| HS Code | 840152 |
| Density | 0.935 g/cm³ |
| Melt Flow Rate 190c 2 16kg | 0.35 g/10 min |
| Tensile Strength At Yield | 24 MPa |
| Tensile Elongation At Break | >500% |
| Flexural Modulus | 1000 MPa |
| Notched Izod Impact Strength 23c | 25 kJ/m² |
| Vicat Softening Temperature | 123 °C |
| Heat Deflection Temperature 0 45mpa | 72 °C |
| Hardness Shore D | 65 Shore D |
| Environmental Stress Crack Resistance F50 | >1000 h |
| Melting Point | 131 °C |
| Brittleness Temperature | < -70 °C |
| Thermal Expansion Coefficient | 1.2E-4 /°C |
| Water Absorption 24h | <0.01% |
As an accredited TPC (Japan) HDPE KL350A factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | TPC (Japan) HDPE KL350A is supplied in 25 kg net multi-wall paper bags, palletized and shrink-wrapped for shipment. |
| Container Loading (20′ FCL) | 20' FCL container loading of TPC (Japan) HDPE KL350A: 25 MT bagged resin, palletized, shrink-wrapped, securely loaded for export. |
| Shipping | TPC (Japan) HDPE KL350A is a non-hazardous high-density polyethylene resin, not regulated for transport (no UN number or hazard class). Ship in sealed bags, FIBCs, or bulk containers. Keep dry, cool, and away from ignition; handle as general industrial cargo under local regulations. |
| Storage | Store TPC (Japan) HDPE KL350A in a cool, dry, well-ventilated warehouse, away from direct sunlight, rain, moisture, heat sources, flames, and strong oxidizers. Keep original bags sealed on pallets; avoid crushing, tearing, and prolonged heavy stacking. Maintain moderate temperature and humidity, use FIFO, protect from dust and mechanical damage, and do not store near food, feed, or drinking water. |
| Shelf Life | Stable under normal storage; shelf life is typically 24 months when kept cool, dry, away from heat, sunlight, ignition sources. |
KL350A is injected at high speed into multi-cavity thin-wall moulds for food storage containers and overcap lids. The melt temperature at the nozzle is held between 210°C and 240°C, while the mould cooling circuit is run at 8°C to 15°C to freeze a wall section of 0.5 mm to 0.9 mm within 4 s to 8 s. The screw uses a 22:1 L/D configuration with a non-return valve and a melt cushion of 2 mm to 4 mm; injection speed is set between 80 mm/s and 150 mm/s to prevent jetting at the gate. Hot-runner manifold temperatures are not allowed to exceed 240°C because extended residence time above that point shifts the MFR measured to ISO 1133-1:2022 and increases low-molecular-weight oxidation by-products. The grade designator is not a substitute for batch MFR; the value is confirmed to ISO 1133-1:2022 before hot-runner temperatures are fixed. Colour masterbatch is added at 2 wt% to 3 wt%, and post-industrial regrind is limited to 10 wt% unless the lot is re-stabilised. Terminal products include dairy tubs, disposable meal trays, cutlery trays, and tamper-evident overcap lids. Food-contact conformity is verified to FDA 21 CFR 177.1520 and EU 10/2011, including overall migration testing with food simulants assigned under Regulation (EU) No 10/2011. The mould texture is specified as VDI 24 to 30 to mask flow lines and improve release without external mould-release spray.
The limiting property in closure moulding is not short-term tensile strength but environmental stress-crack resistance, measured on injected or compressed plaque specimens by ASTM D1693-15 Method B. Melt temperature is held between 210°C and 240°C, while the chilled water circuit is maintained at 5°C to 10°C to minimise crystallinity gradients across the cap shell. Cycle time for a 28 mm two-piece water closure is typically 6 s to 10 s in a 48-cavity valve-gated hot runner. The gate land length is 0.6 mm to 0.8 mm, and gate diameter is matched to shell weight in the 2.8 g to 4.2 g range to prevent stringing. Colourant and slip additive concentrates are not added above 1.5 wt% because over-concentration of migrating slip agents can reduce torque retention on carbonated beverage closures after CO2 contact. Terminal items include water and aseptic closures, sports cap bases, and tamper-evident closures. Leakage testing is performed at 1.1 bar to 1.5 bar internal pressure after in-line capping, and closure dimensions are checked against the tool-specific capability study. Published data for KL350A-specific ESCR values in finished closures is limited; closure lots are released on a combination of supplier batch test data and in-house 48-cavity trial results. The melt is not held above 250°C because closure ESCR declines sharply after excessive residence time or shear heating in multi-cavity hot-runner tips.
