    Specifications
    HS Code 242751
    Density 0.951 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 0.35 g/10 min
    Melting Point 130 °C
    Vicat Softening Temperature 123 °C
    Heat Deflection Temperature 75 °C
    Tensile Strength At Yield 25 MPa
    Tensile Strength At Break 30 MPa
    Elongation At Break 800%
    Flexural Modulus 1.10 GPa
    Shore D Hardness 62
    Environmental Stress Crack Resistance >1000 h
    Low Temperature Brittleness -70 °C
    Thermal Expansion Coefficient 1.2E-4 /°C
    Thermal Conductivity 0.45 W/m·K
    Specific Heat 1.9 J/g·°C
    Water Absorption 0.01%
    Dielectric Constant 2.3
    Volume Resistivity >1E15 ohm·cm
    Dielectric Strength 20 kV/mm

    As an accredited TPC (Japan) HDPE KK351A factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing TPC (Japan) HDPE KK351A supplied in 25 kg multilayer paper bags, palletized and stretch-wrapped for industrial shipment.
    Container Loading (20′ FCL) Container loading (20′ FCL): TPC (Japan) HDPE KK351A, 25 kg bags, about 18 MT net, palletized for sea transport.
    Shipping TPC (Japan) HDPE KK351A is shipped as non-hazardous polyethylene resin pellets in 25 kg PE bags, jumbo bags, or bulk containers. Store and transport in dry, shaded conditions, away from ignition sources, moisture, and contamination. Keep sealed until use; avoid direct sunlight and excessive heat. No special DG handling required.
    Storage Store TPC (Japan) HDPE KK351A in a cool, dry, well-ventilated area away from direct sunlight, heat, flames, and strong oxidizers. Keep original packaging closed to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and excessive temperatures. Stack pallets securely to prevent deformation. Use first-in, first-out stock rotation. Observe local regulations and the supplier’s safety data sheet.
    Shelf Life Typically 24 months if stored unopened in a cool, dry, ventilated area, away from sunlight, heat, moisture, and contamination.
    Application of TPC (Japan) HDPE KK351A

    On a 200 kN clamp-force shuttle blow moulding line with a 60 mm grooved-feed extruder at L/D 24:1, parison stability for TPC (Japan) HDPE KK351A controls wall-thickness distribution in 750 mL to 5 L detergent, fabric-softener, shampoo, and hand-soap bottles. The material is processed at 185–205°C melt temperature measured at the die entry with an immersion thermocouple, with set temperatures profiled from 170°C at the feed throat to 195°C in the metering zone and 200°C at the head tooling. Falling below 175°C produces visible shark-skin on the parison because the elongational viscosity remains too high, while exceeding 220°C lowers melt strength sufficiently to generate parison sag in four-cavity tools with shot spacing above 200 mm. The die gap is programmed from 1.8 mm to 2.6 mm along the parison stroke through a 100-point parison programmer on an accumulator-head machine; die swell in the 28–42% range is compensated by using a conical diverging die with a land length-to-gap ratio of 8:1. A colour masterbatch based on 40% pigment loading in an LLDPE carrier is metered at 2.0–4.0 wt% by a gravimetric dosing unit at the throat; carrier addition above 4.0 wt% shifts the measured top-load strength on a 750 mL bottle below the 180 N threshold measured at 2 mm/min crosshead speed under ASTM D2659-16.

    Batch-to-batch MFR drift of ±0.03 g/10 min under ISO 1133-1:2022 condition 190°C/2.16 kg shifts the parison sag length in a four-cavity shuttle moulder by 6–8 mm; machine operators compensate by adjusting the parison programming curve rather than raising head temperature, because a 5°C head-temperature correction alters container weight by approximately 0.8%. The terminal bottles are ejected at a mould temperature of 25°C after 12°C coolant circulation through aluminium tooling, then conditioned at 23°C and 50% RH for 40 h before environmental stress-crack testing. Under ASTM D1693-15 condition B at 50°C in 10% Igepal CO-630, the low-MFR HDPE class typically exceeds 100 h to F50 when the pinch-off weld thickness is maintained above 0.70 mm and the shoulder thickness above 0.45 mm, as measured by ultrasonic thickness gauge. Failure below these values correlates with pinhole leakage in drop testing at -18°C from 1.2 m on the closure edge.

