Tpc Japan Hdpe Kfy51a

TPC (Japan) HDPE KFY51A

    • Product Name: TPC (Japan) HDPE KFY51A
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 941127
    Density 0.954 g/cm³
    Meltflowrate 0.35 g/10 min (190°C/2.16 kg)
    Tensilestrengthatyield 27 MPa
    Elongationatbreak 700 %
    Flexuralmodulus 1200 MPa
    Izodnotchedimpactstrength 200 J/m
    Shoredhardness 65
    Vicatsofteningpoint 124 °C
    Meltingpoint 132 °C
    Thermalexpansioncoefficient 1.2E-4 cm/cm/°C
    Thermalconductivity 0.4 W/m·K
    Specificheatcapacity 2.3 J/g·°C
    Volumeresistivity 1E16 ohm·cm
    Dielectricconstant 2.3
    Waterabsorption 0.01 %
    Moldshrinkage 2.0-3.0 %

    As an accredited TPC (Japan) HDPE KFY51A factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing TPC (Japan) HDPE KFY51A is supplied in 25 kg polyethylene-lined bags, typically 40 bags on a 1,000 kg pallet.
    Container Loading (20′ FCL) 1×20′ FCL container loaded with TPC Japan HDPE KFY51A resin, 25 kg bags, palletized and shrink-wrapped, approx. 17–18 MT net.
    Shipping HDPE KFY51A (TPC Japan) ships as non-hazardous, non-DG high-density polyethylene resin pellets. Packed in 25 kg PE bags or 500–1000 kg jumbo bags, palletized and stretch-wrapped. Maintain cool, dry conditions; avoid moisture, sunlight, and contamination. No UN number or special transport labeling required.
    Storage Store TPC (Japan) HDPE KFY51A in a cool, dry, well-ventilated warehouse, away from direct sunlight, rain, and moisture. Keep original bags sealed and palletized; avoid contamination, static buildup, and ignition sources. Maintain moderate temperatures, separate from strong oxidizers, and follow recommended stack heights. Use first-in, first-out rotation, spill containment, and comply with the supplier’s SDS and local regulations.
    Shelf Life Typically 24 months when stored unopened in a cool, dry, ventilated area away from direct sunlight and heat.
    Application of TPC (Japan) HDPE KFY51A

    Within extrusion blow molding of agricultural and industrial chemical containers, TPC (Japan) HDPE KFY51A is processed on shuttle and accumulator machines equipped with grooved feed sections and screws at L/D ratios between 24:1 and 30:1; melt temperature measured at the die exit is normally held between 180 °C and 210 °C, while the die head is set to 190–215 °C depending on accumulator capacity. Lot acceptance on the certificate of analysis under ISO 1133-1:2022, condition 190 °C/2.16 kg, and density under ISO 1183-1:2019 should be verified before the accumulator drop time is set, because blow-moulded packaging certified under UN 3H1/ADR/RID must demonstrate stack-leak integrity after 1.2 m drop tests at −18 °C according to chapter 6.1 of the UN Model Regulations and IBC Code. Packed column melt filtration through 60/80/100 mesh screen packs removes charred gels before the parison programme, and the parison swell is typically 35–50 %, so accumulator die gap is set between 1.5 mm and 2.5 mm to maintain circumferential wall thickness after flash removal. Additive loading is limited to 2.0–2.5 wt% carbon black masterbatch for UV stabilization in outdoor warehouse stacking, 0.10–0.30 wt% antistatic masterbatch to control surface resistivity below 1011 Ω per IEC 61340-5-1, and up to 30 wt% clean in-house regrind when the container is not used for food contact; no more than 0.10 wt% zinc stearate is used because higher lubricant concentrations increase Environmental Stress Cracking Risk under ASTM D1693-15 Method B at 50 °C in 100 % Igepal CO-630. Blow pressure ranges from 0.6 MPa to 0.9 MPa, mould temperatures are held at 10–20 °C to shorten cycle times, and the mould vents are cleaned every 4–6 h to prevent diesel-effect staining on the pinch-off line. Terminal products include 5 L to 60 L UN-certified jerrycans, pesticide bottles, fertilizer containers, and industrial detergent drums where the Environmental Stress Cracking Resistance of KFY51A is verified under ASTM D1693-15 Method B at 50 °C in 100 % Igepal CO-630.

