| HS Code | 613460 |
| Density | 0.951 g/cm³ |
| Melt Flow Rate | 0.40 g/10 min (190°C/2.16 kg) |
| Hardness Shore D | 65 |
| Tensile Strength At Yield | 28.0 MPa |
| Tensile Strength At Break | 30.0 MPa |
| Elongation At Break | 500% |
| Flexural Modulus | 1.20 GPa |
| Vicat Softening Point | 124 °C |
| Brittleness Temperature | -70.0 °C |
| Thermal Conductivity | 0.400 W/m·K |
| Specific Heat | 2.30 J/g·°C |
| Dielectric Constant | 2.30 |
| Volume Resistivity | 1.00E+16 ohm·cm |
| Water Absorption | 0.010% |
As an accredited TPC (Japan) HDPE KFZ51Z factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | TPC (Japan) HDPE KFZ51Z is supplied in 25 kg polyethylene-lined bags, palletized and stretch-wrapped for industrial shipment. |
| Container Loading (20′ FCL) | 20′ FCL container can load approximately 17–20 MT of TPC (Japan) HDPE KFZ51Z in 25 kg bags, depending on palletization. |
| Shipping | TPC (Japan) HDPE KFZ51Z, a non-hazardous polyethylene resin, is typically shipped in 25 kg moisture-resistant bags or 1,000 kg jumbo bags, palletized and stretch-wrapped. It is transported by sea or land in closed containers, kept dry, cool, and away from direct sunlight and heat. |
| Storage | TPC (Japan) HDPE KFZ51Z: store indoors at ambient temperature in a clean, dry, well-ventilated warehouse. Keep original bags or containers closed, off the floor, away from direct sunlight, heat, ignition sources, and strong oxidizers. Protect pellets from moisture, dust, and contamination. Use first-in-first-out rotation, stable pallets, and safe stacking heights. Avoid prolonged UV exposure. Follow supplier SDS and local regulations. |
| Shelf Life | Store sealed in original packaging, cool, dry, away from sunlight; recommended shelf life is 24 months from date of manufacture. |
Closure shell production from TPC (Japan) HDPE KFZ51Z is governed by thread geometry, dimensional stability during cooling, and migration compliance for direct food contact. A start-point dry-blend formulation on high-speed closure lines uses 1.5–2.5 wt% colour masterbatch, 0.02–0.05 wt% erucamide slip concentrate, and 0.05–0.10 wt% hindered phenolic antioxidant in 100 parts by weight resin. The slip additive reduces cap removal torque within customer closure specifications; the antioxidant package is selected to survive repeated processing of scrap regrind at 15–30% refeed ratios. Compliance for closures placed on beverages and edible oils is tested under FDA 21 CFR 177.1520(c)3.1a, EU Regulation 10/2011 Annex I and Regulation 1935/2004, with overall migration not exceeding 10 mg/dm² when extracted in food-simulant D2 or E according to the food type. The moulding process uses reciprocating-screw injection moulding machines with clamp force of 250–450 t, a barrel L/D ratio of 20:1–25:1, melt temperature 190–225 °C, mould temperature 8–15 °C, and shot-to-shot cushion control within 2.0–3.5 mm. Moulding records from high-cavitation closure lines show that a lot-to-lot MFR movement of ±0.3 g/10 min under ISO 1133-1:2022 at 190 °C/2.16 kg can alter peak injection pressure by 1.5–3.0 MPa when cavity fill is pressure-limited. Gate diameter is set to 0.5–0.8 mm at the cap centre to prevent stringing and to promote radial flow; valve-gate hot runners with 8–16 drops are balanced by manifold pressure profiling. Typical cycle time for a 2.1 g water closure in a 32-cavity hot-runner tool is 4.5–7.0 s, with demoulding limited by thread unscrewing or collapsing-core mechanics rather than melt solidification. Finished products include 26/22 mm tamper-evident beverage closures, sports drink closures, edible oil cap bodies, and overcaps for composite containers.
