Tpc Japan Hdpe Kfz51c

TPC (Japan) HDPE KFZ51C

    • Product Name: TPC (Japan) HDPE KFZ51C
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 596503
    Density 0.951 g/cm3
    Melt Flow Rate 0.50 g/10 min
    Tensile Strength At Yield 28 MPa
    Tensile Elongation At Break 700 %
    Flexural Modulus 1.10 GPa
    Notched Izod Impact Strength 0.50 J/cm
    Vicat Softening Point 123 °C
    Heat Deflection Temperature At 0 45 Mpa 72 °C
    Brittleness Temperature -70 °C
    Hardness Shore D 66
    Environmental Stress Crack Resistance >1000 h
    Thermal Conductivity 0.40 W/m·K

    As an accredited TPC (Japan) HDPE KFZ51C factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing TPC (Japan) HDPE KFZ51C is supplied in 25 kg net paper bags, palletized and stretch-wrapped for transport.
    Container Loading (20′ FCL) Container Loading (20′ FCL): TPC Japan HDPE KFZ51C in 25 kg bags, palletized, shrink-wrapped, typically about 18–20 MT per container.
    Shipping TPC (Japan) HDPE KFZ51C is a non-hazardous high-density polyethylene resin, typically shipped in 25 kg bags or bulk containers. It is not regulated for transport. Store in a cool, dry, ventilated area, away from heat, ignition sources, moisture, and contamination. Keep packaging closed.
    Storage Store TPC (Japan) HDPE KFZ51C in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, flames, and strong oxidizers. Keep original bags or containers tightly closed, clean, and undamaged, palletized off the floor. Avoid prolonged UV exposure, moisture, and contamination. Do not stack excessively high; use first-in, first-out stock rotation and follow local regulations.
    Shelf Life TPC (Japan) HDPE KFZ51C shelf life: typically 24 months if stored cool, dry, sealed, away from sunlight, heat, and contaminants.
    Application of TPC (Japan) HDPE KFZ51C

    High-stalk film extrusion of vest-style carrier sacks uses the high molecular weight fraction of HDPE KFZ51C to maintain bubble geometry at blow-up ratios between 3.0:1 and 5.0:1. The grade is characterised by a nominal melt flow index of 0.15 g/10 min at 190 °C and 2.16 kg per ISO 1133-1:2022 and a nominal density of 0.951 g/cm³ per ISO 1183-1:2019. In high-stalk HDPE film lines, the extruder is typically a grooved-feed single-screw machine with L/D 30:1 and a barrier screw, delivering melt to a spiral mandrel die with a die gap of 1.2–1.6 mm. The barrel profile is usually set from 180 °C at the feed throat to 210 °C at the adapter, with die zones held at 200–215 °C; melt pressure at the screen changer should remain below the extruder manufacturer’s thrust-bearing limit, commonly 35 MPa for a 75 mm machine. The long-neck high-stalk bubble, with frost line height at 6–10 die diameters, allows strain-induced orientation in the machine direction before crystallisation arrests further molecular movement. This orientation produces the high modulus required for 12–20 µm vest sacks that run on rotary bag machines at high cycle rates. Gauge variation below ±8% across the layflat is normally achievable when the collapsing frame is centred and nip roll pressure is uniform. During downstream conversion, seal bars operate at 140–160 °C against a HDPE seal initiation temperature near 120 °C; excessive seal temperature above 160 °C causes film thinning at the seal edge and reduced handle strength. A converter-specified masterbatch containing synthetic silica antiblock at 2,000–4,000 ppm and erucamide slip at 500–1,000 ppm is often added to prevent blocking on high-speed bag lines, but the additive package must not exceed the concentration at which seal strength degrades. Mechanical property verification for this application is performed under ASTM D882-18 for tensile modulus and yield, ASTM D1922-15 for Elmendorf tear, and ASTM D1709-24 for dart drop, with values reported in the grade certificate of analysis.

    How Does the Grade Function as a Stiffness Core in Three-Layer Heavy-Duty Sack Films?