    What governs gauge uniformity on high-stalk blown-film lines using KFY51A?

    Film converters running 60–100 kg/h per die on high-stalk lines observe that gauge scatter of ±8 % to ±12 % is usually traceable to frost-line instability rather than melt-temperature variation; for KFY51A the frost-line height is set between 5 and 8 die diameters, and the blow-up ratio is constrained to 2.5:1–3.5:1 with a die gap of 0.9–1.4 mm to balance bubble stability and tear strength. Food-contact compliance for monolayer liners is assessed under FDA 21 CFR 177.1520(c) and EU Regulation 10/2011 Annex I Table 1, with specific migration limits for erucamide and silica not exceeding the overall migration limit of 10 mg/dm2 under EU Regulation 10/2011 Annex V test conditions. Slip and antiblock are added at 0.05–0.15 wt% erucamide and 0.10–0.25 wt% synthetic silica with a D50 of 3–5 µm, while 0.02–0.05 wt% fluoropolymer processing aid is included only when melt pressure exceeds 18 MPa and sharkskin is visible on the bubble shoulder. Downstream conversion uses a single-screw extruder at 30:1 L/D with a barrier screw and 0.8 mm screen pack, melt temperatures of 190–210 °C at the die lip, and a dual-nip collapsing frame; terminal output includes freezer liners, cereal pouch liners, bag-in-box liners, and grease-resistant bakery film where water-vapour transmission rate is evaluated under ASTM F1249-20 at 38 °C and 90 % RH, and dart impact is confirmed under ASTM D1709-22 Method A.

    Regulatory ScopeDesignation/ClauseKFY51A Film Control Requirement
    US olefin polymer complianceFDA 21 CFR 177.1520(c)Final liner produced without non-compliant additives; end-test extraction as per FDA guidance
    EU food-contact plasticsEU Regulation 10/2011 Annex I Table 1Overall migration limit 10 mg/dm2 under Annex V; erucamide subject to specific migration verification
    China food-contact additive positive listGB 9685-2016Slip and antiblock addition ratios within approved maximum usage levels; lot traceability retained
    US heavy metals in packagingCONEG model legislationSum of lead, cadmium, mercury, hexavalent chromium ≤ 100 ppm by weight

    Because gate design governs closure dimensional stability when KFY51A replaces random copolymer polypropylene in injection-moulded caps, hot-runner systems with two or four gating points per cavity are run with sequential valve-gate opening to reduce weld-line depth and ovality; before cavity balance is set, lot-specific MFR under ISO 1133-1:2022 condition 190 °C/2.16 kg is checked against the certificate of analysis, and a drift of 0.1 g/10 min has been observed to shift fill time by 0.2–0.4 s in a 48-cavity tool. The grade is plasticated at 200–230 °C in a 25:1 L/D screw with a compression ratio of 2.5:1, and held under injection pressure of 60–90 MPa before switching to a hold pressure of 30–50 MPa at 0.5–1.0 s. Formulation for carbonated beverage closures uses 0.05–0.15 wt% erucamide slip to bring the coefficient of friction under ASTM D1894 to 0.15–0.25 after 24 h ageing, 0.08–0.20 wt% primary antioxidant based on a hindered phenol/phosphate blend, and 1–2 wt% white or custom colour masterbatch; the same formulation avoids calcium stearate above 500 ppm because it can increase screw slip and reduce output predictability. Compliance is governed by FDA 21 CFR 177.1520(c), EU Regulation 10/2011, CONEG heavy-metal limits for packaging, and California Proposition 65 where applicable; terminal caps for 28 mm PCO 1881 and 38 mm neck finishes require dimensional verification under ASTM D2911-23 for flatness and ISO 1115-2 for removal torque. Production experience shows that clamp force below 2 kN/cm² of projected cavity area causes flash on the tamper-evident band, while cooling time below 8 s in a 48-cavity tool produces hinge whitening when the cap is opened at −4 °C.