In thin-wall food-contact moulding, KFZ51Z is run at wall thicknesses of 0.40–0.70 mm in multi-cavity stack tools where flow length-to-thickness ratios exceed 250:1 on certain container geometries. The compound is dry-blended with 1.0–2.0 wt% white masterbatch, 0.3–0.8 wt% fluoropolymer process aid, and 0.1–0.2 wt% acid scavenger per 100 parts KFZ51Z. The process aid suppresses melt fracture and die-lip build-up; the acid scavenger prevents discolouration when post-industrial scrap regrind is added at 10–20%. Resin stored in silos below dew point requires a 2 h hopper-air purge at 30–40 °C to prevent screw surging from surface condensation. Food-contact compliance is confirmed under FDA 21 CFR 177.1520(c)2.1 and EU Regulation 10/2011, with specific attention to additive migration limits in Annex II and overall migration ≤10 mg/dm². The moulding window requires a 20:1–25:1 L/D screw, melt temperature 185–215 °C, nozzle temperature 195–215 °C, and chilled mould temperature 10–20 °C; injection speed is held between 150–250 mm/s to avoid flow hesitation at thin ribs. Hot-runner valve-gate tip size is normally 0.6–1.0 mm, and part weight repeatability is held within ±0.05 g in 4- or 8-cavity stack moulds. Barrel residence time above 220 °C is kept below 5 min to limit oxidative odour precursors that can impair dairy or frozen dessert flavour profiles. Terminal components in this segment include dairy spread tubs, portion cups, food-service containers, and frozen dessert tubs with embossed lid seats.
Industrial pail production with KFZ51Z is constrained by the contradiction between low-temperature drop impact and top-load stiffness. A compound start-point uses 100 parts KFZ51Z blended with 5–15 wt% metallocene or linear low-density polyethylene impact modifier, 0.5–1.0 wt% primary antioxidant, 0.2–0.4 wt% phosphite secondary antioxidant, and 1.0–2.0 wt% colour masterbatch. At impact modifier additions above 15 wt%, top-load stiffness under stacking can fall below customer warehouse loading specifications, while below 5 wt% the pail sidewall may become brittle when tested at -18 °C according to UN drop test procedures. Compliance for dangerous goods packaging requires the UN mark 1H2/Y1.5/100 and tests under the UN Model Regulations Chapter 6.1, with modal variants in ADR/RID and IATA; selected pails additionally comply with FDA 21 CFR 177.1520 when intended for food-grade chemical concentrates. The forming operation uses large injection moulding machines with clamp force 600–1200 t, a 20:1–24:1 L/D barrier screw, melt temperature 190–230 °C, mould temperature 15–30 °C, and sidewall thickness 2.0–3.2 mm. Injection pressure is typically maintained at 120–160 MPa to achieve full packing into thick rim and handle sections. Cycle time is governed by sidewall crystallisation and is typically 12–20 s cooling for a 5 L pail; 20 L pails require additional holding and cooling time. Post-mould dimensional inspection at 48 h is required because HDPE shrinkage continues beyond immediate demoulding, and top-load testing is repeated after 48 h conditioning at 23 °C/50% RH. Terminal products include open-top pails of 5–20 L for paints, printing inks, adhesives, lubricant concentrates, and solvent-free chemical powders.
| Sector | Regulatory/material standard | Test method | Limiting criterion |
|---|---|---|---|
| Beverage closures | FDA 21 CFR 177.1520(c)3.1a; EU 10/2011 | EU OML EN 1186-1; ISO 1133-1:2022 | OML ≤10 mg/dm²; MFR drift limited |
| Thin-wall food containers | FDA 21 CFR 177.1520(c)2.1; EU 10/2011 | ASTM D1238-23; ISO 527-2 | OML ≤10 mg/dm²; tensile yield retained |
| UN industrial pails | UN 1H2/Y1.5/100; ADR/RID; IATA | UN drop test Chapter 6.1 | No fracture at -18 °C |
| Washer reservoirs | REACH 1907/2006; RoHS 2011/65/EU | OEM fluid compatibility test | No stress cracking in methanol/EG |
| Crates/pallets | REACH 1907/2006; ISO 8611-1:2021 | ISO 180; ISO 178 | Impact retention after recyclate |
| Personal care/package components | REACH 1907/2006; FDA 21 CFR 177.1520 | ASTM D638-14 | Snap-fit elongation before yield |
Windshield washer reservoirs and overflow recovery bottles are moulded from KFZ51Z as two injection-moulded half shells subsequently joined by hot-plate welding. The formulation uses 100 parts KFZ51Z with 0.2–0.4 wt% hindered phenolic antioxidant, 0.1–0.2 wt% phosphite processing stabiliser, and 1.0–2.0 wt% carbon black or UV-stabilised masterbatch for exterior exposure. This sector is not regulated as food contact; material compliance is anchored to REACH 1907/2006 SVHC screening, RoHS Directive 2011/65/EU, and OEM-specific hydrocarbon resistance tests for washer fluid, methanol, and ethylene glycol. Shell injection uses machines with clamp force 800–1200 t, melt temperature 200–230 °C, mould temperature 15–30 °C, and wall thickness 2.5–3.5 mm; the tooling is often two-cavity due to part volume. Hot-plate welding at 210–230 °C plate temperature and 60–90 s cycle time produces a continuous weld seam, which is then leak-tested at 30–50 kPa internal air pressure; some OEM specifications add a burst test at 150–250 kPa. Ribbed wall sections require gate placement that avoids trapped gas causing short shots at the weld seam, and core-pull sequencing is used for bracket features. For underhood thermal exposure above 80 °C, this grade is not specified; polypropylene or polyamide should be selected for sustained hot-oil or close-coupled engine environments. Finished components include windshield washer bottles, coolant recovery bottles, and non-food fluid reservoirs for off-road equipment.
