Tpc Japan Hdpe Kl353a

TPC (Japan) HDPE KL353A

    • Product Name: TPC (Japan) HDPE KL353A
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 908056
    Density 0.954 g/cm³
    Melt Flow Rate 0.35 g/10 min (190°C/2.16 kg)
    Tensile Strength At Yield 30 MPa
    Tensile Elongation At Break >700%
    Flexural Modulus 1200 MPa
    Notched Izod Impact Strength 60 kJ/m²
    Vicat Softening Temperature 127°C
    Heat Deflection Temperature 75°C at 0.45 MPa
    Shore D Hardness 65
    Melting Point 134°C
    Water Absorption <0.01%
    Environmental Stress Crack Resistance >1000 h
    Volume Resistivity >1E16 Ω·cm
    Dielectric Strength 20 kV/mm
    Coefficient Of Linear Thermal Expansion 1.2E-4 /°C
    Thermal Conductivity 0.4 W/m·K
    Mold Shrinkage 1.5-3.0%

    As an accredited TPC (Japan) HDPE KL353A factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing TPC (Japan) HDPE KL353A typically comes in 25 kg polyethylene-lined paper bags, 40 bags per pallet (1,000 kg), shrink-wrapped.
    Container Loading (20′ FCL) 20′ FCL container loading of TPC (Japan) HDPE KL353A: 25 kg bags, palletized, stretch-wrapped, and securely stowed for ocean shipment.
    Shipping TPC (Japan) HDPE KL353A ships as a non-hazardous, solid high-density polyethylene resin. It is not regulated under DOT, IMDG, IATA, or ADR. Supplied in 25 kg bags or octabins, palletized and stretch-wrapped. Keep dry, avoid heat, direct sunlight, and contamination. No UN number or hazard class required.
    Storage Store TPC (Japan) HDPE KL353A in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, and flames. Keep original bags or containers sealed to prevent moisture, dust, and contamination. Avoid contact with strong oxidizing agents. Stack on clean pallets without excessive height. Use first-in, first-out stock rotation and follow the supplier’s SDS and local regulations.
    Shelf Life Store in a cool, dry, ventilated area away from sunlight; shelf life is typically two years in unopened original packaging.
    Application of TPC (Japan) HDPE KL353A

    The conversion of high-molecular-weight HDPE resin into thin-gauge tubular blown film for T-shirt bag stock imposes a specific set of extrusion constraints that diverge from LDPE-grade practice. Melt temperature at the die is maintained within 190–220 °C, with the lower bound dictated by viscosity-related screw torque and the upper bound set by oxidative degradation that manifests as gel formation and a perceivable drop in bubble stability. Die gaps in the range of 0.8–1.5 mm are preferred; narrower gaps amplify melt fracture initiation at the die lip, while wider gaps transfer excessive draw energy to the haul-off section and produce gauge variation. Blow-up ratio (BUR) is conventionally set between 3.5:1 and 5:1 for this polymer class, with the elevated BUR compensates for molecular orientation anisotropy and improves transverse-direction Elmendorf tear resistance. The characteristic high-stalk geometry requires a frost line height of approximately 6–8 die diameters above the air ring, a setting that allows sufficient relaxation time for the molten polymer to respond to biaxial orientation before crystallization arrests further deformation. Production-scale lines equipped with barrier screws having L/D ratios of 24:1 to 32:1 and grooved feed sections report output ceilings governed by bubble oscillation rather than available extruder throughput. Gauge uniformity across the web, measured by a capacitance-scanning head, typically deteriorates beyond a drawdown ratio of 3.5:1 from the die gap to final film thickness. Tensile properties of the resulting film, assessed per ISO 527-3 or ASTM D882, show a consistent machine-direction bias that must be compensated by BUR adjustment. Dart drop impact resistance, tested under ASTM D1709 Method A, and Elmendorf tear values under ASTM D1922 are the primary specification gateways for bag stock acceptance; typical commercial tolerances require maintaining both parameters within a documented control band of ±10% across the lot. Pre-drying is unnecessary at ambient relative humidity below 60%, but above this threshold, a hopper dryer set at 70–80 °C for 2–3 hours prevents surface moisture from generating microbubble defects that appear as optical haze nonconformities under ASTM D1003 measurement.

