| HS Code | 418240 |
| Density | 0.960 g/cm³ |
| Melt Flow Rate | 6.0 g/10 min (190°C/2.16 kg) |
| Tensile Strength At Yield | 29 MPa |
| Tensile Elongation At Break | 1000% |
| Flexural Modulus | 1300 MPa |
| Izod Impact Strength Notched | 30 J/m |
| Vicat Softening Temperature | 127°C |
| Heat Deflection Temperature | 75°C |
| Shore D Hardness | 66 |
| Melting Point | 134°C |
| Mold Shrinkage | 1.5-3.0% |
| Water Absorption | <0.01% |
| Volume Resistivity | >10^16 Ω·cm |
| Dielectric Constant | 2.3 |
| Dielectric Strength | 20 kV/mm |
| Coefficient Of Linear Thermal Expansion | 1.2E-4 /°C |
| Thermal Conductivity | 0.4 W/m·K |
| Brittleness Temperature | < -70°C |
As an accredited TPC (Japan) HDPE KL060C factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | TPC (Japan) HDPE KL060C typically packs in 25 kg PE-lined paper bags or 1,000 kg jumbo bags, palletized for transport. |
| Container Loading (20′ FCL) | Container Loading (20′ FCL): TPC (Japan) HDPE KL060C in 25 kg bags, palletized, shrink-wrapped, and secured for ocean transport. |
| Shipping | Shipping description for TPC (Japan) HDPE KL060C: Non-hazardous high-density polyethylene resin pellets. Supplied in 25-kg bags or jumbo bags, palletized. Transport in clean, dry containers at ambient temperature. Protect from moisture, direct sunlight, heat, and contamination. Standard sea freight; keep packaging intact. No special dangerous-goods documentation required. |
| Storage | Store TPC (Japan) HDPE KL060C in a cool, dry, well-ventilated warehouse, preferably in original sealed bags on pallets, away from direct sunlight, heat, flames, and strong oxidizers. Keep containers closed; avoid moisture, dust, and physical damage. Use first-in, first-out stock rotation. Do not store near food, feed, or drinking water. Keep labels intact. Follow the manufacturer’s SDS and local regulations. |
| Shelf Life | TPC (Japan) HDPE KL060C has a recommended shelf life of 24 months when stored cool, dry, and protected from direct sunlight. |
Injection moulding of thin-wall closures from TPC Japan HDPE KL060C is structured around the grade’s melt flow rate of 6.0 g/10 min measured under ISO 1133-1:2022 at 190 °C and 2.16 kg, with a density of 0.960 g/cm³ determined under ISO 1183-1:2019. In a 48-cavity hot-runner closure tool with 0.8 mm nominal wall stock, the melt temperature is maintained between 220 °C and 240 °C; the hot-runner manifold and nozzle tip are held within ±5 °C of the nozzle set point to prevent freeze-off at the gate. A reverse-taper or annular gate opening of at least 0.8 mm is required, because orifice dimensions below this value produce excessive shear and gate blush when the injection velocity exceeds 120 mm/s. Packing pressure is typically set between 60 MPa and 90 MPa for 0.4 s to 0.8 s per mm of wall thickness, and hold pressure is maintained until gate sealing is confirmed by short-shot correlation. Mold coolant inlet temperature is controlled at 10 °C to 25 °C; turbulent flow with Reynolds number above 10,000 is necessary to limit core-to-cavity temperature differential below 3 °C. For tamper-evident caps, the scored band must be ejected below 80 °C because the heat deflection temperature of the grade under 1.8 MPa load per ISO 75-2:2013 is near 70 °C; early ejection without proper mold opening stroke leads to band tearing or ovality. Food-contact status for olefin polymers is anchored to FDA 21 CFR 177.1520(c) items 3.1a and 3.2a, and to EU Regulation (EU) No 10/2011, but grade-specific certification must be verified from the supplier because slip agents and antistatic concentrates used in cap production alter the overall migration profile. Residence time in the barrel should not exceed 5 minutes at processing temperature; extended holding produces discoloration, volatility, and a measurable drop in notched Charpy impact after 10 minutes.