    If KFY51A is directed to sheet extrusion for thermoformed trays, which chill-roll parameters close the shrinkage window?

    Sheet extrusion lines processing KFY51A into 0.3–1.2 mm monolayer sheet set the melt pump discharge temperature at 190–220 °C and use a 35:1 L/D single-screw with a Maddock mixing section to homogenize the regrind fraction; chill-roll temperatures are the dominant shrinkage control variable, with the first roll at 70–85 °C, the second at 60–75 °C, and the third at 40–55 °C, because lower roll temperatures freeze in orientation and increase longitudinal shrinkage above 3 % after reheating to 90 °C. Compliance for food trays relies on EU Regulation 10/2011 Annex I and Commission Regulation 2023/2006 on GMP, while the US route is FDA 21 CFR 177.1520(c) with end-test extraction as per FDA guidance using 10 % ethanol at 49 °C for 10 days. Formulation addition is typically 0.10–0.30 wt% nucleating agent masterbatch to raise crystallization temperature and reduce cycle time when measured under ISO 11357-3:2018 at 10 °C/min, 0.10–0.20 wt% antistatic masterbatch, and 20–40 wt% post-industrial sheet regrind that has been repelletized and dried to below 200 ppm moisture; slip levels above 0.15 wt% are excluded because they transfer to the chill roll and cause haze bands. The downstream process uses a coat-hanger die with a 0.8–1.0 mm lip gap, pressure roll loading of 4–6 N/mm, and edge trim rewound at 10–15 % of line speed; terminal product types are portion cups, dairy tubs, tamper-evident deli trays, and clamshells where KFY51A contributes high modulus but limits deep-draw ratios to less than 2.5:1 without plug assist.

    Monofilament and Raffia Extrusion Operating Windows for KFY51A

    In monofilament and raffia extrusion, KFY51A is run with a water-quench system at 25–35 °C and a 1.2–2.0 mm die opening to suppress premature radial orientation before drawing; the grade is extruded at 190–220 °C through a 24:1–30:1 L/D single-screw with 100/120/150 mesh filtration to remove gels that would otherwise cause denier breaks at draw ratios of 6.5:1–9.5:1. Compliance for agricultural twines and nets references ISO 2307:2019 for knot strength and linear density, ASTM D3218-07 for polyolefin monofilaments, and REACH Annex XVII restricted substances; UV stabilization is achieved by adding 1–3 wt% hindered amine light-stabilizer masterbatch with 0.10–0.25 wt% titanium dioxide rutile for opacity, while 0.02–0.05 wt% fluoropolymer processing aid is introduced only if melt pressure exceeds 15 MPa. The downstream process routes the drawn strand through a hot-air oven at 90–120 °C with a 4–5 m residence time, after which the strand is annealed at 2–4 % relaxation and wound under 0.2–0.5 N tension to maintain 200–400 denier consistency; terminal products include baler twines, agricultural shade nets, anti-hail nets, and geotextile yarns where tensile strength under ISO 2062:2009 is measured on conditioned specimens at 20 °C and 65 % relative humidity.

    Extrusion blow molding of pharmaceutical closures with KFY51A demands stricter melt-filtration discipline

    Blow-fill-seal and small-bottle applications for pharmaceutical closures require KFY51A to be processed with a 100/150/200 mesh screen pack and an extruder shutdown protocol that prevents black spec formation during barrel residence times exceeding 20 min; the melt temperature is limited to 180–205 °C to avoid thermal degradation products migrating into the drug product. Compliance under USP <661.1> and USP <661.2>, EU Regulation 10/2011, and FDA 21 CFR 177.1520(c) requires extractable screening with 50 % ethanol at 40 °C for 3 days and nonvolatile residue below 10 mg per packaging unit. Formulation addition is restricted to 0.05–0.10 wt% erucamide or oleamide and 0.02–0.08 wt% antioxidant masterbatch; pigments are limited to titanium dioxide at 1.0–2.0 wt% or carbon black at 0.5–1.0 wt% when light-blocking is required, and no process aids, release agents, or antistatic additives are added without drug-contact migration testing. The blow-moulding process uses a reciprocating screw with 20:1–24:1 L/D, accumulator head with conical mandrel, parison die gap of 1.0–2.0 mm, and mould temperature of 5–15 °C; terminal outputs are 50 mL to 1,000 mL high-density polyethylene pharmaceutical bottles, ophthalmic dropper bottles, and oral liquid containers, though published data for KFY51A-specific extractables in lipidic formulations is limited and must be generated on the actual drug-product line.

