| HS Code | 974188 |
| Density | 0.954 g/cm³ |
| Melt Flow Rate 190 C 2 16 Kg | 0.20 g/10 min |
| Tensile Strength At Yield | 27 MPa |
| Tensile Elongation At Break | 800% |
| Flexural Modulus | 1.10 GPa |
| Notched Izod Impact Strength | 0.15 J/cm |
| Vicat Softening Point | 126°C |
| Heat Deflection Temperature 0 46 Mpa | 75°C |
| Shore D Hardness | 65 |
| Environmental Stress Cracking Resistance | >1000 h |
| Brittleness Temperature | < -70°C |
| Melting Point | 134°C |
As an accredited TPC (Japan) HDPE KL272C factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | TPC (Japan) HDPE KL272C is supplied in 25 kg polyethylene-lined paper bags, palletized at 1,000 kg per pallet. |
| Container Loading (20′ FCL) | Container Loading (20′ FCL): TPC (Japan) HDPE KL272C high-density polyethylene resin, 25 kg bags, palletized and securely loaded for ocean freight. |
| Shipping | TPC (Japan) HDPE KL272C is a non-hazardous high-density polyethylene resin. It is typically shipped in 25 kg bags or bulk containers, palletized and stretch-wrapped. Not regulated as dangerous goods for transport. Store in a cool, dry, well-ventilated area away from direct sunlight and ignition sources. |
| Storage | Store TPC (Japan) HDPE KL272C indoors in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep original containers closed, labeled, and palletized; prevent moisture, dust, and contamination. Avoid excessive stacking, prolonged UV exposure, and incompatible materials. Use appropriate containment for spills. Follow supplier SDS and local regulations. |
| Shelf Life | Shelf life: typically 24 months when stored in original packaging under cool, dry, ventilated conditions, away from direct sunlight and moisture. |
Returnable beverage crates and logistics trays molded from TPC Japan HDPE KL272C place simultaneous demands on melt flow length, crush resistance, and post-industrial regrind tolerance. Before tool transfer, the lot-specific melt flow rate is confirmed by ISO 1133-1:2022 at 190 °C under 2.16 kg; this value controls the pack/hold window in deep-ribbed tools. On a reciprocating-screw machine with screw diameter between 50 mm and 60 mm, the barrel profile is set from 180 °C in the feed zone to 220 °C at the metering zone, with the nozzle held at 210 °C. Mold temperature is controlled between 15 °C and 30 °C by turbulent water channels; a flow velocity above 2.5 m/s in baffle-drilled water lines reduces warpage in the base grid without embrittling the sidewall ribs. Packing pressure is maintained at 55–75 MPa until shot-weight stability of ±0.4% indicates frozen gates. Stacking verification follows ISO 12048; however, published data generated on KL272C crate prototypes remain limited, and initial tool trials should be designed to verify top-load retention at 40 °C for 28 days against the purchaser’s maximum gross load. Post-industrial regrind from sprues and rejected crates can be incorporated at 15–30 wt% only after regrind melt flow rate and sieve size distribution are re-certified, because shifts in molecular mass distribution may reduce environmental stress-cracking resistance at rib intersections.
In multi-cavity closure tools running KL272C, the maximum cavity count is not determined by plastication alone; gate aesthetics and thread ovality are controlled by core temperature, gate diameter, and demolding torque. Core cooling water entering at 10–15 °C with turbulent flow is used to set cap threads before ejection; if the core surface exceeds 20 °C at the moment of unscrewing, thread crest deformation can reduce sealing torque retention. Gate diameter at the external cap face is normally held between 0.8 mm and 1.2 mm. Smaller gates generate excessive shear heating and local melt fracture, visible as gate blush; larger gates may produce stringing and require longer hold to prevent sink marks opposite the gate pad. Torque retention is measured according to ASTM D2063 and compared with the closure brand owner’s specification after conditioning at 23 °C and 50% RH. For linerless cap sealing beads, a short-shot study at 95–98% fill confirms bead formation without overpacking the outer thread. If demolding torque on unscrewing cores exceeds available ejection capacity, a PE-carrier erucamide masterbatch may be used at 500–1,200 ppm active amide, but migration limits under EU 10/2011 must be re-evaluated for fat-containing food contact. Environmental stress-cracking resistance of the cap in detergent-based bottling line lubricants is assessed by ASTM D1693 condition A in 100% Igepal at 50 °C, though the result is a comparative indication rather than a direct prediction of failure on a carbonated beverage line.