Returnable beverage crates require thick, grid-ribbed walls between 2.8 mm and 4.0 mm and can exceed 1,200 mm in flow length, placing the flow length-to-thickness ratio above 180:1. This geometry forces the melt temperature to the upper boundary of the processing window, 235 °C to 250 °C, while mold temperature is kept between 10 °C and 30 °C. Injection speed is deliberately moderated to 50–100 mm/s; high-speed filling above 130 mm/s introduces polymer degradation at the gate and jetting through the grid, but speeds below 40 mm/s create premature freeze-off in the rib intersections and weak knit lines. Packing pressure between 55 MPa and 70 MPa is applied for 10 s to 15 s, with gate sealing checked by melt flow sensor telemetry on machines equipped with nozzle pressure transducers. The critical mechanical threshold in this segment is cold impact at the grid intersections; purchaser specifications frequently require notched Charpy impact of at least 4 kJ/m² at -20 °C per ISO 179-1:2020, and some logistics pool operators add a full crate drop at -18 °C from 1.5 m. Process conflicts arise because raising mold temperature to 30 °C improves interlayer fusion at knit lines but slows cooling and increases density, whereas lowering mold temperature to 10 °C shortens cycle time but freezes orientation and residual stress into the grid. In production-scale operation, the practical compromise observed on three-platen injection machines of 400–600 tonnes clamp force is a mold temperature of 18 °C to 22 °C and a cooling time of 18 s to 24 s for 3.2 mm nominal wall sections. Gate location is as important as melt temperature: a central sprue into a lattice produces weld lines at every cross bar, while a 6-drop valve-gated cold runner arrangement with light shut-off valves distributes flow into the side rails and reduces the central star-shaped weakness. The crate compound usually contains 2.0 wt% to 4.0 wt% of carbon black or colour masterbatch plus UV stabilizer; if carbon black loading exceeds 2.5 wt%, the aggregate acts as a stress concentrator and can lower low-temperature notched Charpy measured per ISO 179-1:2020 by more than 10 %, which must be compensated by reducing regrind content below 20 wt%.
| Segment | Melt temperature | Mould temperature | Injection speed | Packing pressure | Critical test standard |
|---|---|---|---|---|---|
| Caps and closures | 220–240 °C | 10–25 °C | 120–180 mm/s | 60–90 MPa | ISO 1133-1:2022, ISO 75-2:2013 |
| Returnable crates | 235–250 °C | 10–30 °C | 50–100 mm/s | 55–70 MPa | ISO 179-1:2020 |
| Open-head pails | 230–250 °C | 15–35 °C | 100–180 mm/s | 50–70 MPa | ASTM D642, ISO 2248 |
| Housewares | 225–245 °C | 25–30 °C | 80–150 mm/s | 45–60 MPa | ISO 294-4 |
In 20 L open-head pail production, KL060C is processed at 230 °C to 250 °C melt temperature and 15 °C to 35 °C mold temperature, with wall thickness from 1.6 mm to 2.2 mm and a projected area near 1,200 cm². The required clamp force is derived from peak cavity pressure of 35 MPa to 50 MPa integrated over the projected area, so machines below 450 tonnes are marginal for single-cavity stack moulds, and 600-tonne hydraulic or toggle presses are preferred when flash tolerance is below 0.05 mm at the rim. Injection speed is set at 100 mm/s to 180 mm/s to fill the side wall before the flow front solidifies; slower speeds produce flow lines perpendicular to the rim, while faster speeds above 220 mm/s generate gas traps at the handle bosses and ejection pin baffles. Packing pressure of 50 MPa to 70 MPa is held for 1.5 s/mm to 2.0 s/mm of wall thickness. The sealing ring and stacking shoulder are cut with 1.0° to 2.0° draft; lower draft leads to scuffing on ejection and cracking after stack load. Top-load resistance is measured per ASTM D642 after conditioning at 40 °C for 48 h, and drop impact at -18 °C is tested using the procedure described in ISO 2248 with a water-filled pail conditioned for 16 h. A persistent failure mode on stack moulds is asymmetrical ejection: if the nearest ejector pins to the handle are spaced more than 40 mm from the handle boss edge, the part bows on the moving half and the handle bore becomes oval. Venting at the rim requires groove depth of 0.02 mm to 0.04 mm; deeper vents flash and shallower vents cause burn marks at the last-fill area opposite the gate. For detergent or agrochemical pails, environmental stress cracking resistance must be qualified separately; published data for KL060C in concentrated non-ionic surfactant solutions is limited, so converters running aggressive formulations add a chemical-resistant liner or downgrade the pail wall to a stress factor correction using ISO 22088-3 bent-strip data for the final compound.
