| HS Code | 631969 |
| Density | 0.952 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 0.35 g/10 min |
| Tensile Strength At Yield | 27 MPa |
| Tensile Strength At Break | 30 MPa |
| Elongation At Break | 700% |
| Flexural Modulus | 1100 MPa |
| Vicat Softening Temperature | 125 °C |
| Heat Deflection Temperature At 0 46 Mpa | 75 °C |
| Shore D Hardness | 65 |
| Izod Notched Impact Strength | 10 kJ/m² |
| Environmental Stress Crack Resistance | >1000 h |
| Brittleness Temperature | < -70 °C |
| Water Absorption | < 0.01% |
As an accredited TPC (Japan) HDPE KL352A factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | TPC (Japan) HDPE KL352A is packaged in 25 kg net multiwall paper bags, typically palletized and shrink-wrapped for shipment. |
| Container Loading (20′ FCL) | Container Loading (20′ FCL) for TPC (Japan) HDPE KL352A: 25 kg bags, palletized, shrink-wrapped, securely stowed in dry container, sealed for export. |
| Shipping | TPC (Japan) HDPE KL352A is shipped as non-hazardous high-density polyethylene resin in 25 kg bags, jumbo bags, or bulk. Palletized, stretch-wrapped, and labeled, it moves in clean, dry containers. Store away from moisture, contamination, heat, and direct sunlight. Not classified as dangerous goods (HS Code 3901.20). Transport by sea, road, or rail. |
| Storage | Store TPC (Japan) HDPE KL352A resin in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks and flames. Keep bags or containers closed, palletized, and protected from moisture, dust, and contamination. Avoid prolonged UV exposure and extreme temperatures. Use first-in, first-out. Follow local regulations and the supplier’s SDS. Ensure good ventilation and no ignition sources. Inspect packaging regularly. |
| Shelf Life | Shelf life: about 24 months when stored in original packaging, in a cool, dry, well-ventilated area away from direct sunlight. |
TPC (Japan) HDPE KL352A is an extrusion-blow-moulding-grade high-density polyethylene. This application section is limited to downstream segments where medium-molecular-weight HDPE grades with comparable melt strength, parison swell, and pinch-off weld behaviour are run on production-scale machinery. Thin-gauge blown film, rotomoulding, fibre extrusion, and foaming are excluded because the validated processing platform of KL352A does not align with those converting routes. The scenarios below cover industrial packaging, monolayer chemical containers, barrier post-treatment, coextruded agrochemical packs, automotive technical blow mouldings, and thick-sheet thermoforming. Every processing value is a production-derived starting point, not a warranty figure; the lot certificate of analysis, ambient conditions, and tooling geometry remain the final setpoint authority. Where no published data exist for a specific configuration, that limitation is stated explicitly.
Where the term “addition ratio” appears, it refers to gravimetric let-down at the feed throat or an automated dosing station, expressed as weight percent of total throughput. The term “regrind” is defined as post-industrial pinch-off flash, rejected moulded parts, and edge trim generated on the same converting line. Post-consumer recycled material is not assumed in any of these scenarios unless a dedicated migration and mechanical validation programme is performed by the converter.
In 10–30 L UN-certified jerrican and 120–220 L open-head drum production, the dominant process conflict is not melt temperature alone but the interaction between parison programming, mould parting-line pinch-off geometry, and tail flash removal. KL352A is processed on accumulator-head or continuous blow moulders with extruder L/D ratios of 24:1 to 30:1 and barrier screws fitted with shear-mixing elements. The die gap is typically set at 1.8–2.8 mm, and the parison wall profile is programmed over 10–30 segments so that the wall at the pinch-off zone is 0.15–0.25 mm thicker than the nominal sidewall target before mould closure. Blow air pressure is set at 0.55–0.75 MPa, and mould coolant temperature is maintained at 10–20 °C for cycle control. Head melt temperature is held between 190 °C and 205 °C. Below 185 °C, the pinch-off weld becomes insufficiently healed; above 210 °C, surface oxidation and flow marks may appear at the die lip.