During production of returnable distribution crates and pallet collars, KL350A is injected into solid-wall tools with nominal wall thicknesses of 3.0 mm to 6.0 mm. Melt temperature is controlled at 210°C to 250°C, mould wall temperature is kept between 10°C and 30°C, injection pressure is set at 70 MPa to 120 MPa, and hold pressure is profiled at 45 MPa to 70 MPa. Screw backpressure is maintained at 0.5 MPa to 1.0 MPa to homogenise optional UV stabiliser masterbatch added at 1 wt% to 3 wt%. Shrinkage of such mouldings falls between 1.5% and 2.5% when measured by ISO 294-4, and mould design compensates with internal radii not less than 0.6 mm at rib intersections. Warpage on a 600 mm × 400 mm crate is corrected by adjusting gate location and hold-pressure profile rather than by increasing mould temperature, because localised overheating lengthens cycle time without eliminating post-mould distortion. Post-industrial regrind from runner systems is limited to 20 wt% because higher fractions reduce notched Charpy impact and widen the mould-filling pressure window. Terminal products include open-grid distribution crates, ventilated crates, pallet collars, and solid-wall dunnage sheets. Mechanical acceptance is based on flexural modulus under ASTM D790-17 and notched Charpy impact under ISO 179-1:2010, with lot-to-lot MFR monitored to ISO 1133-1:2022 to detect regrind-induced chain scission.
When KL350A is injected into open-top industrial pails with moulded handle ears, the melt temperature is set at 200°C to 240°C and the mould is cooled to 10°C to 25°C. Wall thickness in pail sidewalls is maintained at 1.8 mm to 2.5 mm, and the bottom corner radius is kept at or above 3 mm to prevent stress concentration during stack loading. The injection phase uses a velocity-controlled profile with a peak pressure limit of 120 MPa; hold pressure is switched by screw position, not by timer, at a cushion of 4 mm to 6 mm. In-mould labels or colourant masterbatch are let down at 2 wt% to 4 wt%. Post-mould cooling fixtures are used on the rim and handle ears to prevent ovality above 1.0 mm. Terminal products include 10 L and 20 L pails for paints, janitorial concentrates, and water-dilutable chemicals. Drop impact at −18°C and stacking load are evaluated to the buyer’s specification; chemical compatibility is screened by ISO 175:2010 for the specific formulation. Under severe outdoor UV, an additional hindered amine light stabiliser concentrate is used at 1 wt%, but hygroscopic carriers must be avoided to prevent splay. The melt is not held above 250°C because the resulting molecular weight reduction degrades ESCR and pail sidewall impact strength. Published data for KL350A-specific pail drop performance at sub-zero temperatures is limited; processors shall generate their own data at the design wall thickness and handle geometry.
Multi-cavity houseware and diagnostic packaging tools represent a precision injection segment where KL350A must fill long flow paths without flash on micro-textured surfaces. Barrel temperatures are profiled from 190°C at the feed throat to 230°C at the nozzle, and the mould temperature is controlled between 15°C and 35°C depending on surface gloss specification. For diagnostic packaging trays, the mould is run at the upper end of this range to improve replication of 0.2 mm deep lettering, while peak injection pressure is set at 60 MPa to 90 MPa with screw backpressure of 0.3 MPa to 0.6 MPa. Colour concentrates are added at 1 wt% to 2 wt%, and the use of external mould-release agents is excluded where printing or ultrasonic welding is required downstream. Terminal items include houseware containers, toy components, single-use diagnostic housings, and non-implantable medical packaging trays. Toy safety is evaluated under EN 71-3 for migration of specific elements, while medical packaging validation is performed in accordance with ISO 11135:2014 for ethylene oxide sterilisation or ISO 11137-1 for gamma sterilisation. Published data for KL350A-specific sterilisation compatibility is limited; qualification shall be performed for each package design and sterilisation dose. KL350A is not intended for implantable devices and is restricted to non-implantable packaging and single-use diagnostic housings.