    Does USP <661.1> Extractables Testing of Virgin KK351A Remain Predictive After In-House Regrind Fractions Reach 25 wt%?

    For pharmaceutical tablet and powder bottles in 100 mL to 1 L formats, the regulatory baseline is compliance of the monolayer HDPE with FDA 21 CFR 177.1520(c), USP <661.1>, and Ph. Eur. 3.1.3. Extractables testing by high-performance liquid chromatography with ultraviolet detection and gas chromatography–mass spectrometry after 50% ethanol/water and 0.9% saline extraction at 70°C for 24 h should show total organic carbon below 2.0 mg/L and no target polyolefin oligomer above the Ph. Eur. threshold. In-house regrind from trimmings and rejected bottles at up to 25 wt% does not alter the base resin compliance provided the regrind is dry, free of label adhesive, and passed through a 100 mesh screen pack. Above 25 wt%, the extractables curve may rise due to thermo-oxidative degradation compounds generated by repeated shear; pharmaceutical-grade production therefore uses dedicated extruders with polished screw surfaces and HEPA-filtered blow air. The processing window is 180–200°C melt temperature, low-shear screw speed of 20–40 rpm, and a bottle venting system that prevents contamination from ambient mould release agents. Terminal products are child-resistant and tamper-evident HDPE tablet bottles with 38 mm or 45 mm closure diameters. Autoclaving at 121°C is outside the continuous-use envelope; the Vicat softening point under ISO 306/A50 is 124–127°C for this HDPE class, so terminal sterilization for repetitive use should be limited to ethylene oxide or 25 kGy gamma irradiation at fewer than two cycles, because post-irradiation embrittlement is measurable after 50 kGy.

    Compliance StandardTest ConditionAcceptance Criterion
    FDA 21 CFR 177.1520(c)Olefin polymer identity, density and melting point verificationDensity 0.940–0.965 g/cm³ under ISO 1183-1:2019; melting point not less than 100°C
    USP <661.1>Purified water and alcohol extraction at 70°C for 24 hTotal organic carbon below 2.0 mg/L; no heavy metals above 1 ppm
    Ph. Eur. 3.1.3Hexane-extractable matter at 50°C for 3 hExtractable matter not more than 2.0% by mass; sulfated ash not more than 1.0%
    EU Regulation No 10/2011Overall migration in 10% ethanol and 3% acetic acid, 10 days at 40°COverall migration not more than 10 mg/dm²

    Coextruded Barrier Containers Reconfigure the Melt Temperature Window for the HDPE Structural Layer

    In six-layer coextrusion blow moulding for 1 L agrochemical and food-sauce bottles, KK351A functions as the outer and inner structural layers, while EVOH with ethylene content of 32 mol% provides oxygen barrier. The melt temperature setpoints diverge: HDPE is held at 190–210°C, maleic anhydride-grafted LLDPE tie resin at 195–215°C, and EVOH at 210–225°C. A six-layer spiral mandrel die with a 300 mm diameter head is fed by two 90 mm HDPE extruders, one 60 mm tie extruder, and one 60 mm EVOH extruder; individual layer percentages are controlled by gear-pump speed ratios. The layer distribution is set at 28 wt% outer HDPE, 30 wt% post-industrial regrind HDPE, 2 wt% tie, 4 wt% EVOH, 2 wt% tie, and 34 wt% inner HDPE. The regrind layer is restricted to post-industrial bottle trim, not post-consumer resin, unless the bottle is intended for non-food agricultural products under UN packaging certifications. Interface stability is achieved by matching the viscosity ratio of the tie resin to HDPE at the die: a tie resin with melt flow rate of 0.8–1.2 g/10 min at 190°C/2.16 kg produces a stable interface at shear rates below 600 s⁻¹; above this shear rate, interfacial wave instability may appear as a cloudy band. The oxygen transmission rate for the barrier bottle is measured under ASTM D3985-17 at 23°C and 50% RH on both sides; the inclusion of 4 wt% EVOH reduces OTR from above 120 cm³/(m²·day·atm) for monolayer HDPE to 0.8–2.5 cm³/(m²·day·atm) for 500 µm wall thickness. Terminal product is an oval 1 L herbicide or soy-sauce bottle with a 45 mm neck and induction-sealable HDPE cap. Process limitation: EVOH is hygroscopic and must be pre-dried at 70–80°C for 4–6 h in a desiccant dryer to -40°C dew point; residual moisture above 0.1 wt% creates bubble streaks in the barrier layer.