Crate and pallet conversions using KFZ51Z typically incorporate post-industrial regrind because thick-section parts tolerate moderate melt viscosity shifts, but the recyclate fraction must be controlled to prevent step changes in flexural modulus and low-temperature impact. A start-point formulation is 100 parts virgin KFZ51Z plus 5–20 wt% clean post-industrial HDPE regrind, 0.5–1.5 wt% antioxidant masterbatch, and 1.0–2.0 wt% colour masterbatch. Revalidation is required at the 5.0 wt% recyclate threshold because the Izod notched impact and flexural modulus of the moulded crate can shift beyond customer specification when the melt flow rate of the recyclate differs from the virgin lot by more than 0.5 g/10 min when measured according to ISO 1133-1:2022 at 190 °C/2.16 kg. Compliance for non-food logistics articles is anchored to REACH 1907/2006, RoHS 2011/65/EU, and ISO 8611-1:2021 for pallet performance; beverage crate impact testing follows customer-specific drop tests at -18 °C. Processing on injection moulding machines requires clamp force 1000–2500 t, melt temperature 190–230 °C, mould temperature 15–30 °C, and cooling time driven by thick rib intersections of 3.0–6.0 mm. Sink marks at rib-to-wall junctions are controlled by gas-assisted injection or sequential valve gating rather than by reducing holding pressure alone; gate size in this sector is usually 1.5–2.5 mm, with packing time 8–15 s set by gate freeze-off. Terminal products include beverage crates, fruit crates, logistics containers, automotive dunnage trays, and reusable Euro boxes.
For personal care and household product packaging components, KFZ51Z is moulded where the part combines a snap-fit closure feature with a tall, draw-intensive body or threaded collar. The dry-blend formulation uses 100 parts KFZ51Z, 0.5–1.5 wt% white or custom masterbatch, 0.02–0.05 wt% slip additive, and 0.05–0.10 wt% antioxidant; no impact modifier is specified unless drop tests demand otherwise, because over-modification can reduce snap-fit interference retention. Compliance is assessed under EU cosmetics packaging Regulation 1223/2009 Article 17 for product-packaging compatibility, REACH 1907/2006, and FDA 21 CFR 177.1520 when the package is used for food-like delivery. Process conditions include clamp force 180–450 t, melt temperature 190–220 °C, mould temperature 10–20 °C, and cycle times of 8–14 s for multi-cavity tooling. Deep draw features require a mould opening stroke sufficient to clear the part height and a hydraulic core pull for internal thread or snap-collar release; stripping plates are preferred for shallow snap features to reduce cycle time. Published data for this specific configuration is limited when attempting to correlate slip additive concentration with snap-fit removal force after 30 days, so validation is performed on finished components under customer-defined assembly torque protocols. Terminal products include dispensing cap bases for personal care bottles, trigger sprayer collars, and household cleaning product caps.