    Free Quote

    Competitive TPC (Japan) HDPE KFY51A prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    TPC (Japan) HDPE KFY51A is a high-density polyethylene resin designated as a specific grade within the producer’s HDPE portfolio. The identifier KFY51A encodes a base-polymer architecture, stabiliser package, and nominal melt viscosity, but public secondary sources provide limited independently verifiable numerical values. Published data for this specific configuration is limited. Downstream specifications therefore require verification against the lot-specific certificate of analysis and the producer’s technical datasheet. For objective grade introduction, the resin is characterised by the polymer class rather than by unverified single-point values. High-density polyethylene grades in this class are routinely tested according to ISO 1133-1:2022 for melt mass-flow rate, ISO 1183-1:2019 for density, ISO 527-2:2012 for tensile properties, ISO 178:2019 for flexural modulus, ISO 179-1/1eA for notched Charpy impact strength, ISO 306/A120 for Vicat softening temperature, and ASTM D1693 for environmental stress-cracking resistance. These methods define the technical boundary within which HDPE KFY51A should be compared with other HDPE grades.

    Which Comparative Tests Are Relevant to TPC (Japan) HDPE KFY51A?

    Because the product is a high-density polyethylene, the primary differentiators against other HDPE products are melt flow rate, density, molecular weight distribution, comonomer type, and additive formulation. Melt flow rate is measured at 190 °C under 2.16 kg; high-load melt index under 21.6 kg provides a flow-rate ratio that correlates with shear sensitivity. A broader molecular weight distribution increases shear thinning and improves extrusion processability while increasing die swell. A narrower distribution reduces die swell and improves injection dimensional stability. Without a lot-specific certificate of analysis, assigning KFY51A to one of these categories is not appropriate. The non-polar linear backbone of HDPE provides chemical resistance, while density is controlled by short-chain branching introduced through α-olefin comonomers such as 1-butene or 1-hexene. Density is normally reported after conditioning at 23 °C and 50% relative humidity under ISO 1183-1:2019.

    Grade differentiation is also dominated by environmental stress-cracking resistance measured under ASTM D1693. The test uses a notched specimen immersed in a surfactant at 50 °C. A fractional-melt blow-moulding HDPE may exhibit crack initiation times of several hundred hours, whereas a high-flow injection-moulding grade may fail within a few hours. Published data for this specific configuration is limited, so HDPE KFY51A should not be assigned an ESCR ranking without a producer-certified test report. Melt processability should be compared by capillary rheometry at shear rates from 100 s⁻¹ to 10,000 s⁻¹ and by dynamic oscillatory sweep from 0.01 rad/s to 500 rad/s at 190 °C. Zero-shear viscosity, crossover frequency, and elastic modulus from such tests indicate molecular weight distribution and long-chain branching effects.

    Additive Stabilisation and Oxidation Boundaries

    TPC (Japan) HDPE KFY51A is supplied with a proprietary stabiliser system. In high-density polyethylene, the stabiliser package typically includes a hindered phenol primary antioxidant and a phosphite secondary antioxidant. Oxidation induction time is measured by differential scanning calorimetry under ISO 11357-6 at 210 °C. Long-term thermal ageing is assessed by ISO 4577 or ASTM D3012. Processing above 280 °C can accelerate chain scission, increase carbonyl index, and reduce molecular weight. Pre-drying is generally unnecessary below 0.05% surface moisture, but resin stored at relative humidity above 60% may require drying at 80 °C for 2–3 h. Unverified addition of amine-based stabilisers or flame-retardant additives may interfere with the existing package and cause discolouration or premature oxidation.