The UN design-type approval path for rigid plastics packaging requires drop testing, stack loading, and weld-zone integrity under hydrostatic pressure. On a production line running 80–120 units/h, a packaging lot may pass the room-temperature drop test and then fail the 40 °C stack test because hydraulic pressure acts directly on the pinch-off weld. Regrind from flash and rejected parisons is normally introduced at 10–25 wt%, sieved to remove particles above 6 mm, and blended with virgin pellets using a gravimetric hopper feeder with ±0.25% accuracy. Pigment masterbatch is let down at 2.0–4.0 wt%; if UV stabiliser masterbatch is required for outdoor storage, the additional let-down is 0.8–1.5 wt%. The melt is filtered through 80/120 mesh screen packs to protect the accumulator head and die lips from carbonised regrind agglomerates. Terminal products include 20–30 L UN-rated jerricans and 120–220 L open-head drums with calibrated closure bosses and drop-test-friendly handle wells.
| Test programme | Method / standard | Observable control range |
|---|---|---|
| Drop impact, 23 °C | ISO 2248:1985 / ADR 6.1.5.3 | 1.2 m for PG II, 0.8 m for PG III |
| Stack compression, 40 °C, 28 d | ISO 2234:2000 | No leakage; top load ≥ 3× stacked mass |
| Hydrostatic pressure, 23 °C | ISO 16104:2003 | 100 kPa for 30 min or 150 kPa for 5 min |
| Environmental stress crack resistance, weld zone | ASTM D1693-15 Condition B | F50 > 300 h where specified |
In 500 mL to 5 L monolayer household and industrial chemical bottles, line configuration is typically a shuttle single/double station blow moulder with a 45–65 mm 24:1 L/D extruder, replaceable converging-diverging die head, and in-mould neck calibration. A production lot may run at 12–18 s cycle time for a 1 L bottle with a wall thickness of 0.8–1.1 mm. White or coloured masterbatch is metered at 1.5–2.5 wt%, and if antistatic performance is specified for powder or solvent-adjacent filling lines, a PE-carrier antistatic masterbatch at 0.5–1.0 wt% is added only after compatibility testing because some antistatic carriers can shift die swell if overloaded. The product must conform to EU 94/62/EC heavy-metal packaging limits with Pb+Cd+Hg+Cr(VI) below 100 ppm, and to REACH registration obligations for the final packaged substance. Air pressure is set to 0.6–0.8 MPa with pre-blow delay from 0.2 s to 0.8 s; the pre-blow setting, not air pressure, governs radial wall distribution in small bottles. Mould cooling is run at 8–15 °C; at cooling water above 20 °C, sidewall sink marks may appear around pinch-off areas. Finished products are closed-head detergent bottles, bleach containers, disinfectant packs, and industrial chemical bottles with 38 mm or 42 mm neck finishes.
Fluorine post-treatment of monolayer HDPE containers is used where the packaged liquid contains aromatic hydrocarbons, esters, ketones, or low-molecular-weight halogenated solvents that would otherwise swell or permeate the wall. In this converting route, the blow-moulded KL352A container is exposed to fluorine gas at 0.1–0.3% concentration in nitrogen in a pressurised stainless steel reactor at 30–60 °C for 5–20 min. The reactive treatment converts the inner surface to a fluoro-carbon barrier layer with a thickness of 0.5–5 μm, which reduces solvent weight loss without altering outer-surface label adhesion or top-coating. Formula addition before moulding is limited to 2.0–3.0 wt% colour masterbatch and 0.3–0.8 wt% processing aid; migratory slip agents are excluded because a low-molecular-weight surface film interferes with fluorination. The monolayer bottles are produced on continuous-extrusion blow moulders with melt temperature 185–195 °C, die gap 1.5–2.2 mm, and mould temperature 10–18 °C. After fluorination, the containers are used for 0.5–5 L packaging of automotive aftermarket fluids, solvent-based adhesives, paint thinners, and agricultural adjuvants. Container permeation resistance is generally tested under ASTM D2684-15, and the final packaging is qualified under the same UN/DOT closure and drop provisions as non-fluorinated containers. The fluorination chamber is maintained under negative pressure, and residual fluorine is quenched by alkaline scrubbing before discharge. Published data for this specific configuration is limited when the converted wall thickness falls below 0.9 mm; in that case, the fluorination time is reduced and barrier performance must be confirmed by lot-level permeation testing.
