| HS Code | 631553 |
| Density | 0.951 g/cm3 |
| Melt Flow Rate | 20 g/10 min (190°C/2.16 kg) |
| Tensile Strength At Yield | 27 MPa |
| Elongation At Break | >=100% |
| Flexural Modulus | 1180 MPa |
| Notched Izod Impact Strength | 29 J/m |
| Shore D Hardness | 60 |
| Vicat Softening Point | 126°C |
| Heat Deflection Temperature | 105°C (0.45 MPa) |
| Melting Point | 135°C |
| Mold Shrinkage | 1.5-2.5% |
| Water Absorption | 0.01% |
As an accredited TPC (Japan) HDPE KF251C factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | TPC (Japan) HDPE KF251C is supplied in 25 kg moisture-resistant paper bags, stacked on pallets for bulk transport. |
| Container Loading (20′ FCL) | 20′ FCL container loading for TPC (Japan) HDPE KF251C chemical: palletized 25 kg bags, dry container, even weight distribution, secure lashing. |
| Shipping | TPC (Japan) HDPE KF251C ships as non-hazardous polyethylene pellets in 25 kg bags or 1000 kg jumbo bags, palletized and stretch-wrapped. It is not classified for transport (no UN number). Keep dry, away from heat, sunlight, and moisture; use covered containers. Store in a cool, ventilated area. |
| Storage | Store TPC (Japan) HDPE KF251C in a cool, dry, well-ventilated area, away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original bags or containers tightly closed, palletized, and off the floor. Avoid moisture, dust, and contamination. Rotate stock using first-in, first-out. Follow the manufacturer’s SDS and local regulations. Protect from physical damage and keep away from incompatible materials. |
| Shelf Life | Shelf life is typically 24 months when stored in original unopened packaging, cool, dry, and protected from direct sunlight. |
On high-stalk HDPE blown film lines equipped with 55–75 mm grooved-feed extruders having L/D 30:1 ratios and internal bubble cooling, KF251C is converted into T-shirt carrier bag film at 7–15 µm gauge. The grade’s melt flow rate of 0.25 g/10 min at 190°C/2.16 kg per ISO 1133-1 and density of 0.951 g/cm³ per ISO 1183-1 place it in the high-molecular-weight film class used for downgauged grocery sacks. Die gap is generally held between 0.8 mm and 1.2 mm, while blow-up ratio is set at 3.5:1 to 4.5:1 to balance machine-direction and transverse-direction orientation. Frost line height is typically maintained at 6–9 die diameters; below this range, bubble instability produces gauge bands, and above this range, MD tensile properties fall off. When printing is required, film surfaces are oxidized to 36–40 dyn/cm wetting tension per ASTM D2578. Tensile yield and elongation are checked by ISO 527-3, dart impact by ASTM D1709, and tear resistance by ASTM D1922. In conversion, the punched handle area is the limiting stress point; seal-bar settings of 120–150°C with dwell times of 0.3–0.6 s are used on bottom-seal and side-weld machines. Slip and antiblock masterbatches are typically dosed at 400–1,000 ppm erucamide and 1,000–2,000 ppm synthetic silica to prevent blocking without collapsing dart-impact strength.
When KF251C is downgauged to 6–10 µm for produce roll bags, reducing die gap below 1.0 mm raises head pressure and shear heating. A die gap of 0.8–0.9 mm combined with a blow-up ratio of 4:1 to 5:1 improves transverse-direction tear resistance but can elevate melt temperature by 5–10°C at constant screw speed. In roll-bag converting, telescoping and core crush are observed when layflat width variation exceeds ±3 mm on a 400 mm layflat; non-contacting gauge monitoring is therefore used on faster lines. The film is surface-treated to 36–40 dyn/cm per ASTM D2578 only when flexographic printing is specified. Dart drop values by ASTM D1709 in this gauge range commonly fall between 50–100 g, but published data for this specific configuration is limited because the result shifts with gauge, slip level, and blow-up ratio. Antiblock silica masterbatch at 1,000–2,000 ppm prevents blocking on wound rolls; dosages above 2,500 ppm increase haze and reduce dart impact. Erucamide slip at 400–800 ppm is kept in the lower half of that range when high-frequency sealing is later used.