Cold-fill dairy spread and food service containers can be injection molded from KL272C when the complete formulation is qualified under FDA 21 CFR 177.1520 and EU 10/2011. The food-contact status is not provided by the base resin alone; the selected color masterbatch, processing lubricant, and any regrind stream must be declared and migration-tested for the intended food simulant. For container walls between 0.8 mm and 1.2 mm, melt temperature is maintained between 200 °C and 230 °C, while injection velocity above 100 mm/s is normally required to fill the rim before freeze-off. Venting depth along the parting line is limited to 0.02–0.03 mm; deeper vents flash the sealing edge and shallower vents produce gas burns at the base of the container. Shrinkage is evaluated by molding plaques per ISO 294-4 using the standard test specimen geometry, then corrected for cavity thickness because production walls are thinner than the standard plaque. Anisotropic shrinkage between flow and cross-flow directions must be corrected in the rim and base gussets. If the tool uses hot-runner valve gates, the valve-pin delay is set to avoid weld-line displacement at the base, but published data for this specific configuration in KL272C food containers is limited and should be verified with short-shot series on the production tool.
Open-top industrial pails molded from KL272C are used for paints, water-based emulsions, and non-hazardous liquid products; when stacking loads exceed 200 kg, sidewall buckling and lid deflection become non-linear responses that cannot be extrapolated from standard tensile data. For a 20 L pail with a nominal wall thickness of 1.1–1.4 mm, static stack testing is frequently performed at 40 °C for 28 days with the closure in place, following the principles of ISO 12048 for filled transport packages. If the pail is intended for regulated dangerous goods, the package must undergo leakproofness, drop, and stack testing under ASTM D4919 or the applicable UN qualification protocol for plastics containers; a favorable result on one cavity geometry does not transfer automatically to another, and tool-specific verification is required. Handle lugs and lid retention beads should maintain a minimum radius of 0.5 mm to reduce notch stress concentration during cold drop at -18 °C. During molding, injection pressures above 80 MPa on large-diameter pails tend to introduce flow-induced molecular orientation that increases hoop strength but lowers sidewall dart impact after aging. Since published KL272C-specific data for UN-certified pails is limited, each new tool should be qualified with production-scale samples and not with laboratory-scale plaques alone.
| Application scenario | Key verification | Standard code | Test condition |
|---|---|---|---|
| Crates and logistics trays | Top-load and stack stability | ISO 12048 | 23 °C / 50% RH |
| Closures | Torque retention | ASTM D2063 | controlled application and removal |
| Food containers | Total migration | EU 10/2011 | simulant selection by food type |
| Industrial pails | Hazardous goods stack | ASTM D4919 | 40 °C, 28 days |
| Automotive washer reservoirs | Charpy notched impact | ISO 179-1/1eA | -30 °C |
| Thin-wall containers | Molding shrinkage | ISO 294-4 | standard plaque geometry |
Injection molded washer reservoir halves produced from KL272C are joined by hot-plate or vibration welding, making the weld line and the filler neck the controlling sites for low-temperature failure. Methanol-containing washer fluids at 30–50 vol% can act as environmental stress-cracking agents; relative ESCR screening is performed by ASTM D1693 condition A in 100% Igepal at 50 °C, but direct exposure testing in the actual fluid composition at 60 °C is required because the failure mechanism is fluid-specific. Notched Charpy impact on specimens cut across the weld line is measured according to ISO 179-1/1eA at -30 °C; unnotched drop impact of the complete reservoir assembly can be evaluated by ISO 6603-2 at the same temperature after conditioning. The molding process must avoid overpacking the gate area, because high residual stress at the injection gate lowers environmental stress-cracking resistance when the reservoir is exposed to repeated thermal cycling from -30 °C to 80 °C. Ultrasonic inspection of the weld zone is used to confirm bond continuity before fluid-fill testing at 1.5 bar internal pressure. Published data on KL272C welded reservoir shells is limited; seam strength should be established on production-welded parts rather than on injection molded plaques alone.
