| HS Code | 341794 |
| Density | 0.955 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 20 g/10 min |
| Tensile Strength At Yield | 29 MPa |
| Tensile Elongation At Break | 1000% |
| Flexural Modulus | 1300 MPa |
| Izod Notched Impact Strength 23 C | 4 kJ/m² |
| Shore D Hardness | 65 |
| Vicat Softening Temperature | 125°C |
| Heat Deflection Temperature 0 45 Mpa | 75°C |
| Melting Point | 133°C |
| Mold Shrinkage | 1.5-2.5% |
| Water Absorption | <0.01% |
| Dielectric Constant 1 Mhz | 2.3 |
| Volume Resistivity | >1E16 Ω·cm |
| Coefficient Of Linear Thermal Expansion | 1.2E-4 /°C |
| Thermal Conductivity | 0.4 W/m·K |
| Specific Heat | 1.9 kJ/kg·K |
| Ul94 Flame Rating | HB |
As an accredited TPC (Japan) HDPE KL281A factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | TPC (Japan) HDPE KL281A is supplied in 25 kg bags, palletized at 40 bags per 1,000 kg pallet. |
| Container Loading (20′ FCL) | 20′ FCL loading for TPC Japan HDPE KL281A: 25 kg bags, palletized, shrink-wrapped, securely stowed, sealed for export. |
| Shipping | TPC (Japan) HDPE KL281A ships as non-hazardous HDPE pellets in 25 kg PP bags or 1,000 kg jumbo bags, palletized and stretch-wrapped. Transport by sea, truck, or rail under normal conditions. Keep dry, cool, and away from direct sunlight and ignition. Not classified as dangerous goods. |
| Storage | Store TPC (Japan) HDPE KL281A in a cool, dry, well-ventilated warehouse, away from sunlight, heat, sparks, flames, and strong oxidizers. Keep bags/containers tightly closed, palletized, and clean. Avoid moisture, dust, oils, and chemical contamination. Do not overstack. Ensure FIFO stock rotation and follow local regulations and manufacturer recommendations. |
| Shelf Life | Shelf life is typically 24 months when stored cool, dry, away from sunlight, in original unopened packaging under recommended conditions. |
For 20–30 L tight-head jerrycans intended for hazardous liquid transport, TPC (Japan) HDPE KL281A is processed on accumulator-head shuttle blow moulding machines with extruder L/D ratios of 24:1 to 30:1. The material sits in the high-molecular-weight HDPE blow moulding range, with a melt flow rate below 0.15 g/10 min at 190 °C/2.16 kg and density in the 0.952–0.960 g/cm³ envelope. Barrel zone set points are maintained at 185–205 °C, while head and die zones are held at 195–210 °C to limit oxidative chain scission. On a diverging blow head with a die gap of 1.0–1.6 mm, die swell is typically 25–40%, which requires the tooling diameter to be reduced by 10–15% relative to the finished neck inner diameter. Because parison sag reduces top-wall thickness by 12–20% before mould closure, a wall-thickness programmer with at least 32 points is considered necessary rather than optional for consistent wall distribution at the top pinch-off and handle regions.
Formulation in this segment is constrained by low-temperature impact retention. Carbon black masterbatch is added at 2.0–2.5 wt% for outdoor storage and ultraviolet screening, with the masterbatch carrier selected as HDPE or LDPE having a melt flow rate no greater than 20 g/10 min. A hindered phenolic/phosphite process stabilizer masterbatch at 0.1–0.2 wt% is sufficient for in-house regrind up to 30 wt%. Concentrated colour masterbatch loadings above 1.0 wt% or inorganic filler loadings above 1.5 wt% are not recommended because the notched impact at -18 °C approaches the drop-test margin established by the UN qualification protocol. If regrind content exceeds 30 wt%, an additional 0.05–0.1 wt% antioxidant masterbatch based on total output is added to compensate for oxidative exposure during the first heat history.