    On production-scale six-layer lines, the most frequent process conflict is encapsulation of the EVOH layer by lower-viscosity HDPE at the spiral mandrel exit when the EVOH extruder output varies by more than ±0.3 kg/h; the defect appears as a wandering clear band through the bottle sidewall. Operators verify layer distribution by cutting bottle cross-sections at 10 positions and measuring with an optical microscope; the EVOH layer thickness tolerance is ±0.5 µm at a nominal 20 µm. If EVOH thickness falls below 18 µm, the oxygen transmission rate under ASTM D3985-17 degrades to 4–6 cm³/(m²·day·atm).

    LayerWeight FractionExtruder Melt TemperatureFunction
    Outer HDPE28 wt%190–210°CStructural and shelf appearance
    Regrind HDPE30 wt%190–210°CPost-industrial trim reuse
    Tie resin2 wt%195–215°CAdhesion to EVOH
    EVOH4 wt%210–225°COxygen barrier
    Tie resin2 wt%195–215°CAdhesion to EVOH
    Inner HDPE34 wt%190–210°CProduct contact layer

    For UN-certified 20 L to 30 L closed-head jerry cans manufactured from KK351A, the mandatory design proof under UN Model Regulations Chapter 6.1 requires drop testing from 1.2 m at -18°C after conditioning, a stack test for 28 days at 40°C equal to a superimposed load of 3.0 m of filled product, and a hydraulic pressure test at 100 kPa for 30 min. The HDPE grade is processed in an accumulator-head blow moulder with a 120 mm grooved-feed extruder at L/D 28:1, shot capacity of 12 kg, melt temperature 190–215°C, and die gap 2.5–4.0 mm. The parison is pre-blown at 0.03–0.06 MPa to prevent collapse, then expanded into water-cooled aluminium tooling at 10–15°C with blow pressure of 0.8–1.0 MPa. Minimum wall thickness is 1.5 mm at the sidewall and 2.5 mm at the shoulder and bottom chime; these values are required to satisfy the stack test without creep buckling. Post-industrial regrind is incorporated at 20–30 wt% after melt filtration through a 100 mesh screen, but regrind above 40 wt% lowers the -18°C drop-impact survival rate below the 3-from-3 pass criterion due to a measurable increase in stiffness and a fall in elongation at break under ASTM D638-14. The terminal product is a 20 L UN 3H1 jerry can for hydrocarbon solvents, lubricants, and non-oxidizing aqueous chemicals. The moulding is not recommended for 98% sulfuric acid or 65% nitric acid, because oxidative attack at wall-stress points produces environmental stress cracking within 48 h under ASTM D543-21 immersion at 40°C.

    Hydraulic pressure failures on production lines frequently originate at the pinch-off weld when the flash land length is below 6 mm; a hardened tool-steel pinch-off insert with a 2.5 mm radius reduces weld-line stress cracking. The mould venting pattern must provide 0.02–0.05 mm deep vents on the bottom chime, because trapped air at the mould cavity perimeter produces local thinning below 1.2 mm.