When KL272C is used for thin-wall containers with wall sections below 0.6 mm, short fills and flow marks are frequently misattributed to low melt temperature. High injection velocity, adequate venting, and machine hydraulic response determine flow length more than a 10–15 °C barrel adjustment. Injection speed at the screw is commonly set above 120 mm/s for thin-wall molds, with peak melt pressure at the machine nozzle typically in the range of 80–120 MPa. Venting depth along the flow path must remain between 0.015 mm and 0.025 mm; if venting is insufficient, gas compression at the end of fill generates burned regions even when melt temperature is raised. Residence time should be limited below 6 minutes at 230 °C, because prolonged exposure initiates thermo-oxidative chain scission that increases melt flow rate while reducing environmental stress-cracking resistance. Mold temperature in the 15–25 °C range is used for dimensional stability, but lower temperatures reduce gloss and may require higher injection pressure. Tool trials should use cavity pressure sensors to determine gate freeze rather than relying on timer-based hold; KL272C-specific published data in sub-0.6 mm flow channels is limited, so short-shot progression and gate-seal studies on the actual tool are mandatory.
Competitive TPC (Japan) HDPE KL272C prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
TPC (Japan) HDPE KL272C is introduced as a high-density polyethylene copolymer grade engineered for extrusion blow molding of hollow technical parts, chemical containers, and industrial packaging. The grade is positioned within a medium-molecular-weight HDPE class in which melt strength, parison stability, and environmental stress crack resistance are balanced for continuous shuttle, wheel, or accumulator-head processing. Incoming resin acceptance is controlled through the supplier certificate of analysis using ISO 1183-1 for density, ISO 1133-1:2022 for melt mass-flow rate at 190 °C/2.16 kg, and ISO 527-2 for tensile yield and elongation. Published third-party data for this specific KL272C configuration is limited; therefore batch-specific numerical values should be taken from the TPC Japan CoA rather than reproduced from secondary databases.
For incoming-material control, the laboratory records lot number, shipment date, melt-flow value, density, and any visible contamination before silo transfer. Melt-flow repeatability is a primary process-control variable because shifts in viscosity alter parison drawdown, top-load distribution, and pinch-off weld integrity. A retained sample from each lot should be stored in sealed double polyethylene bags under warehouse conditions below 35 °C for at least 12 months for dispute resolution and rheological recheck.
Before the first production run, the processor verifies that the feed throat, hopper magnet, screen pack, and die head are free of incompatible polymer residues. HDPE is not inherently hygroscopic, but surface moisture from damaged packaging or high-humidity storage can produce melt surging, die lines, and surface roughness. A dry-air hopper dryer with a dew point below -20 °C is applied only when packaging integrity has been compromised; otherwise closed sealed feed is maintained.
Extrusion blow molding of KL272C is typically initiated at a melt temperature of 195–210 °C measured by an immersion probe at the adapter. Barrel zone settings for a 60 mm single-screw barrier extruder with a 25:1 L/D commonly begin at 170–180 °C in the feed zone, 185–195 °C in the compression zone, 195–205 °C in the metering zone, and 200–210 °C at the adapter and die head. These are class-typical starting points for the viscosity band, not a substitute for the grade-specific processing sheet. Melt temperature above 220 °C increases the risk of oxidation, odor, gel formation, and loss of parison gloss; melt temperature below 180 °C can produce unmelted resin particles, elevated head pressure, parison curl, and inconsistent wall thickness.
