% virgin KL371A for UN-tested monolayers; a maximum of 10 wt% regrind generated from the same UN design-type lot is permitted only in a non-contact layer when a multilayer construction is used. UV stabilizer concentrate is added at 1.5 wt% of total compound when the container is intended for outdoor storage. Leakproofness is tested under UN Manual of Tests and Criteria, Section 6.1.5, and hydraulic pressure is applied to 100 kPa for 30 min in design-type testing; drop tests are performed from 1.2 m or 1.8 m depending on packing group, with the filled container conditioned to -18 °C for winter-grade formulations. Terminal products include 1 L, 5 L, 10 L, and 20 L narrow-neck jerrycans for organophosphate and pyrethroid formulations, as well as surfactant adjuvants.
Lubricant and automotive fluid bottles are produced by extrusion blow molding with the same melt-processing window as household containers, but the differentiation arises in the neck finish and closure interface. The neck finish for 946 mL and 4.73 L oil bottles is calibrated to accept tamper-evident closures; concentricity of the finish is held within 0.3 mm to prevent cap leakage under ASTM D4991 vacuum-decay leak testing. The formulation ratio in non-food lubricant containers permits 20 wt% clean post-industrial regrind when the regrind is generated from the same grade and contains no lubricant residue; carbon black masterbatch is added at 2–3 wt% of total compound to provide opacity and UV-shielding for outdoor retail display. Stress-crack resistance is characterized by ASTM D1693-A because the base oil can act as a surface-active stress-cracking agent; producers request the batch certificate before tool locking. The process uses blow air at 0.55–0.70 MPa, and the mold temperature is maintained at 10–15 °C to reduce base warpage. Terminal parts include 946 mL and 4.73 L motor oil bottles, automatic transmission fluid containers, and gear oil packs.
Blow molded technical parts such as automotive windshield-washer reservoirs and agricultural sprayer tanks are a smaller downstream segment for KL371A and often require OEM-controlled validation because published data for this specific configuration is limited. The processing route is extrusion blow molding with parison programming to maintain wall thickness in convoluted geometries; machines with 70–90 mm screws and 24:1 L/D are typically used, with melt temperatures at 190–210 °C. The structural layer contains 83–98 wt% virgin KL371A, 2 wt% carbon black masterbatch, and up to 15 wt% same-family regrind; no filler or impact modifier is added because it degrades the weld-line strength at pinch points. Low-temperature ductility is verified by ISO 179-1:2010 or ISO 180:2019 at -30 °C, depending on the OEM specification; tensile yield stress is measured by ISO 527-2:2012. Terminal products are 2–5 L washer reservoirs, sprayer tanks, and coolant recovery bottles, all of which require a secondary closure leak test after welding of inserts.
Competitive TPC (Japan) HDPE KL371A prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
TPC (Japan) HDPE KL371A is a high-density polyethylene grade supplied under the manufacturer’s code KL371A. The pelletized product is evaluated for conversion routes in which stiffness, melt strength, and environmental stress crack resistance are jointly controlled. Published data for this specific configuration is limited; the manufacturer’s certificate of analysis and technical datasheet remain the controlling documents for density, melt flow rate, additive composition, and food-contact status. Specification categories typically associated with this grade class include density, melt mass-flow rate, tensile yield stress, flexural modulus, Charpy notched impact strength, and environmental stress crack resistance. The corresponding normative methods are ISO 1183-1:2019 and ASTM D1505-18 for density, ISO 1133-1:2022 and ASTM D1238-23a for melt flow rate, ISO 527-2:2012 and ASTM D638-14 for tensile yield stress, ISO 178:2019 and ASTM D790-17 for flexural modulus, ISO 179-1:2020 for Charpy notched impact, and ASTM D1693-15e1 for environmental stress crack resistance. The grade is commonly discussed for rigid packaging and industrial container end uses, particularly where exposure to surfactants, household chemicals, or low-temperature impact requires resistance to brittle crack propagation.
On production-scale extrusion blow moulding lines, the resin can be processed on single-screw extruders with an L/D ratio of 24:1 to 30:1. Barrier-type screws with a grooved feed section are preferred because they deliver a more uniform melt temperature at screw speeds between 20 rpm and 60 rpm. Rear barrel zone temperatures in the range 170 °C to 180 °C, middle zones at 190 °C to 205 °C, and front zones at 200 °C to 215 °C are commonly used. Melt temperature should be maintained between 180 °C and 220 °C. Above 220 °C, oxidative chain scission accelerates, generating carbonyl species and increasing the risk of off-odour and melt fracture. Below 170 °C, viscosity rise reduces homogenization and can overload the extruder drive or create unmelted particles in the parison. Die head and die temperatures are normally held between 195 °C and 215 °C; a die gap of 1.5 mm to 2.5 mm and polished die land surface finish of Ra ≤ 0.4 μm are used to limit shark-skin defects. Accumulator-head machines should employ parison programming to maintain wall thickness within ±10 % of design when blow-up ratio varies between 1.5:1 and 3:1.