    On injection moulding lines, HDPE KFY51A should be processed with a general-purpose polyolefin screw having an L/D ratio between 20:1 and 25:1 and a compression ratio between 2.5:1 and 3.5:1. Melt temperature should remain appropriate for the grade’s nominal melt flow rate; without a lot-specific MFR, a starting window of 180–220 °C may be considered for medium-flow HDPE grades, but this must be adjusted against producer data. Clamp force calculations require the projected area of the mould cavity. For thin-wall packaging, injection pressures of 80–140 MPa are commonly observed on production-grade polyolefin machines, though the exact pressure for KFY51A is mould-dependent. Gate freeze time and holding pressure profile are influenced by the crystallisation half-time, which for HDPE can fall within 1–10 s in the supercooling range. Excessively high holding pressure can cause flash, while insufficient holding pressure can produce sink marks and dimensional instability.

    When KFY51A Replaces a Fractional-Melt Blow-Moulding Resin in Container Applications

    In blow-moulded containers for household chemicals, a fractional-melt HDPE with melt flow rate below 1.0 g/10 min is often selected for high melt strength and ESCR. If KFY51A is positioned as a higher-flow grade, substitution would reduce parison sag resistance, alter wall-thickness distribution, and shorten cooling time. The difference is measurable through parison sag tests at 190 °C and through spiral-flow moulding. Top-load strength of a finished container is also affected by density; an increase from 0.950 g/cm³ to 0.960 g/cm³ raises stiffness but reduces ESCR. Therefore a like-for-like replacement without revalidation of drop impact at -20 °C and environmental stress-cracking under ASTM D1693 is not recommended.

    Film extrusion of HDPE requires sufficient melt strength to maintain bubble stability. In blown-film lines with die gaps between 1.2 mm and 2.0 mm and blow-up ratios between 3:1 and 5:1, extensional viscosity determines bubble stability. If KFY51A exhibits a lower molecular weight tail, it may process at lower head pressure but show reduced dart impact. In cast film, differences are less pronounced but remain measurable in tensile elongation and tear propagation. Injection-moulded HDPE parts such as caps, crates, and pallets require adequate toughness and stiffness. Notched Charpy impact at 23 °C and -20 °C under ISO 179-1/1eA is a critical comparison point. Without certified values, it is not possible to rank KFY51A against a specific high-flow injection grade.

    Which Compliance Standards Apply to HDPE KFY51A in Regulated End Uses?

    Regulated applications require demonstration of compliance with applicable regional frameworks. For the European Union, plastics intended for food contact are evaluated under Regulation (EU) No 10/2011 and its amendments; the overall migration limit is 10 mg/dm² of food contact surface area. For the United States, high-density polyethylene may be listed under 21 CFR § 177.1520 for olefin polymers, subject to end-use conditions. REACH registration is assessed under Regulation (EC) No 1907/2006. RoHS compliance for electrical and electronic equipment is assessed under Directive 2011/65/EU, although HDPE typically does not contain lead, cadmium, mercury, or hexavalent chromium. Because the additive package is proprietary, a producer letter of compliance is required for specific claims. No compliance statement should be based solely on the polymer class.

    Standardised test methods applicable to HDPE KFY51A characterisation
    PropertyStandard designationTypical test condition
    Melt mass-flow rateISO 1133-1:2022190 °C / 2.16 kg
    High-load melt flow rateISO 1133-1:2022190 °C / 21.6 kg
    DensityISO 1183-1:201923 °C, method D or gradient column
    Tensile yield stress and elongationISO 527-2:201250 mm/min, Type 1B specimen
    Flexural modulusISO 178:20192 mm/min, 23 °C
    Notched Charpy impact strengthISO 179-1/1eA23 °C and -20 °C
    Vicat softening temperatureISO 306/A120120 °C/h, 10 N
    Environmental stress-cracking resistanceASTM D169350 °C, notched specimen, surfactant bath
    Oxidation induction timeISO 11357-6210 °C, oxygen atmosphere
    Ash contentISO 3451-1800 °C, muffle furnace