    What frost line height suppresses transverse-direction gauge bands during thin-gauge HDPE liner film extrusion?

    Industrial liner film in the 6–25 µm thickness band presents a distinct processing conflict: reducing thickness increases the sensitivity of the bubble to ambient air turbulence, while the frost line height must be retracted to limit the residence time in the amorphous state where gauge bands are most readily initiated. The practical resolution depends on the ratio of die diameter to final layflat width. On a 60 mm die running a 3.5:1 BUR, frost line positions between 250 mm and 400 mm above the die face maintain a stable neck geometry without inducing the periodic thickness oscillation that cap gauges record as transverse-direction bands. Dual-lip air rings with internal cooling volumetrically balanced to the extruder output provide the most repeatable bubble control at outputs above 180 kg/h. The degree of alpha-olefin comonomer incorporation (butene or hexene) in the base resin shifts the crystallization onset temperature; higher comonomer content extends the amorphous window and requires a proportionally elevated frost line to delay the freeze-off point beyond the neck transition. Process specialists record that a shift in frost line of ±30 mm correlates with measurable yield stress variation of ±0.3 MPa in the machine direction, a relationship that must be accommodated when certifying lot-to-lot conformity under EN 13501-1 or customer-specific liner integrity protocols. Published data specific to KL353A processing-window interaction with individual air ring manufacturers is limited; empirical calibration on each line remains necessary.

    Extrusion coating of HDPE onto porous surgical paper substrates demonstrates that adhesion is governed by the oxidative pretreatment intensity rather than the rheology of the melt alone. The coating weight is controlled between 12 g/m² and 20 g/m²; below the lower limit, pinhole defects in the coated web exceed acceptable counts per square meter as detected by a high-voltage spark tester in inline inspection. Above the upper limit, curl tendency in the laminated substrate increases because the thermal expansion mismatch between polyolefin and cellulose fiber becomes disproportionate. Ozone treatment of the extrudate curtain at concentrations of 15–30 g/Nm³ with a contact distance of 25–40 mm introduces polar carbonyl functionality at the polymer surface, elevating peel adhesion from the untreated baseline of essentially zero to values exceeding 0.5 N/15 mm when tested under ISO 11339. Chill roll temperature is maintained at 15–20 °C to maximize surface gloss and prevent blocking during reel winding; nip pressure at the rubber backing roll is set to the minimum value that eliminates entrained air pockets, typically 40–60 N/cm of web width. Neck-in of the molten curtain at the die exit must be compensated by setting the die width 60–80 mm beyond the eventual coated width; this offset is a function of draw distance, melt temperature, and air gap, which is ordinarily held below 150 mm to reduce oxidation-related odor formation. Regulatory conformance for peelable medical packaging falls under ISO 11607-1 for sterile barrier system material performance, with supporting extractables data per ISO 10993-18 and biological evaluation under the ISO 10993 series as required by regional notified bodies.

    Blow molding parison sag control and container wall distribution in pharmaceutical bottle production

    Extrusion blow molding of small-volume pharmaceutical containers from this resin class relies on parison programming technology to redistribute material along the axial profile before mold closure. Sag velocity scales with the square of the parison hang length; for a 30 g bottle preform with a hang length approaching 150 mm, unprogrammed sag exceeds acceptable uniformity thresholds within 3–4 seconds. Modern multi-point parison programmers divide the extrusion stroke into 8–32 discrete interpolation points, allowing the die gap to vary continuously from 0.3 mm at the thread region to 1.8 mm at the base pinch-off. Melt temperature windows are deliberately narrow, 180–205 °C, to preserve the intrinsic melt strength that counteracts gravitational elongation; deviation below this band raises backpressure and screw recovery time, while exceeding it produces visible parison curvature and poor base weld integrity. Mold temperature control at 5–15 °C on the cavity side and 10–25 °C on the core side establishes the solidification gradient that determines the location of the knit line. The clamping force requirement for a 60–100 mL bottle does not typically exceed 150–250 kN, measured as the sum of cavity pressure multiplied by projected area. Critical performance specifications for pharmaceutical packaging include drop resistance from 1.5 m onto concrete per USP <671> criteria, Environmental Stress Crack Resistance (ESCR) of the bottle base under ASTM D1693 with a 100% Igepal CO-630 solution, and wall thickness minimum tolerances at specified measurement points verified by a Hall-effect gauge. Batch-to-batch variance in intrinsic viscosity, detectable as a shift in die swell ratio of only 0.03, produces measurable changes in the radial wall distribution of the shoulder region, underscoring the need for resin lot documentation against the molder’s in-process control plan.