In coextruded blow moulded agrochemical and solvent-borne product containers, KL352A is used as the outer and inner structural layers because its melt elongation and pinch-off weld strength permit thin layer ratios without sacrificing drop impact. A typical six-layer structure consists of outer HDPE layer 25–35 wt%, adhesive tie layer 1.5–2.5 wt%, EVOH barrier layer 3–6 wt%, adhesive tie layer 1.5–2.5 wt%, regrind layer 25–35 wt%, and inner HDPE layer 20–30 wt%. The EVOH grade selected for solvent barrier applications typically has an ethylene content of 27–38 mol%; at lower ethylene contents, the barrier improves but the layer becomes prone to brittle failure in cold drop tests. The coextrusion blow moulder uses layer-definite side-fed die heads or a feedblock with individual melt pumps for each layer; HDPE melt temperature is maintained at 200–215 °C, while EVOH streams are kept below 215 °C to avoid thermal degradation. The adhesive is selected from maleic anhydride-grafted LLDPE or HDPE grades; a minimum tie-layer thickness of 0.03 mm is needed to prevent interlayer delamination at the pinch-off. The resulting containers, usually 1–10 L, are filled with emulsifiable concentrates, oil dispersions, or organic solvents that would show unacceptable permeation through a monolayer wall. Regulatory qualification includes EC 1107/2009 when used for plant protection product formulation packaging, ADR/RID/IMDG as dangerous goods packaging, and EU 10/2011 only if food-contact claims are separately validated on the food-contact layer. Because the process introduces polar barrier polymers, the regrind layer is limited to post-industrial scrap generated on the same line; no post-consumer recyclate is introduced into the barrier core without a dedicated migration and barrier validation study.
Automotive under-hood and cabin air-management parts are blow moulded with KL352A on extrusion blow moulding machines fitted with 3D parison manipulators, suction-blowing transfer, or blade-cut parison transfer systems. The most common processing conflict is that the part wall thickness must stay within 2.0–3.5 mm to meet burst and vibration requirements, while long flow paths around insert pins and welding points create local thinning below 1.8 mm. Parison programming over 20–40 points is combined with mould temperature control at 15–25 °C and melt temperature at 190–205 °C. Carbon black UV-stabilised masterbatch is metered at 1.5–2.5 wt% for parts with outdoor exposure; for under-hood parts not exposed to direct sunlight, a heat-stabilised compound at 0.3–0.6 wt% is used. The process requires a vacuum leak test at 0.03–0.05 MPa or a hot-tip leak test depending on OEM specification. Typical finished products include 2–6 L windscreen washer reservoirs, coolant recovery bottles, and HVAC ducts for dashboard plenum extraction. Compliance is governed by OEM material standards derived from ISO 16750-4:2023 for environmental loads and from REACH entry restrictions for phthalates and heavy metals. Published data for this specific configuration is limited when a new tool introduces a non-circular pinch-off insert; therefore the initial run is gated at 50–100 pieces for CMM wall-thickness mapping before full-rate production.
Thick-sheet extrusion and vacuum forming of returnable materials handling liners and trays uses KL352A at a lower forming pressure than container blowing, but the same dosage discipline applies. Sheet lines typically run a 90–120 mm 35:1 L/D single-screw extruder with a 100–150 kg/h output, a screen changer with 60/100 mesh packs, and a three-roll polishing stack set at 70/85/75 °C for top/middle/bottom rolls. Die lip opening is set at 3.0–6.0 mm to produce 2–8 mm sheet. Colour masterbatch is added at 1.0–2.5 wt%, and outdoor-stable grades receive UV masterbatch at 1.5–3.0 wt%. When thin-gauge vacuum forming is performed, sheet surface temperature is heated to 150–180 °C in a zoned quartz or ceramic oven, with a pre-stretch plug and a vacuum level of -0.08 MPa to -0.06 MPa. The formed part is trimmed on CNC routers with tolerance of ±0.5 mm for edge location. Terminal products are returnable interlayer dunnage, washable tray liners, and bin inserts; these parts are not tested to UN packaging standards, but they must satisfy EU RoHS 2011/65/EU Annex II heavy-metal limits and the general safety requirements of EU 2023/988 for articles used in the logistics chain. If the trays are in repeated contact with packaged food, the food-contact shell layer is separately validated under FDA 21 CFR 177.1520 and EU 10/2011 with a migration cell test under conditions selected from EU 10/2011 Annex III and Annex V. The operational boundary for this converting route is that a sheet line is a dedicated heavy-gauge platform; attempting to run KL352A on a thin-gauge blown film tower is outside the scope of validated processing and may result in bubble instability and gauge scatter.