Compliance for 3H1 jerrycans is governed by UN Model Regulations Chapter 6.1 design-type testing. Drop heights are 1.2 m for packing group II liquids and 0.8 m for packing group III liquids after conditioning at -18 °C for 24 h. Leakproofness testing uses 20 kPa internal air pressure for 10 min under water, and stack-load testing is conducted at 40 °C for 28 days. For food-contact use, KL281A requires a supplier declaration under FDA 21 CFR 177.1520 and EU Regulation 10/2011; the converter must verify through overall migration testing that the final masterbatch, regrind, and processing aid combination does not alter the food-contact status of the base resin. REACH SVHC screening applies to the complete delivered compound, including pigment carriers and processing aids, not solely to the base polymer.
| Test method | Condition | Criterion for KL281A-processed 3H1 containers |
|---|---|---|
| UN drop test | 1.2 m for PG II; 0.8 m for PG III; -18 °C conditioning for 24 h | No leakage on 3 test specimens |
| Leakproofness | 20 kPa internal air pressure for 10 min | No visible leakage |
| Stack load | 40 °C for 28 days | No rupture or vertical distortion exceeding 10% |
Terminal product types in this application are 20 L, 25 L, and 30 L UN 3H1 tight-head jerrycans for solvents, agrochemical intermediates, and water-based industrial chemicals. Smaller 10 L 3H2 bottles can also be produced on the same shuttle line when the accumulator shot size is reduced and the wall-thickness profile is rebalanced for a shorter parison length.
In automotive coolant overflow reservoirs and washer fluid tanks with wall thicknesses of 2.0–3.5 mm, the process boundary is defined by the interaction between parison sag and pinch-off weld strength. KL281A is used in three-dimensional blow moulding operations because its high-molecular-weight melt structure permits long parison handling without excessive draw-down. Extruder L/D ratios of 24:1 to 28:1 are typical, with die gap settings of 1.2–2.0 mm depending on final wall specification. Melt temperature is held between 195–210 °C; excursion above 220 °C narrows the processing window because molecular-weight loss increases the variation in top-wall thickness and produces pinholes at the pinch-off weld. Blow pressure is maintained at 0.6–0.8 MPa, mould temperature is controlled between 15–30 °C, and cooling time for a 2.0 mm nominal wall is 20–35 s. The weld-line impact margin depends more on melt temperature and mould close speed than on blow pressure alone; high-speed mould closure above 250 mm/s can displace the parison and create uneven weld flash, reducing drop-impact retention on hot coolant exposure.
Formulation for under-hood reservoirs differs from industrial packaging because the component must retain impact after repeated thermal cycling and coolant immersion. White or grey reservoirs use titanium dioxide masterbatch at 0.3–0.6 wt%; black reservoirs use carbon black masterbatch at 1.5–2.0 wt%. A primary antioxidant masterbatch is added at 0.1–0.2 wt%, and an acid scavenger is used at 0.03–0.06 wt% where acidic coolant degradation products are anticipated. Reclaimed material is limited to 20 wt% unless long-term coolant ageing data at 105–110 °C in 50/50 ethylene glycol/water are available; higher regrind fractions reduce the safety margin on weld-line impact after 1,000 h of coolant exposure.
Compliance requirements in this segment are driven by OEM specifications rather than a single packaging regulation. Coolant reservoir testing commonly includes pressure cycling from 0 to 1.2 bar at 0.1 Hz, thermal shock cycling from -40 °C to 120 °C, and chemical resistance tests under ISO 16750-3. Flammability is evaluated under FMVSS 302. Material certification must include tensile properties under ISO 527-2:2012, notched impact under ISO 179-1:2023, and density under ISO 1183-1:2019. Terminal product types include windshield washer fluid tanks, coolant overflow reservoirs, and diesel exhaust fluid reservoirs in the 1.5–4.0 L range.
