Tpc Japan Hdpe Kf251a

TPC (Japan) HDPE KF251A

    • Product Name: TPC (Japan) HDPE KF251A
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 825344
    Density 0.954 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 0.05 g/10 min
    Tensile Strength At Yield 28 MPa
    Tensile Strength At Break 28 MPa
    Elongation At Break 500%
    Flexural Modulus 1200 MPa
    Notched Izod Impact Strength 200 J/m
    Vicat Softening Point 125 °C
    Brittleness Temperature -70 °C
    Shore D Hardness 60
    Environmental Stress Crack Resistance >1000 h
    Melting Point 133 °C

    As an accredited TPC (Japan) HDPE KF251A factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing TPC (Japan) HDPE KF251A is supplied in 25 kg polyethylene-lined paper bags, typically 40 bags per pallet.
    Container Loading (20′ FCL) TPC (Japan) HDPE KF251A is loaded into a 20′ FCL container in 25 kg bags, palletized and shrink-wrapped for export.
    Shipping TPC (Japan) HDPE KF251A is a high-density polyethylene resin. Shipped in 25 kg bags or 500–1000 kg jumbo bags on pallets, in dry containers. Non-hazardous, not regulated for transport. Store cool, dry, ventilated, away from sunlight, heat, moisture, and contamination. Standard freight handling; no special permits required.
    Storage Store TPC (Japan) HDPE KF251A in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, flames, and strong oxidizers. Keep sealed in original packaging, palletized off the floor and away from walls. Avoid moisture, dust, contamination, punctures, and UV exposure. Do not store near acids, alkalis, or solvents. Observe stacking limits and first-in/first-out rotation. Use clean, dry handling equipment.
    Shelf Life Stable under normal storage; no specific shelf life when kept cool, dry, sealed, and protected from direct sunlight and heat.
    Application of TPC (Japan) HDPE KF251A

    High-density polyethylene grade KF251A supplied by TPC Japan is evaluated first in extrusion blow molding of 20 L to 30 L UN-rated open-head drums and 25 L jerrycans. The lot certificate is checked under ISO 1133-1:2022 at 190 °C/2.16 kg and density under ISO 1183-1:2019; when the certified melt flow rate exceeds 0.30 g/10 min, parison sag on accumulator-head machines with shot capacity above 3.5 kg produces bottom pinch wall thinning and flash variation beyond ±0.15 mm. The compound for natural containers is 100 wt% KF251A with 0.05–0.10 wt% of a hindered phenolic antioxidant and 0.02–0.05 wt% of an acid scavenger, without mineral filler because filler reduces weld-line tensile strength in handle pinch zones. For outdoor chemical storage, 2.0–2.5 wt% of a 40% carbon black masterbatch is added to reach 0.8–1.0 wt% carbon black in the final article, and dispersion is assessed by ISO 18553:2002. Processing is performed on a shuttle blow molder with 100-point parison programmer, die gap 1.2–2.0 mm, blow air 0.6–0.8 MPa, mold temperature 10–25 °C, and clamp force 80–120 t for the 25 L container. Parison drop time is held below 4.0 s, and die exit temperature is measured by infrared pyrometer to maintain ±3 °C circumferential uniformity; wider variation shifts sidewall thickness and reduces top load. Drop testing at -18 °C from 1.2 m under ADR 6.1.5.3 is used for UN certification, and stacking creep is checked at 40 °C for 28 days under ISO 12048:2012. Environmental stress crack resistance of the drum wall is measured by ASTM D1693-15 condition B in 10% Igepal CO-630 at 50 °C; failure below 300 h triggers rejection for fatty chemical packaging. Published data for KF251A-specific processing windows is limited; the starting set points are typical for high-molecular-weight HDPE blow molding grades and must be confirmed against the lot certificate and mold-filling simulation. Pre-drying is not normally required, but surface moisture above 0.05 wt% after outdoor storage warrants 80 °C hopper drying for 2 h.

    Why Does Gate Freeze Time Limit Thin-Wall Container Warpage?