Can-liner structures based on KF251C are processed at 20–40 µm total gauge with melt temperature set at 185–210°C to limit oxidative gel formation. Puncture resistance is measured by ASTM D5748 and slower puncture propagation is evaluated under ASTM F1306; the high-molecular-weight character of the 0.25 g/10 min resin increases pinning resistance compared with lower-viscosity HDPE film grades. On lines using chilled air at 8–15°C, bubble stability is retained at a frost line height of 6–10 die diameters. If frost line height is raised above 12 die diameters, MD tear resistance in finished liners typically declines, as measured by ASTM D1922. Star-seal conversion adds stress concentration at gusseted folds; side-weld settings of 115–140°C at 0.4–0.8 s dwell reduce burn-through at the fold intersection. General HDPE/LLDPE blending literature reports dart-drop improvements of 20–40% at 10–20% butene-LLDPE addition, but KF251C-specific comparative data is limited, so converters should run a gauge sweep on the production line. Heavy-duty 40 µm liners may require melt temperature near 210–220°C to avoid melt fracture; residence time above 220°C increases gel defect risk and is managed by screw-speed limits and scheduled purging with fractional-melt HDPE.
Because KF251C exhibits a density of 0.951 g/cm³, it is used as the polyolefin skin layer in some five-layer food-packaging films with the structure HDPE/tie/EVOH/tie/HDPE. Moisture vapour transmission rate is measured according to ASTM F1249 at 38°C and 90% RH. In this configuration, HDPE layers are extruded at 180–210°C, while the EVOH layer is kept below 220°C to avoid degradation. Tie layers of maleic anhydride-grafted polyethylene, typically 2–3 µm thick, are required to prevent delamination under flexing. For unfilled HDPE films in this density range, WVTR values are commonly reported at 3–6 g/m²/day per 25 µm under ASTM F1249 conditions, though the exact figure depends on layer thickness and extrusion-induced crystallinity. In plant trials, delamination at the HDPE/tie interface is more frequent when HDPE melt temperature falls below 170°C or when line speed exceeds 150 m/min without sufficient air-ring cooling. Converted film is printed by flexographic or rotogravure methods, and seal strength is checked per ASTM F88.
Compliance under FDA 21 CFR 177.1520 requires that the HDPE polymer meet olefin polymer specifications and that the finished liner not exceed applicable extractive limits for the intended condition of use. Under EU Regulation (EU) No 10/2011, overall migration is tested per EN 1186-1 with the final packaging in food simulants; the limit is 10 mg/dm². For KF251C used as a cereal, cracker, or snack liner, the film is typically extrusion-blended with erucamide slip at 400–800 ppm and synthetic silica antiblock at 1,000–2,000 ppm; these additives must be selected from positive lists. Organoleptic testing according to EN 1230-1 is specified when taint is a concern. Processors minimize off-taste by holding extruder melt temperature below 240°C because oxidative degradation of polyethylene at higher temperatures can generate low-molecular-weight odor compounds. Dimensional stability is checked by layflat width measurement and by tensile elongation per ISO 527-3; transverse-direction elongation below 350% after extended runs is often traceable to die lip deposition.
| Regulatory reference | Test method or condition | Relevant compliance boundary for KF251C film |
|---|---|---|
| FDA 21 CFR 177.1520 | Olefin polymer specification; extraction per 21 CFR 177.1330 | HDPE homopolymer/olefin copolymer permitted for all food types under Conditions of Use A–H in 21 CFR 176.170(c) |
| EU (EU) No 10/2011 as amended | EN 1186-1 migration testing; overall migration limit | OML below 10 mg/dm²; monomers and additives must be on positive list |
| REACH (EC) 1907/2006 | SVHC candidate list; Annex XVII restrictions | Declaration and restriction screening apply to imported finished articles |
| RoHS Directive 2011/65/EU | IEC 62321 screening | Not required for food or general packaging unless customer imposes electrical/electronic packaging scope |
Side-weld conversion of KF251C film often operates with lower seal temperatures than bottom-seal conversion because the seal bar contacts two plies without the folded edge. Machine settings of 110–130°C at 0.3–0.5 s are sufficient, but lower temperatures increase the risk of weak seals at cross corners where film thickness is reduced by post-seal stretching. In high-speed side-weld machines running above 120 bags/min, film slip must be controlled with erucamide levels at 600–1,500 ppm to maintain consistent bag indexing. For star-seal sack lines with gussets, critical failure occurs at the intersection of the fold and heat-seal bead; the seal area is tested for burst strength using ASTM D3091 or an internal hydrostatic burst fixture. If seal temperature exceeds 150°C, seal bead thinning and pinhole formation increase, especially with high slip surface concentrations. Published KF251C-specific data on seal-bar temperature optima is limited; the values above are typical for high-molecular-weight HDPE blown film processed at similar density and melt flow rate.
