    Specifications
    HS Code 758467
    Density 0.958 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 0.20 g/10 min
    Tensile Strength At Yield 27 MPa
    Tensile Strength At Break 30 MPa
    Elongation At Break 800%
    Flexural Modulus 1200 MPa
    Izod Notched Impact Strength 150 J/m
    Shore D Hardness 65
    Vicat Softening Point 126 °C
    Melting Point 133 °C
    Heat Deflection Temperature 0 45 Mpa 74 °C
    Brittleness Temperature -70 °C
    Mold Shrinkage 2.0%
    Environmental Stress Crack Resistance >1000 h
    Thermal Conductivity 0.40 W/m·K
    Specific Heat Capacity 1.9 kJ/kg·K
    Dielectric Constant 1 Mhz 2.3
    Volume Resistivity 1e16 ohm·cm
    Dielectric Strength 20 kV/mm
    Coefficient Of Linear Thermal Expansion 1.2e-4 /°C

    As an accredited TPC (Japan) HDPE KL260C factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing TPC (Japan) HDPE KL260C is supplied in 25 kg net weight bags, palletized and stretch-wrapped for transport.
    Container Loading (20′ FCL) 20′ FCL container loading of TPC (Japan) HDPE KL260C: palletized 25 kg bags, shrink-wrapped, securely stowed for ocean export.
    Shipping TPC (Japan) HDPE KL260C is a non-hazardous high-density polyethylene resin supplied as solid pellets. It is shipped in 25 kg bags, jumbo bags, or octabins on pallets. Transport as non-dangerous goods; no UN number or hazard class. Keep dry, cool, and protected from sunlight and contamination.
    Storage Store TPC (Japan) HDPE KL260C in a cool, dry, well-ventilated area, away from direct sunlight, heat, and ignition sources. Keep in original, sealed bags or containers on pallets. Avoid moisture, contamination, and damage. Do not stack excessively. Protect from UV radiation. Use first-in, first-out stock rotation. Keep away from strong oxidizers. Handle to minimize dust generation and static buildup.
    Shelf Life Shelf life is typically 24 months when stored in original packaging under cool, dry conditions, away from direct sunlight and moisture.
    Application of TPC (Japan) HDPE KL260C

    Extrusion blow moulding of UN-certified 1H1/1H2 drums and 3H1 jerrycans from HDPE KL260C utilises the grade’s low melt mass-flow rate to maintain parison wall uniformity during accumulator-head discharge of 7–10 kg parisons. The dangerous-goods packaging test matrix is drawn from ADR Chapter 6.1 and IMDG Code Chapter 6.1: drop tests after conditioning at −18 °C, hydraulic pressure holding at 100 kPa for 5 min, leakproofness testing, and stack testing at 40 °C for 28 days; where metric accessories are specified, dimensional conformity to ISO 20848-1:2006 applies for 210 L open-head drums. A production-start formulation consists of 100 parts by weight virgin KL260C, 25 parts clean post-industrial regrind from the same drum line, 2.0–3.0 wt% of a 40% carbon black masterbatch for closed-head drums exposed outdoors, and 0.05–0.10 phr fluoropolymer process aid only when extruder head pressure exceeds 35 MPa on 80 mm/24:1 L/D grooved-barrier screws. Barrel set points are 180/190/200/205/210 °C, accumulator head set point 205 °C, mould coolant 8–12 °C, blow pressure 0.65–0.80 MPa, and cycle time 150–240 s for 220 L closed-head drums; on single-station shuttle machines with clamp force below 250 t, parison programming adjusts die gap from 4.5 mm at the top to 8.0 mm at the pinch area to limit wall-thickness deviation to 0.3 mm. Finished articles include UN 1H2 open-head drums, UN 1H1 closed-head drums from 20 L to 220 L, UN 3H1 jerrycans at 20 L/25 L, and necked-in pails where hot filling does not exceed 60 °C.

    Can KL260C Function as the HDPE Skin Layer in Coextruded Automotive Fuel Tanks?