    Melt Filtration, Screen-Pack Pressure Drop, and Regrind Blending for Low-MFR HDPE in Closed-Loop Moulding

    A closed-loop regrind stream for KK351A bottle trimmings and reject bottles is fed through a single-screw recycling extruder with a 75 mm screw at L/D 30:1, a vacuum vent at -0.08 MPa, and a hydraulic screen changer carrying a 100/60/100 mesh stack. The pressure drop across the screen pack in virgin material is normally 80–120 bar at 90 rpm; adding 30 wt% ground bottle flake with particle size of 8–12 mm increases the pre-screen melt pressure to 150–200 bar, which requires a melt pump downstream to stabilize die pressure. Melt temperature after the melt pump is limited to 215°C because shear heating from repeated extrusion shifts the melt flow rate from the original 0.30–0.40 g/10 min band under ISO 1133-1:2022 condition 190°C/2.16 kg to a higher value only after five recycling passes; before that, the polymer retains a bimodal molecular weight distribution. A 0.5 wt% antioxidant masterbatch based on a hindered phenolic-phosphite system is added to the ground flake to compensate for chain scission during reprocessing. The blend ratio for non-food containers is 30 wt% recovered regrind and 70 wt% virgin KK351A; for detergent bottles the regrind fraction is raised to 50 wt% when the flake is washed and sorted by near-infrared separation. Terminal output is a pelletized HDPE regrind compound used in the core layer of three-layer soap bottles or in black masterbatch-loaded utility parts. Published data for this specific recycling configuration is limited; the pressure values above reflect equipment manufacturer calculations for polyethylene of equivalent melt viscosity.

    When Hot-Fill Temperatures Approach 65°C in Edible-Oil and Sauce Bottles, the HDT Limit Governs In-Mould Shrinkage

    Edible-oil and soy-sauce bottles in 500 mL to 2 L formats are blow-moulded from KK351A at a melt temperature of 185–205°C with a mould temperature of 20°C. The filling temperature is maintained at 55–65°C immediately after filling; above this range, in-mould shrinkage exceeds 0.8% in the label-panel area because the heat deflection temperature under ISO 75-2/B at 0.45 MPa is 68–72°C for this HDPE class. The bottle wall thickness is designed at 0.5 mm for the label panel and 0.9 mm at the bottom strap to resist panel bulging under hot fill. Fill-line cooling after capping uses water spray at 15°C for 120 s. The food-contact compliance basis is FDA 21 CFR 177.1520(c) and EU Regulation No 10/2011 with overall migration below 10 mg/dm² in 10% ethanol and 3% acetic acid at 40°C for 10 days. A slip additive masterbatch based on erucamide at 0.5–1.0 wt% is dosed into the inner layer to reduce cap torque variability to 0.8–1.2 N·m; the additive must not exceed 1.0 wt% because plate-out on the blow mould core rod increases the rejection rate from surface blush. The terminal product is a 1 L edible-oil bottle with a 38 mm neck finish and a tamper-evident HDPE screw cap. Process limitation: contact with high-peroxide vegetable oils stored above 35°C accelerates oxidative attack at the inner surface, so manufacturers specify a shelf-life test of 12 months at 25°C with sensory panel evaluation of the oil rather than relying solely on migration compliance.

    Free Quote

    Competitive TPC (Japan) HDPE KK351A prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    TPC (Japan) supplies the high-density polyethylene grade designated KK351A as a pelletized olefin resin positioned for injection-moulding applications in which high melt flow reduces injection pressure and shortens cycle time. The grade designation is not a substitute for the revision-controlled technical data sheet; the current certificate of analysis should be consulted for lot-specific melt flow rate, density, and additive composition. In the absence of public lot-specific datasheet values, KK351A is best evaluated against the property envelope commonly reported for high-flow HDPE injection-moulding resins with a nominal melt mass-flow rate near 35 g/10 min when measured under ISO 1133-1:2022 method A or ASTM D1238-23a procedure A at 190 °C with a 2.16 kg piston load. This classification carries direct consequences for average molecular weight, crystallinity, shrinkage, environmental stress crack resistance, and processing behaviour.