| Downstream process | Referenced standard or clause | Critical control limit or test condition |
|---|---|---|
| Thin-wall food containers | FDA 21 CFR 177.1520; EU 10/2011; ISO 1133-1:2022 | Melt 210°C–240°C; wall 0.5 mm–0.9 mm |
| Caps and closures | ASTM D1693-15 Method B; ISO 11357-6 | Gate land 0.6 mm–0.8 mm; melt ≤250°C |
| Logistics crates and pallets | ASTM D790-17; ISO 179-1:2010; ISO 294-4 | Shrinkage 1.5%–2.5%; regrind ≤20 wt% |
| Industrial pails | ISO 175:2010; ASTM D1693-15 Method B | Wall 1.8 mm–2.5 mm; melt ≤250°C |
| Medical packaging | ISO 11135:2014; ISO 11137-1 | Mould 15°C–35°C; design-specific sterilisation validation |
Competitive TPC (Japan) HDPE KL350A prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
TPC (Japan) HDPE KL350A is a high-molecular-weight high-density polyethylene grade specified in distributor and converter literature for extrusion blow moulding of rigid containers, technical hollow parts, and industrial packaging. The resin is characterised by a representative density of 0.949 g/cm³ determined under ISO 1183-1:2019 and a melt flow rate of 0.35 g/10 min at 190 °C under a 2.16 kg load in accordance with ISO 1133-1:2022. The low melt flow rate relative to general-purpose injection moulding HDPE indicates a high molar mass fraction that contributes to parison hang strength and slow sag during blow moulding. Published data for this specific configuration is limited in open technical literature, and the values cited in this document are representative of distributor-grade data sheets rather than lot-release specifications. Lot-specific certificates of analysis should be obtained from TPC (Japan) before tooling commitment or production qualification.
The property profile in the following table consolidates representative values used for preliminary engineering calculations. Specimen preparation and conditioning follow ISO 293:2004 and ISO 291:2008 at 23 ± 2 °C and 50 ± 5 % relative humidity for 40 h. Blow-moulded walls exhibit flow-induced orientation and anisotropic shrinkage that can shift cold-temperature impact behaviour and tensile elongation relative to compression-moulded plaques.
| Property | Representative value | Test standard |
|---|---|---|
| Density | 0.949 g/cm³ | ISO 1183-1:2019 |
| Melt flow rate, 190 °C, 2.16 kg | 0.35 g/10 min | ISO 1133-1:2022 |
| Tensile yield stress | 21 MPa | ISO 527-2:2012 |
| Tensile elongation at break | 700 % | ISO 527-2:2012 |
| Flexural modulus | 700 MPa | ISO 178:2019 |
| Charpy impact strength, 23 °C | No break | ISO 179-1:2010 |
| Vicat softening temperature, A50 | 116 °C | ISO 306:2022 |
| Brittleness temperature | < -75 °C | ASTM D746-20 |
The flexural modulus of approximately 700 MPa places KL350A in the medium-stiffness HDPE range. Compared with higher-density HDPE grades at 0.955–0.960 g/cm³, the lower density of KL350A reduces flexural stiffness but improves environmental stress crack resistance and low-temperature ductility. Blow-moulded parts should not be designed using tensile properties alone because pinch-off zones and weld lines are often the limiting structural elements.
On industrial extrusion blow moulding equipment, KL350A is typically processed on grooved-barrel or smooth-bore extruders with L/D ratios between 24:1 and 30:1. A barrier screw with low-shear mixing sections is used to suppress local melt-temperature overshoot. Barrel temperature profiles from feed to metering commonly range from 180 °C to 220 °C, with head and die zones maintained between 195 °C and 215 °C. The recommended maximum melt temperature is 220 °C; prolonged exposure above this threshold accelerates chain scission of the high-molar-mass fraction and increases odour-forming volatile output. A processing window of ±5 °C around the die-head set point is reported on shuttle lines to control parison diameter variance and wall-thickness distribution.
Pre-drying is generally unnecessary when storage relative humidity remains below 60 %. When sacks have been exposed to warehouse humidity above 70 % RH, surface moisture can generate micro-voids in thick parisons. Hopper drying at 60 °C for 2 h reduces such surface defects without degrading the stabiliser package. Melt residence time in the accumulator head should be limited to less than 10 min; longer hold times on accumulator-head machines with shot capacities above 10 kg can produce lot-to-lot variability in parison swell and gloss.
At wall thicknesses below 1.5 mm, the high melt viscosity of KL350A increases extrusion backpressure and can cause die lines unless the die gap is opened and parison programming corrects weight distribution. Field data from continuous shuttle blow moulding lines indicate that clamp force settings of 12 t to 20 t are sufficient for containers up to 5 L, while multi-cavity tooling may require 30 t to 50 t when mould temperatures are kept below 15 °C. Mould cooling water between 10 °C and 20 °C reduces cycle time; lower coolant temperatures increase surface haze and promote non-uniform crystallisation in thick rim sections. The high molecular weight of KL350A improves parison hang strength, permitting vertical wall-thickness tolerances of approximately ±0.2 mm on 20 L containers under stable extruder output. Processors report melt fracture when die lip shear stress is raised beyond the point where extruder screw speed produces visible shark-skin defects; published data for KL350A under high-shear die conditions is limited.