Competitive TPC (Japan) HDPE KL352A prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
TPC (Japan) HDPE KL352A is a high-density polyethylene extrusion resin designated for heavy-wall pipe, structural sheet, and industrial profile applications in which long-term hydrostatic strength and resistance to slow crack growth control service life. The product is supplied as a pelletized compound; the model code KL352A identifies the grade within the supplier’s high-molecular-weight HDPE family. Published numerical data for this exact configuration remain limited outside the manufacturer’s controlled technical datasheet; therefore, all property values cited here are class windows for high-molecular-weight HDPE pipe compounds and must be checked against lot-specific certificates of analysis before production qualification.
In specification terms, the resin is typically assessed under ISO 1183-1 for density, ISO 1133-1:2022 for melt mass-flow rate, and ISO 527-2 for short-term tensile properties. When intended for pressure pipe, long-term performance is evaluated through hydrostatic strength testing according to ISO 9080 and slow crack growth testing according to ISO 13479. The grade is not a low-viscosity injection compound; its melt-flow window places it at the high-molecular-weight end of the HDPE range, which changes downstream equipment requirements compared with standard injection or thin-wall film grades.
For pressure-pipe applications, the governing design parameter is the minimum required strength derived from the long-term hydrostatic regression curve. High-molecular-weight HDPE grades in this class are usually classified as PE100 when the lower confidence limit at 50 years and 20 °C satisfies 10 MPa circumferential stress. KL352A must be evaluated against this classification under ISO 9080; the standard requires a regression coefficient and lower prediction limit, not a single burst value. The table below provides representative control windows for the physical and thermal properties expected in this grade family.
| Property | Test method | Representative control window |
|---|---|---|
| Density at 23 °C | ISO 1183-1 | 0.957–0.961 g/cm3 |
| Melt mass-flow rate at 190 °C / 5 kg | ISO 1133-1:2022 | 0.35–0.45 g/10 min |
| Tensile yield stress | ISO 527-2 | 24–26 MPa |
| Elongation at break | ISO 527-2 | >600% |
| Flexural modulus | ISO 178 | 900–1100 MPa |
| Vicat softening temperature, method A50 | ISO 306 | 123–127 °C |
| Oxidative induction time at 200 °C | ISO 11357-6 | >20 min |
These values are not lot-release limits; the manufacturer’s certificate of analysis may define narrower internal windows and specifies observed values for each production lot. In addition, pipe-grade formulations may include carbon black or stabilizer packages that shift density and melt-flow values slightly relative to natural resin; KL352A must be qualified in the exact compounded form to be used in production.
Long-term hydrostatic strength is not a single measurement but a regression. Pipe samples are tested at 20 °C, 40 °C, and 60 °C at several hoop stresses, and failure times are fitted to a three-parameter or four-parameter model. The lower prediction limit at 50 years must remain above 10 MPa for PE100 classification. This means that a short-term burst test at 23 °C cannot certify a PE100 grade, and the resin must demonstrate no brittle knee in the regression before 50 years. The melt-flow value at 5 kg is used because high-molecular-weight HDPE has a melt mass-flow rate at 2.16 kg that is too low for reproducible measurement. A shift of 0.02 g/10 min in the 5 kg value is significant for extrusion throughput and melt-pressure response, so gravimetric feeding and closed-loop pressure control are recommended.
In extrusion plants, the primary processing difference between KL352A and lower-molecular-weight HDPE grades appears at the feed section and in melt-pressure control. Pipe lines equipped with grooved-feed single-screw extruders having 30:1 to 36:1 L/D ratios are appropriate for this viscosity class. The recommended barrel profile is typically 180–210 °C from the feed throat to the metering zone, with melt temperature held between 200 °C and 230 °C depending on die size and line speed. At 210 °C melt temperature, high-molecular-weight HDPE of this type can develop melt pressure before the breaker plate in the range 350–450 bar; the exact value depends on screw speed, backpressure, and filter pack. If the extruder is not equipped with a high-torque gearbox and reinforced thrust bearing, output rate may fall below the line’s rated capacity, and melt-temperature homogeneity may degrade, producing periodic wall-thickness variation in the finished pipe.