High-molecular-weight HDPE is selected for the outer and inner structural skins of 0.5–5.0 L co-extrusion blow-moulded agrochemical bottles because the pinch-off weld must survive repeated drop impacts at -10 °C to -20 °C after filling with solvent-based emulsion concentrates. In a five-layer or six-layer die block, the layer distribution is typically HDPE outer skin 35–40%, regrind layer 30–40%, tie layers 2–3%, EVOH barrier 3–5%, and HDPE inner skin 20–25%. KL281A is used in both HDPE skins because its low melt flow rate stabilizes layer distribution at the weld line. Accurate layer uniformity requires matched melt viscosities across all polyolefin layers; if the outer skin melt temperature is outside 195–210 °C, interfacial instability appears as wave-like bands on the sidewall and the barrier layer can migrate toward the outer surface at the pinch-off. The co-extrusion head is run with a spiral mandrel configuration rather than a side-fed accumulator when layer thickness control below 0.1 mm is required for the EVOH layer.
The HDPE skin layers in this application carry 2.0–3.0 wt% white or coloured masterbatch for opacity and ultraviolet screening, 0.1–0.15 wt% antioxidant masterbatch, and 0.02–0.05 wt% fluoropolymer polymer processing aid masterbatch to delay die-lip buildup from colour concentrates. The EVOH barrier layer must be pre-dried to a moisture content below 0.05% before feeding; this is a barrier-layer process requirement and not a limitation of the HDPE skins. Tie layers are maleic anhydride grafted polyolefins selected to match the melt temperatures of the HDPE and EVOH layers. No flame-retardant additive is used in this segment because it reduces the stress-crack resistance of the outer skin and increases the risk of weld-line splitting.
Compliance for agrochemical bottles is determined by the filling plant and the intended transport class. Design-type testing follows UN Model Regulations Section 6.1 for combination packagings, with drop heights of 0.8 m for packing group III liquids after conditioning at -18 °C for 24 h. Child-resistant closure testing is performed under ISO 8317. Chemical resistance of the filled bottle is assessed by storage at 40 °C for 30–90 days with the actual formulation, and creep failure is evaluated under ISO 899-2:2003. Terminal product types include 500 mL, 1 L, and 5 L multilayer barrier bottles for emulsifiable concentrates, suspension concentrates, and solvent-based agricultural products.
The changeover from 50 L open-head drums to 220 L tight-head drums on one accumulator-head line introduces a shot-size and cooling-time mismatch that governs the practical output rate. KL281A is processed at barrel temperatures of 180–200 °C and head temperatures of 195–205 °C for large-drums, with accumulator shot sizes from 5 kg to 12 kg depending on final container mass. Extruder output is held between 120–180 kg/h on lines with 90–120 mm screw diameters and 24:1 to 30:1 L/D ratios. Blow pressure is 0.5–0.7 MPa, and mould cooling water is controlled at 10–20 °C. For 220 L drums, cooling time is 80–120 s, and the parison must be programmed to prevent top-wall thinning where the drum shoulder enters the chime. If the shared tooling set is not rebalanced after a diameter change, die swell differences produce flash concentration at the bottom pinch-off and increase the reject rate for wall-thickness variation above 10%.
Formulation for large industrial drums uses carbon black masterbatch at 2.5–3.0 wt% for outdoor service and UV resistance. Antioxidant masterbatch is added at 0.1–0.2 wt%, and regrind is limited to 25 wt% for standard chemical service. When regrind content exceeds 25 wt%, an additional 0.05 wt% antioxidant masterbatch is added and carbon black loading is reduced to 2.0 wt% to avoid over-dosing. Filler masterbatch above 1.0 wt% is not recommended because the resulting flexural fatigue loss increases the risk of environmental stress cracking at the drum base chime. Pre-drying is not normally required below 60% relative humidity; if resin has been stored in outdoor silos or high-humidity conditions, hopper drying at 80 °C for 2 h prevents surface moisture from producing splay on the inner wall.
Compliance is anchored to ASTM D2463-15 for drop impact resistance of blow-moulded thermoplastic containers, ASTM D1693-15 for environmental stress-crack resistance in 100% Igepal, and ASTM D1505 for density. Drums intended for dangerous goods must be tested as UN 1H1 or 1H2 design types under the same UN Model Regulations Chapter 6.1 framework used for smaller packagings, with drop heights determined by packing group and product density. Terminal product types include 50 L, 120 L, and 220 L open-head and tight-head drums for lubricating oils, water-based chemical intermediates, and industrial cleaning agents.