    When draw ratios exceed 8:1 in HDPE monofilament and oriented tape extrusion for industrial netting

    HDPE monofilament and raffia tape lines achieve tenacity only when the stretching stage operates in the strain-hardening region that lies above the natural draw point. A water quench bath maintained at 30–40 °C freezes the extruded filament into a partially spherulitic state that retains sufficient amorphous tie chains for subsequent orientation; bath temperatures above 45 °C promote crystal thickening that reduces ultimate drawability and induces filament breakage during the first oven pass. The first-stage hot air oven is controlled to 95–110 °C, with the second stage set 15–20 °C higher to permit limited relaxation while the chain orientation is locked. Total draw ratios between 6:1 and 10:1 are typical, with the final denier for netting applications commonly specified in the range of 400–600 denier and tenacity verified under ISO 2062. Relaxation of 2–5% between the final godet pair reduces residual shrinkage that would otherwise distort netting mesh dimensions during service or post-processing. Production line operators recognize the onset of fibrillation as a precursor to filament failure; this defect is suppressed by maintaining the pre-stretch melt temperature below 235 °C and avoiding the presence of polypropylene contamination above 2 wt%, which segregates at the die wall and creates surface striations. Knot strength retention, a critical parameter for agricultural netting, is quantified as the ratio of knot tensile to straight tensile tested per ISO 1805, with acceptance thresholds typically above 65%. The relevant product standard EN 12683 for polymer netting provides the compliance framework for mechanical and dimensional properties. Residual shrinkage after immersion is measured according to ISO 1806, and commercial netting specifications commonly require shrinkage below 5% after 24 h in water at 50 °C.

    Cable sheathing melt strength and die swell characteristics in HDPE insulation extrusion

    The use of high-density polyethylene in cable sheathing applications places contradicting demands on molecular architecture: the polymer must exhibit sufficient melt strength to maintain concentricity during the vertical drop into a cooling trough, while simultaneously demonstrating a high enough melt flow to penetrate the interstices between twisted conductors at practical line speeds. Crosshead dies designed for pressure extrusion operate with land lengths of 10–15 times the annular gap, promoting orientation that improves crush resistance but increases the risk of melt fracture if the die land temperature drops below 190 °C. Typical melt temperatures for sheathing extrusion are 200–230 °C, with conductor preheat in the range of 120–160 °C to prevent premature solidification at the interface; this preheat is critical for achieving the adhesion level required to pass the insulation stripping test under IEC 60811-409. The dielectric constant of HDPE in the frequency range relevant to power and telecom cables is 2.3–2.4 at 1 MHz, with a dissipation factor below 5 × 10⁻⁴, characteristics that make it suitable for low-capacitance constructions. Environmental stress crack resistance of the sheathing compound is tested per ASTM D1693 Condition A, with HDPE-based insulation materials requiring survival of the full 48 h exposure without failure in more than 10% of specimens. Slipping agents or nucleating additives that modify the crystallization kinetics will alter the post-extrusion shrinkage profile; axial shrinkage restrained by water trough temperature gradients should be maintained below 2% when measured according to IEC 60811-502. The demanding cable manufacturers specify the oxidation induction time (OIT) determined by differential scanning calorimetry under ISO 11357-6 at 200 °C, requiring a minimum of 20 min for materials intended for high-temperature service environments. The use of carbon black masterbatch at 2.5 ± 0.5 wt% is indispensable for UV stabilization in outdoor installations, and its dispersion quality must be verified by microtome cross-section inspection under 50× magnification to ensure no agglomerates exceed 10 µm in diameter.