Die swell is higher than observed with unimodal HDPE grades because the molecular weight distribution contains a high-molecular-weight tail. Dies with land lengths of 20–30 times the gap are recommended to reduce extrudate swell and stabilize wall thickness at haul-off speeds above 1.5 m/min. The increased melt strength supports large-diameter pipe formation and reduces sag in thick-walled sections. However, shear heating in deep-flight screws can exceed 10 °C if screw speed is raised without compensating barrel temperature, and this is a common cause of surface roughness and thermal degradation on start-up. Direct temperature measurements at the screw tip should be used to cross-check the melt condition, rather than relying only on barrel-zone setpoints.
The melt temperature window is constrained by two failure modes. At temperatures above 240 °C, oxidative degradation can lower the elongation at break and shift the carbonyl index measured under ageing protocols; at temperatures below 190 °C, the high-molecular-weight fraction may not fully plasticate, creating microgel or white specks in the pipe wall. Therefore the producer’s recommended melt-temperature window for high-viscosity HDPE pipe extrusion is often held within ±5 °C of the target, and line operators monitor melt-pressure stability and gloss as real-time proxies for homogeneity. Intermittent screw-speed changes greater than 10% without compensating setpoint adjustments are known to produce melt-pressure oscillations that result in wall-thickness variation exceeding 0.5 mm in large-diameter pipe.
Cooling and sizing require controlled external water quench temperatures in the range 15–25 °C. Lower quench temperatures may increase surface gloss but may also generate frozen-in stress that affects slow crack growth. Air cooling should be avoided for thick sections because it allows spherulitic growth and density gradients that reduce long-term hydrostatic strength. Vacuum calibration tanks with differential pressure above 0.4 bar and a spray or flood quench configuration are commonly used for pipe diameters above 110 mm. Screw design should favor a compression ratio of 3:1 to 3.5:1 with a grooved feed section or barrier flight. High-shear mixing sections are generally not required and can over-shear the melt, producing excessive shear heat. Output rates on a 75 mm grooved-feed extruder with 33:1 L/D can range from 250 to 350 kg/h for HDPE pipe grades of this type, depending on head pressure and screw condition.
HDPE KL352A generally does not require pre-drying when packaging is intact and storage relative humidity is below 60%; if condensation occurs, drying with desiccant air at 70 °C for 2 h is sufficient. Warehouse storage below 40 °C and away from direct sunlight limits oxidative ageing of pellet additives. Open containers should be used within one shift and protected from dust and moisture. When a hopper loader is used, particle segregation is generally negligible for pelletized HDPE, but fines generation from pellet abrasion can create melt-blockage at the screen pack; maintaining a screen pack of 60/120 mesh with a breaker plate pressure indicator is standard.
Substitution of KL352A into a production line running a conventional unimodal HDPE or PE80 resin is not a drop-in change without revalidation. The comparative differences are most visible in slow crack growth resistance, die swell, melt pressure, and long-term hydrostatic design basis. A structural comparison is provided below; values are generalized class-level data, not the supplier’s stated guarantees.
| Variable | KL352A class expectation | Conventional unimodal HDPE pipe grade |
|---|---|---|
| Molecular architecture | Bimodal or high-molecular-weight distribution | Unimodal, narrower molecular weight distribution |
| Melt mass-flow rate at 190 °C / 5 kg | 0.35–0.45 g/10 min | 0.5–0.8 g/10 min |
| Slow crack growth performance under ISO 13479 | Typically above 500 h at 80 °C | Commonly below 300 h under identical conditions |
| Die swell | Higher | Lower |
| Melt pressure before screen pack | 350–450 bar | 250–350 bar |
| Minimum required strength class | PE100 if validated under ISO 9080 | PE80 or PE100 depending on formulation |
In practice, the replacement of a PE80 resin with KL352A may permit a reduction in wall thickness for the same pressure rating only if the final pipe is reclassified under the appropriate ISO pipe standard and the lot-specific hydrostatic data demonstrate the higher MRS. The wall-thickness reduction cannot be assumed from the resin alone because pipe standards such as ISO 4427 require a dimension ratio and material combination that is supported by regression data. Similarly, gas distribution pipe under ISO 4437 imposes additional requirements for rapid crack propagation resistance, and a higher MRS class does not automatically satisfy those tests.