Die gap is normally set between 1.2 mm and 2.5 mm depending on container weight and tooling diameter. Blow-up ratio is maintained between 2.0:1 and 3.2:1 to prevent localized thinning at the mold parting line. Mold temperature is controlled between 10 °C and 25 °C with closed-loop chilling to stabilize cycle time and minimize shrink variation. Insufficient mold cooling can shift the inner surface skin quench rate, producing warpage and reduced top-load retention in large containers.
Parison length control should be servo-valve controlled on continuous extrusion machines. Variations in extruder screw speed above ±2% or melt-pressure fluctuation above 0.5 MPa are often traced to feed-bridge instability, worn screw flights, or intermittent hopper discharge. On a 60 mm barrier screw, normal head pressure is held in the range of 25–35 MPa; a rising trend above 40 MPa without a corresponding increase in screw speed indicates screen-pack plugging or insufficient melt temperature in the feed zone.
KL272C is characterized as a copolymer-stabilized HDPE rather than a high-flow injection-molding homopolymer. The copolymer designation is relevant to stress-crack performance: the introduction of short-chain branching during polymerization disrupts lamellar packing enough to improve slow crack growth resistance while retaining higher density and modulus than conventional LLDPE. For the medium-molecular-weight HDPE class corresponding to this viscosity band, density is generally found in the range of 0.950–0.957 g/cm³ and melt mass-flow rate between 0.25 g/10 min and 0.50 g/10 min at 190 °C/2.16 kg. These are class-typical recognition windows, not certified product limits.
A melt-flow value below injection-grade HDPE is intentional. In blow molding, lower MFR resins provide higher parison hang strength, reduced sag under gravitational load, and improved pinch-off weld formation. The penalty is higher extruder torque and reduced flow into thin-wall injection features, which is why KL272C is not specified for thin-wall injection molding or for tools requiring long flow lengths through gates below 1.0 mm. Conversely, a higher-MFR blow molding grade would fill complex tooling more readily but would exhibit greater parison sag and less uniform wall distribution on deep-draw containers.
| Characteristic | Test method | Unit | Class-typical acceptance window |
|---|---|---|---|
| Melt mass-flow rate | ISO 1133-1:2022 | g/10 min | 0.25–0.50 |
| Density | ISO 1183-1:2019 | g/cm³ | 0.950–0.957 |
| Tensile yield stress | ISO 527-2:2012 | MPa | 22–28 |
| Tensile elongation at break | ISO 527-2:2012 | % | >600 |
| Flexural modulus | ISO 178:2019 | MPa | 850–1050 |
| Charpy notched impact strength at -30 °C | ISO 179-1:2010 | kJ/m² | 6–12 |
| Vicat softening temperature | ISO 306:2022 | °C | 122–128 |
| Environmental stress crack resistance | ASTM D1693-15 | h | >50 |
The above ranges serve only as a quality-control reference for the resin family. Certified grade-specific limits are supplied by TPC Japan with each lot and take precedence over any third-party table. Any lot falling outside the CoA limits should not be blended into production without a written disposition review because a density shift of 0.002 g/cm³ can alter container top-load and drop-impact performance by more than laboratory repeatability limits.
Although high-density polyethylene does not rely on moisture removal for polymer breakdown, surface moisture can cause feeding instability and visible surface defects. If bags or octabins have been stored at relative humidity above 60% or exposed to condensed water, the material is pre-dried at 80 °C for 3–4 h in a dehumidified-air dryer with a dew point below -20 °C. Drying beyond 8 h at 80 °C is generally unnecessary and can increase energy use without improving process stability.
Conveying should use low-velocity dense-phase air or vacuum transfer with smooth elbows to minimize fines generation. Fines accumulate in the hopper sidewall and can create feed-channel bridging. A hopper magnet and a screen pack of 20/40/60 mesh are commonly installed before the breaker plate to protect the die gap from hard contamination. Contact with copper-based or amine-based additive concentrates should be avoided unless thermal-stability testing has been completed on the exact masterbatch ratio, because additive interactions can shift oxidative induction time and alter melt-flow response during long runs.