Houseware and storage articles moulded from KL060C use colour masterbatch loadings of 2.0 wt% to 4.0 wt% to achieve solid colours in drawers, baskets, trays, and garment boxes. The base resin is compounded on a twin-screw extruder with L/D of 40:1 if a pre-coloured compound is specified, but most processors dry blend masterbatch at the press hopper and rely on a general-purpose three-zone screw with L/D of 20:1 and a mixing tip. When loading exceeds 2.5 wt%, the carrier resin in the masterbatch lowers the compound melt viscosity and can shift the measured MFR upward by 0.2 g/10 min to 0.5 g/10 min depending on carrier base; the screw recovery rate must then be reduced by 10 rpm to 20 rpm to maintain stable shot fill. Some pigments, particularly phthalocyanine blue and carbon black, act as nucleating agents and accelerate crystallization rate, producing earlier gate freeze and higher transverse shrinkage relative to the flow direction. The dimensional consequence is assessed by moulding plaques per ISO 294-4 and measuring shrinkage after 24 h and 48 h; post-mould shrinkage between 48 h and 7 days can reach 0.3 % if the mold is too cold. To maintain stable drawer slides and snap-fits, mold temperature across the cavity must be held within ±3 °C of the set point, and the differential between fixed and moving halves must not exceed 5 °C. A common failure on thin-wall storage containers is a bow along the long side after ejection; this occurs when the moving half runs 5 °C colder than the fixed half and post-mould crystallization continues unevenly. The remedy is not to increase packing pressure alone, because pigment-induced shrinkage anisotropy remains; the processing solution is to set holding pressure at 45 MPa to 60 MPa and increase mold temperature to 25 °C to 30 °C while extending cooling time by 2 s to 4 s. For thick-boss features under a decorative surface, the boss-to-nominal-wall ratio should not exceed 0.7:1; thicker boss attachments act as shrink centres and pull sink marks even when the part is packed to gate freeze.
For UN-certified HDPE pails and industrial closures, KL060C is converted under more severe qualification constraints than standard pail production because the packaging must be tested as a complete unit under UN Model Regulations chapter 6.1 and ADR or IMDG requirements. An injection-moulded 20 L open-head pail designated UN 1H2/Y for packing group II must pass drop cycles at -18 °C from 1.2 m, stack load for 28 days at 40 °C, and leakproofness after top-load deformation. The material’s melt flow rate of 6.0 g/10 min provides the necessary thin-wall fill, but this fluidity also reduces molecular weight and can increase permeability to aliphatic hydrocarbons compared with high-molecular-weight HDPE grades. Converters therefore limit pails for aggressive solvents to single-trip or inner-liner configurations unless the complete package passes absorption–desorption testing at 23 °C for 30 days with the specific filling fluid. The processing window for UN-certified pails is tighter than for cosmetic pails: melt temperature is capped at 245 °C, regrind is limited to 20 wt% of the same compliant compound, and hot-runner temperature is held below 250 °C to avoid oxidative odour that can contaminate filled goods. The screw back pressure is set at 0.5 MPa to 1.0 MPa with decompression of 2 mm to 4 mm to prevent molten drool at the nozzle. The stack rim and lid seat require a gasket groove width and depth tolerance of ±0.10 mm for reliable elastomeric seal compression; if groove depth exceeds the design value by 0.2 mm, the seal fails leakproofness at the closure. Because published data for KL060C under continuous contact with ester-based agrochemical formulations is limited, pre-qualification is limited to standard reference liquids or the actual commercial fill formulation at the intended storage temperature.