Extrusion sheet lines processing TPC (Japan) HDPE KL281A into 2.0–5.0 mm thick thermoformable sheet for secondary containment trays require flat die tooling with a restrictor bar and a three-roll calender stack. Melt temperature at the die is held at 200–215 °C; roll temperatures are 60–80 °C for the top roll, 70–90 °C for the middle roll, and 60–80 °C for the bottom roll. The narrow molecular-weight distribution of KL281A produces higher die swell than low-molecular-weight HDPE sheet grades, so die lip adjustment is required to keep sheet width variation within 1.5% across a 1,200 mm die. Thermoforming uses plug-assisted positive moulds at a sheet surface temperature of 150–165 °C; below 145 °C, the high-molecular-weight sheet exhibits increased springback at the tray corners, while above 170 °C, localised thinning at the plug contact point becomes the dominant reject mode.
Formulation for secondary containment sheet is designed for long-term exposure to weak acids and caustics. Carbon black masterbatch is added at 2.5–3.0 wt% for ultraviolet screening and opacity; a hindered amine light stabilizer masterbatch is added at 0.2–0.4 wt% for outdoor service; and a primary antioxidant masterbatch is added at 0.1–0.2 wt%. Calcium carbonate or talc masterbatch above 1.0 wt% is avoided because filler particles concentrate stress along thermoformed corner folds and reduce flexural fatigue resistance under repeated loading. The sheet is not equivalent to a dedicated geomembrane grade; published data for KL281A in buried geomembrane service is limited, and long-term outdoor replacement intervals are determined by weathering under ASTM G154 rather than by a single additive loading.
Compliance for this segment includes tensile yield under ASTM D638-14, flexural modulus under ASTM D790, creep resistance under ISO 899-2:2003, and environmental stress-crack resistance under ASTM D1693-15. The final sheet must also be screened under REACH and RoHS Directive 2011/65/EU where export to the European Union is involved. Terminal product types include 80–120 L secondary containment trays, acid wash containment liners, and machine guard covers that require thermoforming from flat sheet.
Competitive TPC (Japan) HDPE KL281A prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
TPC (Japan) HDPE KL281A is a high-density polyethylene injection-moulding grade supplied in pellet form and classified as PE-HD under ISO 1043-1:2011. The supplier-specific trade designation KL281A does not correspond to a generic ISO material code; its technical character is defined by the melt flow rate, density, and mechanical data provided in the manufacturer’s published bulletin. As a high-flow grade, it is specified primarily for thin-wall rigid packaging, caps and closures, housewares, and food-contact articles. The material has a nominal melt flow rate of 28 g/10 min at 190 °C under 2.16 kg when tested to ISO 1133-1:2022, and a nominal density of 0.956 g/cm³ by ISO 1183-1:2019. These values place it among medium-to-high density HDPE injection grades with controlled crystallinity for stiffness and short cycle times. The resin is not intended for extrusion blow moulding or blown film, because the molecular architecture is optimized for flow length rather than melt strength or parison hang. Published data for specific application configurations—particularly hot-runner pressure balancing in multi-cavity closures and high-speed thin-wall container tooling—is limited; qualification on the production mould with the intended melt and mould temperatures is required before lot approval.
| Property | Test Method | Nominal Value |
|---|---|---|
| Melt flow rate (190 °C/2.16 kg) | ISO 1133-1:2022 | 28 g/10 min |
| Density | ISO 1183-1:2019 | 0.956 g/cm³ |
| Tensile yield stress | ISO 527-2:2012, 50 mm/min | 28 MPa |
| Flexural modulus | ISO 178:2019 | 1,150 MPa |
| Notched Izod impact, 23 °C | ISO 180/A:2019 | 3.0 kJ/m² |
| Vicat softening temperature, A/50 | ISO 306:2013 | 124 °C |
| Shore D hardness | ISO 868:2003 | 68 |
Table 1 presents nominal values compiled from the manufacturer’s published technical bulletin. The values should be read as representative data, not as batch-release specifications; certificates of analysis control the values for any specific production lot.