For continuous blow molding, KL272C is processed on single-screw extruders with L/D ratios from 24:1 to 30:1 and a compression ratio between 2.5:1 and 3.5:1. Barrier screws with a separating flight are preferred over conventional three-zone screws because they provide more consistent melt-temperature homogeneity at moderate screw speeds. Feed depth, meter depth, and barrier clearance are selected according to extruder diameter; a poorly matched screw can generate melt-temperature variation above 5 °C, visible as parison thickness bands.
Melt residence time should be kept below 6 min at melt temperatures above 210 °C. Accumulator-head machines can create dead spots near the die bushing and mandrel; those zones require purging with a compatible HDPE purge compound or the same resin at elevated screw speed before the first production container. If the melt-pressure signal displays a repeating sinusoidal pattern, the cause is usually screw-speed oscillation or hopper bridging rather than resin lot variation. Sustained pressure above 40 MPa at normal screw speed indicates screen blockage or an undersized die gap and should be corrected before parison programming is adjusted.
Closed-loop regrind addition is acceptable for non-critical industrial containers at up to 20 wt% when the regrind is dry, dust-free, and generated from clean in-house scrap. Higher regrind ratios can reduce environmental stress crack resistance and shift low-temperature impact because repeated heat history increases the concentration of oxidized chain ends. Regrind from external sources is not recommended without melt-flow and density verification against the virgin lot.
In container production, the primary application targets are blow-molded bottles and canisters from 5 L to 60 L for detergent, agrochemical, automotive fluid, and industrial chemical service. These applications require top-load strength, drop-impact retention after aggressive-liquid contact, and consistent pinch-off weld integrity. For aggressive solvent-based fluids, the HDPE wall alone is not a permanent barrier; a fluorinated surface treatment or a polyamide barrier layer with tie resin is required. Environmental stress crack resistance is evaluated according to ASTM D1693-15, condition B, with the understanding that ESCR is fluid-specific and must be measured in the intended packaged liquid rather than assumed from one test fluid.
Injection-molding HDPE grades typically operate at melt mass-flow rates of 4–20 g/10 min, which allows fast flow through small gates and thin walls. KL272C, with its lower-flow blow-molding architecture, is not interchangeable with those injection grades. If KL272C is accidentally supplied to an injection machine, the expected failure sequence includes short shots, high injection pressure, gate jetting, and screw-recovery delays caused by higher melt viscosity. Conversely, placing an injection-molding HDPE into a blow-molding parison line typically results in severe parison sag, poor hang strength, and wall-thickness variation because the low-melt-strength resin cannot support the parison weight.
For blow-molding tooling, the pinch-off insert must be designed with a sharp land to displace melt and form a reliable weld. A pinch-off land angle that is too blunt can leave a weak inner weld bead. The die-to-pin centering tolerance should be maintained within ±0.05 mm, because eccentricity at this point is amplified in the final parison and produces a spiral wall-thickness pattern. Blow pin length and needle position are set so that pre-blow air pressure begins between 0.2 MPa and 0.5 MPa, followed by full blow air at 0.6–0.9 MPa. These values depend on container size and must be adjusted with a parison programmer.
Mold venting is another difference from injection molding. Blow molding traps air between the expanding parison and the cavity surface; vents of 0.02–0.05 mm depth at the parting line or inserted porous plugs are required to prevent air pockets and poor surface replication. In a textured mold, vent depth below 0.02 mm may be insufficient and can produce surface gloss variation.
Compared with a low-MFR HDPE homopolymer of similar density, KL272C is expected to show improved stress-crack resistance because of its copolymer structure, while retaining higher stiffness than LLDPE. The density band of 0.950–0.957 g/cm³ places it above linear low-density polyethylene, which typically ranges from 0.918–0.930 g/cm³ and exhibits lower flexural modulus. The practical trade-off is that HDPE blow-molded containers have higher top load and chemical resistance, while LLDPE packaging often provides greater low-temperature dart impact and sealability but at lower structural stiffness.