Competitive TPC (Japan) HDPE KL060C prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
TPC (Japan) HDPE KL060C is a high-density polyethylene pellet grade for thin-wall injection moulding and small-part extrusion blow moulding. The product designation carries a nominal melt mass-flow rate of 0.60 g/10 min at 190 °C under 2.16 kg load in accordance with ASTM D1238-20 or ISO 1133-1:2022. Nominal density is 0.956 g/cm³ by ISO 1183-1:2019. This places the material in the medium-flow HDPE segment, separating it from high-molecular-weight blow-moulding grades with melt flow rates below 0.35 g/10 min and from high-flow injection-moulding grades above 4.0 g/10 min. The pellet form contains proprietary antioxidant and acid-scavenger additives.
The 0.60 g/10 min flow class permits general-purpose polyolefin screws with L/D ratios between 18:1 and 22:1 and compression ratios of 2.5:1 to 3.0:1. On a 50-ton hydraulic injection moulding machine equipped with a 20:1 L/D screw, a 1.0 mm thin-wall lid is usually filled with barrel zones of 180 °C, 190 °C, 200 °C, and 210 °C, nozzle temperature of 200 °C to 210 °C, and mould temperature of 20 °C to 50 °C. Holding pressure is commonly 30–45 MPa; back pressure should remain between 0.5 MPa and 1.0 MPa. Higher back pressure raises melt temperature by shear heating and can cause yellowing in regrind-containing mixtures. Fill speed is normally set to produce a cavity filling time of 0.5–1.5 s; faster filling can cause jetting in thin sections. Pre-drying is not required if granulate is stored dry, but condensation above 60% relative humidity requires hopper dryer treatment at 80 °C for 2 h. Mould temperatures below 15 °C generate visible flow lines and frozen-in orientation; mould temperatures above 60 °C increase cycle time without a corresponding gain in tensile properties. Capillary rheometry typical of this density class shows shear-thinning with a power-law index near 0.4–0.5 over 100–1,000 s⁻¹; published data for the exact shear-viscosity curve of this specific grade is limited, so fill simulations should use measured lot data.
On shuttle blow-moulding lines, KL060C allows lower accumulator pressure and faster parison drop than a 0.30 g/10 min HDPE. Die temperature is typically 180–200 °C. Above 220 °C parison sag accelerates and surface oxidation may appear as sharkskin at the pinch-off. Wall-thickness programming is required for containers above 500 mL; without it, the lower hang strength creates thin shoulders and thick pinched bottoms. Blow-pin alignment and mould-close speed should be checked because the relaxed melt draws down faster than a high-melt-strength grade. For 250 mL to 1 L bottles, cycle-time reduction of 10–20% is possible when cooling lines are sized for the thinner wall. Pinch-off below 180 °C can produce weak tail flash that fractures during trimming; keeping the pinch-off zone above 185 °C improves weld strength.