    Differences between HDPE KFY51A and other HDPE products are resolved by comparing melt rheology, density, and molecular weight distribution. For example, a high-density polyethylene film grade with a density of 0.952 g/cm³ and an MFR of 0.3 g/10 min may show different stiffness and ESCR from an injection-moulding grade with an MFR of 20 g/10 min. These differences are design variables rather than defects. Without certified values for KFY51A, a direct numerical comparison cannot be made. The user should request the producer’s certificate of analysis and compare melt flow rate, flow-rate ratio, density, tensile yield stress, elongation at break, flexural modulus, notched Charpy impact at two temperatures, Vicat softening temperature, and ESCR at a specified failure criterion. Lot-to-lot variance in HDPE can be as low as ±5% for melt flow rate and ±0.002 g/cm³ for density in controlled reactor grades, but this is not a guarantee for HDPE KFY51A.

    Generic HDPE grade-class differentiation framework — applicable to KFY51A only after producer data are inserted
    Processing classCommon melt flow rate rangeCommon density rangePrimary comparison failure mode
    Blow moulding0.2–1.0 g/10 min0.950–0.958 g/cm³parison sag, environmental stress-cracking
    Film and sheet0.1–1.2 g/10 min0.941–0.958 g/cm³melt fracture, bubble instability
    Injection moulding4–60 g/10 min0.952–0.965 g/cm³warpage, low notched impact
    Rotational moulding2–8 g/10 min0.940–0.950 g/cm³incomplete fusion, pinholes
    Pipe extrusion0.2–0.8 g/10 min0.948–0.958 g/cm³slow crack growth, hydrostatic failure

    Compounding of HDPE KFY51A with functional additives requires attention to the base resin’s melt flow rate and thermal stability. If the grade is compounded with carbon black masterbatch for UV stabilisation, the masterbatch carrier should be compatible with high-density polyethylene to avoid weld-line weakness. A co-rotating twin-screw extruder with L/D of 32:1 to 40:1 and a side feeder for filler is typical. Barrel temperatures are often ramped from 160 °C at the feed throat to 210 °C at the die, unless the producer datasheet indicates otherwise. If talc is added at 20 wt%, melt viscosity increases and tensile modulus rises, but notched impact strength can drop sharply. This trade-off is quantified by ISO 527-2:2012 and ISO 179-1/1eA. The exact filler-loading tolerance of KFY51A depends on the base polymer molecular weight distribution and stabiliser content.

    Warpage in injection-moulded HDPE parts is driven by differential shrinkage and crystallinity. KFY51A, as a high-density polyethylene, crystallises at cooling rates determined by mould temperature. If mould temperature is increased from 20 °C to 60 °C, shrinkage and warpage may change. Shrinkage of HDPE is influenced by density and molecular orientation; mould-flow simulation should use measured pressure-volume-temperature data, not generic HDPE values. The producer may supply pvT data on request. For cap applications, strip torque performance is a function of modulus, wall thickness, and thread design. Environmental stress-cracking in the presence of detergents or oils is evaluated by ASTM D1693 or ISO 22088. Published data for this specific configuration is limited.

    Thermal Degradation and Oxidation Stabilisation in HDPE KFY51A

    Thermal degradation in HDPE occurs by random chain scission and by oxidation initiated at unsaturated sites. The stabiliser package in KFY51A is designed to reduce hydroperoxide formation and radical propagation. Oxidation induction time under ISO 11357-6 serves as a quality-control instrument but does not directly predict long-term service life. In multiple extrusion passes, melt flow rate can increase due to chain scission; a change of more than 20% from the virgin value indicates degradation. For injection moulding, residence time at melt temperature should not exceed 10 min. For extrusion, the residence time distribution in the barrel and die should be checked by purging with a colour marker. If the grade is used in hot-water pipe applications, hydrostatic strength must be tested according to ISO 9080 and ISO 1167, but only if the grade is specifically designed for pressure pipe.

    Top