    Operating parameterDie diameter 50 mmDie diameter 75 mmDie diameter 100 mm
    Melt temperature range190–210 °C195–215 °C200–220 °C
    Typical BUR for bag stock3.0:1–4.0:13.5:1–4.5:14.0:1–5.0:1
    Frost line height250–350 mm350–500 mm450–600 mm
    Output ceiling (bubble-stability limited)120–150 kg/h180–220 kg/h260–320 kg/h
    Drawdown ratio (die gap to final film)2.0:1–3.0:12.5:1–3.5:13.0:1–4.0:1
    Gauge uniformity tolerance (2σ)±8–10%±6–8%±5–7%
    Application segmentPrimary standardSupporting designationTest method reference
    Food-contact film for dry goodsFDA 21 CFR 177.1520EU 10/2011ASTM D1238 for MFR; total migration per EN 1186
    Medical packaging / sterile barrierISO 11607-1ISO 10993-18Peel strength per ISO 11339; air leak per ASTM F2096
    Industrial netting / monofilamentEN 12683ISO 1805, ISO 1806Tensile and knot strength; shrinkage in hot water
    Cable insulation and sheathingIEC 60811-409IEC 60811-502, ISO 11357-6Stripping force; shrinkage; OIT at 200 °C
    Blow-molded pharmaceutical containersUSP <671>ASTM D1693, D2561Drop test; ESCR; wall distribution via Hall-effect gauge
    Free Quote

    Competitive TPC (Japan) HDPE KL353A prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    In high-density polyethylene conversion, grade selection is determined by the interaction of melt flow rate, density, molecular weight distribution, and additive stabilization. TPC (Japan) HDPE KL353A is supplied as a pelletised high-density polyethylene for extrusion blow moulding and heavy-gauge sheet extrusion. The nominal melt flow rate is typically 0.35 g/10 min when measured under ISO 1133-1:2022 at 190 °C/2.16 kg, and the nominal solid-state density is typically 0.953 g/cm³ under ASTM D1505. These values place the grade in the intermediate melt-strength band of the high-density polyethylene spectrum, where parison stability, wall-thickness control, and environmental stress-cracking resistance are selected over maximum stiffness or maximum flow. KL353A is used in rigid industrial packagings, intermediate bulk container liners, and deep-draw sheet products that require resistance to deformation during demoulding and filling. The pellet form is compatible with conventional single-screw extrusion, accumulator-head blow moulding, and sheet calendering lines. All numerical values in this text are typical lot data; contractual specification limits must be taken from the current supplier certificate of analysis.

    What processing window is required for KL353A on blow-moulding equipment?

    Processing of KL353A is normally performed on single-screw extruders with an L/D ratio of at least 24:1 and a barrier or Maddock mixing section. Barrel temperature profiles are set from 170–180 °C in the feed zone to 190–200 °C in the compression zone, with head and die temperatures maintained at 200–220 °C. Melt temperature should remain below 230 °C; above this threshold oxidative degradation accelerates and surface defects, gel formation, and loss of environmental stress-cracking resistance become more probable. In accumulator-head blow moulding, parison length is controlled by melt pressure, accumulator fill speed, and die gap. A melt pump is recommended when downstream clamp cycles impose intermittent demand, because a constant melt pump discharge pressure reduces parison weight variation. Die gaps are commonly set between 1.5 mm and 3.0 mm for final wall thicknesses of 0.8–2.5 mm, but the exact gap must be adjusted for part length and blow ratio. Blow ratios above 3:1 increase the risk of thickness reversal at pinch-off zones and bottom corners. Mould temperature is usually held at 10–25 °C to achieve rapid solidification; textured mould surfaces may require a slightly higher cavity temperature to replicate detail.

    For sheet extrusion, a typical line consists of a 90 mm single-screw extruder, a 1,200 mm coat-hanger die, and a three-roll calendering stack. Melt temperature at the die lips is held at 205–215 °C. Roll temperatures are staggered from approximately 80 °C on the first roll to 60 °C on the third roll to release sheet without differential shrinkage. KL353A has a higher melt viscosity than injection-moulding HDPE but lower viscosity than fractional-melt pipe HDPE; therefore, sheet lines running this grade can use lower melt temperatures than high-viscosity HDPE without exceeding extruder drive limits. Edge-trim recycling is usually possible at regrind addition up to 30 wt% if the regrind is dry, free of fines, and not thermally degraded. Higher regrind additions reduce ESCR and should be validated on the finished part.