    The resin is understood to be produced by a gas-phase or slurry polymerisation route, but the specific catalyst, comonomer level, and molecular architecture have not been published in a form that permits independent verification for this grade. Consequently, statements below distinguish between properties fixed by the nominal melt-flow class and supplier-specific values that require documentation. Published data for the exact additive composition of KK351A is limited.

    What Does the KK351A Designation Signify in the TPC Japan Injection-Moulding Hierarchy?

    The suffix “35” in some high-density polyethylene grade nomenclatures is associated with the melt-flow decade rather than a defined lot value, but this convention is not universal across producers. For KK351A, the primary processing parameter is the melt mass-flow rate determined to ISO 1133-1:2022 method A at 190 °C and 2.16 kg. If the grade conforms to the high-flow injection-moulding class implied by the designation, the melt flow rate typically falls between 25 g/10 min and 45 g/10 min. A resin in this range has shorter molecular chains and a narrower molecular weight distribution than blow-moulding or pipe grades, which reduces shear viscosity but also sacrifices environmental stress crack resistance and notched impact strength. The solid density is normally reported to ISO 1183-1:2019 at 23 °C as a value between 0.950 g/cm³ and 0.958 g/cm³. These values are typical class data rather than lot certification.

    The melt viscosity curve is shear-thinning. At 230 °C and an apparent shear rate of 100 s⁻¹, high-flow HDPE of this type may exhibit apparent viscosity below 200 Pa·s, which is too low for stable parison formation in blow moulding and too low for pipe extrusion. This is why KK351A-type resins are not interchangeable with high-melt-strength HDPE grades. The differentiation is rheological and mechanical rather than purely density-driven.

    On a 1200 kN injection-moulding machine equipped with a 40 mm diameter, 20:1 L/D general-purpose polyolefin screw and a compression ratio between 2.5:1 and 3.5:1, high-flow HDPE of this class is processed using a barrel temperature profile from 180 °C through 230 °C. The nozzle is normally held at 200 °C to 230 °C. Mould temperature is set at 20 °C to 50 °C; lower mould temperatures accelerate skin solidification and reduce cycle time but increase moulded-in stress and can produce flow marks. The injection velocity should be moderate to high for thin-wall filling. Excessive residence time above 260 °C can create odour, discoloration, and surface defects. Pre-drying is not normally required if pellet moisture remains below 0.1%. At relative humidity above 60%, storage in sealed hoppers or pre-drying at 80 °C for 2 h may be applied to wet regrind or condensation-contaminated pellets. Regrind addition above 30% should be paired with periodic melt-flow verification because screw work and thermal history can shift the effective melt flow rate.

    During production-scale trials of high-flow HDPE in a 1.2 mm wall container, short-shot defects were most commonly corrected by increasing nozzle temperature and injection velocity rather than increasing holding pressure. This is consistent with the flow-limited behaviour of a low-viscosity semicrystalline melt. Gate blush and jetting appear when the melt front is accelerated through undersized gates, so gate diameters of at least 0.8 mm to 1.2 mm are common for this wall range. Sink marks opposite thick bosses are controlled by holding pressure and packing time, not by melt temperature alone. The processing window is wider than that of a 10 g/10 min HDPE because the low melt viscosity reduces pressure dependence, but the lower molecular weight narrows the acceptable impact-performance boundary.