Competitive TPC (Japan) HDPE KFZ51Z prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
TPC (Japan) HDPE KFZ51Z is a high-density polyethylene grade supplied primarily for extrusion blow molding, thick-sheet forming, and structural chemical packaging in which melt strength, environmental stress crack resistance, and controlled parison sag are controlling variables. The product designation belongs to the producer’s high-molecular-weight HDPE series; exact melt flow rate, density, tensile properties, and stabilizer content are governed by the lot-specific certificate of analysis and the producer’s technical data sheet rather than by generic literature. For specification verification, density is determined according to ISO 1183-1:2019, melt mass-flow rate and high-load melt flow rate by ISO 1133-1:2022, tensile properties by ISO 527-2:2012, and environmental stress crack resistance by ASTM D1693-15. The material is typically selected where a higher melt viscosity is required than standard blow molding grades with 0.3–2 g/10 min melt flow rate under 190°C/2.16 kg; however, the precise melt viscosity relationship must be read from the producer’s certificate of analysis.
In public databases, published data for this specific configuration is limited; therefore grade-specific numerical values should not be transferred from other KFZ-series or HDPE grades. As a class, high-density polyethylene is generally specified in the density range 0.94–0.97 g/cm³ according to ISO 1183-1:2019. High-load melt index testing at 190°C/21.6 kg is used when the 2.16 kg value falls below 0.1 g/10 min. These ranges are class-typical and are not a substitute for the supplier’s release value.
High-molecular-weight HDPE grades of this class display pronounced shear thinning, but published pressure-versus-shear-rate data for this specific configuration is limited. On production-scale single-screw extruders with grooved feed zones, L/D 30:1 or greater, and barrier screws, barrel temperature profiles are generally maintained between 180°C and 220°C, with the head and die zones between 200°C and 230°C. Melt temperature at the die exit should be measured by an immersion thermocouple and kept below 240°C; prolonged excursions above this limit can reduce antioxidant activity and lower ESCR through thermo-oxidative chain scission. Feed-zone screw cooling is required to maintain solids conveying; feed-zone barrel temperatures above 100°C may produce premature melting and feed fluctuation. Head pressure and back pressure are die-dependent, but this molecular weight class typically requires back pressure in the 10–25 MPa range on a 75 mm extruder at a throughput matched to the screw design. The exact KFZ51Z window must be established from the producer’s processing guide. Die lip gaps below 1.0 mm on blow molding heads are more likely to initiate melt fracture; corrective action consists of widening the land or raising melt temperature within the 240°C upper limit.
Predrying is not normally required for HDPE under closed indoor storage, but when stored stock is moved into a high-humidity molding room with relative humidity above 60%, surface condensation can occur. Under these conditions, a desiccant dryer set at 70°C for 2 h or a dry-air hopper at 60°C for 4 h is applied before extrusion. Regrind containing unknown pigment concentrates should not be combined with unpigmented KFZ51Z without prior testing, because metal-containing colorants can shorten long-term heat stability and alter Directive 2011/65/EU RoHS compliance.
Substitution should proceed only after comparison of melt flow rate, high-load melt flow rate, die swell, and ASTM D1693-15 ESCR data. Standard blow molding HDPE grades are often specified at 0.3–2 g/10 min under ISO 1133-1:2022 condition 190°C/2.16 kg; KFZ51Z is a high-molecular-weight grade with lower standard-condition melt flow. The higher molecular weight contributes to greater parison hang time and more uniform wall thickness in large parts, but it also raises screw torque, melt temperature, and head pressure. Compared with PE100 pipe resins, which are certified under ISO 9080 and ISO 12162 to a minimum required strength of 10.0 MPa at 20°C for 50 years, KFZ51Z is not normally specified as a pressure-pipe material unless the producer’s technical data sheet contains PE100 or PE80 grade listing. Compared with HDPE film grades, which are evaluated for gel count, coefficient of friction, and draw-down stability, KFZ51Z is evaluated primarily for ESCR, drop impact, and wall-thickness creep behavior. The grade should not be assumed to contain slip or antiblock additives unless those additives are explicitly listed.
Within the supplier’s HDPE portfolio, KFZ51Z should also be distinguished from HDPE grades intended for high-speed thin-wall injection molding, which require much higher melt flow and lower molecular weight. Injection molding HDPE grades are often specified with ISO 1133-1:2022 values above 5 g/10 min at 190°C/2.16 kg, whereas KFZ51Z is positioned on the high-molecular-weight side. This separation has direct consequences for tooling design: thin-wall injection molds with flow length/wall thickness ratios above 150:1 are inappropriate for KFZ51Z unless the producer has demonstrated sufficient flow length on the specific tool. The material is therefore confined to processes using parison, sheet, or thick-section flow channels, where high melt strength is beneficial.