    In three-layer heavy-duty sack coextrusion, HDPE KFZ51C is placed in the core layer to raise modulus and resistance to stress relaxation, while metallocene LLDPE skins provide hot-tack strength and dart impact. The process window is governed by the viscosity difference between the 0.15 g/10 min HDPE core and the 1.0 g/10 min mLLDPE skins, which is controlled by separate extruders feeding a 3-layer spiral mandrel die. The core extruder is normally operated at 205–215 °C and the skin extruders at 195–205 °C; interlayer interfacial instability appears if the die temperature drops below 195 °C because the HDPE relaxation time exceeds the residence time in the spiral channels. Layer distribution is maintained at 20/60/20 or 25/50/25 for total film thickness from 50 µm to 80 µm, with the core layer not exceeding 60% because higher core fractions reduce seal initiation temperature and cause seal-bar sticking. Screen packs of 60/80/100 mesh are used in the core extruder to trap unmelted high-molecular-weight gels, and specific output is often limited by melt pressure rather than motor load on L/D 30:1 grooved-feed machines. Published data for this exact KFZ51C-based coextruded structure is limited; the layer distribution and thermal profile are starting conditions derived from high-molecular-weight HDPE blown film technology and must be confirmed on pilot lines. Tensile performance is tested under ASTM D882-18, tear resistance under ASTM D1922-15, and puncture resistance under ASTM D5748-22. The primary operational boundary is bubble geometry: the high-stalk core requires a collapsing frame that can accept a long neck; if the nip is positioned too close, the HDPE film exhibits gauge bands at ±12–15% deviation due to insufficient melt relaxation. Seal strength in heavy-duty sacks is dominated by the skin layer, but migration of high-density polymer into the seal region reduces seal initiation temperature if the core layer exceeds 60% of total thickness. Production-scale failure modes include bubble instability during transient viscosity changes after resin changes and weld-line retention in the core layer when melt temperature falls below 200 °C at the die lip.

    In thin-gauge municipal refuse sacks, HDPE KFZ51C is usually employed as a stiffness component in blends with LLDPE or post-consumer recycled HDPE. Extrusion is performed on single-screw blown film lines with L/D 24:1 to 30:1 barrels and die gaps of 1.0–1.8 mm; the high-stalk bubble is shortened to a frost line height of 4–6 die diameters because the LLDPE fraction reduces melt stability. Blend ratios of 30–50 wt% KFZ51C in LLDPE are common, with the exact ratio adjusted until the film reaches the purchaser’s minimum modulus under ISO 527-3:2018 and dart drop under ASTM D1709-24. For municipal refuse sacks of 12–25 µm thickness, specifications typically require a secant modulus above 400 MPa and dart drop of ≥120 g; these values are used as internal quality gates, not universal standards. Post-consumer recyclate addition above 20 wt% reduces dart impact and raises gel count unless melt filtration of 80 mesh or finer is used; on production lines with a two-stage cooling ring, gauge variation increases when the recyclate HDPE fraction has a lower molecular weight than the KFZ51C component. Calcium carbonate filler is limited to 5–10 wt% in the refuse sack layer because higher loadings lower tear resistance under ASTM D1922-15 and produce die-lip build-up at melt temperatures below 200 °C. The resulting film is converted on bag machines at seal bar temperatures of 135–155 °C; seal strength must be verified after the post-cooling cycle because HDPE crystallises rapidly and the hot seal can appear adequate while still molten. Gauge bands near the film edges are a recurring production issue when the collapsing frame angle is increased beyond 20° to suit thin-gauge LLDPE lines, and corrective action normally involves reducing blow-up ratio to 3.0:1 or shifting the frost line upward by 1–2 die diameters.

