| HS Code | 341619 |
| Density | 0.953 g/cm³ |
| Melt Flow Rate | 0.20 g/10 min (190°C/2.16 kg) |
| Tensile Strength At Yield | 29.0 MPa |
| Tensile Strength At Break | 38.0 MPa |
| Elongation At Break | 600% |
| Flexural Modulus | 1.20 GPa |
| Charpy Notched Impact Strength | 15.0 kJ/m² |
| Shore D Hardness | 66 |
| Vicat Softening Point | 126 °C |
| Melting Point | 134 °C |
| Thermal Conductivity | 0.440 W/m·K |
| Coefficient Of Linear Thermal Expansion | 1.20E-4 cm/cm/°C |
| Specific Heat Capacity | 1.90 J/g·°C |
| Dielectric Constant | 2.30 |
| Dissipation Factor | 0.000300 |
| Volume Resistivity | 1.00E+15 ohm·cm |
| Environmental Stress Crack Resistance | >1000 h |
As an accredited TPC (Japan) HDPE KF138D factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | TPC (Japan) HDPE KF138D is typically packed in 25 kg moisture-resistant bags, 40 bags per pallet, totaling 1,000 kg per pallet. |
| Container Loading (20′ FCL) | 20′ FCL container loading for TPC (Japan) HDPE KF138D: 25 kg bags, palletized, shrink-wrapped, max 18–20 MT, seaworthy export packing. |
| Shipping | TPC (Japan) HDPE KF138D is a non-hazardous high-density polyethylene resin in pellet form. It ships as general cargo in 25 kg bags or 1,000 kg jumbo bags. Keep dry, away from heat, sunlight, and moisture. No UN number required; not classified as dangerous goods. |
| Storage | Store TPC (Japan) HDPE KF138D in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and flames. Keep original packaging sealed to prevent moisture, dust, and contamination. Keep containers tightly closed when not in use. Avoid contact with strong oxidizers. Use first-in, first-out stock rotation. Ground and bond equipment to control static. Follow local regulations and material safety data sheet. |
| Shelf Life | Typically 24 months from manufacture when stored in original packaging under cool, dry, ventilated conditions, away from direct sunlight. |
TPC (Japan) HDPE KF138D is processed as a monolayer blown film for dry cereal liners and non-greasy snack packaging only after the conversion line is qualified under EU Regulation No 10/2011 Annex I and EN 1186-1:2002 for overall migration; specific migration of olefin oligomers is measured by EN 13130-1:2004, and North American shipments fall under FDA 21 CFR §177.1520 paragraph (c), which imposes n-hexane extractive limits according to food contact temperature and fat type. On a conventional blown-film line the resin is extruded through a single-screw extruder with L/D 28:1 and a spiral mandrel die with die gap 1.4 mm to 1.8 mm; melt temperature is maintained at 200 °C to 210 °C, die body 5 °C to 10 °C below the melt set point, blow-up ratio 2.2:1 to 3.0:1, and frost-line height 550 mm to 750 mm. This envelope produces film of 15 µm to 25 µm for terminal cereal liners, cracker sleeves, and non-greasy snack pouches. At that gauge, film is tested for dart impact by ASTM D1709 Method A, Elmendorf tear by ASTM D1922, tensile properties by ASTM D882, and moisture vapor transmission by ASTM F1249 at 38 °C and 90% RH; HDPE film of this class typically exhibits machine-direction tensile strength of 30 MPa to 45 MPa, elongation at break of 400% to 800%, and moisture vapor transmission in the range 3 g·m-2·d-1 to 8 g·m-2·d-1. Processors should not transfer these properties to finished packs without confirming lot-specific tensile and barrier data, because slight density variation within the HDPE family shifts water vapor transmission more than thickness variation of the same percentage.