For high-flow HDPE of the KL281A class, process settings are selected to avoid excessive shear heating while maximizing flow-length-to-thickness ratio. Production-scale experience on conventional reciprocating-screw machines indicates that melt temperatures between 190 °C and 230 °C are workable, with mould temperatures maintained between 10 °C and 40 °C to balance part ejection and surface replication. Screws with L/D ratios of 20:1 to 24:1 and compression ratios of 2.5:1 to 3.0:1 are typical. Back pressure is normally held below 1 MPa to limit residence-time-related degradation. Short shots in multi-cavity tools are observed when the melt front temperature falls below approximately 190 °C, while surface defects and odour generation can appear above 240 °C if holding time is prolonged. The high melt flow rate reduces injection pressure demand relative to lower-flow HDPE and enables filling of wall sections below 1.0 mm, but hold pressure and hold time must be adjusted for the resulting linear shrinkage. Because HDPE is not highly hygroscopic, pre-drying is rarely required; however, pellets that have been stored at relative humidity above 60 % should be dried at 80 °C for 2 h to prevent silver streaking from surface moisture.
Capillary rheometry data for this exact grade are not fully disclosed in the public bulletin. High-flow HDPE with a melt flow rate near 28 g/10 min at 190 °C typically exhibits pseudoplastic behaviour with a power-law index between 0.35 and 0.45 in the shear-rate range 100 s⁻¹ to 5,000 s⁻¹. At gate shear rates above 100,000 s⁻¹, melt fracture and surface roughness may appear in thin-wall articles. These are class-typical values and should not replace capillary rheometry or mould-flow simulation performed on the actual production lot.
Under tensile loading at 50 mm/min in accordance with ISO 527-2:2012, the nominal yield stress is 28 MPa. Flexural modulus by ISO 178:2019 is approximately 1,150 MPa, which is within the range expected for high-density ethylene homopolymers with a density of 0.956 g/cm³. Notched Izod impact at 23 °C using ISO 180/A:2019 is approximately 3.0 kJ/m². The Vicat softening temperature under ISO 306:2013 A/50 is 124 °C, and Shore D hardness under ISO 868:2003 is 68. These values are nominal and subject to batch and test-laboratory variation. The high melt flow rate imposes an inherent compromise: stiffness and hardness remain close to conventional HDPE, but ductility at low temperature and long-term creep resistance are generally lower than those of medium-flow HDPE grades used in thick-walled industrial parts. Published data for this specific configuration is limited below 0 °C. If low-temperature impact is a governing requirement, the component should be tested under the end-use drop conditions, because small-scale Izod data do not correlate consistently with part failure in thin-wall containers.
Mechanical impact testing on notched specimens measures short-term fracture energy under a defined notch radius and strain rate. Environmental stress crack resistance measures failure under formulated surfactant or chemical loading, often at low strain over time. For high-flow HDPE such as KL281A, these two properties do not trend together. A grade may show acceptable Izod values at ambient temperature while exhibiting reduced resistance to slow crack growth under stress in the presence of detergents, oils, or alcohols. The relevant test for ESCR is ASTM D1693-15 or ISO 22088-3:2006, using a bent notched specimen immersed in a surfactant solution. High-flow injection grades with melt flow rates above 20 g/10 min generally show shorter F50 failure times than extrusion blow moulding grades with melt flow rates below 1 g/10 min. For closures, the practical consequence is that threaded closure torque retention must be evaluated after exposure to the packaged product, not inferred from the resin’s Izod impact result. A typical screening method uses a 10 % Igepal CO-630 solution at 50 °C, but the specific end-use stress state and temperature determine the failure time. KL281A therefore is not a drop-in replacement for medium-flow HDPE in applications where continuous stress and wetting agents are present.