    Direct Food-Contact Liners and the Olefin Polymer Provisions

    Compliance for direct food-contact liners is assigned to the finished package converter, not the resin producer, because additives and processing conditions determine migration behaviour. HDPE KFZ51C can be used in monolayer cereal liners, bread bags, and fresh produce bags when the resin meets FDA 21 CFR 177.1520(c) specifications and the auxiliary slip/antiblock package is cleared for the intended food type. For EU applications, overall migration is tested under EU Regulation No 10/2011, Annex V, with a limit of 10 mg/dm² for the finished plastic article. Aqueous simulants of 10% ethanol and 3% acetic acid are used for hydrophilic foods, while fatty foods require vegetable oil or 95% ethanol; film samples are conditioned under time-temperature conditions selected from Annex V. The grade’s low melt index of 0.15 g/10 min can increase melt pressure in small extruders, so screen packs are kept to 60/80 mesh and barrel temperatures are held at 190–210 °C to avoid oxidative by-products that can affect organoleptic performance. Moisture vapour transmission rates for HDPE film of this density are typically in the range of 4–8 g/m²·day at 38 °C and 90% RH under ISO 15106-1:2021, but oxygen transmission is insufficient for oxygen-sensitive products without a barrier coating or coextruded EVOH layer. Sensory transfer testing under ASTM E1870-22 is recommended for direct food contact; residual odour is more commonly caused by oxidised low-molecular-weight species from excessive melt temperature than by the base polymer. The following compliance matrix is used during qualification.

    Compliance parameterStandard or clauseSpecification
    Olefin polymer food-contact clearanceFDA 21 CFR 177.1520(c)Resin conforms by manufacturer; final package compliance by converter
    Overall migrationEU Regulation No 10/2011, Annex V≤10 mg/dm² for monolayer film
    Specific migration of metalsEU Regulation No 10/2011, Annex IIVerify with food simulant assigned to food type
    Sensory odour and tasteASTM E1870-22No product-odour transfer at 60 °C/24 h for aqueous simulant

    When fibre drums, rigid bulk containers, or pails require removable barrier liners, HDPE KFZ51C can be extruded into unsupported tubular film from 50 µm to 100 µm. For chemical compatibility, the film is used with mildly alkaline, non-oxidising aqueous fluids and dry free-flowing solids; strong oxidisers, aromatic solvents, and low-molecular-weight hydrocarbons require coextruded barrier layers or prior immersion testing under ASTM D543-21. Because HDPE has surface resistivity above 10¹⁴ ohm/sq under ASTM D257-14, drums filled with combustible powders specify a migratory antistatic additive that reduces surface resistivity to 10¹⁰–10¹² ohm/sq and static decay to less than 2 s under MIL-PRF-81705D. Blown film extrusion for industrial liners is run on grooved-feed extruders with L/D 30:1 and a die gap of 1.6–2.2 mm to accommodate the heavier gauge. The collapsing frame is configured with long spreader bars and air-turning bars to prevent blocking; post-gusset widths are held to ±5 mm for insertion into fibre drums. Seal integrity of bottom-weld liners is tested under ASTM F88/F88M-23, with a minimum seal strength tied to the filled weight and drop height specification of the drum. In applications requiring bulk food ingredient liners, the film must also meet the migration and organoleptic requirements described for direct food contact; in non-food chemical liners, REACH compliance for the supplied masterbatch and pigment must be documented by the converter. A practical limit is the film’s low elongation in the transverse direction relative to LLDPE, which can lead to puncture at sharp drum edges when liners are inserted without deburring or protective top cuffs.

    Free Quote

    Competitive TPC (Japan) HDPE KFZ51C prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    TPC (Japan) HDPE KFZ51C is a high-molecular-weight high-density polyethylene resin supplied for extrusion blow moulding of large rigid hollow articles. The published datasheet identifies a density of 0.951 g/cm³ determined according to ASTM D1505 and a melt flow rate of 0.19 g/10 min at 190°C/2.16 kg according to ASTM D1238. The grade is classified as a low-flow, high-molecular-weight HDPE in the blow moulding range. The high melt viscosity contributes to parison stability during long hang times; it also increases back-pressure and motor load on continuous extrusion blow moulding machines with grooved-barrel feed sections. Suppliers list the resin for rigid containers requiring environmental stress crack resistance, such as chemical jerry cans, agricultural chemical bottles, and intermediate bulk container liners. The resin is supplied as natural or pre-coloured pellets; the colour package must be assessed for lot-to-lot extraction performance under the applicable food-contact regulation. Published data for the detailed z-average molecular weight and comonomer distribution is limited.