    When Thin-Wall Packaging Uses the High-Flow Melt Index as a Cycle-Time Lever

    Thin-wall food containers, caps, and overcaps can use a 35 g/10 min class resin because injection pressure may be 15% to 30% lower than with a 10 g/10 min HDPE grade, although the actual reduction depends on gate geometry, flow length, and melt temperature. Flow-length-to-wall-thickness ratios of 150:1 to 250:1 are common for thin-wall polyolefin moulding at 200 °C, provided gate size and venting are adequate. Packing pressure must be adjusted to prevent sink marks and post-mould dimensional instability. Mould shrinkage of high-flow HDPE in the parallel direction is typically 1.2% to 1.8% and in the transverse direction 1.5% to 2.0% when measured after 24 h at 23 °C using ISO 294-4:2018. Shrinkage anisotropy increases with fill orientation, so gate location and wall-thickness uniformity are stronger process variables for KK351A than for nucleated polypropylene grades. Because low molecular weight shortens relaxation time, frozen-in stress may be lower than in high-molecular-weight HDPE, but sub-zero impact performance is reduced. Published data for the exact thin-wall impact behaviour of KK351A is limited.

    Closures moulded from high-flow HDPE in this melt-index class require a balance of stiffness, environmental stress crack resistance, and organoleptic neutrality. The flexural modulus measured to ISO 178:2019 is generally between 1000 MPa and 1500 MPa for a solid density near 0.954 g/cm³. Ductile or brittle failure in closure tether and hinge applications depends on wall thickness, gate geometry, and mould temperature. A living hinge in HDPE is less fatigue-resistant than in polypropylene homopolymer, and repeated flexing can initiate stress whitening at the hinge root. For KK351A, closure applications should be validated under application-specific torque, seal-integrity, and drop testing. The low melt viscosity also improves replication of knurls, thread details, and tamper-evident bands, but long-term creep under constant sealing load is governed by crystallinity and mould cooling rate more than by melt flow rate alone.

    Mechanical Property Benchmarks and Moulding-Condition Sensitivity

    The table below compiles typical published ranges for the high-flow HDPE injection-moulding class into which KK351A falls. These ranges are not a substitute for lot-specific certification and should be used only for preliminary feasibility screening.

    Typical property ranges for high-flow HDPE injection-moulding grades with a nominal MFR of 25–45 g/10 min
    Property Test method Typical range Conditioning or specimen note
    Melt mass-flow rate ISO 1133-1:2022 method A / ASTM D1238-23a procedure A 25–45 g/10 min 190 °C, 2.16 kg
    Density ISO 1183-1:2019 / ASTM D1505 0.950–0.958 g/cm³ 23 °C
    Tensile yield stress ISO 527-2:2012 24–30 MPa Type 1A specimen, 50 mm/min
    Tensile elongation at yield ISO 527-2:2012 8–12% Type 1A specimen
    Flexural modulus ISO 178:2019 1000–1500 MPa 2 mm/min
    Notched Izod impact ASTM D256-23a 20–60 J/m 3.2 mm, 23 °C
    Vicat softening temperature ISO 306:2022 A120 120–127 °C 10 N load
    Mould shrinkage, parallel ISO 294-4:2018 1.2–1.8% After 24 h, 23 °C

    Specimen moulding conditions have a larger effect on impact and shrinkage than the small density differences within this product class. A mould temperature at the low end of the 20–50 °C range can reduce the notched Izod impact value measured to ASTM D256-23a at 23 °C by up to one-third in some semicrystalline HDPE formulations; for KK351A, published data for this specific configuration is limited. The direction of flow and the location of the gate should therefore be recorded on any comparative test report.

    Chemical compatibility is governed by density, molecular weight, and residual stress, not solely by the HDPE designation. High-flow HDPE of this class typically exhibits a notched Izod impact value between 20 J/m and 60 J/m at 23 °C, but contact with strong oxidizers, aromatic hydrocarbons, or chlorinated solvents can reduce local ductility. Stress-crack resistance measured by ASTM D1693-15e1 condition A in 100% Igepal CO-630 at 50 °C is expected to be lower than that of a medium-flow blow-moulding HDPE. For KK351A, a specific F50 value should be taken from the technical data sheet because published data for this specific configuration is limited. Applications requiring continuous exposure to detergents, oils, or agricultural chemicals should be validated by package testing under the expected service temperature and stress.