On blow molding lines, KFZ51Z is evaluated for large containers with sidewall thickness above 4 mm, including industrial drums, intermediate bulk containers, and chemical storage vessels. Validation should include drop impact at -40°C per ASTM D2463, top-load creep at 40°C per ASTM D4577 or equivalent, and ESCR testing of molded panels rather than pellet-only data. If the part is destined for food contact, migration testing under the intended temperature and simulant conditions must be conducted under 21 CFR §177.1520 and Regulation (EU) No 10/2011 as amended; food-contact status is not automatically conferred by the polymer type alone.
Compared with polypropylene and LLDPE alternatives used in chemical packaging, KFZ51Z exhibits different stress cracking behavior but lower stiffness than polypropylene at elevated temperature. Flexural modulus of HDPE is generally below 1500 MPa under ISO 178:2019, and heat distortion temperature is generally below 80°C under ISO 75-2:2013 Method A, while polypropylene often exceeds these values. Such differences limit continuous service under load above 60°C; selection must be based on creep modulus at the service temperature, not room-temperature data alone.
The bent-strip ESCR test ASTM D1693-15 is commonly run in 10% by volume Igepal CO-630 solution at 50°C, with F50 failure time reported. For geomembrane or long-term stress-cracking evaluation, notched constant tensile load testing per ASTM D5397-20 at 50°C in the same surfactant is applied. HDPE crystallinity in the 60–80% range, measured by differential scanning calorimetry under ISO 11357-3:2018, contributes to low permeation but does not eliminate swelling or stress cracking in aggressive media. Oxidative induction time by ISO 11357-6:2018 is used to monitor antioxidant package depletion; a significant reduction in OIT after multiple heat histories indicates stabilizer loss and requires process adjustment. Contact with strong oxidizing acids above 60°C, chlorinated solvents, or aromatic hydrocarbons under sustained stress should be avoided because stress cracking severity increases with temperature and concentration; published data for this specific configuration is limited for multi-component industrial mixtures.
Two HDPE lots with identical density and high-load melt index can differ in ESCR by more than 2× if the comonomer placement or molecular weight distribution differs. Therefore KFZ51Z should be qualified using the producer’s internal control chart for ESCR, not solely by density and melt flow. When rheological comparison is required, small-amplitude oscillatory shear is performed on a controlled-stress rheometer under nitrogen at 190°C; the crossover frequency is used as an indicator of molecular weight distribution breadth. Published data for this specific configuration is limited; processors should request rheological data from TPC Japan when lot-to-lot consistency in blow molding parison sag is critical.
Batch-to-batch process control on actual manufacturing lines typically tracks density by ISO 1183-1:2019, high-load melt index by ISO 1133-1:2022, and notched Charpy impact by ISO 179-1:2010. If the supplier’s control chart shows high-load melt index drift above ±10% of the release value, parison sag and part weight can shift sufficiently to require adjustments to die programming. Blow molding machines with closed-loop parison control and clamp force above 1000 kN are recommended when wall-thickness tolerance is below ±0.5 mm. These process limits are equipment-specific and should be verified by a capability study on the intended tooling.
The following standards are used to verify polymer identity, mechanical specification, and regulatory status for olefin homopolymers in the form supplied:
| Category | Reference designation | Verification objective |
|---|---|---|
| Density | ISO 1183-1:2019 | Specification check for high-density classification |
| Melt flow | ISO 1133-1:2022 | Standard and high-load MFR at 190°C |
| Tensile properties | ISO 527-2:2012 | Yield stress, elongation at yield, break |
| ESCR | ASTM D1693-15 | F50 failure time in Igepal at 50°C |
| Impact resistance | ISO 179-1:2010 | Charpy notched impact at 23°C |
| US food contact | 21 CFR §177.1520 | Olefin polymer identity and extractives |
| EU food contact | Regulation (EU) No 10/2011 | Overall migration and specific migration |
| EU RoHS | Directive 2011/65/EU Annex II | Heavy metal and brominated flame retardant limits in colorants |
In extrusion blow molding of a 20 L drum tool with 6 mm sidewall, die programming is generally adjusted after collecting 0.5 h of steady-state production data; the high molecular weight of KFZ51Z can retain heat in thick sections, and ejection before adequate cooling can cause post-mold shrinkage above 1.5% under ISO 294-4:2003 test conditions. Molds with internal cooling channels at 8–12°C and blow pressure above 0.8 MPa are typically used; these values are starting points and do not replace tool-specific optimization.