    PropertyTest methodTypical value
    Melt flow rate at 190°C/2.16 kgASTM D12380.19 g/10 min
    Density at 23°CASTM D15050.951 g/cm³
    Tensile strength at yield, 50 mm/minASTM D63826 MPa
    Elongation at break, 50 mm/minASTM D638>600%
    Flexural modulus, 1.3 mm/minASTM D7901,100 MPa
    Environmental stress crack resistance F50, 100% Igepal, condition BASTM D1693>600 h
    Notched Izod impact, 23°CASTM D25630 kJ/m²
    Shore D hardnessASTM D224063
    Vicat softening temperature, 10 NASTM D1525124°C
    Brittleness temperatureASTM D746-75°C

    The above values are single-point laboratory measurements from compression-moulded or injection-moulded specimens, not statistical lot-certification ranges. Batch-to-batch variance on incoming resin lots is typically evaluated by melt flow rate and density prior to hopper loading; converter-specific lot acceptance limits are commonly set at ±0.002 g/cm³ for density and ±0.03 g/10 min for melt flow rate. The corresponding ISO designations are ISO 1183-1 for density, ISO 1133-1:2022 for melt flow rate, ISO 527-2 for tensile properties, ISO 179-1 for Charpy impact, and ISO 22088-3 for environmental stress crack resistance. Users comparing certificates should note that specimen thickness, thermal history, and conditioning differ between the ASTM and ISO methods.

    The density of 0.951 g/cm³ corresponds to a crystalline volume fraction of approximately 68%, calculated from a two-phase model using 0.855 g/cm³ for the amorphous phase and 1.000 g/cm³ for the crystalline polyethylene lattice. The high molecular weight and density positioned between medium-density and high-density polyethylene produce a balance of stiffness and resistance to slow crack growth. A blow moulding grade with a density of 0.960 g/cm³ and a melt flow rate near 0.30 g/10 min will often show higher top-load strength but lower environmental stress crack resistance and lower low-temperature impact than KFZ51C. The melt flow rate ratio between 2.16 kg and 5 kg loads is frequently used as an indirect measure of molecular weight distribution; the published datasheet for KFZ51C does not list a high-load melt flow rate, so the melt flow rate ratio cannot be calculated from the available data.

    What Melt Strength and Parison Sag Limits Are Relevant for Large-Volume Accumulator-Head Machines?

    With a melt flow rate of 0.19 g/10 min, KFZ51C exhibits high melt viscosity at typical extrusion blow moulding shear rates. Capillary rheometry at 190°C can be used to quantify apparent shear viscosity versus shear rate; the exact die swell ratio for a given production die is not listed in the published datasheet, and plant trials with the production tooling are required. The viscosity allows parison lengths above 1,000 mm to be hung without severe drawdown, provided the die gap is increased to compensate for higher die swell. Melt temperature should be maintained between 190°C and 210°C; operation above 230°C increases the risk of residence-time-dependent oxidation, odour generation, and yellowing in unpigmented parts. At the die head, typical head pressure is 15 MPa to 25 MPa depending on die gap, accumulator capacity, and shot size. Melt temperature stability should be held within ±5°C of the setpoint to avoid visible parison length variation on automated part removal systems.

    On single-station shuttle blow moulding machines with accumulator heads, KFZ51C is typically processed at a melt temperature of 190°C to 210°C and a mould temperature of 15°C to 30°C. Pre-drying is not normally required for closed-loop vacuum-conveyed resin at dry ambient conditions; however, if pellets are stored at relative humidity above 60% or exposed to condensation, a hopper dryer at 70°C for 2 h reduces surface moisture and prevents parison splay. The moisture absorption of HDPE is below 0.01% at 23°C and 50% relative humidity according to ASTM D570. The screw should use a single-flight, low-shear design with a barrier or mixing section, L/D ratio 24:1 to 30:1, and compression ratio 2.2:1 to 3.2:1. High-shear dispersive mixing elements are not required for this neat olefin polymer. Melt temperature is monitored at the die adapter; thermocouple immersion depth should be maintained at ≥50 mm to avoid false low readings. When moving from a higher-flow blow moulding grade, the die gap is typically increased by 10% to 20% to maintain parison wall thickness uniformity because of the higher die swell of KFZ51C.