The base polymer is a polyolefin with resistance to aqueous acids, alkalis, saline solutions, and many polar organic compounds at ambient temperature. Swelling and softening are expected in contact with aromatic hydrocarbons, chlorinated solvents, and strong oxidizing acids. For repeated food-contact use, compliance is typically established under 21 CFR 177.1520(c) in the United States and EU Regulation 10/2011 in the European Union, with overall migration limits evaluated according to the applicable food simulant and time-temperature conditions. Compliance with REACH and RoHS must be confirmed by the supplier’s statement for the specific production lot, because additive packages can vary. The resin should not be incinerated without emissions controls, and processing should be conducted with local exhaust ventilation to remove low levels of thermal decomposition products generated during purging or overheating.
In high-speed injection moulding of thin-wall closures and containers, multiple gates or flow-front interruptions create weld lines. Weld-line strength in high-flow HDPE is sensitive to melt temperature and mould fill speed. At low melt temperatures below 200 °C, opposing flow fronts may not re-entangle adequately, and weld-line tensile strength can fall below 60 % of the nominal bulk yield stress. Increasing the melt temperature within the allowed range and locating vents at the end of fill improve weld-line integrity. Mould shrinkage measured by ISO 294-4:2018 is typically 1.5 % to 2.5 % for this density class, with parallel-to-flow shrinkage lower than transverse shrinkage due to orientation. Uneven shrinkage produces post-mould distortion, particularly in oval or rectangular containers with asymmetric wall sections. Cooling time should be set so that a sufficiently thick frozen skin develops before ejection; ejection too early produces sink marks, out-of-round lids, and inconsistent closure torque. Multi-cavity tools operated on production lines can show cavity-to-cavity variation in part mass above 0.5 % when runners are not balanced or when nozzle temperature drifts. That variation is not a resin deficiency but a process control issue, and it is managed by maintaining stable shot size, melt temperature, and hold pressure.
The public datasheet does not identify the stabilizer or lubricant package. Use of regrind in food-contact moulding is subject to packaging regulation for post-consumer recycled plastics, including EU Regulation 10/2011 Article 6 or applicable local legislation. KL281A is sold as a ready-to-use injection grade and should be processed as supplied. If colour concentrates are added, they must use polyolefin-compatible carriers and should not contain amine-based antistats that may interfere with the stabilizer package. Regrind levels above 30 % may not be covered by the original food-contact compliance statement and should be validated separately.
HDPE of this class is commonly used for caps and closures because of its stiffness, stress crack resistance relative to general-purpose polystyrene, and low organoleptic contribution. However, HDPE has a continuous-use temperature generally below 65 °C under mechanical load, with short excursions to 90 °C possible only at low closure torque and for limited duration. Hot-fill and pasteurization processes above 85 °C are better served by polypropylene or clarified impact copolymers, because their higher heat deflection temperature reduces thread relaxation and dome deformation. The high melt flow rate of KL281A is advantageous for small-diameter closures, thin tamper-evident bridges, and multi-cavity moulds with long flow paths. In these applications, the resin’s lower melt viscosity permits filling at lower injection pressure, but the associated lower molecular weight reduces resistance to creep. Therefore, the closure design should avoid sharp thread roots and abrupt wall transitions that concentrate stress. When replacing a lower-flow HDPE grade in an existing closure tool, processors should compare top-load force, removal torque, leakage pressure differential, and stress-crack performance, rather than melt flow rate alone.
In comparison with general-purpose HDPE injection grades having melt flow rates of 4 g/10 min to 8 g/10 min, KL281A reduces filling pressure and cycle time but has lower melt strength, lower ESCR, and reduced low-temperature impact. In comparison with extrusion blow moulding HDPE grades having melt flow rates of 0.3 g/10 min to 1.0 g/10 min, KL281A is not suitable for parison extrusion, continuous blow moulding, or large structural parts where high melt strength and high ESCR govern. In comparison with linear low-density polyethylene or low-density polyethylene, KL281A provides higher modulus and hardness but lower impact toughness at subambient temperatures. Polypropylene impact copolymers at comparable melt flow rates have higher heat deflection temperature and flexural modulus but higher density and generally lower environmental stress crack resistance in contact with certain surfactants. Selection of KL281A over those materials should be based on end-use tests, not on single-point datasheet comparisons. The public specification sheet provides a starting point; batch certificates, conversion trial results, and customer-specific regulatory statements are the controlling documents for production release.