    Injection molding of thin-wall dairy spread containers and snap-on lids from KF251A is constrained by gate freeze time rather than overall cycle time. On a high-speed injection machine with screw L/D 22:1 to 24:1, compression ratio 2.0:1 to 2.5:1, and a check-ring non-return valve, the melt temperature is set at 210–240 °C and mold temperature at 15–30 °C. For nominal wall thickness of 0.8–1.2 mm, the gate diameter is 0.6–1.0 mm; gate freeze occurs at 0.5–0.8 s under typical high-speed filling, after which no packing pressure can compensate volumetric shrinkage. The formulation is 99.80–99.95 wt% KF251A with 0.05–0.15 wt% of a nucleating agent and 0.03–0.08 wt% of a slip agent, all components selected to meet overall migration below 10 mg/dm2 under EU 10/2011 and olefin polymer conditions under FDA 21 CFR 177.1520. Holding pressure is set at 60–80 MPa for 0.3–0.6 s, and screw cushion is held at 3–5 mm to avoid pressure loss through the check ring. Part mass variation is controlled within ±0.2%; larger variation shifts lid tear-tab opening force beyond 15–25 N, measured at 100 mm/min according to ISO 527-2:2012. Shrinkage in the container bottom is measured after 48 h at 23 °C and must remain below 1.2%; post-mold warpage is measured on a granite plate with feeler gauge and should not exceed 0.8 mm across 100 mm span. The finished products are thin-wall containers and lids for cold-fill dairy and deli applications, not suitable for hot-fill above 65 °C unless dimensional stability is separately validated.

    When Five-Layer Barrier Bottles Run HDPE Outer Layers with EVOH Core

    Coextrusion blow molding of 500 mL to 1 L agrochemical barrier bottles uses KF251A as the outer and inner structural layers in a five-layer configuration. The layer stack is HDPE outer/adhesive/EVOH/adhesive/regrind, with KF251A outer layers at 35–40 wt% of total wall, tie resin at 2–4 wt%, EVOH at 3–5 wt%, and the remainder as post-industrial regrind containing 50–60 wt% of the bottle. Each layer thickness is controlled by a five-extruder setup with gravimetric dosing; outer-layer melt temperature is 200–220 °C, EVOH is held at 190–210 °C, and the die head is 205–215 °C. Layer thickness fluctuation must remain within ±10% per layer because a thin EVOH layer below 3 µm causes oxygen transmission rate to exceed 0.5 cm3/m2·day·atm measured at 23 °C and 50% relative humidity under ISO 15105-2:2003. The outer HDPE layer is formulated with 0.05–0.10 wt% of an acid neutralizer and 0.02–0.05 wt% of a processing lubricant; pigment masterbatch is limited to 1.0–2.0 wt% because heavy pigment loading increases die-lip build-up on long runs. Blow air pressure is 0.5–0.7 MPa, and mold temperature is 10–20 °C. The terminal article is a solvent-resistant agrochemical bottle, with closure torque retention tested at 1.5 N·m after 24 h; container drop at 1.2 m after conditioning at -10 °C is specified. KF251A should not be blended with recycled polypropylene above 5 wt% in the outer layer, because phase incompatibility reduces bottle sidewall impact by more than 20% under instrumented drop testing. Published data for KF251A in this exact five-layer stack is limited; layer distribution must be validated on a pilot line before production.

    The following matrix consolidates the regulatory test methods and acceptance thresholds referenced across the downstream routes.

    ApplicationMandatory referenceTest methodAcceptance threshold
    Food contact containersEU 10/2011; FDA 21 CFR 177.1520Overall migration, 10 days at 40 °C, simulant B10 mg/dm2
    UN-rated drumsADR 6.1.5.3Drop test, -18 °CNo leakage after 1.2 m
    Outdoor pipeISO 9969:2016Ring stiffness, 3% deflectionSN4 or SN8 class
    Electrostatic protective sheetIEC 61340-5-1Surface resistance109–1011 Ω
    Food contact lidsFDA 21 CFR 177.1520Extractables per condition of useComplies with 21 CFR 177.1520(c)

    For subsurface drainage and stormwater detention, corrugated pipe with outside diameters from 110 mm to 200 mm is produced from KF251A on a single-screw extruder with grooved feed section, screw diameter 60–90 mm, L/D 30:1–33:1, and a corrugator with water-cooled mold blocks. The compound consists of 96.0–97.5 wt% KF251A, 2.5–4.0 wt% of a 40% carbon black masterbatch, and 0.05–0.10 wt% of a secondary antioxidant for long-term heat stability in buried service. Melt temperature at the die adapter is 200–230 °C; die head pressure is maintained at 15–25 MPa, and mold block vacuum is adjusted to hold inside radius tolerances within ±0.5 mm. Ring stiffness is tested under ISO 9969:2016 at 3% deflection, with SN4 or SN8 classification required by the drainage design. Impact resistance of the corrugated wall is checked by the staircase method under EN 744:1995. Carbon black content and dispersion are verified by ASTM D3350 cell classification and ISO 18553:2002; UV stabilization for exposed pipe sections requires 2.0–2.5 wt% carbon black. The finished pipe is used in land drainage, culverts, and stormwater retention fields. KF251A is not assigned for pressure potable water service unless the finished pipe is listed to NSF/ANSI/CAN 61 and passes hydrostatic sustained pressure testing under ISO 1167-1:2006.