Pre-drying at 80 °C for 2 h in a desiccant-bed dryer is recommended when storage relative humidity exceeds 60 % or when surface condensation is visible. HDPE does not require hydrolytic drying under normal indoor storage; excessive drying can oxidize the stabilizer surface if the resin is held above 90 °C for long periods. Keep purge material and startup scrap separate because thermally degraded HDPE reduces pinning strength and may contaminate the parison weld. Injection moulding evaluation, if the grade is released for injection applications, should start at melt temperatures between 200 °C and 250 °C and mould temperatures between 10 °C and 40 °C. The melt pressure at the nozzle should be recorded; a nozzle pressure drop above 25 % of total machine pressure often indicates an undersized sprue bushing or gate freeze-off.
Capillary rheometry at 190 °C and 210 °C is recommended to establish lot-to-lot viscosity variation. For low-melt-flow blow-moulding HDPE in the same general class, apparent shear viscosity at 100 s⁻¹ commonly lies between 600 Pa·s and 1500 Pa·s, while at 1000 s⁻¹ the range narrows to approximately 150 Pa·s to 300 Pa·s. These are class-typical ranges and do not replace KL371A-specific data. Melt elasticity inferred from die swell generally increases with increasing weight-average molecular weight and broadening molecular weight distribution. A narrow distribution improves surface finish and reduces melt shrinkage; a broader distribution improves parison hang strength but raises die swell variability. Published data for this specific configuration is limited, so the processor should establish a flow rate ratio using ISO 1133-1:2022 with 21.6 kg and 2.16 kg loads to monitor molecular weight distribution changes.
Batch-to-batch variability is best monitored by differential scanning calorimetry, capillary rheometry, and melt flow rate ratio rather than by single-point melt flow alone. A differential scanning calorimetry heating run from 40 °C to 180 °C at 10 K/min under nitrogen is used to record peak melting temperature and crystallinity. For HDPE, peak melting temperature commonly lies between 128 °C and 138 °C; published data for this specific configuration is limited. The degree of crystallinity controls density, modulus, and permeation; a change of 0.002 g/cm³ in density can shift flexural modulus and barrier performance. Melt flow rate ratio, measured with 21.6 kg and 2.16 kg loads under ISO 1133-1:2022, is used to infer molecular weight distribution changes that affect parison sway and weld strength. Such measurements belong in a lot-acceptance procedure for production lines using automatic wall-thickness control.
The following matrix identifies the standard methods used to audit property claims for high-density polyethylene blow-moulding grades. Grade-specific numerical limits are controlled by the manufacturer’s product specification; they are not reproduced here because published data for this specific configuration is limited.
| Property category | Normative method | Test condition | Relevance to processing or use |
|---|---|---|---|
| Density | ISO 1183-1:2019 / ASTM D1505-18 | 23 °C immersion or gradient column | Controls stiffening, shrinkage, and permeability coefficient for small containers |
| Melt mass-flow rate | ISO 1133-1:2022 / ASTM D1238-23a | 190 °C, 2.16 kg | Correlates with extruder amperage, parison sag, and injection fill pressure |
| Tensile yield stress | ISO 527-2:2012 / ASTM D638-14 | 50 mm/min, Type 1A or Type IV specimen | Indicates short-term load capacity in compressed stacking |
| Flexural modulus | ISO 178:2019 / ASTM D790-17 | 2 mm/min, 3-point bend | Estimates rigid-container top-load and sidewall deflection |
| Charpy notched impact strength | ISO 179-1:2020 | 23 °C and -30 °C, Type A notch | Distinguishes brittle failure at subambient temperature for filled and unfilled parts |
| Environmental stress crack resistance | ASTM D1693-15e1 | 50 °C, 10 % or 100 % Igepal CO-630 | Predicts crack resistance under surfactant exposure in rigid packaging |
| Vicat softening temperature | ISO 306:2022 method A50 | 50 °C/h, 10 N | Sets maximum short-term hot-fill or washing temperature |
| Shore D hardness | ISO 868:2003 | 15 s reading | Useful for scratch and indentation response in handling systems |
Differences from other products in the same TPC (Japan) HDPE portfolio are usually more visible in low-temperature Charpy impact and environmental stress crack resistance than in tensile yield strength. An injection-moulding grade with a higher melt flow rate can reduce fill pressure in thin-wall closures but commonly exhibits lower ESCR because lower average molecular weight reduces the time for crack initiation under stress in the presence of surface-active agents. A film grade with a melt flow rate below 0.3 g/10 min provides better dart impact and tear propagation resistance after stretching but generally lacks the melt rigidity needed for parison control in blow moulding. A bimodal pipe grade may provide hydrostatic design stress above 8 MPa at 20 °C for 50 years, but the material is not optimized for cut-in-place bottle top load or blow-moulded bottle pinch-off weld strength. Direct substitution should not be made without comparative trials on the intended tool because fill pressure, gate freeze-off, and parison sag are machine-specific variables.