    Storage and handling before processing affects surface quality. High-density polyethylene is not hygroscopic, but cold pellets exposed to humid air can condense surface moisture and produce splay or voiding in the extrudate. If pellets are brought into a warm production hall from unheated storage, hopper drying at 80 °C for 2 h is used. Drying beyond 4 h at 80 °C has no benefit and can oxidise the pellet surface if the dryer air is not dry. Silo and surge-bin grounding is required because polyethylene pellets generate static charge and fines. Fines removal by cyclone or sieve is advisable when regrind exceeds 10% of total throughput, because fines cause feed bridging and melt temperature fluctuation.

    The specification sheet does not replace a certificate of analysis for KL353A

    Commercial high-density polyethylene datasheets contain nominal values, not lot-specific acceptance limits. For KL353A, typical data may include tensile yield strength of 28 MPa under ASTM D638-14, flexural modulus of 1,180 MPa under ASTM D790-17, and notched Izod impact in the range 4–6 kJ/m² under ASTM D256. These values are sensitive to specimen cooling rate, thickness, and additive package. A purchase specification should therefore include melt flow rate with a tolerance of ±0.05 g/10 min around nominal, density with a tolerance of ±0.002 g/cm³, and a minimum ESCR F50 value under ASTM D1693 condition B. Published data for the exact ESCR of KL353A are limited; qualification must be performed on moulded parts or compression-moulded plaques rather than relying solely on generic resin databases. The certificate of analysis should also report ash content, colour, and stabilizer levels, because these influence organoleptic properties and long-term oxidation resistance in packaging applications.

    The following table compares the nominal coordinates of KL353A with adjacent high-density polyethylene processing classes. Values are typical ranges and are not contractual specification limits.

    Comparative melt flow and density coordinates for HDPE processing classes
    Processing classMelt flow rate at 190 °C/2.16 kg (g/10 min)Density (g/cm³)Primary design compromise
    KL353A intermediate blow moulding and sheet0.350.953Balanced parison stability and ESCR
    Fractional-melt pipe HDPE0.05–0.100.948–0.950High slow-crack-growth resistance; low output
    Blown film HDPE0.04–0.100.950–0.953High dart impact and melt strength; high head pressure
    Injection moulding HDPE10–300.960–0.965High flow and stiffness; unsuitable for parison retention

    When KL353A replaces a lower-melt-flow HDPE in existing tools

    Substitution of KL353A for a fractional-melt HDPE with melt flow rate below 0.10 g/10 min reduces head pressure and screw torque but shortens parison hang time and increases sag on deep parts. Existing tools with long parison lengths, multi-cavity needle blow pins, or large pinch-off areas may require rebalancing of the die gap controller and increased accumulator fill speed. Because KL353A has lower molecular weight than fractional-melt HDPE, its environmental stress-cracking resistance is typically lower; heavy-duty detergent bottles or containers exposed to nonionic surfactants must be revalidated by ASTM D1693 or full-container stress-crack testing. If the melt flow rate is higher than 10 g/10 min, injection-moulding HDPE lacks sufficient melt strength to hold a parison; KL353A increases melt strength but also increases cooling time because the thicker walls solidify more slowly. For blown film applications, KL353A’s 0.35 g/10 min melt flow rate is generally higher than the 0.04–0.10 g/10 min range used for high-molecular-weight film and may produce low dart impact and excessive bubble instability. For pipe extrusion, KL353A is not a PE100-class resin and should not be substituted in pressure-rated pipe systems where long-term hydrostatic strength is required.

    In injection moulding, KL353A is not an appropriate grade. Its melt flow rate is far below the 10–30 g/10 min range typical for high-density polyethylene injection moulding. Attempting to process KL353A in an injection press produces high fill pressures, short shots, and frozen-in orientation, especially in thin-wall closures or crates. Prototype development using a high-flow letdown blend invalidates the ESCR and food-contact status of the original grade and should not be used for compliance testing.