    Sheet Extrusion for Thermoformed Pallet Separators and Dunnage Trays

    KF251A is converted into extruded sheet at thickness 1.5–4.0 mm using a single-screw extruder with L/D 28:1–32:1, a screen pack with 60/80/100 mesh, and a coathanger die of 1.2–1.8 m width. Melt temperature at the die entry is 210–230 °C; roll stack temperatures are set at 60 °C, 70 °C, and 80 °C from bottom to top for sheet thickness tolerance within ±0.05 mm. The compound for general pallet separators is 80 wt% KF251A and 20 wt% post-industrial regrind from the same sheet line, with 0.03–0.06 wt% antioxidant. For electronics dunnage trays, an antistatic masterbatch is added at 1.0–3.0 wt% to achieve surface resistance of 109–1011 Ω per IEC 61340-5-1; the antistatic additive is humidity-dependent, and performance is verified at 12% relative humidity. REACH SVHC content is controlled below 0.1% w/w per article. Thermoforming is performed on a contact-heat machine with sheet surface temperature 160–180 °C, mold temperature 60–80 °C, and forming pressure 0.4–0.6 MPa. The finished product includes pallet separator sheets, ESD-safe dunnage trays, and interlayer sheets for glass transport. Load-bearing at 40 °C is checked by compression creep under ISO 12048:2012 for stacked pallet height of 1.5 m; deflection greater than 10 mm over 24 h is rejected. RoHS 2011/65/EU Annex II limits apply to ESD trays: lead 1000 mg/kg, cadmium 100 mg/kg, mercury 1000 mg/kg, and hexavalent chromium 1000 mg/kg are the maximum homogeneous material thresholds.

    On monofilament extrusion lines equipped with a water quench tank and forced-air hot oven, KF251A is drawn into filaments of 0.25–0.45 mm final diameter for knitted shade cloth and anti-hail netting. The undrawn filament exits a single-screw extruder with L/D 24:1–28:1 through a spinneret plate with hole diameter 1.2–1.8 mm into a water bath at 25–35 °C. First-stage draw ratio is set between 1:6.5 and 1:8.5, followed by hot-air relaxation of 5–8% at 95–115 °C to reduce post-installation shrinkage below 2% measured at 80 °C for 30 min. UV stabilization uses 2.0–3.0 wt% of a HALS masterbatch and 1.0–2.0 wt% of a UV absorber masterbatch; accelerated weathering under ISO 4892-2:2013 method A cycle 1 requires tensile strength retention above 50% after 3000 h for agricultural shade netting. The knitted fabric is produced on warp knitting machines with gauge E6 or E9; mesh opening is set at 4–8 mm for insect exclusion and 8–12 mm for hail protection. Final tensile strength of a single filament is measured by ISO 2062:2009; a reduction greater than 15% between post-draw and after-weathering values triggers additive package review. The terminal article is UV-stabilized shade netting and anti-hail mesh for greenhouse and orchard use.

    Closure Creep Resistance Is Governed by Torque Retention and Post-Mold Shrinkage

    Injection molded pail lids and tamper-evident caps are produced from KF251A on hot-runner valve-gated molds with 16–32 cavities, melt temperature 230–250 °C, mold temperature 10–25 °C, and cycle time 12–18 s for wall thickness 1.5–2.5 mm. The gate diameter is 1.0–1.2 mm, and screw cushion is held at 3–5 mm to maintain packing pressure 50–70 MPa for 1.0–2.0 s. The formulation is 99.7–99.9 wt% KF251A with 0.1–0.3 wt% of an antioxidant package and no slip agent in the lid sealing area, because surface slip agents above 0.05 wt% can reduce lid-to-pail friction and lower tamper-evident pull-up torque. Closure creep is tested by applying a constant torque of 2.0 N·m at 40 °C for 7 days; rotation beyond 15° under load is rejected. Stress crack resistance of the tamper-evident hinge is checked by bending a molded strap over a 10 mm mandrel; no whitening or crack after 300 s at 23 °C is the release criterion. Food contact lids comply with FDA 21 CFR 177.1520 and EU 10/2011 overall migration below 10 mg/dm2. The finished products are 5-gallon pail lids, drum closure plugs, and caps for industrial and food containers. KF251A lot-to-lot melt flow variation above ±0.03 g/10 min requires adjustment of injection speed or gate diameter to maintain consistent sealing ring dimensions.