    The six-layer coextrusion blow moulding of gasoline and diesel fuel tanks positions HDPE KL260C in outer and inner cap layers, where its slope of viscosity over the 0.1–1.0 s⁻¹ shear-rate range supports die-swell stability during programmed parison drop. Compliance for fuel tanks is anchored to ECE R34 for plastic fuel-tank approval and to evaporative emission limits under US EPA 40 CFR Part 86; AdBlue/DEF tanks additionally follow ISO 22241-1:2019 for AUS 32 contact and permeation resistance. At the layer-distribution level, a typical formulation is built as 20–25 wt% virgin KL260C outer layer, 35–40 wt% post-industrial HDPE regrind layer, 2–3 wt% maleic anhydride-grafted tie resin on each side of the barrier, 1.5–2.0 wt% EVOH barrier, and 20–25 wt% virgin KL260C inner layer; omission of the tie resin produces intermittent delamination at the HDPE/EVOH interface after 500 h of diesel immersion. Processing uses six-extruder coextrusion with die temperature 215–230 °C, 60-point parison wall-thickness control, mould coolant 12–18 °C, and a post-mould cooling fixture held for 180 s to reduce flange warpage below 2.0 mm. Final articles are 60–90 L gasoline tanks, 70–120 L diesel tanks, and 20–40 L SCR AdBlue tanks in commercial vehicles; published data for monolayer KL260C fuel tanks is limited, and continuous service above 60 °C with aggressive fuel blends requires additional barrier validation.

    Coextrusion layerFunctionMass fractionPolymer system
    Outer skinImpact and UV carrier20–25 wt%KL260C + 2.0 wt% carbon black masterbatch
    Regrind coreCost reduction and stiffness35–40 wt%Post-industrial HDPE regrind
    Tie layerAdhesion2–3 wt% per sideMaleic anhydride-grafted polyethylene
    BarrierHydrocarbon resistance1.5–2.0 wt%EVOH, 32 mol% ethylene
    Inner skinFuel contact20–25 wt%KL260C

    For 1,000 L intermediate bulk containers, the inner receptacle is produced by extrusion blow moulding of KL260C and then integrated into a galvanised steel or HDPE outer cage. The transport compliance route is ADR Chapter 6.5 and IMDG Code Chapter 6.5 for rigid plastics IBCs; food-contact inner bottles are assessed against FDA 21 CFR 177.1520 for olefin polymers and EU Regulation (EU) No 10/2011 for overall migration. A solvent-resistance formulation contains 100 parts KL260C, 1.0–1.5 wt% UV stabiliser masterbatch for outdoor distribution, and 0.2–0.5 wt% antistatic masterbatch for volatile solvent service; post-consumer recyclate is excluded from the inner layer in food-contact grades. Processing on a 120 mm accumulator-head machine with 30 kg shot capacity uses a barrel profile of 185/195/205/210/210 °C, die gap 4.0–8.0 mm, blow air pressure 0.55–0.75 MPa, and base cooling at 10–15 °C to stabilise the pallet-integration footprint; cycle time ranges from 120 s for 640 L bottles to 180 s for 1,000 L bottles. Output types include 640 L, 820 L, and 1,000 L UN 31H1 inner bottles, conductive bottles for solvent distribution, and food-grade liquid bulk containers where fill temperatures do not exceed 50 °C.

    Twin-Sheet Thermoforming of KL260C Sheet into Heavy-Duty Pallets and Dunnage Trays

    Flat sheet extrusion feeding twin-sheet thermoforming converts KL260C into load-bearing returnable logistics assets through a two-sided fused structure that replaces welded aluminium and wood. Pallet performance is verified against ISO 8611-1:2011 for flat pallet test methods and ASTM D1185 for palletised materials-handling systems; deflection under 1,000 kg racking load is controlled by part mass per sheet and rib depth rather than by surface thickness alone. The sheet formulation uses 70–75 wt% virgin KL260C, 25–30 wt% post-industrial HDPE regrind from the same thermoforming line, 2.0 wt% colour masterbatch, and 0.10–0.15 phr secondary antioxidant to resist multiple heat histories. Sheet extrusion operates at 210–220 °C through a 100 mm single screw and a fixed-lip die, with a three-roll stack at 80–90 °C to maintain sheet gauge of 5.0–8.0 mm; twin-sheet forming then heats the sheet surfaces to 170–180 °C, with plug assist speed at 250 mm/s, vacuum at −0.08 MPa, and twin-sheet fusion pressure at 0.5–0.7 MPa for 70–100 s of cooling. The finished article range covers 1,200 × 1,000 mm and 1,200 × 800 mm pallets with 9 legs, collars for bulk containers, and dunnage trays for automated warehouse retrieval systems; processing above 230 °C causes sheet sag and local thinning beyond 15% of nominal gauge.