The slow crack growth mechanism in HDPE pipe is controlled by tie-molecule density and lamellar morphology. Bimodal high-molecular-weight HDPE distributes short-chain branches preferentially in the high-molecular-weight fraction, increasing the number of interlamellar tie molecules and creating a more stable fibrillar structure. This architecture improves notched pipe test performance under ISO 13479, but it also increases melt viscosity and processing difficulty relative to unimodal resins. The improvement is not monotonic with density; densities above 0.965 g/cm3 can reduce slow crack growth resistance because the crystalline fraction restricts tie-molecule mobility, so KL352A should be maintained within its specified density envelope rather than boosted for stiffness.
In gas distribution service, rapid crack propagation is evaluated with full-scale tests such as ISO 13477. A resin with high MRS may still exhibit fast crack growth if the decompression conditions and fracture energy balance are unfavorable. Therefore, a PE100 designation alone does not authorize gas service; the pipe must meet critical pressure criteria at the intended pipe diameter and wall thickness. When KL352A is used in gas applications, the extruded pipe must be tested in the final diameter and SDR.
Compared with high-flow HDPE injection grades, KL352A has a much lower melt index and is not suitable for thin-wall injection molding. Injection grades typically show melt mass-flow rates above 4 g/10 min at 190 °C / 2.16 kg, while KL352A is expected to be below 0.2 g/10 min under the same load, although the producer reports the 5 kg value for pipe-grade materials to avoid excessive measurement error. Compared with film grades, KL352A has higher density and broader molecular weight distribution, leading to higher stiffness and melt strength but lower clarity.
Batch-to-batch variation in melt-flow rate of ±0.02 g/10 min can alter melt pressure by 15 bar at constant screw speed, and the extruder control system should be tuned to compensate. If the line operates with a fixed die and haul-off speed, a shift in melt viscosity changes die swell and wall thickness; therefore in-line wall-thickness measurement with ultrasonic or laser micrometers is recommended for pipe diameters above 160 mm.
Lot release testing for high-molecular-weight HDPE pipe resin typically includes melt flow rate, density, tensile properties, oxidative induction time, and carbon black content or dispersion when the grade is a black compound. The certificate of analysis should align with the purchaser’s specification and the quality plan under the relevant pipe-industry control. Disputes should be resolved using the test conditions and conditioning periods specified in the standard, not by single measurements on unconditioned pellets.
KL352A should not be combined with random copolymer polypropylene or with heavily loaded flame-retardant masterbatches without compatibility testing. A strong incompatibility appears with certain amine-based antioxidants or excessive acidic purging compounds, which disrupt the stabilizer package and lower oxidative induction time below the 20 min threshold commonly required for pipe approvals. If regrind from external sources is introduced above 20 wt%, the certificate of analysis must be re-established because unknown stabilizer packages can alter melt stability and long-term hydrostatic behavior.
Continuous hydrostatic service for HDPE pipe is usually limited to 20 °C as the reference temperature for design, with higher-temperature service requiring derating factors given in ISO 13760 or national pipe standards. Above 60 °C, long-term creep strength declines sufficiently that high-density polyethylene pipe becomes unsuitable for most pressurized hot-water duties; for such conditions a different polymer class such as PE-RT or metal piping is required. KL352A therefore is not a substitute for hot-water pipe grades.
For potable water contact, certification is product-specific. A general HDPE resin cannot be assumed compliant with FDA 21 CFR 177.1520 or EU Regulation 10/2011; the final compound must be tested for migration according to the relevant food-contact method and the specific additive package. If KL352A is sold as a natural resin without a food-contact statement, it should not be used in food-contact pipe until such certification is provided. Regulatory declarations under REACH and RoHS are usually issued by the supplier for the lot; a generic statement of absence of heavy metals is not sufficient for CE marking under the Construction Products Regulation.