Post-consumer recycled high-density polyethylene is let down into KF138D at 10 wt% to 25 wt% in non-food refuse sack and building-film applications using gravimetric dosing at the main feed throat; the recycled fraction is screened through an 80/120/80 mesh screen pack to remove gel particles above 250 µm. This is not a food-contact application, and the blend is controlled under packaging heavy-metal limits of 94/62/EC with total lead, cadmium, mercury, and hexavalent chromium below 100 mg/kg; under REACH, the recycled fraction must be sourced through a documented authorized recycler because contaminant composition directly shifts dart impact and melt-pressure stability. Though HDPE is not hygroscopic, surface moisture from storage at relative humidity above 60% can generate microbubbles at melt temperature; when feedstock has been stored in unsealed silos or bags, pre-drying at 70 °C for 2 h to 4 h is applied before extrusion. On the extrusion side, the let-down blend increases melt elasticity and narrows the bubble stability window; processors commonly raise die temperatures by 3 °C to 5 °C and reduce screw speed by 8% to 12% relative to neat KF138D to avoid melt fracture at the die lip. Dart impact retention measured by ASTM D1709 Method A typically degrades non-linearly with recycle addition; published data for this specific KF138D/PCR configuration is limited, and the relationship becomes steep when the recycled fraction contains more than 3 wt% polyethylene wax contamination from label adhesives. Terminal products are non-food heavy-gauge refuse sacks and building-site film; these are converted on bottom-seal or side-seal bag machines with seal settings adjusted upward by 5 °C to 10 °C because the PCR fraction broadens the seal melting endotherm.
Three-layer blown film lines for frozen seafood and liquid paste packaging use KF138D as the central stiffness and moisture-barrier layer at 55 wt% to 70 wt%, with ethylene-vinyl acetate copolymer skins at 15 wt% to 20 wt% per layer and, when required, an anhydride-modified polyethylene tie layer at 5 wt% to 10 wt%. The EVA skins are selected with vinyl acetate content of 6% to 12% to lower heat-seal initiation below 85 °C to 95 °C; this is confirmed by heat-seal strength testing under ASTM F88/F88M and hot-tack testing under ASTM F1921. The KF138D core layer is extruded through a three-layer spiral mandrel die with layer ratio control better than ±2%; melt temperature per layer is set at 205 °C to 215 °C for the HDPE core and 185 °C to 200 °C for the EVA skins to limit thermal degradation of vinyl acetate groups. Film gauge of 45 µm to 80 µm is produced at a die gap of 1.6 mm to 2.0 mm. From a compliance standpoint, EVA skins are not always accepted for direct fatty food contact; for high-fat applications, the skin layer is replaced with an LLDPE skin or a polyolefin plastomer meeting EU 10/2011 and FDA 21 CFR §177.1520, and migration of the EVA layer through the core is prevented by the continuous HDPE core layer. The terminal products are three-layer coextruded pouches and liner films where the outer skins provide low-temperature puncture resistance and seal through residual moisture, while the KF138D core provides creep resistance and moisture vapor transmission below 5 g·m-2·d-1 at 38 °C and 90% RH.
On high-stalk extrusion lines producing T-shirt carrier bags and produce bags from KF138D at 7 µm to 14 µm, the stalk height is maintained between 2.0 and 3.5 die diameters to separate molecular orientation from bubble expansion; this geometry shifts the orientation balance toward the machine direction and permits a blow-up ratio of 3.0:1 to 4.5:1 without losing bubble stability. Frost-line height is critically limited to ±50 mm; excursions above this band produce visible gauge bands at the collapsing frame and reduce tear resistance measured by ASTM D1922. Melt temperature is set at 195 °C to 210 °C, the die gap is narrowed to 0.8 mm to 1.2 mm, and internal bubble cooling is used to raise specific output without exceeding 8 °C of frost-line temperature drift. At this gauge, film is tested for gauge uniformity by ISO 4593 or ASTM D6988, with maximum acceptable variation of ±5% from the mean for registered converting on high-speed bag machines; the carrier film is printed by flexography only after corona treatment is confirmed at a wetting tension of at least 38 mN/m by ASTM D2578. Terminal products are printed and unprinted T-shirt grocery sacks, produce bags, and inner bin liners; holes at the bag mouth are punched after sealing, and the film must resist Elmendorf tear propagation in the machine direction at values which are strongly dependent on orientation ratio but generally decline when the blow-up ratio falls below 2.5:1.