    When KFZ51C Replaces a Conventional 0.3 g/10 min Blow Moulding HDPE in Chemical Containers

    In direct substitution of a general-purpose blow moulding HDPE with a melt flow rate near 0.3 g/10 min, KFZ51C shifts the processing economy toward higher melt pressure and lower throughput at the same screw speed. The advantage appears in slow crack growth resistance: F50 under ASTM D1693 condition B for many general-purpose HDPE grades is below 50 h, while KFZ51C is specified at >600 h. This is relevant for agricultural emulsifiable concentrates and surfactants that cause environmental stress cracking in lower-molecular-weight HDPE. The molar mass distribution of KFZ51C also gives higher notched Izod impact retention at -30°C; comparative data for a specific general-purpose grade should be confirmed from the datasheet of that grade. Converters replacing an existing HDPE must re-qualify drop-impact performance under ASTM D2463 or equivalent, because impact performance is geometry-dependent and cannot be predicted solely from resin datasheet values.

    Field use of KFZ51C is concentrated in large-part extrusion blow moulding where slow crack growth resistance and drop-impact retention after long outdoor exposure are critical. Typical production line examples include 20 L to 200 L open-top drums, 25 L monolayer jerry cans for agricultural emulsifiable concentrates, and 1,000 L intermediate bulk container liners. On accumulator-head machines with a 120 mm screw diameter, production output is normally limited by parison length and die swell rather than plastication capacity. Published data for specific output rates on a defined machine size is limited. When converting a mould from a higher-flow HDPE, the operator must validate wall thickness distribution and pinch-off weld strength on every cavity. Weld strength is tested by hydrostatic pressure or drop impact according to ASTM D2463. A mould temperature of 15°C to 20°C is preferred for faster solidification of thick-wall sections. The pinch-off zone should be kept clean and free of mould release; residual release agents can lower weld strength in chemical containers even when the resin itself has high environmental stress crack resistance.

    Chemical resistance in actual packaging is influenced by stress, temperature, and chemical concentration. HDPE resists concentrated hydrochloric acid, sodium hydroxide, and many agricultural formulations at ambient temperature, but aromatic solvents, ketones, and some surfactants can cause environmental stress cracking. The F50 time under ASTM D1693 with 100% Igepal is a laboratory screening test, not a substitute for storage testing with the actual chemical mixture. For aggressive formulations, converters should run a 60°C oven-aged containment test for 14 days with the filled bottle at 50% nominal volume and observe weight loss, deformation, and wall cracking. When KFZ51C is supplied as a pre-coloured compound, the pigment masterbatch carrier should be an HDPE with similar melt viscosity to avoid pigment streaks in the parison. Batch-to-batch variance in pigment dispersion can affect weld-line strength and drop impact; converters typically specify a filter pressure value under EN 13900-5 or equivalent to verify dispersion.

    For food-contact applications, the converter must verify that the polymer complies with FDA 21 CFR 177.1520 paragraph (c) 2.1 or 2.2 depending on the end-use temperature and extraction test results. In the European Union, compliance must be evaluated against Commission Regulation (EU) No 10/2011 and subsequent amendments, including overall migration testing under EN 1186. For industrial and chemical packaging, finished containers should be reviewed under UN 6.1 packaging requirements for dangerous goods where applicable. Under Regulation (EC) No 1907/2006 (REACH), the polymer itself is exempt from registration as a polymer under Article 2(9), but monomers and any additives are not exempt. The RoHS Directive 2011/65/EU does not restrict polyethylene, but converters must verify that cadmium, lead, and other restricted substances are absent in pre-coloured masterbatches.

    KFZ51C is not supplied with an antimicrobial additive. It must not be combined with amine-based antistatic agents or certain phenolic antioxidants that can alter the stabilization package and cause discolouration or environmental stress crack resistance reduction. The grade is not intended for injection moulding, rotational moulding, or blown film because the high molecular weight produces excessive injection viscosity or non-uniform film gauge. Published data for long-term outdoor weathering of KFZ51C without carbon black is limited; UV-stabilized pre-coloured compounds must be tested against ASTM D2565 or ISO 4892-2 for the specific wall thickness and end-use exposure period.