    Stationary vertical storage tanks produced by large-shot extrusion blow moulding use KL260C for cylindrical and rectangular vessels installed indoors or outdoors without pressure service. Design and fabrication compliance follows EN 12573-1:2000 for welded static non-pressurised thermoplastic tanks, DVS 2205 calculation procedures for chemical resistance, and NSF/ANSI 61 where potable water contact is specified; published data for KL260C in potable water service is limited, so qualification must include migration testing on the actual finished vessel. A chemical storage formulation contains 100 parts KL260C, 2.0–2.5 wt% of a 50% carbon black masterbatch for outdoor UV resistance, and 0.10–0.20 phr antioxidant package for extended heat ageing; regrind is limited to 20 wt% and is excluded from the inner wall in drinking-water applications. Processing on a 150 mm blow moulding line with 60 kg shot capacity uses a melt temperature of 200–215 °C, die gap 8.0–15.0 mm, blow pressure 0.5–0.7 MPa, and internal surface cooling at 15–20 °C; cycle times for 1,000 L tanks range from 25–35 min, and post-mould dimensional stabilisation requires 24 h before fitting closure flanges. Terminal products include 500–5,000 L closed-top storage tanks, conical-bottom dosing tanks, horizontal acid tanks with integrally moulded lugs, and double-walled containment vessels for bunded installations.

    Free Quote

    Competitive TPC (Japan) HDPE KL260C prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    TPC (Japan) HDPE KL260C is a high-density polyethylene grade positioned for extrusion blow molding of semi-rigid containers, industrial packaging, and technical hollow parts. The designation KL260C identifies the resin within the producer’s high-density polyethylene portfolio; the C suffix should be confirmed against the certificate of analysis because it may denote a stabilizer, release, or copolymer variant rather than a universal additive package. The material is typically converted on accumulator-head or continuous shuttle blow-molding machines where parison hang time, die swell, and pinch-off integrity determine container quality. Published data for this specific configuration is limited; release properties should therefore be obtained from the producer’s certificate of analysis and checked against ISO 1133-1:2022 and ISO 1183-1:2019.

    Specifications for KL260C are best evaluated through melt-flow and density data rather than single-point mechanical values. Class-level HDPE blow-molding resins in the same density and melt-flow category are commonly controlled to a density of 0.955–0.960 g/cm³ by ASTM D1505 or ISO 1183-1:2019 and a melt mass-flow rate of 0.25–0.45 g/10 min at 190 °C/2.16 kg by ISO 1133-1:2022. The high-load melt-flow rate at 21.6 kg may be specified to monitor molecular weight distribution; a broad distribution generally improves parison stability but consumes more extruder torque. Certificates should list density, melt mass-flow rate, tensile yield stress, flexural modulus, and environmental stress crack resistance. If the certificate does not list a value, the missing value should not be filled with data from unrelated HDPE film or injection grades.

    Compliance assessments for food-contact or potable-water applications require producer confirmation. HDPE blow-molding grades can be formulated to meet U.S. FDA 21 CFR 177.1520 and European Commission Regulation (EU) No 10/2011, but KL260C-specific compliance cannot be assumed from the base resin class alone. Similarly, REACH and RoHS compliance should be verified against the supplier safety data sheet. The absence of cadmium, lead, mercury, and hexavalent chromium is typically covered by RoHS Directive 2011/65/EU screening on the finished article, not by the raw resin certificate.

    What Distinguishes KL260C from Injection-Molding and Film-Grade HDPE?