Heavy-duty liner production using KF138D as the viscosity backbone at 80 µm to 150 µm is carried out on low-shear blown-film extruders with L/D 30:1 and screw cooling, because the high melt viscosity of the grade raises melt temperature through adiabatic shear heating; screw speed is limited to 80 rpm to 120 rpm depending on extruder diameter from 65 mm to 90 mm. The melt temperature is kept below 220 °C, and the die gap is increased to 1.8 mm to 2.2 mm to reduce die-lip shear stress and delay shark-skin melt fracture. In this application KF138D is typically blended with 15 wt% to 25 wt% metallocene LLDPE to raise dart impact at freezer temperatures; the blend is assessed for dart impact by ASTM D1709 Method B, slow puncture by ASTM D5748, and tensile impact by ISO 8256. Terminal products are free-standing FIBC liners, drum liners, and heavy-gauge industrial sacks; FIBC liners are fabricated to fit 1,000 kg flexible intermediate bulk containers, and the film must pass 60° tear propagation and crease-flex tests specified by the FIBC manufacturer rather than a single harmonized standard. Compliance for hazardous goods liners is limited to the packaging certification of the assembled FIBC under UN 13H2 or UN 13H4, not to the liner film alone.
On vertical form-fill-seal lines for frozen vegetables and ice-glazed foods, KF138D is used as a component layer in a coextruded film at total thickness of 35 µm to 55 µm, with the HDPE core at 40 wt% to 60 wt% and the sealant layer at 25 wt% to 35 wt%; the sealant is selected from LLDPE or plastomer because the high-density core alone requires sealing temperatures above 130 °C, which destabilizes the VFFS jaw cycle. Seal initiation temperature is measured by ASTM F88/F88M across a temperature gradient of 90 °C to 140 °C; the film is released for production when seal strength exceeds 10 N/15 mm at 110 °C and 0.3 s dwell. Hot-tack strength is tested under ASTM F1921 at a simulated filling temperature of 5 °C to account for frozen product contact immediately after sealing. The HDPE layer contributes dimensional stability and puncture resistance to the pack, measured by ASTM F1306 slow puncture; the low-temperature ductility of the total structure is evaluated by ASTM D1709 Method B after conditioning at -18 °C for 24 h. Compliance for frozen food packaging follows FDA 21 CFR §177.1520 for the HDPE core and the appropriate olefin polymer regulation for the sealant; when the pack is marketed in the European Union, overall migration is tested by EN 1186-1:2002 using food simulant A for frozen non-fatty foods. Terminal products are pillow packs and cushion packs for frozen vegetables, prepared meals, and ice-glazed seafood.
Agricultural silage cover and bale wrap produced with KF138D as a dense, stiff layer in a multi-layer structure differs from conventional LDPE silage covers because the HDPE layer is used at 10 wt% to 20 wt% of the total coextruded film to reduce oxygen transmission and increase puncture resistance against stalk puncture. The film is typically 150 µm to 200 µm in total thickness, and the HDPE layer is embedded between LLDPE skins at a die gap of 2.0 mm to 2.4 mm; UV stabilization is introduced through a hindered amine light stabilizer masterbatch at 3 wt% to 6 wt% in the outer skin only, because the HDPE core has no direct sunlight exposure after installation. Oxygen permeability is measured by ASTM D3985 at 23 °C and 0% RH, and the target is below 2,000 cm³·m-2·d-1·bar-1 for the total structure to limit aerobic spoilage at the silage surface. Terminal products are silage bags, horizontal silage covers, and bale wrap films; the operational boundary is that HDPE-based films have lower puncture elongation at subzero temperatures than metallocene LLDPE films, so the edges must be protected from direct mechanical stress by rope-reinforced hems or sandbag anchoring, and the film is not recommended for bale wrapping at ambient temperatures below -20 °C unless the LLDPE skins exceed 60 wt% of the structure.
Competitive TPC (Japan) HDPE KF138D prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
TPC (Japan) HDPE KF138D is a high-molecular-weight high-density polyethylene film extrusion grade. The designation KF138D places the product in the KF series typically directed at blown-film applications where thin-gauge stiffness, bubble stability, and melt strength are process-critical. A reliable numeric specification must be extracted from the producer lot certificate because density, melt flow rate, and additive package are controlled batch-to-batch and published data for this specific configuration is limited. The fixed test methodology is not ambiguous: melt flow rate is measured according to ISO 1133-1:2022 at 190 °C through a 2.16 kg load, and density is determined by ISO 1183-1:2019. Industrial databases covering Japanese and Thai high-molecular-weight HDPE film resins commonly place high-density film grades in the 0.945–0.955 g/cm³ density band and the 0.04–0.15 g/10 min melt flow rate band. KF138D is therefore evaluated as a low-MFR, high-density film resin rather than as an injection-moulding or blow-moulding HDPE.