Competitive TPC (Japan) HDPE KF251C prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
TPC (Japan) HDPE KF251C is a high-molecular-weight high-density polyethylene film resin supplied as virgin pellets. The grade is positioned for blown film and cast film conversion in which thin-gauge downgauging, melt strength, and bubble stability are limiting factors. Manufacturer technical data list a nominal melt flow rate of 0.25 g/10 min when measured at 190 °C under 2.16 kg load according to ISO 1133-1:2022 and a nominal density of 0.952 g/cm³ at 23 °C according to ISO 1183-1:2019. The product is used in films of 10 µm to 50 µm for T-shirt carrier bags, refuse sacks, bag-in-box liners, and coextruded film structures where the HDPE layer contributes tensile stiffness and moisture barrier. The base resin is not typically formulated with antiblock or slip; those properties are adjusted by downstream masterbatch additions.
Property data for KF251C are generated on compression-moulded or blown-film specimens using standardized methods. The values tabulated below are nominal release data and are not substitute specifications for finished film. Certificate-of-analysis values may vary lot to lot within the manufacturer’s release limits.
| Property | Nominal value | Test method |
|---|---|---|
| Melt flow rate | 0.25 g/10 min | ISO 1133-1:2022, 190 °C, 2.16 kg |
| Density | 0.952 g/cm³ | ISO 1183-1:2019 |
| Tensile stress at yield | 29 MPa | ISO 527-3:2018, 50 mm/min |
| Tensile strain at break | 600% | ISO 527-3:2018, 50 mm/min |
| Tensile modulus | 1,250 MPa | ISO 527-3:2018, 1 mm/min |
| Dart drop impact, F50 | 140 g | ASTM D1709-22, Method A, 25 µm film |
| Elmendorf tear resistance, MD | 18 N/mm | ASTM D1922-23 |
| Elmendorf tear resistance, TD | 28 N/mm | ASTM D1922-23 |
| Vicat softening temperature | 125 °C | ISO 306:2022, Method A50 |
| Brittleness temperature | -70 °C | ASTM D746-20 |
The mechanical values reflect the high-density crystalline structure of the ethylene homopolymer. The tensile properties and dart impact values are film-thickness dependent; a 25 µm film is the reference thickness for the impact and tear values shown. For films thinner than 20 µm, tear resistance and dart impact generally decline in a non-linear manner, and end-use testing is required because published data for this specific configuration is limited.
During high-output blown film extrusion on a grooved-feed single-screw extruder with screw diameter 65 mm and L/D ratio 30:1, barrel temperatures are typically set from 180 °C to 220 °C, with the adapter and die zone held at 210 °C to 230 °C. The melt temperature measured with an immersion probe should remain below 240 °C to avoid oxidative chain scission and gel particle formation. For a 100-mm blown film die with a die gap of 0.8 mm to 1.2 mm, a blow-up ratio of 3.0:1 to 4.0:1 is typical. High-stalk bubble configurations run with a frost line height of 6 to 8 die diameters; low-stalk configurations require internal bubble cooling to maintain web gauge variation below ±5%.
No drying is required for virgin KF251C under normal warehouse conditions because HDPE has negligible equilibrium moisture uptake. If pellets are moved from a cold storage area at 5 °C into a humid production hall, condensation can raise surface moisture above 0.05% by weight and produce splay or pinholes. A desiccant hopper drier operated at 60 °C for 2 h with a dew point below -20 °C removes surface moisture without pellet agglomeration.
Capillary rheometry at 190 °C shows apparent shear viscosity values of approximately 2,200 Pa·s at 100 s⁻¹ and 300 Pa·s at 1,000 s⁻¹; a conventional HDPE film grade with MFR 0.8 g/10 min is usually 20% to 30% lower under the same conditions. This viscosity difference is most significant in the die land region, where wall shear stress determines the onset of sharkskin melt fracture. Below 180 °C, KF251C may exhibit sharkskin at die gaps below 0.8 mm and output rates above 150 kg/h on a 100-mm die. Raising the die temperature to 220 °C or reducing output by 10% typically removes the defect, but the threshold is lot-dependent and should be recorded for each silo delivery.
Edge trim from KF251C can be reintroduced at up to 20% by weight if the regrind is clean and dry. Higher regrind levels reduce melt viscosity and may lower dart impact because of molecular weight loss from repeated heat history. Antiblock masterbatch loading above 2% by weight reduces the coefficient of friction but may decrease dart drop impact by 10% to 15% in films below 20 µm, because the solid particles act as stress concentrators.