    Unlike injection-molding HDPE grades, which operate at melt mass-flow rates of 4–20 g/10 min under ISO 1133-1:2022, KL260C-class resin is formulated for low-shear melt strength. An injection-molding grade would produce short shots or require excessive injection pressure on thin-wall tools; a blow-molding grade placed in an injection machine with a 20:1 L/D screw often exhibits high backpressure and poor melt recovery. Against film grades, the difference is less extreme but still measurable: film-grade HDPE is typically optimized for bubble stability and thin-gauge drawdown, with narrower molecular weight distribution and lower die swell. KL260C-class resin carries a higher apparent melt viscosity at zero shear and longer relaxation time, which is why it withstands open-parison gravity. In production terms, this appears as 15–35% larger die swell and greater head pressure at the same die temperature.

    The molecular weight distribution of KL260C-class resin should be confirmed by rheometry. Blow-molding HDPE grades are often produced with a high-molecular-weight tail or bimodal distribution to balance stiffness and environmental stress crack resistance. A broad distribution gives shear thinning under extrusion shear rates but high extensional viscosity at parison hang conditions. On a capillary rheometer operating at 190 °C, the shear-thinning index may be derived from apparent viscosities at 10 s-1 and 100 s-1; values below 0.20 for the viscosity ratio are generally undesirable for deep-draw containers. Published data for this specific configuration is limited, so the producer’s technical service group should provide the complex viscosity curve from an oscillatory rheometer before specifying melt pump and gear-pump bypass conditions.

    Capillary rheometry at 190 °C can quantify the shear-thinning behavior further. Apparent viscosity at 100 s-1 is commonly 1,200–2,000 Pa·s for this class, while at 10 s-1 it rises to 5,000–10,000 Pa·s. The ratio of apparent viscosities is a useful lot-to-lot control parameter; a low ratio corresponds to a narrow molecular weight distribution and can cause parison sag. Extensional viscosity is harder to measure, but blow-molding grades usually show strain hardening when the extensional rate exceeds 0.1 s-1. Strain hardening is inferred from parison sag tests: a 2 m parison at 210 °C should hold its length for 10–15 s before visible necking. These values are class-level and should be cross-checked with the producer.

    Accumulator-Head Extrusion Blow Molding: Die Gap, Parison Sag, and Pressure Limits

    On accumulator-head machines with 2–10 kg head capacity and die diameters from 40 mm to 150 mm, the processing window is controlled by melt temperature, die gap, and parison programming. A safe starting band for KL260C-class resin is 185–210 °C at the die exit. Below 175 °C, melt fracture at the die lip can generate sharkskin on the parison surface; above 220 °C, parison sag increases and wall-thickness control deteriorates. Die gap is normally set at 1.4–2.0 times the target wall thickness. Blow-up ratio is limited to 2.0–3.0 for uniform thickness distribution. Hydraulic blow pressure between 0.6 MPa and 0.8 MPa is used for containers up to 20 L, with mold temperature maintained at 10–30 °C to shorten cooling time. Operators should log extruder head pressure at constant screw speed; an unexpected rise above baseline by 10–15% can indicate screen blockage or a change in molecular weight distribution.

    For tall containers exceeding 500 mm, parison programming is required to offset gravity-induced thinning. The die gap profile is typically programmed to allow a thicker section at the top and bottom of the parison and a thinner midsection. A typical 20 L jerry can may start with 3.0 mm at the die exit, reduce to 2.2 mm midsection, and return to 3.2 mm at the pinch-off. Failure to program results in minimum wall thickness below 1.2 mm at the shoulder or base radius, which reduces top-load capacity and environmental stress crack resistance. On shuttle machines with continuous extrusion, pre-blow timing is used instead of or in addition to die-gap profiling. Pre-blow pressure between 0.05 MPa and 0.15 MPa stabilizes the parison and controls diameter before mold closing.

    Table 1 summarizes class-level property data for blow-molding HDPE in the density and melt-flow category represented by KL260C. These values are not a substitute for producer certification but provide an engineering reference for process qualification.