On a 90 mm grooved-feed single-screw extruder with L/D 33, this resin class is typically processed with controlled feed pressure to limit surging. Adapter melt temperature is held between 190 °C and 230 °C, the die gap is set from 1.4 mm to 2.2 mm, blow-up ratio is held at 2:1 to 4:1, and frost line height is adjusted from 400 mm to 900 mm depending on die diameter and output. If the die gap is narrowed below 1.2 mm to improve gauge uniformity, melt fracture risk increases, particularly above 120 kg/h on a 250 mm die. The processing window narrows at higher line speed because HDPE melts with low shear viscosity relaxation times generate bubble instability when frost line oscillation exceeds ±50 mm.
The principal difference is melt flow behaviour. Injection-moulding HDPE grades are designed for low pressure drop during cavity filling and therefore carry melt flow rates in the 5–20 g/10 min range. Blow-moulding grades used for bottles and containers are intermediate, commonly 0.2–0.7 g/10 min to provide parison melt strength without excessive back pressure. KF138D-type film grades occupy the lower MFR film extrusion class, generally 0.04–0.15 g/10 min, which favours bubble consolidation and thin gauge reduction but demands larger extruder barrels and higher drive torque. In density terms, HDPE film grades are often slightly below bottle grades to preserve environmental stress crack resistance; bottle and injection grades may reach 0.955–0.968 g/cm³, while film grades tend to remain at 0.945–0.955 g/cm³. That difference controls stiffness, water vapour transmission rate, and seal response.
| Property or processing variable | KF138D film-grade family expectation | General-purpose HDPE injection-grade reference | Relevant standard |
|---|---|---|---|
| Melt flow rate at 190 °C, 2.16 kg | 0.04–0.15 g/10 min | 5–20 g/10 min | ISO 1133-1:2022 |
| Density | 0.945–0.955 g/cm³ | 0.955–0.968 g/cm³ | ISO 1183-1:2019 |
| Tensile characterisation | Film tensile properties measured on 25 µm blown film | Rigid specimen tensile testing after injection moulding | ISO 527-3:2018 / ISO 527-2:2012 |
| Impact assessment | Dart drop on film | Notched Izod on rigid specimen | ISO 7765-1:1988 / ISO 180:2023 |
Comparative differentiation between KF138D and low-density polyethylene films is based on tensile modulus, moisture vapour transmission rate, and seal initiation temperature. LDPE grades with density in the 0.918–0.930 g/cm³ range show lower machine-direction modulus at equal film thickness and typically seal at lower temperature. HDPE film at 25 µm produces a lower moisture vapour transmission rate than LDPE of equal thickness when measured according to ISO 15106-2:2016 or ASTM F1249-20 at 38 °C and 90 % RH. LLDPE improves dart impact and puncture resistance but generally reduces tensile modulus; converters routinely blend LLDPE at 10–30 % by mass into HDPE to adjust tear and impact behaviour in bag structures.
High-molecular-weight HDPE film extrusion relies on grooved feeding to maintain solids conveying against high head pressure. On a 65 mm grooved-feed extruder with a 120 mm die and 1.8 mm die gap, field experience with this melt class indicates stable operation when screen-pack differential pressure remains below 80 bar. A rise above 80–100 bar produces gate velocity variation, visible thickness bands, and higher motor load. Screen changes are therefore scheduled at 80–100 bar differential rather than at fixed time intervals. Melt temperature measured at the adapter should not exceed 230 °C because prolonged residence time at high temperature increases polymer degradation, shifts surface oxidation, and reduces film dart impact. Pre-drying is required when ambient relative humidity exceeds 60 %, as residual moisture at film extrusion temperatures can generate surface defects and reduce output stability.
Rheological measurement of high-density film grades in the 0.04–0.15 g/10 min class is commonly performed on a capillary rheometer at 190 °C with a Göttfert Rheotens pull-off unit. Melt strength values for this family are higher than those of LLDPE at equal extrusion temperature by approximately 2–3 cN. Because published data for KF138D is limited, Rheotens values must be treated as family reference values and confirmed on the production lot rather than used as a purchase specification. The critical comparative point is that melt strength, not MFR alone, determines whether a thin-gauge bubble remains stable at high blow-up ratio.