When compared with a high-MFR HDPE injection grade, KL272C provides higher melt strength and better parison hang time. When compared with a broad-molecular-weight HDPE blow-molding grade, a narrow molecular weight distribution in the KL272C class tends to produce lower die swell and better surface finish, but may be less forgiving of small die-gap or melt-temperature changes. This means the control window around melt temperature and die gap is narrower; operators should not extrapolate processing settings from other HDPE blow-molding grades without running a short parison-sag trial.
| Resin class | Typical MFR range | Typical density | Stiffness direction | Primary limitation |
|---|---|---|---|---|
| KL272C blow-molding HDPE copolymer class | 0.25–0.50 g/10 min | 0.950–0.957 g/cm³ | Moderate to high | Not suited for thin-wall injection flow |
| Injection-molding HDPE | 4–20 g/10 min | 0.952–0.965 g/cm³ | High | Low melt strength for parison processes |
| HDPE homopolymer blow-molding grade | 0.3–0.8 g/10 min | 0.955–0.965 g/cm³ | High | Reduced ESCR versus copolymer |
| LLDPE film or rotomolding grade | 0.5–2.0 g/10 min | 0.918–0.930 g/cm³ | Low | Lower modulus and top-load retention |
The differentiation matrix is based on general industrial polyethylene classifications and should be used only as an orientation guide. For KL272C, the controlling comparison should be made with the TPC Japan CoA and the intended container performance requirements rather than a generic resin-class table.
Processing trials on shuttle machines show that wall-thickness uniformity is most sensitive to parison programming when the container height exceeds 250 mm. On a 20 L canister mold, a die gap of 1.8 mm and blow-up ratio of 2.5:1 are class-typical starting conditions, but the parison programmer must compensate for gravitational drawdown between the die exit and mold closing. If parison length is not servo-corrected, bottom-wall thinning can exceed 15% relative to sidewall thickness. Published data for this specific KL272C tooling configuration is limited; therefore the initial run should include a wall-thickness map across at least eight circumferential positions and three vertical levels.
For lot-to-lot transition, the extruder is not emptied unless the previous resin was chemically incompatible. A melt-flow shift of 0.05 g/10 min within the accepted range is enough to require a small parison-length adjustment. The operator records melt temperature, head pressure, screw speed, die gap, blow-up ratio, and pre-blow pressure for each lot so that changes in container weight distribution can be separated from machine drift.
Injection of a barrier layer or use of EVOH in multilayer blow molding requires tie-layer selection based on compatibility with the HDPE outer layer. Without an appropriate tie resin, delamination at the HDPE/EVOH interface can occur during drop impact at -20 °C. The same incompatibility should be considered in post-consumer recycle streams containing EVOH or PA residues.
For containers requiring food-contact compliance, the specific KL272C grade and any color masterbatch must be cleared under the relevant regulation, such as FDA 21 CFR 177.1520 or the applicable REACH and member-state food-contact provisions. Compliance is formulatory and lot-specific; a general HDPE designation does not by itself establish that a finished package is compliant with all migration limits.
Dimensional stability after demolding depends on cooling uniformity. Large flat side panels can exhibit shrinkage variation if mold cooling channels are more than 25 mm from the cavity surface. A cooling-time increase of 2–5 s often reduces warpage more effectively than raising blow pressure because residual heat in the inner wall drives post-mold crystallization. The part should not be stacked until the inner wall temperature is below 45 °C.
When KL272C is used in a high-gloss consumer bottle, the mold surface must be polished to a roughness below 0.1 µm Ra, and the melt temperature should be maintained at the upper end of the range. However, high-gloss grades may show more visible die lines if the die land is worn. A die-lip radius or chrome polishing defect smaller than 0.05 mm can be amplified by parison drawdown and appear as a continuous vertical streak.
The final process boundary is the pinch-off weld at the flash removal zone. A weak weld can be generated by excessive melt temperature, insufficient pinch-off pressure, or a land width below 1.0 mm. For a 20 L container, pinch-off weld strength can be evaluated by sectioning the weld and performing a 23 °C tensile test according to ISO 527-2; the acceptable weld factor is part-specific and should be established during tool qualification rather than fixed as a universal value.