    Because Food-Contact Status Depends on Formulation, Not Polymer Class Alone

    Unpigmented high-density polyethylene can comply with FDA 21 CFR 177.1520(d)(2)(i) for food-contact use when the final article meets end-use extractives and migration tests. For EU applications, Commission Regulation (EU) 10/2011 sets an overall migration limit of 10 mg/dm² of food-contact surface, verified by EN 1186 or EN 13130 test methods. The resin should also be assessed under REACH Regulation (EC) No 1907/2006 for candidate-list substances at 0.1% w/w and under Directive 2011/65/EU (RoHS) Annex II for lead, mercury, cadmium, hexavalent chromium, polybrominated biphenyls, and polybrominated diphenyl ethers. KK351A should not be assumed compliant merely because it is an HDPE; masterbatch pigments, antistatic additives, slip agents, or processing aids introduced by the converter can change the regulatory profile. Supplier documentation such as a food-contact statement or EU declaration of compliance must be requested for the specific lot and final formulation.

    Compliance documentation checklist for KK351A conversion
    Regulatory framework Key limit or requirement Documentation to request
    FDA 21 CFR 177.1520(d)(2)(i) Olefin polymer clearance conditions Food-contact status statement
    EU 10/2011 Overall migration 10 mg/dm² EU declaration of compliance
    REACH 1907/2006 SVHC 0.1% w/w REACH compliance statement
    RoHS 2011/65/EU Annex II Cd 0.01% w/w; Pb, Hg, Cr6+, PBB, PBDE 0.1% w/w RoHS test report

    For applications where high-flow capability is not mandatory, KK351A differs from blow-moulding and pipe HDPE grades in measurable ways. Blow-moulding grades often have a melt flow rate from 0.2 g/10 min to 1.5 g/10 min at 190 °C and 2.16 kg, giving higher melt strength and parison uniformity but longer cycle times and higher injection pressure if forced into injection moulding. A 35 g/10 min class injection grade has lower environmental stress crack resistance and lower notched impact strength, so it is typically unsuitable for pressure pipe, chemical storage tanks, and geomembranes where ASTM D1693-15e1 F50 lifetimes of 100 h to greater than 1000 h may be specified. Conversely, the high-flow class offers lower clamp force requirements, shorter cooling time, and finer replication of mould detail. The differentiation is therefore primarily rheological and mechanical, not density-driven.

    For thin-wall rigid packaging, polypropylene impact copolymers are an alternative material class. They may provide higher heat deflection temperature and better hinge performance but often require higher injection pressures and exhibit lower low-temperature toughness than HDPE. The choice between KK351A-type HDPE and a polypropylene impact copolymer should therefore be based on service temperature, hinge fatigue, moisture barrier, and impact requirements rather than on injection moulding cycle time alone.

    Under Extended Regrind Fractions, Lot-to-Lot Consistency Becomes the Controlling Variable

    Batch-to-batch variation in high-flow HDPE is most visible in melt-flow drift during extended regrind campaigns. On a 600 kN moulding machine running a 1.2 mm wall container, the addition of 20% regrind can raise the melt flow rate by 1–3 g/10 min depending on regrind history and screw work; this shifts holding-pressure requirements and can increase flash or improve fill. To maintain dimensional control, melt-flow should be measured every 4 h during long runs and injection pressure adjusted within a ±5 bar band. If KK351A is blended with lower-viscosity HDPE grades, the mixture may show compounding-induced non-uniformity unless a gravimetric blender or metering hopper is used. Surface defects such as melt fracture or gate blush can occur above an apparent shear rate of 1000 s⁻¹, although published data for this specific configuration is limited. Polypropylene contamination above 3% should be avoided because inhomogeneous polypropylene domains can produce delamination and visible haze in HDPE mouldings.

    Top