    Free Quote

    Competitive TPC (Japan) HDPE KF251A prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    TPC (Japan) HDPE KF251A is a high-molecular-weight high-density polyethylene resin intended primarily for extrusion blow moulding of large, thick-walled containers and industrial components. The grade is reported with a nominal density of 0.950 g/cm³ according to ISO 1183-1:2019 and a melt flow rate of 0.05 g/10 min at 190 °C under 2.16 kg load according to ISO 1133-1:2022. The low melt flow rate places KF251A in the high-viscosity segment of HDPE, where molecular weight is high enough to raise zero-shear viscosity and melt strength but not so high as to require compression moulding or ram extrusion. The resin is supplied in pellet form and is used where environmental stress cracking resistance, drop impact at low temperature, and parison stability are critical process requirements.

    As supplied, the pellet surface is hydrophobic, but condensation inside outdoor silos or contaminated conveying lines can introduce surface moisture. Surface moisture is removed by pre-drying at 80 °C for 2–4 h using a desiccant or hot-air drier when storage relative humidity exceeds 60%. The material should not be exposed to prolonged ultraviolet radiation before processing because photolytic degradation can shift the molecular weight distribution and reduce environmental stress cracking resistance. Published data for this specific configuration under long-term UV ageing is limited, and outdoor service requires a separately specified carbon-black or stabilizer package.

    What Distinguishes KF251A from Conventional Blow Moulding HDPE Grades?

    Unlike medium-flow blow moulding resins with melt flow rates in the 0.20–0.50 g/10 min range, KF251A operates in a high-viscosity region that produces a more stable parison and slower sag under gravity. The practical consequence is that large mouldings with wall thicknesses above 2 mm can be produced with more uniform wall distribution, but extruder torque and melt pressure are higher. Compared with high-flow injection grades having melt flow rates of 8–20 g/10 min, KF251A is unsuitable for thin-wall injection moulding because the melt has insufficient flow length and high pressure drop across narrow gates. In comparison with bimodal pipe grades, KF251A generally prioritizes blow-moulding melt strength over slow crack growth behaviour; direct published values comparing KF251A with bimodal pipe resins under ISO 9080 are limited.

    Parameter Test method KF251A expected range Medium-flow blow moulding HDPE High-flow injection HDPE
    Melt flow rate ISO 1133-1:2022 0.03–0.10 g/10 min 0.20–0.50 g/10 min 8–20 g/10 min
    Density ISO 1183-1:2019 0.948–0.953 g/cm³ 0.952–0.958 g/cm³ 0.952–0.960 g/cm³
    Tensile yield stress ISO 527-2:2012 25–30 MPa 26–31 MPa 27–32 MPa
    Elongation at break ISO 527-2:2012 >600% 500–700% 200–600%
    ESCR, 10% Igepal, 50 °C ASTM D1693-15 >600 h 30–150 h <20 h
    Notched Izod impact, 23 °C ISO 180:2023 8–12 kJ/m² 6–10 kJ/m² 4–8 kJ/m²

    Values in the table are class-typical ranges for grade selection, not guaranteed product specifications. KF251A-specific values should be confirmed against the manufacturer’s certificate of analysis and current technical datasheet because batch-to-batch variation, additive package, and test laboratory conditions influence reported results.

    The greater melt viscosity of KF251A changes extrusion behaviour at the die. Die swell is typically higher than that of medium-flow HDPE, and the extrudate retains more elastic memory after leaving the die land. This requires die geometry to be adjusted: a longer land length relative to the die gap is used to relax molecular orientation and reduce surface roughness. When tooling is changed from a medium-flow blow moulding grade, the same die gap may produce higher backpressure and lower output for KF251A. The processing window is therefore tighter, but the product provides improved parison strength, which is critical for containers with high length-to-diameter ratios or heavy shot weights.

    Melt Rheology, Extruder Configuration, and Processing Boundaries

    KF251A is processed on single-screw extruders with 25:1 to 30:1 L/D ratios and a grooved-barrel feed section. A barrier screw with a mixing section is preferred because the high-viscosity resin requires efficient melting and homogenization without excessive shear heating. Typical barrel temperature settings begin at 170–190 °C in the feed zone, rise to 190–210 °C in the compression zone, and stabilize at 200–220 °C in the metering zone. Die-head temperatures are maintained at 210–230 °C. The melt temperature should not exceed 240 °C because oxidative degradation can generate gels, reduce ESCR, and create surface defects in the final moulding.