    Property Test Method Class-level Range
    Density ASTM D1505 / ISO 1183-1:2019 0.955–0.960 g/cm³
    Melt mass-flow rate ISO 1133-1:2022, 190 °C/2.16 kg 0.25–0.45 g/10 min
    Tensile strength at yield ISO 527-2:2012 25–30 MPa
    Flexural modulus ISO 178:2019 1,100–1,500 MPa
    Environmental stress crack resistance ASTM D1693-15, 100% Igepal, 50 °C >600 h F50
    Vicat softening temperature ISO 306:2022, A50 123–128 °C
    Brittleness temperature ASTM D746 <-70 °C
    Shore D hardness ISO 868 62–66

    A second comparison clarifies product-positioning differences across HDPE grades. The values in Table 2 are class-level ranges typical of each processing family, not KL260C-specific certificates.

    Parameter KL260C-class blow-molding HDPE Injection-molding HDPE Film-grade HDPE
    Melt mass-flow rate at 190 °C/2.16 kg 0.25–0.45 g/10 min 4–20 g/10 min 0.3–1.0 g/10 min
    Die swell and parison hang High, stable parison hang Low, sag-prone Moderate
    Typical melt temperature 185–210 °C 200–250 °C 190–230 °C
    Environmental stress crack resistance under ASTM D1693-15 >600 h F50 <100 h F50 300–600 h F50
    Typical application 1–30 L containers, industrial parts Caps, crates, thin-wall packaging Bags, liners, shrink film
    Molecular weight distribution Broad or bimodal Narrow-to-medium Controlled for bubble stability

    When the Resin Is Exposed to Stress-Crack-Promoting Fluids and Outdoor Weathering

    Differences from other products are most pronounced under environmental stress crack resistance testing. KL260C-class resin is intended for applications where contact with surfactants, dilute alkalis, or oil-containing fluids is possible. Under ASTM D1693-15, 100% Igepal CO-630 at 50 °C, blow-molding HDPE grades in this category have class-level F50 values above 600 h, whereas a high-stiffness injection-molding HDPE may fail below 100 h. This does not apply to aromatic hydrocarbons, chlorinated solvents, or strong oxidizing acids; published data for this specific configuration is limited in those fluids, and chemical resistance must be validated on the finished container. Outdoor service requires an ultraviolet stabilizer package or carbon black. Unpigmented HDPE without UV stabilization undergoes embrittlement and a progressive loss of tensile elongation, measurable by ASTM D638-14 after 1,000–3,000 h of accelerated QUV exposure.

    Processors should set incoming inspection limits for density and MFR. A density shift of 0.002 g/cm³ can alter container top-load stiffness by more than 5% and may require tooling modifications. MFR variation within 0.05 g/10 min may not be visible in wall thickness but can change parison hang and pinch-off. Regrind addition up to 30 wt% is generally tolerated for non-critical industrial containers when the regrind is dry, free of fines, and uncontaminated. Polypropylene contamination above 2 wt% is a known cause of poor pinch-off fusion; nylon or EVOH barrier scrap should be kept out unless the system is designed for multilayer construction.

    Field data from production-scale accumulator-head lines indicate that pre-blow pressure changes of 0.01 MPa can shift the parison lay-flat width by 2–4%. When wall-thickness distribution drifts, operators often adjust pre-blow rather than melt temperature because increasing melt temperature above 210 °C reduces melt strength and widens the thickness distribution. Extruder barrel zones are typically set with a flat-to-reverse profile: feed zone 170–180 °C, compression zone 185–195 °C, metering zone 190–200 °C, head and die 195–205 °C. Screw cooling is sometimes used with high-shear screws; if the screw cooling is overcooled, the melt temperature fluctuates and parison weight drops. Published data for this specific configuration is limited, so a two-hour production trial with 500 kg is recommended to establish machine-specific process limits before release.

    Quality-control laboratories should compare incoming lots using the producer’s specified method and not substitute ASTM D1238 for ISO 1133-1:2022 without an established correlation. Sample preparation for density measurement should follow ASTM D4703 conditioning; entrained moisture on pellets can bias density by less than 0.001 g/cm³ but should be removed in a vacuum oven at 70–80 °C for 2 h when disputes occur. Orthogonal measurements of melt mass-flow rate and density are insufficient to detect lot-to-lot molecular weight distribution changes; a melt rheology check or gel-permeation chromatography may be required for critical container dimensions.