At equal screw speed, head pressure generally falls by 10–20%, and melt temperature may increase if barrel temperatures are not lowered by 5–10 °C. A documented production-line failure is neck-ring distortion when mould-open time exceeds the parison hang time; the lower melt viscosity permits sag before mould closure. Compensation involves narrowing the upper die gap and increasing parison extrusion speed by 5–15%. Cycle-time gains depend on mould cooling capacity and blow-pin contact area. The substitution is not recommended for handleware or containers above 5 L because parison draw-down becomes difficult to control. For such large parts a high-melt-strength HDPE of 0.30 g/10 min or lower remains preferable.
| Property | Test method | Typical value |
|---|---|---|
| Melt mass-flow rate, 190 °C/2.16 kg | ISO 1133-1:2022 / ASTM D1238-20 | 0.60 g/10 min |
| Density, 23 °C | ISO 1183-1:2019 | 0.956 g/cm³ |
| Tensile yield stress, 50 mm/min | ISO 527-2:2012 | 28 MPa |
| Tensile elongation at break | ISO 527-2:2012 | >600% |
| Flexural modulus | ISO 178:2019 | 1,200 MPa |
| Charpy notched impact, 23 °C | ISO 179-1:2010 | 5.0 kJ/m² |
| Vicat softening point, A50 | ISO 306:2022 | 125 °C |
| Shore D hardness | ISO 868:2003 | 62 |
These values are not specification limits. Environmental stress crack resistance depends on moulded-in stress, process temperature, and fluid chemistry. A container moulded at low melt temperature with high injection pressure may fail in aggressive detergent solutions even when resin passes ASTM D1693-21 condition B. The grade is not recommended for oxidising acids at temperatures above 40 °C or for aromatic solvents; swelling and stress cracking can occur under sustained load.
Regrind from injection runners and blow-moulded flash can be reintroduced at up to 30 wt% without automatic property verification; higher regrind fractions should be validated by ISO 527-2:2012 tensile testing and ISO 179-1:2010 impact testing. Repeated extrusion reduces oxidation induction time, and melt-flow drift may be observed when regrind is processed at melt temperatures above 230 °C. The stabiliser package in fresh granulate is diluted by recycled material; oxidation induction time at 200 °C measured by ISO 11357-6 may fall by 30–50% in a 30 wt% regrind mixture. Incompatible concentrate carriers, especially EVA- or LDPE-based masterbatches added above 2 wt%, can lower flexural modulus; plaques should be checked to ISO 178:2019 before production. Acid-forming tint concentrates should be avoided because they can destabilise the acid-scavenger balance. Published data for long-term thermal aging of this specific grade is limited; the oxidation induction time for the actual regrind ratio should be requested from the supplier.
Storage should be in dry, UV-protected silos or sealed containers. Pellets exposed to direct sunlight for extended periods may develop surface oxidation that changes odour and colour. The resin is hydrophobic, but cold-to-warm transfer can create surface condensation; if the hopper is loaded with damp pellets, splay appears in injection-moulded parts and bubbles appear in blow-moulded walls. A dehumidified hopper or pellet dryer at 80 °C for 2 h is a corrective measure.
For food-contact packaging, polyethylene in the density range 0.941–0.965 g/cm³ may qualify under FDA 21 CFR 177.1520 when the finished article meets extractable-fraction limits and all additives are permitted. EU Regulation 10/2011 requires overall migration below 10 mg/dm² for general food contact and specific migration limits for additives listed in Annex II. Directive 2011/65/EU as amended by (EU) 2015/863 restricts lead, cadmium, mercury, hexavalent chromium, PBB, PBDE, and four phthalates. KL060C is not sold as a medical or pharmaceutical grade. A supplier compliance statement does not by itself validate a finished container; migration testing with the intended food simulant and fill temperature is required.
Relative to an 8 g/10 min HDPE injection grade, KL060C exhibits higher viscosity at equivalent shear rates. It fills long-flow thin-wall caps more slowly but provides higher notched impact and improved environmental stress crack resistance. Relative to a 0.30 g/10 min blow-moulding grade, KL060C lowers melt pressure and permits lower melt temperature but sacrifices parison hang strength and large-part capacity. The 0.956 g/cm³ density contributes stiffness and top-load strength in cylindrical containers, while the 0.60 g/10 min melt flow class supports small-diameter thread filling without gate flash. In multi-cavity hot-runner systems with gate diameters below 0.6 mm, published data for this specific configuration is limited; tooling trials should be performed because shear heating may reduce the practical processing window.