For direct food-contact packaging, polyolefin base resins fall under FDA 21 CFR 177.1520, REACH regulation EC 1907/2006, and RoHS directive 2011/65/EU. The base resin is not sufficient for converter compliance because slip, antiblock, and processing-aid masterbatches used in the same extruder must also meet migration limits under EU 10/2011. KF138D should be handled with dry-air drying when storage humidity has exceeded 60 % RH. Avoid combining the melt with halogenated flame-retardant systems that liberate acid species at barrel temperatures above 200 °C; acid generation accelerates screw root corrosion and die wear. For food-contact film, the converter must also verify that recovered trim used in the same line does not introduce unlisted contaminants.
| Requirement | Applicable standard or regulation | Verification scope |
|---|---|---|
| Melt flow rate | ISO 1133-1:2022 | Lot release by producer |
| Density | ISO 1183-1:2019 | Lot release or conversion check |
| Migration in food contact | EU 10/2011 | Finished film, including masterbatch and reclaim |
| US food-contact clearance | FDA 21 CFR 177.1520 | Olefin polymer base resin and additives |
| Chemical safety | EC 1907/2006 | Substance registration and SVHC screening |
| Electrical and electronic equipment restriction | 2011/65/EU | Heavy metal screens for non-packaging industrial uses |
Among high-stiffness blown-film applications, KF138D is typically evaluated for T-shirt carrier bags, flat-back bags, deli wrap, and liners where gauge reduction from 35 µm to 18 µm requires sufficient bubble stability. The grade is not optimised for stretch film, which requires very low density and highcling additives, nor for heavy-duty industrial sack film where bimodal HDPE with higher stress crack resistance may be preferred. On a 65 mm grooved-feed line with a 120 mm die, film-grade HDPE in this class can maintain stable gauge when screw speed and external cooling air are adjusted to hold frost line height constant within ±30 mm. Gauge variation outside ±5 % is normally traceable to screen-pack pressure rise, die gap asymmetry, or uneven air-ring cooling rather than to base resin viscosity alone.
High back-pressure in a grooved-feed extruder shifts the melt residence time distribution and increases melt temperature heterogeneity. If screen-pack pressure drop rises from 80 bar to 120 bar, the melt at the screen pack can shear-heat enough to shift the local melt temperature by 5–10 °C, causing viscosity loss and bubble flapping. Production-scale failure modes observed on high-molecular-weight HDPE film extruders include screen-pack blind-off from oxidised gel particles, pressure transducer diaphragm fouling, and die lip polymer degradation. These failures are not eliminated by changing the resin grade alone; they require screen-pack mesh sequencing, pressure monitoring, and die lip cleaning. For KF138D, the recommended operational boundary is therefore a clean screen pack below 80 bar differential and direct melt temperature measurement not exceeding 230 °C at the adapter.
Mechanical evaluation of blown film uses machine-direction and transverse-direction tensile testing according to ISO 527-3:2018, Elmendorf tear according to ISO 6383-2:1983, dart impact according to ISO 7765-1:1988, and thickness profile measurement by capacitance gauge or beta gauge. Environmental stress crack resistance is measured on rigid specimens according to ASTM D1693-21 in 10 % Igepal CO-630 at 50 °C. In the high-density film family, ESCR failure time generally exceeds 100 h when density is kept below 0.955 g/cm³, but ESCR falls steeply as density approaches 0.960 g/cm³. Because KF138D lot density and comonomer content control that balance, no reliable inference can be made from the grade designation alone; published data for this specific configuration is limited. A converter must use the producer lot certificate for density, MFR, comonomer type, and additive package before setting final film specifications.
Compared with bimodal high-density film resins, a conventional unimodal high-molecular-weight HDPE such as the KF138D class may show lower dart impact at equal density but simpler bubble stability and easier gauge control on older blown-film lines. Compared with a single-site catalysed HDPE, the KF138D family typically exhibits broader molecular weight distribution and higher shear sensitivity, which can be an advantage in grooved-feed extrusion but a disadvantage for very high drawdown. The selection between KF138D and other products therefore depends on conversion equipment, downstream sealing technology, and the required balance between stiffness and puncture resistance in the finished bag or wrapper.