    The die land length is normally set at 10–15 times the die gap. For large parisons used in industrial container production, die gaps in the range of 1.5–2.5 mm are common. If the die gap is reduced below 1.5 mm, die pressure can rise sharply and melt fracture may appear as sharkskin on the parison surface. Shear rates above approximately 1,000 s⁻¹ should be avoided unless the die is specifically designed for high-viscosity HDPE. When surface roughness is observed, remedies include raising die temperature within the allowed range, widening the die gap, increasing die land length, or reducing screw speed. The exact threshold varies with molecular weight distribution and melt temperature; published data for KF251A under commercial die geometries is limited.

    For extrusion blow moulding, blow pressure is typically set between 0.6 MPa and 0.9 MPa. Mould temperature is maintained at 10–20 °C to achieve sufficient cooling rate without excessive condensation on cold mould surfaces. Cooling time scales with wall thickness squared and is a major contributor to cycle time for heavy-wall containers. A 2 mm wall section may require cooling times of approximately 10–15 s, while wall sections above 5 mm can exceed 40 s depending on mould cooling efficiency and coolant temperature. These values are process-specific and should be optimized on the production machine.

    At the feed throat, pellet bridging and screw slip are controlled by keeping the grooved feed zone below 60 °C. Accumulator heads are preferred when shot sizes exceed approximately 10 L because KF251A’s high viscosity reduces flow redistribution in continuous shuttle systems. Parison programming is required for containers with variable wall profiles. The melt strength of KF251A reduces sag relative to lower-molecular-weight grades, but excessive melt temperature can still create drawdown in large parisons. Operators should monitor sag length after parison extrusion and adjust head temperature or extrusion speed before wall thickness variation becomes unacceptable.

    When Container Wall Thickness, ESCR, and Top-Load Failure Intersect

    KF251A is specified for blow moulded industrial pails, narrow-neck containers, intermediate bulk containers, and drums where resistance to aggressive liquids and rough handling is required. Applications in the 5 L to 200 L range are typical for this melt-flow class. Environmental stress cracking resistance under ASTM D1693-15 conditions using 10% Igepal at 50 °C is often reported above 600 h for high-molecular-weight HDPE grades; actual KF251A values must be confirmed from the supplier. Drop impact tests for completed containers are conducted according to ASTM D2463-15, and top-load resistance is measured at 23 °C with compressive platens meeting standard fixture requirements. Low-temperature impact is commonly evaluated at -20 °C to simulate cold-chain handling.

    Wall thickness redistributes stress in a non-linear manner. Thicker walls reduce hoop stress under internal pressure but increase cooling time and total part mass. KF251A is selected when a container must pass a specified drop height after filling with a stress-cracking fluid, such as a surfactant solution or aggressive agricultural chemical. The combination of high ESCR and high melt strength allows the moulded part to maintain thickness at corners and pinch-off zones. The pinch-off weld line remains a process-limiting region: insufficient tail flash compression and low material temperature can produce weak weld lines that fail drop tests even when the base resin has acceptable ESCR. Tooling should provide adequate pinch-off land width and compression ratio, and the parison tail should be trimmed cleanly to avoid crack initiation points.

    For dangerous goods packaging, qualification is normally performed under national or international modal regulations based on the UN Model Regulations, including Chapter 6.1 for drums and Chapter 6.5 for intermediate bulk containers. KF251A does not by itself guarantee compliance; the finished container design, wall distribution, cap closure, gasket, and production method all influence certification. Published data for KF251A in specific UN packaging configurations is limited, and end users must run prescribed drop, leakproofness, and stack tests on the actual container.

    Compliance under food-contact regulations is evaluated using FDA 21 CFR 177.1520 for olefin polymers in the United States and Commission Regulation (EU) No 10/2011 for plastic materials intended to contact food in the European Union. RoHS Directive 2011/65/EU as amended by (EU) 2015/863 and REACH Regulation (EC) No 1907/2006 are applicable for electrical and electronic equipment and for substances of very high concern. The grade is a hydrocarbon polymer not intentionally formulated with heavy-metal pigments or flame retardants, but specific migration and compliance documentation require manufacturer certification based on the exact additive package and processing history.

    KF251A is not recommended for high-speed thin-wall injection moulding, transparent applications, or continuous service above 60 °C in strongly oxidizing media. The resin should not be combined with certain amine-based stabilizers or oxidants that can accelerate thermo-oxidative degradation at elevated processing temperatures. Long residence time above 240 °C, repeated regrind cycles above 30% regrind content, and uncontrolled moisture on hydroscopic colour masterbatch carriers can reduce ESCR and impact performance. No formulation or processing adjustment should be accepted without pilot-scale verification on the intended production line, because laboratory specimens do not reproduce the thickness gradients, weld lines, and cooling rates of commercial blow mouldings.