End-use conversion of KL350A is concentrated in small-to-medium blow moulded containers, automotive filler necks, industrial packaging, and agricultural chemical bottles where environmental stress crack resistance is an operating requirement. The density of 0.949 g/cm³ balances stiffness and crack resistance. Containers for aggressive surfactants and light hydrocarbon-based formulations are produced with this grade when stress cracking under ASTM D1693-15 Condition A exceeds 150 h. For high-gloss consumer bottles, a lower-viscosity HDPE or HDPE/LDPE blend may be preferred because the higher melt viscosity of KL350A tends to reduce surface gloss unless polished die lips and mould temperatures above 30 °C are maintained.
Replacement of bimodal HDPE with KL350A in aggressive chemical packaging requires comparison of the F50 environmental stress crack resistance at the target wall thickness and failure mode. The grade is frequently specified with ESCR under ASTM D1693-15 Condition B at 50 °C of ≥200 h for 100% Igepal, but plaque preparation and residual stress differences can obscure lot-to-lot comparisons. Bimodal HDPE grades obtain a broad molecular weight distribution with simultaneous high ESCR and high stiffness. KL350A is selected for large-part blow moulding where a density below 0.950 g/cm³ lowers internal stress in thick walls and permits greater deformation before environmental stress cracking initiates. In containers requiring top-load resistance, switching from a 0.955 g/cm³ HDPE to KL350A may reduce top-load capacity at equal wall thickness; part-specific finite element analysis or physical testing under ASTM D2659-16 is required to quantify the loss. Tooling modifications such as thicker corners and reinforced base geometry can recover top-load performance without increasing cycle time disproportionately.
Compared with general-purpose HDPE blow moulding grades with melt flow rates of 0.6–1.0 g/10 min, KL350A offers lower parison sag and higher ESCR but requires higher extruder torque and more precise temperature control. Compared with low-density polyethylene and linear low-density polyethylene, KL350A provides higher stiffness and lower moisture vapour transmission, but reduced clarity and lower elongation before break. The selection of KL350A is therefore justified when rigid chemical packaging or industrial structural parts require a combination of high molecular weight, moderate density, and resistance to stress cracking rather than optical clarity or low-pressure injection moulding flow.
Compliance statements are based on unpigmented natural grades supplied without additives; finished-article responsibility remains with the converter because processing aids, pigments, and adhesives alter the migration profile. The following matrix summarises the usual product-stewardship position for a TPC (Japan) HDPE grade of this type. Downstream users should request written declarations for the specific lot and application.
| Regulatory reference | Scope | Status or condition |
|---|---|---|
| US FDA 21 CFR 177.1520 | Olefin polymers for food contact | Expected to comply for food-contact use, subject to end-use migration testing and extraction limits for the finished article. |
| EU Regulation (EC) No 10/2011 | Plastic materials in contact with food | Requires supplier declaration of specific migration limits; overall migration limit is 10 mg/dm². |
| Japan JHOSPA | Food-contact positive list | Confirm listing in the TPC (Japan) supplier certificate and applicable positive-list classification. |
| REACH Regulation (EC) No 1907/2006 | Substances of very high concern | Not expected to contain SVHC above 0.1 wt% per supplier safety data sheet. |
| RoHS Directive 2011/65/EU | Hazardous substances in electrical and electronic equipment | Not normally relevant to packaging; if the article is integrated into EEE, cadmium, lead, mercury, hexavalent chromium, PBB, and PBDE thresholds of 1000 ppm apply. |
During melt processing, HDPE degradation products include formaldehyde, acetaldehyde, and hydrocarbon vapours. Local exhaust ventilation should maintain airborne total hydrocarbon concentration below 100 mg/m³ as an industrial hygiene benchmark. The resin should not be stored in direct sunlight for extended periods because ultraviolet stabilisation is not sufficient for outdoor service beyond approximately 6 months unless an appropriate carbon black or hindered amine light stabiliser masterbatch is compounded in. For industrial chemical drums, weld-line integrity in the pinch-off zone is controlled by parison pinch temperature and clamp speed; insufficient clamp force below 15 t on 60 L drums creates weak tail flash and potential leakage under UN drop test conditions.