If KL371A is run in high-speed injection moulding cells for closures or cosmetic components, the processor should collect pressure-drop curves from the barrel to the cavity. For thin-wall parts below 0.8 mm, flow-length to wall-thickness ratio becomes the controlling factor. At melt temperatures from 200 °C to 250 °C, the frozen layer grows rapidly when mould temperature is below 15 °C; this produces a skin-core morphology that can raise tensile yield stress but lower weld-line strength. Gate velocity should be held below approximately 300 m/s to avoid jetting; a fan gate or tab gate with land length of 0.5 mm to 1.0 mm reduces gate freeze-off while preserving shear heating. The machine should be equipped with closed-loop injection speed control and cavity pressure sensors so that switch-over from velocity to pressure is triggered at 95 % to 98 % of cavity fill. Injection pressure, packing pressure, and holding time should be adjusted to maintain a cushion between 3 mm and 6 mm.
For blow moulding, high-speed cycling raises different limits. When cooling time dominates cycle time, blow pin temperature and mould cooling circuit design become critical. Chilled water at 10 °C to 15 °C and turbulent flow in the mould channels with Reynolds number above 4,000 improve heat removal, but condensation on the mould surface must be controlled. The pinch-off region is a common failure site in production; its weld line can be evaluated by drop impact at -20 °C after 24 h conditioning. A poorly optimized pinch-off, with residual land width below 0.3 mm or excessive flash, can reduce burst pressure and produce leakers. Published data for this specific configuration is limited; the processor should set alarm limits using initial lots and monitor melt temperature, tonnage, and blow pin alignment.
| Parameter | Blow moulding envelope | Injection moulding envelope | Failure marker at boundary |
|---|---|---|---|
| Melt temperature | 180 °C to 220 °C | 200 °C to 250 °C | Oxidation odour, gel accumulation, viscosity loss |
| Mould temperature | 10 °C to 40 °C | 10 °C to 40 °C | Condensation, warp, or premature gate freeze-off |
| Screw L/D ratio | 24:1 to 30:1 | 18:1 to 24:1 | High melt temperature variation or insufficient dosage |
| Die gap / gate dimension | 1.5 mm to 2.5 mm | 0.5 mm to 1.0 mm land length | Shark-skin, jetting, or gate stick |
| Injection speed / melt pressure | Parison drop 0.5 s to 3 s | Gate velocity below 300 m/s; packing 60 % to 80 % of fill pressure | Jetting, weld-line cracking, sink marks |
| Pre-drying | 80 °C for 2 h if RH > 60 % | Same condition only if surface moisture observed | Surface splay from volatiles |
These envelopes are class-typical and not a substitute for the manufacturer’s starting parameter sheet. The limiting condition on many production lines is not the resin but the auxiliary equipment: the blow pin scrubber cycle, the chilled water stability, or the air blow timer. A process audit should therefore include verification of mould temperature control, air pressure at 0.6 MPa to 0.8 MPa during bottle inflation, and clamp force margin on injection machines. Poor cooling water flow with Reynolds number below 2,000 can lengthen cycle times by more than 15 % and produce inconsistent part mass.
Regulatory compliance for KL371A depends on the finished article and the specific lot. Polyethylene homopolymers and copolymers may qualify under FDA 21 CFR 177.1520 for food-contact applications when the final article meets the intended-use conditions and any applicable migration limits. For the European Union, Regulation (EU) 10/2011 requires compliance with overall migration limit of 10 mg/dm² for plastic food-contact materials; specific migration testing is required for intentionally added dual-use additives. For electrical and electronic equipment housings, the material formulation must satisfy the maximum concentration values in Directive 2011/65/EU for lead, mercury, cadmium, hexavalent chromium, polybrominated biphenyls, and polybrominated diphenyl ethers. REACH registration and SVHC statement should be confirmed from the supplier for each shipment. Do not assume that food-contact or medical approval covers all origins of KL371A, because additive packages and catalyst residues can vary among production sites and lot ranges.
Environmental stress crack resistance data are generated by ASTM D1693-15e1 using notched specimens bent into a channel and immersed in a nonylphenoxy poly(ethyleneoxy) ethanol solution at 50 °C. The F50 time denotes the point at which 50 % of specimens fail. Class-typical blow-moulding HDPE grades often show F50 values above 100 h under Condition A and above 500 h under Condition B; published data for this specific configuration is limited. The transition from ductile yielding to brittle cracking is accelerated by high external stress, high moulded-in residual stress, and sharp corners. In production, the pinch-off weld, the neck corner, and the rim of the container are the strictest ESCR sites. Blow-moulding grades with lower melt flow and higher molecular weight generally show longer F50 than thin-wall injection grades, but their parison sag is higher, so part weight can drift if melt temperature control is poor.
For outdoor service, carbon black at 2.0 % to 2.5 % by mass with an average primary particle size below 25 nm and adequate dispersion can provide ultraviolet shielding. Dispersion quality is checked by ISO 18553:2002 or microscopy; agglomerates above 60 μm are considered unacceptable for pressure-containing parts. Natural or coloured grades without UV stabilizer are limited to indoor applications or short-term outdoor exposure. Avoid blending KL371A with heavily oxidized regrind or with olefin waxes above 2 % because ESCR can fall sharply even when melt flow rate remains within specification. Storage in dry, shaded conditions at or below 40 °C is recommended; prolonged storage above 50 °C can consume the primary antioxidant and alter melt stability.