    Environmental stress cracking and chemical exposure boundaries

    Environmental stress-cracking resistance in high-density polyethylene is controlled by density, molecular weight, comonomer type, and cooling-induced crystallinity. At 0.953 g/cm³, KL353A is in the intermediate ESCR band, which supports moderate detergent and industrial packaging applications but not aggressive hot surfactant or chlorinated solvent service. Polar solvents such as water, alcohols, dilute acids, and alkalis are generally compatible at ambient temperature. Aromatic hydrocarbons, chlorinated solvents, and strong oxidizing acids cause swelling or surface degradation. Ketones and esters can initiate surface crazing when tensile stress and chemical exposure act simultaneously. Moulded-in residual stress from rapid cooling increases sensitivity; therefore, sharp corner radii and deep draw ratios should be minimised in parts exposed to stress-cracking agents. Full-container testing at 60 °C and 0.5 MPa internal pressure is preferred over flat coupon data for aggressive filling environments, because weld-line and pinch-off stresses dominate field failures.

    Measure the pinch-off weld line before qualifying the mould

    Pinch-off weld-line splitting is a recurrent failure mode in blow-moulded industrial containers, and it is often incorrectly attributed to resin lot changes. On production-scale accumulator blow-moulding lines, splitting is most often caused by insufficient pinch-off insert sharpness, low clamp tonnage, or parison temperature below the processing window. With KL353A’s intermediate molecular weight, weld strength is lower than that of fractional-melt HDPE; pinch-off inserts should be sharp, and clamp force should be sufficient to compress the parison without bouncing. For a typical 20-L container, clamp force requirements are often in the range 150–250 kN, but the exact value depends on part shape and wall thickness. Parison oscillation and shark-skin melt fracture are also observed when the shear rate at the die lip exceeds the critical value for the molecular weight distribution. Increasing die gap or reducing screw speed normally eliminates shark skin; a fluoropolymer process aid can be used at the feed throat if high output cannot be sacrificed. The output limit is equipment-specific and must be established by a designed experiment, not by visual inspection alone.

    Thermal degradation pathways during long residence times

    High-density polyethylene degrades by simultaneous chain scission and crosslinking, with the dominant route depending on oxygen availability and residence time. In the extruder barrel below 230 °C, degradation is slow; however, stagnant melt zones in the adaptor, screen pack, and die can generate gel particles and black specks when the line is stopped without purging. KL353A should be purged with a fractional-melt HDPE or a commercial purging compound before shutdown. If the melt temperature exceeds 260 °C, oxidative chain scission accelerates and produces lower-viscosity material, which changes parison sag and reduces ESCR. Under nitrogen-purge differential scanning calorimetry, the oxidative induction time of stabilised HDPE is typically above 20 min at 200 °C under ASTM D3895; the exact value for KL353A must be read from the supplier’s lot certificate. Published data for this specific configuration is limited.

    Incoming inspection should focus on melt flow rate and density before the material is committed to production. A change of 0.02 g/10 min in melt flow rate can alter parison length by several millimetres on large accumulator machines. Density changes of 0.001 g/cm³ are less visible but can shift shrinkage and stacking height in finished containers. Operators should retain a reference lot and test new lots side by side on a small blow-moulding machine before release to high-volume packaging lines. Moisture and fines are not routinely tested but should be checked if there is evidence of conveying problems or surface defects.

    Regulatory documentation for KL353A is application-specific. For food-contact use, a supplier may evaluate the grade against FDA 21 CFR 177.1520, which covers olefin polymers subject to migration limits and end-use restrictions. Compliance with REACH Regulation 1907/2006 and RoHS Directive 2011/65/EU requires lot-specific supplier statements; screening for lead, cadmium, mercury, hexavalent chromium, PBB, and PBDE is typically performed by XRF under IEC 62321. Industrial packaging for non-food use may be covered by supplier declarations on heavy-metal content under US CONEG or 94/62/EC. Pharmaceutical and medical applications require USP 661.1 and 661.2 testing on the finished article, because conversion and sterilization can change extractables. A resin certificate alone is not sufficient for medical device or pharmaceutical registration.

    Colour concentrates, antistatic agents, and slip agents can alter the crystallisation rate and ESCR of KL353A. Fluoropolymer process aids, when used to eliminate shark-skin, are generally compatible but must be added at the feed throat and should not exceed 0.1% of total throughput. Antistatic concentrates may absorb moisture; they should be dried separately or added only in a vented compounding step. Avoid combinations with pro-oxidant additives intended for degradable films, because these will reduce long-term heat aging and may invalidate food-contact status.

    Top