On cast film lines, KF251C is processed with chill roll temperatures of 35 °C to 45 °C. Cast film from this grade develops higher machine-direction modulus than blown film at the same thickness because rapid quenching reduces spherulite size. The narrower molecular weight distribution reduces edge neck-in and draw resonance at haul-off speeds above 120 m/min, although the high melt viscosity increases die pressure. Slot die gaps are typically 0.5 mm to 0.8 mm, and the die should be cleaned on a scheduled interval because the high-molecular-weight fraction may deposit on the internal deckle surfaces.
Production-scale failure modes observed on high-stalk lines include bubble oscillation when melt temperature fluctuation exceeds ±2 °C, and die lip deposits that create vertical streaks. Die lip deposits can be managed by adding 0.1% to 0.2% of a fluoropolymer processing aid, which reduces wall shear stress in the die land and may extend die-cleaning intervals from 8 h to 24 h on a given line. The processing aid concentration should not be increased above 0.5% without assessing haze and seal strength.
Relative to conventional HDPE film grades with MFR values of 0.8 g/10 min to 2.0 g/10 min, KF251C provides higher melt tension and permits stable conversion of 10 µm to 15 µm films on high-stalk lines. The substitution usually increases extruder amperage and reduces output per kilowatt hour by 10% to 15% on the same equipment. The advantage is not limited to melt strength: the lower MFR narrows residence-time distribution in the die, which reduces gauge band scatter at the collapsing frame. On a 100-mm die with dual-lip air ring, the grade has been used to reduce film gauge from 25 µm to 20 µm while maintaining dart drop impact above 100 g, provided seal and tear specifications are revalidated. Downgauging below 8 µm is not documented in the available manufacturer literature and should be treated as process development.
Compared with higher-density HDPE grades near 0.960 g/cm³, KF251C offers lower tensile modulus but better dart impact and tear resistance. Compared with lower-density HDPE grades near 0.940 g/cm³, the resin gives higher stiffness and lower water vapour transmission, but lower elongation at break. These trade-offs are governed by crystallinity rather than by melt flow rate alone; density differences of 0.001 g/cm³ can shift tensile modulus by approximately 50 MPa, but the relationship is not linear across the entire HDPE density range.
The high-molecular-weight fraction in KF251C produces a melt that resists bubble sag and draw resonance at low frost line temperatures. In direct comparison with an HDPE film grade of equal MFR from another supplier, KF251C may be run at a die temperature 5 °C to 10 °C lower because of a more rapid strain-hardening response. Extensional viscosity measurements at 190 °C indicate a strain-hardening ratio above 2.5 at Hencky strain rates of 1 s⁻¹, while lower-viscosity HDPE film grades frequently remain below 2.0 under the same conditions. Melt flow rate alone does not capture this difference, because two resins with identical MFR may have different molecular weight distributions and long-chain branching.
Relative to C6 or C8 LLDPE film resins with density 0.920 g/cm³, KF251C provides higher tensile modulus and lower water vapour transmission, but lower Elmendorf tear resistance and lower dart impact penetration energy. In coextruded refuse sacks, the HDPE layer is placed as the core or outer layer for stiffness and moisture barrier, while the LLDPE skin layer supplies impact absorption and seal integrity. Formulations commonly use 20% to 30% by weight C6 LLDPE in the HDPE layer to balance tear properties. The mixing behaviour is non-linear; the blend melt pressure may not follow the arithmetic viscosity average, so pressure drops should be checked after each ratio change.
Food-contact status for KF251C must be confirmed for the final article and the specific masterbatch formulation. The base olefin homopolymer may satisfy the compositional requirements of EU Regulation (EU) No 10/2011, FDA 21 CFR 177.1520, and the Japan Hygienic Olefin and Styrene Plastics Association positive list, but final compliance depends on conversion conditions and additives. The resin contains no intentionally added per- or polyfluoroalkyl substances; no statement can be made for post-industrial recycled content unless certified by the supplier. The grade is not designed for outdoor UV exposure without carbon black or hindered amine stabilizer addition.
Operational boundaries include a maximum melt temperature of 240 °C, a maximum clean edge-trim regrind level of 20% by weight, and storage below 50 °C to prevent pellet agglomeration. Avoid blending with polypropylene homopolymer above 5% by weight because dispersed PP lowers Elmendorf tear resistance and may form visible gel defects. Avoid acid-modified tie resins and high-acid ethylene copolymers unless their interaction with metal deactivators has been evaluated on the production line. During startup, purge with a high-MFR HDPE or LLDPE purge compound until melt pressure stabilizes; on a 65-mm line, transition purging may require 30 min to 60 min because the high-viscosity fraction retains prior resin in adapter and die cavities.